JPS56102358A - Surface defect preventing method of ingot in continuous casting - Google Patents

Surface defect preventing method of ingot in continuous casting

Info

Publication number
JPS56102358A
JPS56102358A JP325380A JP325380A JPS56102358A JP S56102358 A JPS56102358 A JP S56102358A JP 325380 A JP325380 A JP 325380A JP 325380 A JP325380 A JP 325380A JP S56102358 A JPS56102358 A JP S56102358A
Authority
JP
Japan
Prior art keywords
ingot
continuous casting
surface defect
preventing method
defect preventing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP325380A
Other languages
Japanese (ja)
Inventor
Junichi Hasunuma
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP325380A priority Critical patent/JPS56102358A/en
Publication of JPS56102358A publication Critical patent/JPS56102358A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To pressure-weld the surface of an ingot, prevent surface cracking and improve yield by enclosing and screwing-down the ingot at a surface temp. and draft higher than specified right under a continuous casting mold.
CONSTITUTION: An ingot 2 is enclosed and screwed down from the surroundings by rolls 3a, 3b, 4a, 4b, right under a continuous casting mold 1. At this time, the ingot 2 is screwed down from the surroundings until the draft by the formula I reaches ≥2.0% in the state that the surface temp. of the ingot 2 is above 1,100°C, whereby the surface of the ingot is pressure-welded.
COPYRIGHT: (C)1981,JPO&Japio
JP325380A 1980-01-14 1980-01-14 Surface defect preventing method of ingot in continuous casting Pending JPS56102358A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP325380A JPS56102358A (en) 1980-01-14 1980-01-14 Surface defect preventing method of ingot in continuous casting

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP325380A JPS56102358A (en) 1980-01-14 1980-01-14 Surface defect preventing method of ingot in continuous casting

Publications (1)

Publication Number Publication Date
JPS56102358A true JPS56102358A (en) 1981-08-15

Family

ID=11552292

Family Applications (1)

Application Number Title Priority Date Filing Date
JP325380A Pending JPS56102358A (en) 1980-01-14 1980-01-14 Surface defect preventing method of ingot in continuous casting

Country Status (1)

Country Link
JP (1) JPS56102358A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4709572A (en) * 1984-07-31 1987-12-01 Sumitomo Metal Industries, Ltd. Method of processing continuously cast slabs
JPH01254350A (en) * 1988-04-04 1989-10-11 Sumitomo Light Metal Ind Ltd Continuous casting method using electromagnetic field

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4709572A (en) * 1984-07-31 1987-12-01 Sumitomo Metal Industries, Ltd. Method of processing continuously cast slabs
JPH01254350A (en) * 1988-04-04 1989-10-11 Sumitomo Light Metal Ind Ltd Continuous casting method using electromagnetic field

Similar Documents

Publication Publication Date Title
JPS5383910A (en) Immersion cooling apparatus for high temperatus matallic pipe
JPS56102358A (en) Surface defect preventing method of ingot in continuous casting
JPS51131410A (en) Method for adding low-boiling metal to molten metal
JPS5310311A (en) Rolls inside furnace for process line
JPS53105319A (en) Highly density mounting frame for electronic components
JPS5233143A (en) Compressive molten bath method by industive heat way
JPS56109149A (en) Continuous casting method of less surface cracking
JPS53116072A (en) Electrode forming method for semiconductor device
JPS52120901A (en) Electroslag melting
JPS53110914A (en) Method and apparatus for adding inoculation or alloy elements in die castin g
JPS5614054A (en) Steel ingot casting mold
JPS5377815A (en) Converter slag separating method
JPS5561368A (en) Casting method of thin-walled casting
JPS5335893A (en) Reactor spray system
JPS57142752A (en) Slab casting method in vertically bent type continuous casting machine
JPS53106617A (en) Manufacture of molten killed steel for continuous casting
JPS542219A (en) Heat treating method for alloy 800 seamless pipe formed from centrifugal cast pipe as rough pipe
JPS52102811A (en) Treating apparatus for discharged scale from heating furnace
JPS53130259A (en) Controlling method for shape of rolled metal
JPS5775252A (en) Production of sound steel ingot
JPS52133004A (en) Method and apparatus for separating molten metal from solid or semi/molten slag
JPS53133518A (en) Casting and heat treating method for aluminum alloy
JPS55158876A (en) Production of grating body for lead storage battery
JPS51139515A (en) Continuous casting killed billet with few surface cracking
JPS5323864A (en) Treating method for sludge by freezing