JPS5497555A - Method of preventing stress corrosion cracking - Google Patents

Method of preventing stress corrosion cracking

Info

Publication number
JPS5497555A
JPS5497555A JP471978A JP471978A JPS5497555A JP S5497555 A JPS5497555 A JP S5497555A JP 471978 A JP471978 A JP 471978A JP 471978 A JP471978 A JP 471978A JP S5497555 A JPS5497555 A JP S5497555A
Authority
JP
Japan
Prior art keywords
build
corrosion cracking
stress corrosion
welding
preventing stress
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP471978A
Other languages
Japanese (ja)
Inventor
Ryoichi Ishii
Satoru Matsumura
Kiyoshi Ishikawa
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toshiba Corp
Original Assignee
Toshiba Corp
Tokyo Shibaura Electric Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toshiba Corp, Tokyo Shibaura Electric Co Ltd filed Critical Toshiba Corp
Priority to JP471978A priority Critical patent/JPS5497555A/en
Publication of JPS5497555A publication Critical patent/JPS5497555A/en
Pending legal-status Critical Current

Abstract

PURPOSE: One side of base material is build-up welded, the other side is caused to generate compressive stress, thereby to prevent stress corrosion cracking.
CONSTITUTION: An build up welding 2 is deposited on the existing pipe 1 in the radialand longituidinal directions on such an area where stress corrosion cracking is expected to occur, such a place as the outer face of the pipe joining portion. The build-up welding, when cooling down, causes a contraction Δ1, generating inwardly directed force, to the effect such that the existing pipe 1 is bound by a hoop. Material of build-up welding 2 is, preferably, selected to have a thermal expansion coefficient less than that of the piping material 1.
COPYRIGHT: (C)1979,JPO&Japio
JP471978A 1978-01-19 1978-01-19 Method of preventing stress corrosion cracking Pending JPS5497555A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP471978A JPS5497555A (en) 1978-01-19 1978-01-19 Method of preventing stress corrosion cracking

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP471978A JPS5497555A (en) 1978-01-19 1978-01-19 Method of preventing stress corrosion cracking

Publications (1)

Publication Number Publication Date
JPS5497555A true JPS5497555A (en) 1979-08-01

Family

ID=11591683

Family Applications (1)

Application Number Title Priority Date Filing Date
JP471978A Pending JPS5497555A (en) 1978-01-19 1978-01-19 Method of preventing stress corrosion cracking

Country Status (1)

Country Link
JP (1) JPS5497555A (en)

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5431062A (en) * 1977-08-12 1979-03-07 Hitachi Ltd Manufacture of structure superior in stress corrosion cracking resistivity

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5431062A (en) * 1977-08-12 1979-03-07 Hitachi Ltd Manufacture of structure superior in stress corrosion cracking resistivity

Similar Documents

Publication Publication Date Title
JPS5592285A (en) Welding method of hard metal
JPS5431062A (en) Manufacture of structure superior in stress corrosion cracking resistivity
JPS5497555A (en) Method of preventing stress corrosion cracking
JPS5775296A (en) Method for improving residual stress of welded joint part of pipe
JPS54155153A (en) Preventing method for stress corrosion cracking for sensitized zone of welding
JPS5429859A (en) Diffusion welding method utilizing transformation
JPS52125816A (en) Pipe connecting method
JPS553565A (en) Repairing method for tube
JPS5422098A (en) Nuclear fuel element and its producing method
JPS5294557A (en) Heat pipe with self-expansion capability
JPS53138945A (en) Bonding method for aluminum and iron
JPS5627321A (en) Manufacture of fireproof 2-layer pipe joint
JPS5219863A (en) Method of producing impeller for fluid coupling made of metal plate
JPS52147510A (en) Metallic material having damping capacity and it production
JPS53130242A (en) Welding method for manufacture of thick-walled large diameter welded steel pipe
JPS52118615A (en) Specials welded joint
JPS53118241A (en) Welding method for steel intended for use at extra low temperature
JPS5770083A (en) Brazing method
JPS53110938A (en) Joint welding positioner of steel pipe
JPS53142343A (en) Welding procedure
JPS5411843A (en) Method of and apparatus for underwater welding
JPS5413434A (en) Corrosion preventing method for welded steel tube
JPS5392806A (en) Prevention of coking in vapor line of residual oil cracking reactor
JPS5478535A (en) Repairing method for chimney lining
JPS5232149A (en) Method of jointing pipes with heat absorbing plate