JPS56167772A - Preparation of magnetic paint - Google Patents
Preparation of magnetic paintInfo
- Publication number
- JPS56167772A JPS56167772A JP7231280A JP7231280A JPS56167772A JP S56167772 A JPS56167772 A JP S56167772A JP 7231280 A JP7231280 A JP 7231280A JP 7231280 A JP7231280 A JP 7231280A JP S56167772 A JPS56167772 A JP S56167772A
- Authority
- JP
- Japan
- Prior art keywords
- magnetic powder
- preparation
- abrasive material
- magnetic
- magnetic paint
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To avoid damage of a needlelike shape of a magnetic powder by performing admixing and dispersion of each component in two specified steps, in the preparation of a magnetic paint contg. a polyurethane resin and a vinyl chloride- vinyl acetate copolymer as binders.
CONSTITUTION: In the preparation of a magnetic paint consisting of a magnetic powder, binder, lubricant, abrasive material and additive by use of said two polymers as the binder, an iron metal power (a magnetic powder) and a polyurethane resin are primarily dispersed and then secondarily dispersed with addition of the abrasive material and a vinyl chloride-vinyl acetate copolymer. Alumina, silicon carbide, etc. of a particle size about 0.05W3μ in an amt. of about 0.01W10pts.wt. per 100pts.wt.said magnetic powder, is used as abrasive material.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7231280A JPS56167772A (en) | 1980-05-29 | 1980-05-29 | Preparation of magnetic paint |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7231280A JPS56167772A (en) | 1980-05-29 | 1980-05-29 | Preparation of magnetic paint |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS56167772A true JPS56167772A (en) | 1981-12-23 |
Family
ID=13485621
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7231280A Pending JPS56167772A (en) | 1980-05-29 | 1980-05-29 | Preparation of magnetic paint |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56167772A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4634632A (en) * | 1983-12-09 | 1987-01-06 | Fuji Photo Film Co., Ltd. | Magnetic recording medium |
US4761243A (en) * | 1985-12-07 | 1988-08-02 | Fuji Photo Film Co., Ltd. | Process for the preparation of magnetic paint |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS52151898A (en) * | 1976-06-11 | 1977-12-16 | Hitachi Ltd | Manufacturing method of magnetic paint |
JPS5538693A (en) * | 1978-09-13 | 1980-03-18 | Toyo Tire & Rubber Co Ltd | Magnetic recording medium |
-
1980
- 1980-05-29 JP JP7231280A patent/JPS56167772A/en active Pending
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS52151898A (en) * | 1976-06-11 | 1977-12-16 | Hitachi Ltd | Manufacturing method of magnetic paint |
JPS5538693A (en) * | 1978-09-13 | 1980-03-18 | Toyo Tire & Rubber Co Ltd | Magnetic recording medium |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4634632A (en) * | 1983-12-09 | 1987-01-06 | Fuji Photo Film Co., Ltd. | Magnetic recording medium |
US4761243A (en) * | 1985-12-07 | 1988-08-02 | Fuji Photo Film Co., Ltd. | Process for the preparation of magnetic paint |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
IE801180L (en) | Hydraulic cement compositions. | |
JPS57133521A (en) | Magnetic recording medium | |
JPS5552538A (en) | Manufacture of magnetic paint for magnetic recording medium | |
JPS55105253A (en) | Magnetic developer and its preparation | |
JPS56167772A (en) | Preparation of magnetic paint | |
JPS5538671A (en) | Magnetic recording medium | |
JPS5570936A (en) | Magnetic recording media | |
JPS54107710A (en) | Magnetic recording binder | |
JPS56167769A (en) | Preparation of magnetic paint | |
JPS56167771A (en) | Preparation of magnetic paint | |
JPS5278954A (en) | Polyester films | |
JPS5715671A (en) | Burr removing grinder material | |
JPS569345A (en) | Carbon sphere dispersed metal or alloy material | |
JPS57179943A (en) | High-density magnetic recording medium | |
JPS5755973A (en) | Preparation of magnetic paint | |
JPS56167770A (en) | Preparation of magnetic paint | |
JPS5764328A (en) | Magnetic recording medium | |
JPS55106269A (en) | Paint and metal plate coated therewith | |
JPS55142064A (en) | Preparation of magnetic coating material | |
JPS52151898A (en) | Manufacturing method of magnetic paint | |
JPS5746324A (en) | Magnetic recording medium | |
JPS54123919A (en) | Lubricant for magnetic recording | |
JPS5746325A (en) | Magnetic recording medium | |
JPS5756330A (en) | Hexagonal ferrite powder | |
JPS5347480A (en) | Method for increasing density of coagulated particles |