JPS5548491A - Penetration forming welding method for large-diameter steel tube - Google Patents
Penetration forming welding method for large-diameter steel tubeInfo
- Publication number
- JPS5548491A JPS5548491A JP11932578A JP11932578A JPS5548491A JP S5548491 A JPS5548491 A JP S5548491A JP 11932578 A JP11932578 A JP 11932578A JP 11932578 A JP11932578 A JP 11932578A JP S5548491 A JPS5548491 A JP S5548491A
- Authority
- JP
- Japan
- Prior art keywords
- route
- inert gas
- steel tube
- welding method
- diameter steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To make back weld penetration even by carrying out welding by flowing inert gas through a hollow, by forming a hollow route by butting groove faces mutually.
CONSTITUTION: Route surfaces 2 of groove faces of large-diameter pipes 1 and 1' are butted each other to form route 3. Next, while inert gas is flowed through route 3, arc 6 is generated by tungsten electrode 5 of TIG torch 4, thereby welding the both. At this time, the back penetration states of internal surfaces of pipes 1 and 1' are controlled by adjusting the feed amount of inert gas flowing through route 3.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11932578A JPS5548491A (en) | 1978-09-29 | 1978-09-29 | Penetration forming welding method for large-diameter steel tube |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11932578A JPS5548491A (en) | 1978-09-29 | 1978-09-29 | Penetration forming welding method for large-diameter steel tube |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5548491A true JPS5548491A (en) | 1980-04-07 |
Family
ID=14758664
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11932578A Pending JPS5548491A (en) | 1978-09-29 | 1978-09-29 | Penetration forming welding method for large-diameter steel tube |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5548491A (en) |
-
1978
- 1978-09-29 JP JP11932578A patent/JPS5548491A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS558308A (en) | Welding method for forming thick walled steel pipe | |
JPS5548491A (en) | Penetration forming welding method for large-diameter steel tube | |
JPS55117575A (en) | Arc welding method | |
GB1349985A (en) | Method of welding | |
JPS5573479A (en) | Tandem system high speed arc welding method | |
JPS56151192A (en) | V-groove welded tube | |
JPS5684172A (en) | 2-electrode tig welding method | |
JPS5493652A (en) | Method and apparatus for manufacture of crossed pipe parts | |
JPS5577992A (en) | Electrogas arc welding method | |
ES259837U (en) | Gas-shielded arc welding employing two separately supplied gases | |
JPS5481158A (en) | Manufacture of welded tube | |
JPS564378A (en) | Inert gas shielded arc welding method | |
GB1500251A (en) | Method of gas shielded arc welding | |
JPS5493651A (en) | Narrow gap one side welding method | |
JPS5797874A (en) | Tig welding method for silicon steel sheet | |
JPS555179A (en) | Circumferential welder of stationary pipe | |
JPS56141984A (en) | Coil connecting method in spiral steel tube manufacturing equipment | |
JPH0635067B2 (en) | Welding method for high alloy clad steel pipe | |
JPS5395850A (en) | Multiple wire submerged arc welding method | |
SU823026A1 (en) | Method of producing variable chemical composition alloy by welding | |
JPS56168969A (en) | Arc welding method | |
JPS5485153A (en) | Multi-layer overplay welding method by plasma welding | |
JPS5464046A (en) | Two electrode welding of pipe | |
Dannenmann | Complete Mechanical Pipe Welding in Apparatus, Boiler and Pipeline Construction | |
JPS53137043A (en) | Inert gas arc welding method for steel for low temperature use |