JPS57149090A - Production for t-shaped welded joint having minute fillet - Google Patents
Production for t-shaped welded joint having minute filletInfo
- Publication number
- JPS57149090A JPS57149090A JP3486081A JP3486081A JPS57149090A JP S57149090 A JPS57149090 A JP S57149090A JP 3486081 A JP3486081 A JP 3486081A JP 3486081 A JP3486081 A JP 3486081A JP S57149090 A JPS57149090 A JP S57149090A
- Authority
- JP
- Japan
- Prior art keywords
- minute
- plate
- thickness
- welded joint
- fillet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To make a welding with minute fillets possible to reduce the thermal distortion, by welding a lateral plate and a longitudinal plate after forming a groove, which has a form required to result a melted state to give to the lateral plate an almost equal thickness to the longitudinal plate. CONSTITUTION:A groove 3 having a bottom part 1b having a thickness W approximately equal to a thickness t1 of a longitudinal plate 2 and a thickness t2 is formed on a lateral plate 1 on the extension of the longitudinal plate 2 brought into contact with the lateral plate. Welding is started from the groove 3 to weld the lateral plate 1 and the longitudinal plate 2 under the state where minute fillets 4 are provided. Thus, a T-shaped welded joint having minute fillets is obtained.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3486081A JPS57149090A (en) | 1981-03-10 | 1981-03-10 | Production for t-shaped welded joint having minute fillet |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3486081A JPS57149090A (en) | 1981-03-10 | 1981-03-10 | Production for t-shaped welded joint having minute fillet |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS57149090A true JPS57149090A (en) | 1982-09-14 |
Family
ID=12425916
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3486081A Pending JPS57149090A (en) | 1981-03-10 | 1981-03-10 | Production for t-shaped welded joint having minute fillet |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57149090A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2009255172A (en) * | 2008-03-26 | 2009-11-05 | Ebara Corp | Method for manufacturing t-type joint |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5497547A (en) * | 1978-01-12 | 1979-08-01 | Nuovo Pignone Spa | Arc welding of blade to disk of rotating machine |
-
1981
- 1981-03-10 JP JP3486081A patent/JPS57149090A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5497547A (en) * | 1978-01-12 | 1979-08-01 | Nuovo Pignone Spa | Arc welding of blade to disk of rotating machine |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2009255172A (en) * | 2008-03-26 | 2009-11-05 | Ebara Corp | Method for manufacturing t-type joint |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS535045A (en) | Process for conding together metallic portions by arc fusion welding | |
ES508860A0 (en) | AN IMPROVED PROCEDURE FOR THE PRODUCTION OF METAL IN MELTING IN A CUBILOTE OVEN. | |
JPS57149090A (en) | Production for t-shaped welded joint having minute fillet | |
SE8701056D0 (en) | PROCEDURE AND INSTALLATION FOR WELDING OF TIN PLATE MATERIAL | |
GB1472002A (en) | Welding method | |
GB8318589D0 (en) | Welded constructions and components | |
JPS6462286A (en) | Resistance welding method for steel sheet | |
JPS57199590A (en) | Arc welding joint | |
GB2066715B (en) | Workpiece assembly for welded butt joint | |
JPS53138945A (en) | Bonding method for aluminum and iron | |
JPS53149848A (en) | Friction pressure welding method for copper and aluminum | |
GB2106818B (en) | Machine for pressure contact butt welding of pipes | |
Minks | Contact/Base Welded Joint and Method of Producing Same | |
JPS5768289A (en) | Arc welding method | |
JPS53119241A (en) | Welding method for slightly weldable materials and dehydrogenation apparatus welding | |
JPS5618296A (en) | Conjoining method of end plug to clad pipe | |
GB1517555A (en) | Fusion butt-welding process for joining steel plates | |
JPS5545539A (en) | Welding method of edge joint | |
SU642120A1 (en) | Apparatus for shaping the back side of a weld at welding annular butt joints | |
JPS5471055A (en) | Method of joining round steel bars | |
FR2285200A1 (en) | Joining metal parts, esp. plates - where joint contains holes and molten metal is cast into the holes | |
JPS5557490A (en) | Method for manufacturing an endless ink ribbon | |
JPS57171589A (en) | Spot welding method for corner of box | |
JPS53108025A (en) | Heat treating method for weld zone of heat resisting alloy | |
JPS52129645A (en) | Welding groove for tee type fillet weld joints |