JPS53110950A - Prevention of terminal end defficiency formed during welding pipe joint portion by plural welding bars - Google Patents
Prevention of terminal end defficiency formed during welding pipe joint portion by plural welding barsInfo
- Publication number
- JPS53110950A JPS53110950A JP1224778A JP1224778A JPS53110950A JP S53110950 A JPS53110950 A JP S53110950A JP 1224778 A JP1224778 A JP 1224778A JP 1224778 A JP1224778 A JP 1224778A JP S53110950 A JPS53110950 A JP S53110950A
- Authority
- JP
- Japan
- Prior art keywords
- defficiency
- prevention
- joint portion
- pipe joint
- terminal end
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/02—Seam welding; Backing means; Inserts
- B23K9/025—Seam welding; Backing means; Inserts for rectilinear seams
- B23K9/0253—Seam welding; Backing means; Inserts for rectilinear seams for the longitudinal seam of tubes
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K9/00—Arc welding or cutting
- B23K9/02—Seam welding; Backing means; Inserts
- B23K9/0203—Inserts
Landscapes
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Plasma & Fusion (AREA)
- Mechanical Engineering (AREA)
- Arc Welding In General (AREA)
- Butt Welding And Welding Of Specific Article (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE2710713A DE2710713C3 (de) | 1977-03-09 | 1977-03-09 | Verfahren zur Vermeidung von Anfangsfehlern beim Mehrdraht-Längsnahtschweißen von Rohren |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS53110950A true JPS53110950A (en) | 1978-09-28 |
Family
ID=6003407
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1224778A Pending JPS53110950A (en) | 1977-03-09 | 1978-02-06 | Prevention of terminal end defficiency formed during welding pipe joint portion by plural welding bars |
Country Status (5)
Country | Link |
---|---|
JP (1) | JPS53110950A (it) |
DE (1) | DE2710713C3 (it) |
FR (1) | FR2382969A1 (it) |
GB (1) | GB1597042A (it) |
IT (1) | IT1093200B (it) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62230478A (ja) * | 1986-03-31 | 1987-10-09 | Sumitomo Metal Ind Ltd | タブ板自動溶接装置 |
US6568077B1 (en) * | 2000-05-11 | 2003-05-27 | General Electric Company | Blisk weld repair |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2564396A (en) * | 1949-11-01 | 1951-08-14 | Republic Steel Corp | Seam welding procedure for pipe manufacture |
DE2609201C3 (de) * | 1976-03-05 | 1979-07-19 | Kobe Steel Ltd., Kobe, Hyogo (Japan) | Verfahren zum Verhüten von Endkraterrissen beim Lichtbogenschweißen von Stumpfnähten durch Vorschweißbleche |
-
1977
- 1977-03-09 DE DE2710713A patent/DE2710713C3/de not_active Expired
-
1978
- 1978-02-06 JP JP1224778A patent/JPS53110950A/ja active Pending
- 1978-02-21 GB GB6894/78A patent/GB1597042A/en not_active Expired
- 1978-03-09 IT IT20987/78A patent/IT1093200B/it active
- 1978-03-09 FR FR7806767A patent/FR2382969A1/fr active Granted
Also Published As
Publication number | Publication date |
---|---|
IT7820987A0 (it) | 1978-03-09 |
DE2710713B2 (de) | 1980-03-13 |
IT1093200B (it) | 1985-07-19 |
GB1597042A (en) | 1981-09-03 |
DE2710713A1 (de) | 1978-09-14 |
DE2710713C3 (de) | 1980-12-04 |
FR2382969B1 (it) | 1982-02-19 |
FR2382969A1 (fr) | 1978-10-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5454325A (en) | Pipe joint | |
GB2011008B (en) | Wedge connector especially for tubular scaffolding | |
AU3929878A (en) | Pipe joints | |
JPS53103969A (en) | Prevention of terminal end defficiency formed during welding pipe joint portion by plural welding bars | |
JPS55158892A (en) | Method of mutually welding pair of metallic pipe portion | |
JPS53148712A (en) | Pipe joint | |
JPS5418438A (en) | Welded pipe assembly and method of making same | |
JPS53110950A (en) | Prevention of terminal end defficiency formed during welding pipe joint portion by plural welding bars | |
AU2322977A (en) | Coupler of pipe structure | |
DE3274724D1 (en) | Method of forming electric welded steel tube | |
DE3271490D1 (en) | Welding electrode | |
GB1556700A (en) | Welding of submerged pipe ends | |
JPS545839A (en) | Pipe butting welding | |
JPS53108053A (en) | Soldering of many pipes | |
GB2012903B (en) | Pipe joining | |
JPS53127339A (en) | Method of welding steel pipe*etc* | |
GB1524516A (en) | Fillet welded joint | |
AU3388278A (en) | Methods of arc welding at superatmospheric pressures | |
IT1093106B (it) | Procedimento per la saldatura elettrica di tubi di acciaio | |
GB1540880A (en) | Arc welding under water | |
JPS5418437A (en) | Method of welding pipe members | |
JPS53109219A (en) | Improvement of pipe joint | |
JPS53128552A (en) | Arc welding method | |
JPS5392358A (en) | Removement of spot welding portion | |
GB1537957A (en) | Welding of pipes |