JPS56134079A - Narrow groove welding method - Google Patents

Narrow groove welding method

Info

Publication number
JPS56134079A
JPS56134079A JP3834880A JP3834880A JPS56134079A JP S56134079 A JPS56134079 A JP S56134079A JP 3834880 A JP3834880 A JP 3834880A JP 3834880 A JP3834880 A JP 3834880A JP S56134079 A JPS56134079 A JP S56134079A
Authority
JP
Japan
Prior art keywords
groove
members
nozzle
slopes
gas flow
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP3834880A
Other languages
Japanese (ja)
Inventor
Takao Mihara
Toshiaki Morichika
Takeshi Torigoe
Shoji Musha
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kubota Corp
Original Assignee
Kubota Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kubota Corp filed Critical Kubota Corp
Priority to JP3834880A priority Critical patent/JPS56134079A/en
Publication of JPS56134079A publication Critical patent/JPS56134079A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To conduct the shielding gas injected from a nozzle into the groove, fill within the groove and prevent the formation of blowholes by working shielding gas guiding slopes to the upper part of the deep narrow groove formed between two members.
CONSTITUTION: A deep narrow groove 9 is formed between end faces 61, 71 opposing to members 6, 7 in proximity, and the upper part of the groove 9 is expanded by slopes 63, 73, and is thereby metched approximately with the inside diameter of an injection nozzle 2. Next, a backing strip 5 is fitted on the back side of the groove 9, and a welding torch 1 is opposed toward the center of the groove 9, thence with the injection nozzle 2 held approached to the members, welding is started. Then, the central part of the shielding gas flow from the nozzle 2 directly strikes the inside part of the groove 9, and the outside circumferential part of the gas flow in conducted by the slopes 63, 73 into the groove 9. Hence, the greater part of the injection gas flow flows into the groove 9, thereby preventing the influx of air and welding the narrow groove 9.
COPYRIGHT: (C)1981,JPO&Japio
JP3834880A 1980-03-25 1980-03-25 Narrow groove welding method Pending JPS56134079A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP3834880A JPS56134079A (en) 1980-03-25 1980-03-25 Narrow groove welding method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP3834880A JPS56134079A (en) 1980-03-25 1980-03-25 Narrow groove welding method

Publications (1)

Publication Number Publication Date
JPS56134079A true JPS56134079A (en) 1981-10-20

Family

ID=12522767

Family Applications (1)

Application Number Title Priority Date Filing Date
JP3834880A Pending JPS56134079A (en) 1980-03-25 1980-03-25 Narrow groove welding method

Country Status (1)

Country Link
JP (1) JPS56134079A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102500893A (en) * 2011-10-20 2012-06-20 中国核工业二三建设有限公司 Welding equipment and use method thereof

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102500893A (en) * 2011-10-20 2012-06-20 中国核工业二三建设有限公司 Welding equipment and use method thereof

Similar Documents

Publication Publication Date Title
JPS56126533A (en) Wire cut spark machining device
JPS56134079A (en) Narrow groove welding method
JPS5527418A (en) Welding or cutting method
JPS5581086A (en) Tig welding equipment
JPS55117575A (en) Arc welding method
JPS5445436A (en) Cooler for diesel engine
JPS53142348A (en) Welding method for metallic pipe
JPS5469537A (en) Joining method for tube and tube plate in heat exchanger or the like
JPS5689442A (en) Fluid injection nozzle of wire cut type spark erosion machine
JPS55112536A (en) Mounting method of thermocouple onto tube wall
JPS57112960A (en) Heat resistant roll having spiral internal water groove
JPS5438489A (en) Fuel rod
JPS53106361A (en) Submerged arc welding method for steel plate
JPS5714475A (en) Back shielding method of gas shielded arc welding
JPS5317903A (en) Manufacturing method of stator iron core
JPS535389A (en) Fuel assembly
JPS57142778A (en) Welding torch for narrow groove welding
JPS5573474A (en) Butt welding method of thin-wall tubular bodiy
JPS5214857A (en) Carbon grounding bar manufacturing method
JPS5536011A (en) Inclined steel pipe field welding implementing method and its device
JPS56148490A (en) Circular butt welding of tube using gas shielded welding
JPS5796733A (en) Discharge machining process
JPS5750284A (en) Method for preventing sticking of spatter for butt resistance welding machine
JPS5731490A (en) Tube end welding device
JPS56165586A (en) Welding method for inside of tube