JPS5632350A - Glass product tempering method - Google Patents
Glass product tempering methodInfo
- Publication number
- JPS5632350A JPS5632350A JP10411079A JP10411079A JPS5632350A JP S5632350 A JPS5632350 A JP S5632350A JP 10411079 A JP10411079 A JP 10411079A JP 10411079 A JP10411079 A JP 10411079A JP S5632350 A JPS5632350 A JP S5632350A
- Authority
- JP
- Japan
- Prior art keywords
- salt
- soln
- glass
- contg
- potassium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To temper an Na salt-contg. glass product by bringing it into contact with a soln. of a boron-contg. K salt or a mixed soln. of the salt and other K salt and holding the product at a temp. near the strain point of the glass for a fixed time to carry out ion exchange of Na+ and K+.
CONSTITUTION: An Na salt-contg. glass product is dipped in a soln. of a boron- contg. K salt or a mixed soln. of the salt and other K salt or coated with the soln. and held at a temp. near the strain point of the glass for a fixed time to temper the glass product by ion exchange. By using the boron-contg. K salt, borate glass is formed once on the glass surface, and at the same time, the ion exchange is carried out. Thus, the K salt does not run away and scts effectively with hihg wettability to the glass. A soln. of potassium metaborate and/or potassium borate or a mixed soln. of the potassium salt and potassium nitrate is used, and the soln. may be neutralized.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10411079A JPS5632350A (en) | 1979-08-17 | 1979-08-17 | Glass product tempering method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10411079A JPS5632350A (en) | 1979-08-17 | 1979-08-17 | Glass product tempering method |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5632350A true JPS5632350A (en) | 1981-04-01 |
JPS5730822B2 JPS5730822B2 (en) | 1982-07-01 |
Family
ID=14371979
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10411079A Granted JPS5632350A (en) | 1979-08-17 | 1979-08-17 | Glass product tempering method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5632350A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2019064276A1 (en) * | 2017-09-29 | 2019-04-04 | Agp America S.A. | Method of strengthening glass substrates |
WO2019130205A1 (en) * | 2017-12-27 | 2019-07-04 | Agp America S.A. | Method for strengthening and bending glass sheets |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4134746A (en) * | 1977-08-18 | 1979-01-16 | Domglas Inc. | Method of strengthening glass articles |
-
1979
- 1979-08-17 JP JP10411079A patent/JPS5632350A/en active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4134746A (en) * | 1977-08-18 | 1979-01-16 | Domglas Inc. | Method of strengthening glass articles |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2019064276A1 (en) * | 2017-09-29 | 2019-04-04 | Agp America S.A. | Method of strengthening glass substrates |
WO2019130205A1 (en) * | 2017-12-27 | 2019-07-04 | Agp America S.A. | Method for strengthening and bending glass sheets |
Also Published As
Publication number | Publication date |
---|---|
JPS5730822B2 (en) | 1982-07-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3275273D1 (en) | Polyolefin coating containing an ionomer for metal substrates | |
JPS5595645A (en) | Tempering treatment method for inorganic glass | |
EP0204565A3 (en) | Process for coating the internal surface of a metal tube with a neutron absorber | |
BE882503A (en) | PROCESS FOR APPLYING AN ANTI-CORROSIVE COATING ON METAL OBJECTS, IN PARTICULAR ON LIQUEFIED GAS BOTTLES | |
YU284779A (en) | Process for inhibiting the formation deposits on metal surfaces in an aqueous medium | |
JPS57129845A (en) | Glass bottle provided with both mechanical strength and chemical durability and its manufacture | |
JPS5632350A (en) | Glass product tempering method | |
IT7925327A0 (en) | PROCESS FOR DOPPING SILICON BODIES WITH BORON. | |
ES455693A1 (en) | Electrolytic ion migration into glass | |
JPS5437012A (en) | Apparatus for eliminating comtaminants | |
DE2963744D1 (en) | Perfluoroalkylalkylenemercapto group containing non-ionic surfactants, process for their manufacture and their use | |
JPS5650145A (en) | Glass tempering method | |
BR7906342A (en) | PROCESS AND APPLIANCE FOR ORIENTATION AND SIZING OF BATTERY GRILLS AND ARTICLES FORMED THROUGH THIS MEDIUM | |
JPS53106654A (en) | Assembly method for sileeved roll | |
JPS52148519A (en) | Chemical tempering process for glass vessel | |
JPS55141571A (en) | Surface treatment of perforating steel tool for steel pipe | |
JPS5299483A (en) | Method of fixing workpiece to be machined | |
JPS5575944A (en) | Glass surface treating method | |
JPS5390906A (en) | Manufacture of magnetic disk | |
JPS5394378A (en) | Surface treatment of polyacetal molded article | |
JPS57209735A (en) | Hot plastic working method for metallic material | |
JPS5694153A (en) | Process for making solar energy selective absorption film | |
JPS5684479A (en) | Protection of copper surface | |
JPS5411828A (en) | Anti-corrosion magnetic material member | |
STEFFEN | Laser processing in practice(metal working) |