JPS5144542B2 - - Google Patents
Info
- Publication number
- JPS5144542B2 JPS5144542B2 JP9754672A JP9754672A JPS5144542B2 JP S5144542 B2 JPS5144542 B2 JP S5144542B2 JP 9754672 A JP9754672 A JP 9754672A JP 9754672 A JP9754672 A JP 9754672A JP S5144542 B2 JPS5144542 B2 JP S5144542B2
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Curing Cements, Concrete, And Artificial Stone (AREA)
- Adhesives Or Adhesive Processes (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9754672A JPS5144542B2 (zh) | 1972-09-28 | 1972-09-28 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9754672A JPS5144542B2 (zh) | 1972-09-28 | 1972-09-28 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS4954442A JPS4954442A (zh) | 1974-05-27 |
JPS5144542B2 true JPS5144542B2 (zh) | 1976-11-29 |
Family
ID=14195223
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9754672A Expired JPS5144542B2 (zh) | 1972-09-28 | 1972-09-28 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5144542B2 (zh) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN102603191A (zh) * | 2012-04-10 | 2012-07-25 | 达州市海蓝冶金设备制造有限公司 | 一种含钛熔融高炉渣制取微晶玻璃的方法 |
Families Citing this family (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5258070A (en) * | 1975-11-08 | 1977-05-13 | Nisshin Eng | Hardening conposite utilizing industrial waste materials |
JPS5271523A (en) * | 1975-12-11 | 1977-06-15 | Nisshin Eng | Production method of setting compound with exhaust gas desulfurization sludge |
JPS58140356A (ja) * | 1982-02-09 | 1983-08-20 | 電気化学工業株式会社 | ライニング材 |
JPS5930741A (ja) * | 1982-08-16 | 1984-02-18 | 電気化学工業株式会社 | 耐酸性大なる遠心成型体 |
JPS6016856A (ja) * | 1983-07-08 | 1985-01-28 | 日本化学工業株式会社 | けい酸アルカリ用硬化剤 |
AU763762B2 (en) * | 1999-06-24 | 2003-07-31 | Paroc Group Oy Ab | Method for manufacturing a binder and use thereof |
WO2006075805A1 (ja) * | 2005-01-17 | 2006-07-20 | Yasutalou Fujii | 使用時混合型無機系接着組成物 |
JP6005408B2 (ja) * | 2012-06-14 | 2016-10-12 | 西松建設株式会社 | ジオポリマー組成物の製造方法、構造物の製造方法、および地盤改良方法 |
JP6100432B1 (ja) * | 2016-09-14 | 2017-03-22 | 光洋産業株式会社 | 床用再剥離型接着剤及びこれを用いた床仕上げ方法 |
-
1972
- 1972-09-28 JP JP9754672A patent/JPS5144542B2/ja not_active Expired
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN102603191A (zh) * | 2012-04-10 | 2012-07-25 | 达州市海蓝冶金设备制造有限公司 | 一种含钛熔融高炉渣制取微晶玻璃的方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS4954442A (zh) | 1974-05-27 |