JPS5025892A - - Google Patents
Info
- Publication number
- JPS5025892A JPS5025892A JP7849473A JP7849473A JPS5025892A JP S5025892 A JPS5025892 A JP S5025892A JP 7849473 A JP7849473 A JP 7849473A JP 7849473 A JP7849473 A JP 7849473A JP S5025892 A JPS5025892 A JP S5025892A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7849473A JPS5727226B2 (ja) | 1973-07-13 | 1973-07-13 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7849473A JPS5727226B2 (ja) | 1973-07-13 | 1973-07-13 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5025892A true JPS5025892A (ja) | 1975-03-18 |
JPS5727226B2 JPS5727226B2 (ja) | 1982-06-09 |
Family
ID=13663514
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7849473A Expired JPS5727226B2 (ja) | 1973-07-13 | 1973-07-13 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5727226B2 (ja) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4991022A (ja) * | 1972-12-31 | 1974-08-30 | ||
JPS54137422A (en) * | 1978-04-18 | 1979-10-25 | Nippon Kokan Kk <Nkk> | Manufacture of extra-low carbon high tensile steel with very high ductility |
JPS55100926A (en) * | 1979-01-25 | 1980-08-01 | Kobe Steel Ltd | Prevention of strength irregularity in outer circumference of hot rolled coil |
JPS5829830A (ja) * | 1981-08-13 | 1983-02-22 | Toyo Soda Mfg Co Ltd | 成形された高分子材料の表面処理方法 |
JPS5829836A (ja) * | 1981-08-13 | 1983-02-22 | Toyo Soda Mfg Co Ltd | 成形された高分子材料の表面処理方法 |
US4535010A (en) * | 1982-10-18 | 1985-08-13 | Pharmacia Ab | Method of forming polymeric layers |
-
1973
- 1973-07-13 JP JP7849473A patent/JPS5727226B2/ja not_active Expired
Cited By (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4991022A (ja) * | 1972-12-31 | 1974-08-30 | ||
JPS5545614B2 (ja) * | 1972-12-31 | 1980-11-19 | ||
JPS54137422A (en) * | 1978-04-18 | 1979-10-25 | Nippon Kokan Kk <Nkk> | Manufacture of extra-low carbon high tensile steel with very high ductility |
JPS5828327B2 (ja) * | 1978-04-18 | 1983-06-15 | 日本鋼管株式会社 | 極めて優れた延性を有する極低炭素高張力鋼の製造方法 |
JPS55100926A (en) * | 1979-01-25 | 1980-08-01 | Kobe Steel Ltd | Prevention of strength irregularity in outer circumference of hot rolled coil |
JPS5829830A (ja) * | 1981-08-13 | 1983-02-22 | Toyo Soda Mfg Co Ltd | 成形された高分子材料の表面処理方法 |
JPS5829836A (ja) * | 1981-08-13 | 1983-02-22 | Toyo Soda Mfg Co Ltd | 成形された高分子材料の表面処理方法 |
JPS6358171B2 (ja) * | 1981-08-13 | 1988-11-15 | Tosoh Corp | |
JPH0227370B2 (ja) * | 1981-08-13 | 1990-06-15 | Tosoh Corp | |
US4535010A (en) * | 1982-10-18 | 1985-08-13 | Pharmacia Ab | Method of forming polymeric layers |
Also Published As
Publication number | Publication date |
---|---|
JPS5727226B2 (ja) | 1982-06-09 |