JPS5451910A - Soaking method - Google Patents
Soaking methodInfo
- Publication number
- JPS5451910A JPS5451910A JP11886777A JP11886777A JPS5451910A JP S5451910 A JPS5451910 A JP S5451910A JP 11886777 A JP11886777 A JP 11886777A JP 11886777 A JP11886777 A JP 11886777A JP S5451910 A JPS5451910 A JP S5451910A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- ingots
- soaking
- temp
- soaking pit
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To greatly reduce the original unit of fuel for soaking, by lowering temp in a soaking pit and shortening retention time by utilizing recuperation by the heat accumulation of the inside of steel ingots when soaking the steel ingots of rimmed steel and semi-killed steel. CONSTITUTION:Since the track time of the steel ingots of rimmed steel and semi- killed steel is short, there exist non-coagulated portions at the insides of steel ingots at the time when the ingots are charged into a soaking pit, and the coagulation rate of the section is not more than 60%. Thus, since the insides of steel ingots have a large quantity of accumulated heat, the temp of the inside of the soaking pit is made to be the low temp of 1100-1250 deg.C. The retention time in the soaking pit is also shortened to 3 hrs.. Temp rises due to recuperation from non-coagulated portions at the insides of steel ingots, and the ingots can be blooming milled without having no effect on mill torque and deformability in blooming mill and without lowering mill yield. Thus, this method greatly reduces the original unit of fuel for the soaking pit per steel ingot.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11886777A JPS5451910A (en) | 1977-10-03 | 1977-10-03 | Soaking method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11886777A JPS5451910A (en) | 1977-10-03 | 1977-10-03 | Soaking method |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5451910A true JPS5451910A (en) | 1979-04-24 |
Family
ID=14747078
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11886777A Pending JPS5451910A (en) | 1977-10-03 | 1977-10-03 | Soaking method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5451910A (en) |
-
1977
- 1977-10-03 JP JP11886777A patent/JPS5451910A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS55113865A (en) | Leveling aging method for age hardening type titanium alloy member | |
JPS5451910A (en) | Soaking method | |
JPS5389817A (en) | Manufacture of steel bar for low temperature | |
JPS5241735A (en) | Temperature control method of reactor | |
JPS5310311A (en) | Rolls inside furnace for process line | |
JPS5451912A (en) | Method of soaking pit | |
JPS54106061A (en) | Blooming method for killed steel | |
JPS5577901A (en) | Preventing method for surface cracking of billet in hot rolling pass | |
JPS5451911A (en) | Method of soaking steel ingot | |
JPS52116718A (en) | Vibration damping steel material and its production process | |
JPS5416357A (en) | Looper controller | |
JPS5323864A (en) | Treating method for sludge by freezing | |
JPS56102358A (en) | Surface defect preventing method of ingot in continuous casting | |
JPS535017A (en) | High tensile cold rolled steel sheet and its production method | |
JPS52120911A (en) | Prevention of crack at grain boundary at high temperature | |
JPS53119215A (en) | Steel rolling method | |
JPS5351301A (en) | Direct kindling absorptive type high temperature reproducer | |
Kazadzhan et al. | The Effect of Heat Treatment on the Structure and Magnetic Properties of Electrical Engineering Isotropic Steel | |
JPS52120901A (en) | Electroslag melting | |
JPS5514847A (en) | High-nitrogen carbon steel for machine structural use | |
JPS5435828A (en) | Descaling method for hot rolled steel strip | |
JPS5362726A (en) | Method and apparatus for preparatment of temper rolling | |
JPS54112364A (en) | Roll for sendzimir mill and its heat treating method | |
JPS5262121A (en) | Process for improving toughness of boron steel | |
JPS5418409A (en) | Adding method for linear addition agent |