JPH11255211A - Method for lap welding paired triangular tops formed by folding end of resin film bag packaging plural paper rolls - Google Patents

Method for lap welding paired triangular tops formed by folding end of resin film bag packaging plural paper rolls

Info

Publication number
JPH11255211A
JPH11255211A JP10073226A JP7322698A JPH11255211A JP H11255211 A JPH11255211 A JP H11255211A JP 10073226 A JP10073226 A JP 10073226A JP 7322698 A JP7322698 A JP 7322698A JP H11255211 A JPH11255211 A JP H11255211A
Authority
JP
Japan
Prior art keywords
welding
triangular
roller
pair
resin film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP10073226A
Other languages
Japanese (ja)
Other versions
JP4154448B2 (en
Inventor
Rokuro Watanabe
六郎 渡邊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP07322698A priority Critical patent/JP4154448B2/en
Publication of JPH11255211A publication Critical patent/JPH11255211A/en
Application granted granted Critical
Publication of JP4154448B2 publication Critical patent/JP4154448B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide a method for lap welding a pair of triangular tops of a bag capable of withstanding gravity at the time of taking up the bag to transport it even in the case of using a welded portion as a carrying handle by forming a tight welded portion which permits no bubbles to be embraced therein. SOLUTION: A heatable roller 5 having a plurality of grooves or protruding stripes 6, which extend along the circumference of the roller, and a receiving plate 10 for the roller 5 are prepared. The receiving plate 10 is inserted into a space directly under a pair of triangular tops 1c, 1d, which are in a state that they are overlapped each other and, by rotatively moving the roller 5 from one side of an upper face of both the tops in the overlapping state to the other side thereof, a stripe-like welded portion, in which welded zones and non-welded zones are alternately arranged, is formed.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】この発明は、複数のロールペ
ーパーを包装して樹脂フィルム製袋の端部折り重ね時に
生じる一対の3角状頂部の重ね合わせ部を溶着する方法
に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method of wrapping a plurality of roll papers and welding a pair of triangular apical portions formed at the time of folding an end portion of a resin film bag.

【0002】[0002]

【従来の技術】前記一対の3角状頂部の重ね合わせ部
は、従来から、複数のロールペーパーを包装した樹脂フ
ィルム製袋の包装作業における最終仕上工程で熱溶着さ
れている。
2. Description of the Related Art The overlapping portion of a pair of triangular peaks has been conventionally heat-sealed in a final finishing step in a packaging operation of a resin film bag in which a plurality of roll papers are packaged.

【0003】本願出願人による特公平5−67506
は、更に、その熱溶着重合部に樹脂フィルム製テープを
付着させて手提げを可能にした考えを開示する。
[0003] Japanese Patent Publication No. 5-67506 filed by the present applicant
Discloses a concept in which a tape made of a resin film is attached to the heat-welded polymerized portion to enable a handbag.

【0004】[0004]

【発明が解決しようとする課題】前記一対の3角状頂部
の重ね合わせ部は、上記したように、手提げとして使用
され、従って、そこに手指を入れ、持ち上げて運搬する
場合に、包装物全体の自重が負荷される要部であるか
ら、その重量に耐える溶着強度が要求される。
As described above, the overlapping portion of the pair of triangular apexes is used as a handbag, and therefore, when the user puts his / her finger, lifts, and transports the package, the entire package is used. Since the main part is loaded with its own weight, a welding strength that can withstand the weight is required.

【0005】しかしながら、前記重ね合わせ部は、従
来、いわゆるベタ着けと称して、一対の3角状頂部の重
ね合わせ部全体を一様に熱溶着するため、接着部位の内
層に気泡が閉じ込められ、その逃げ場がなく、接着状態
が斑(マダラ)状となり、非接着部分を内包した部分的
溶着であったので、そこに手指を掛けて持ち上げると、
その重量を支えられず、一対の3角状頂部が分離するこ
とが多かった。
[0005] However, the overlapping portion is conventionally so-called solid attachment, in which the entire overlapping portion of the pair of triangular peaks is uniformly heat-welded, so that air bubbles are trapped in the inner layer of the bonding portion, Since there was no escape place, the adhesion state became a spot (madara) shape, and it was partial welding containing the non-adhesion part, so when you lift it with your fingers,
It was not possible to support its weight, and a pair of triangular peaks often separated.

【0006】そのような気泡内包状態の溶着部を補強す
るために、その溶着部位に、樹脂フィルム製テープを付
着させようとしても、付着する基板となる前記溶着部位
に斑(マダラ)状の気泡が分散内包されていると、その
気泡内包部と溶着部との間に凹凸による段差が生じ、接
着不安定となって、樹脂フィルム製テープを一様に密着
させることが困難となり、補強の成果を奏し得なかっ
た。
[0006] In order to reinforce such a welded portion in a bubble-enclosed state, even if an attempt is made to attach a tape made of a resin film to the welded portion, a spot-like air bubble is formed on the welded portion serving as a substrate to be attached. Is dispersed and included, a step due to unevenness is generated between the bubble inclusion portion and the welded portion, the adhesive becomes unstable, and it becomes difficult to uniformly adhere the resin film tape, and the result of reinforcement Could not be played.

【0007】この発明の第1の目的は、上記の課題を解
決して、気泡が内包し得ない緊密な溶着部を形成して、
その溶着部を手提げに用いても持ち上げ運搬時の重力に
耐え得る一対の3角状頂部の重ね合わせ溶着方法を提供
することである。
[0007] A first object of the present invention is to solve the above-mentioned problems and form a tight welded portion in which air bubbles cannot be included.
It is an object of the present invention to provide a method of overlapping a pair of triangular vertices that can withstand gravity during lifting and transportation even when the welded portion is used as a handhold.

【0008】この発明の第2の目的は、上記の課題を解
決して、手提げ用の樹脂フィルム製テープを強固に付着
させ得る基板となり得る一対の3角状頂部の重ね合わせ
溶着方法を提供することである。
A second object of the present invention is to solve the above-mentioned problems and to provide a method of overlapping and welding a pair of triangular tops which can be used as a substrate on which a resin film tape for carrying can be firmly adhered. That is.

【0009】[0009]

【課題を解決するための手段】この発明は、複数のロー
ルペーパーを包装した樹脂フィルム製袋の端部折り重ね
時に生じる一対の3角状頂部の重ね合わせ溶着に際し
て、円周方向に沿った複数の凹溝又は突条を有する加熱
可能なローラーとそのローラーの受板とを用意し、前記
一対の3角状頂部が互いに重なり合った状態の直下に前
記受板を挿入すると共に、その受板上で重なり合った状
態の前記一対の3角状頂部の上面における一側から他側
へ向けて前記ローラーを転動させて、前記重なり合った
一対の3角状頂部に対して溶着帯と非溶着帯とを交互に
配した縞状の溶着を生ぜしめるものである。
SUMMARY OF THE INVENTION According to the present invention, a plurality of triangular apexes are welded along a circumferential direction when a pair of triangular apexes are formed at the end of a resin film bag in which a plurality of roll papers are wrapped. Prepare a heatable roller having a concave groove or a ridge and a receiving plate of the roller, and insert the receiving plate directly under a state where the pair of triangular apexes overlap each other, and on the receiving plate Rolling the roller from one side to the other side of the upper surface of the pair of triangular apexes in an overlapping state, the welding zone and the non-welding zone for the overlapping pair of the triangular apex. Are alternately arranged to produce striped welding.

【0010】前記ローラーは、前記双方の3角状の頂部
間を結ぶ線と平行する方向に、または、前記双方の3角
状の頂部間を結ぶ線と交わる方向に、転動させる。
The roller rolls in a direction parallel to a line connecting the two triangular peaks or in a direction intersecting a line connecting the two triangular peaks.

【0011】[0011]

【実施例】図1において、樹脂フィルム製袋1はその袋
内に複数のロールペーパーたとえば4個を3段積み合計
12個を内挿し、その袋の端部を、まず、一方の対抗端
側1a及び1bから互いに折り重ねると、他方の対抗端
1c及び1dが一対の3角形状に折りたたまれるので、
その一対の3角状頂部を互いに重ね合わせると、袋口が
閉じられることは周知である。そして、その一対の3角
状頂部の重ね合わせ部2を一様に熱溶着して閉じること
も周知である。
In FIG. 1, a resin film bag 1 has a total of 12 roll papers, for example, four roll papers, for example, four stacked in three stages, and the end of the bag is first placed on one of the opposite ends. When folded from 1a and 1b, the other opposing ends 1c and 1d are folded into a pair of triangles,
It is well known that the bag mouth is closed when the pair of triangular vertices overlap one another. It is also known that the overlapping portions 2 of the pair of triangular vertices are uniformly welded and closed.

【0012】ところで、この発明では、その周知の一様
な熱溶着ではその溶着部位の内層の各所に斑(マダラ)
状の気泡が閉じ込められて溶着されるので、重力負荷時
におけるせん断方向の強度が不足して、それが原因でそ
の重合溶着が外れてしまう傾向が強かった。そこで、こ
の発明ではその重ね合わせ部2の熱溶着を、溶着帯と、
非溶着帯とを交互に配した縞状の溶着とするものであ
り、その具体的一実施例を図2及び図3に示す。
By the way, according to the present invention, in the well-known uniform thermal welding, spots (madara) are formed on various parts of the inner layer at the welding site.
Since the bubbles were trapped and welded, the strength in the shear direction under a gravitational load was insufficient, and there was a strong tendency for the polymerized weld to come off. Therefore, in the present invention, the heat welding of the overlapping portion 2 is performed by using a welding zone,
This is a striped welding in which non-welding zones are alternately arranged, and a specific example thereof is shown in FIGS. 2 and 3.

【0013】図2において、一対の3角状頂部の重ね合
わせ部2は、双方の頂部間を結ぶ線と平行する方向に沿
って溶着帯3と非溶着帯4とを交互に配することによっ
て、全体として、交互直線状の縞模様の溶着部が形成さ
れる。
In FIG. 2, the overlapping portion 2 of a pair of triangular peaks is formed by alternately arranging welding zones 3 and non-welding zones 4 along a direction parallel to a line connecting both tops. As a whole, a welded portion having an alternate linear stripe pattern is formed.

【0014】図3は、その縞模様の溶着状態を形成する
一実施例を示し、5は、円周方向に沿った複数の突条
6,6,6・・・・を有する加熱可能なローラーであって、
その軸7の両端はそれぞれアーム8及び9の各自由端に
回動自由に支持されている。10は受板であって、その
ローラー5の作動時に一対の3角状頂部の重ね合わせ部
2の直下に挿入される。
FIG. 3 shows an embodiment for forming the welded state of the striped pattern. Reference numeral 5 denotes a heatable roller having a plurality of ridges 6, 6, 6,... And
Both ends of the shaft 7 are rotatably supported by free ends of arms 8 and 9, respectively. Reference numeral 10 denotes a receiving plate, which is inserted just below the overlapping portion 2 of the pair of triangular vertices when the roller 5 is operated.

【0015】図3において、受板10を重ね合わせ部2
の直下に挿入した後、加熱したローラー5をその重ね合
わせ部2の上面に圧接すると同時に、その実線位置から
破線位置に転動させた後、ローラー5をその重ね合わせ
部2の上面から離すと、ローラー5の突条6の部分のみ
が重ね合わせ部2に接して溶着帯3が形成され、ローラ
ー5の突条6間の凹溝の部分が重ね合わせ部2から浮い
た状態で転動するので、非溶着帯4が形成され、全体と
して図2で示す縞模様の溶着が形成される。
In FIG. 3, the receiving plate 10 is
After pressing the heated roller 5 against the upper surface of the overlapping portion 2 at the same time as rolling the roller 5 from the solid line position to the broken line position and then separating the roller 5 from the upper surface of the overlapping portion 2 Only the ridge 6 of the roller 5 contacts the overlapping portion 2 to form the welding zone 3, and the concave groove between the ridges 6 of the roller 5 rolls while floating from the overlapping portion 2. Therefore, the non-welded zone 4 is formed, and the striped weld shown in FIG. 2 is formed as a whole.

【0016】この特殊な加熱ローラー5の転動によっ
て、押圧する重ね合わせ部2は、突条6によって生じる
溶着帯3上の気泡がその突条6の双方に隣接する非溶着
帯4または非溶着部に逃げて、溶着帯3内に残留しない
から、溶着帯3は細いながらもその中に気泡を閉じ込め
ない純粋真性な溶着が一様に確保され、そのような溶着
帯3を数本設けることによって溶着強度が格段と向上す
る。
The rolling of the special heating roller 5 causes the overlapping portion 2 to press, so that the air bubbles on the welding zone 3 generated by the ridge 6 cause the non-welding zone 4 or the non-welding zone to be adjacent to both of the ridges 6. The welding zone 3 does not remain in the welding zone 3, so that the welding zone 3 is thin, but a pure intrinsic welding that does not trap air bubbles is uniformly secured therein, and several such welding zones 3 are provided. Thereby, the welding strength is significantly improved.

【0017】図3で示すローラー5は突条6,6,6・・
・・を有する実施例を示したが、突条でなく、複数の凹溝
を列設しても同様の効果が生じる。
The roller 5 shown in FIG.
Although the embodiment having... Has been shown, the same effect can be obtained by arranging a plurality of concave grooves instead of ridges.

【0018】図4は、溶着帯3と非溶着帯4との配列
を、双方の3角状の頂部1c,1d間を結ぶ線と交わる
方向に設けた実施例を示す。
FIG. 4 shows an embodiment in which the arrangement of the welding zone 3 and the non-welding zone 4 is provided in a direction intersecting a line connecting the two triangular tops 1c and 1d.

【0019】[0019]

【発明の効果】以上詳述したように、この発明は、円周
方向に沿った複数の凹溝または突条を有する加熱可能な
ローラーを使用して、一対の3角状頂部の重なり合い部
に対して、溶着帯と非溶着帯とを交互に配した縞状の溶
着を生ぜしめたので、溶着帯内の気泡がその両側に隣接
する非溶着帯に逃げて、溶着帯内に残留しないから、そ
のような溶着帯を数本配設することによって、互いに細
いながらも純粋真正な溶着が一様に確保され、かくし
て、溶着総合強度を格段と向上させた溶着部を生ぜしめ
ることに成功したので、その溶着部を手提げに用いて
も、持ち上げ運搬時に負荷される重力に十分に耐えるこ
とが出来るようになった。
As described in detail above, the present invention uses a heatable roller having a plurality of circumferentially extending concave grooves or ridges to form a pair of triangular apex overlapping portions. On the other hand, since a band-like welding in which the welding zone and the non-welding zone were alternately arranged was caused, bubbles in the welding zone escaped to the non-welding zone adjacent on both sides thereof and did not remain in the welding zone. By arranging several such welding zones, thin and genuine pure and genuine welding was uniformly secured, and thus a welded part with significantly improved overall welding strength was successfully produced. Therefore, even if the welded portion is used as a handbag, it is possible to sufficiently withstand the gravitational force applied during lifting and carrying.

【0020】更に、この発明は、その溶着部に手提げ用
の樹脂フィルム製テープを付着させたい場合には、数本
の溶着帯間に隣接する数本の非溶着帯が溶着帯に対して
一様かつ均等に突出しているので、それらの非溶着帯と
テープとの間に緊密な溶着関係が生じるので、手提げ用
の樹脂フィルム製テープの付着に対しても格段の効果を
奏する。
Further, according to the present invention, when it is desired to attach a resin film tape for carrying to the welded portion, several non-welded zones adjacent to each other between the several welded zones are one with respect to the welded zone. Since they protrude likewise and evenly, a tight welding relationship is created between the non-welded zone and the tape, and a remarkable effect is also exerted on the adhesion of the resin film tape for carrying.

【図面の簡単な説明】[Brief description of the drawings]

【図1】この発明による溶着方法によって溶着された、
複数のロールペーパーを包装した樹脂フィルム製袋の端
部折り重ね時に生じる一対の3角状頂部の重ね合わせ部
の縞状溶着状態を示す具体的一実施例の斜視図、
FIG. 1 is welded by a welding method according to the invention;
FIG. 9 is a perspective view of a specific example showing a striped welding state of an overlapping portion of a pair of triangular apexes generated at the time of folding an end portion of a resin film bag wrapped with a plurality of roll papers,

【図2】図1の拡大詳細平面図、FIG. 2 is an enlarged detailed plan view of FIG. 1;

【図3】図2で示す縞状溶着部の作成過程を説明する平
面図、
FIG. 3 is a plan view illustrating a process of forming a striped welded portion shown in FIG. 2;

【図4】縞状溶着状態の他の実施例を示す平面図、FIG. 4 is a plan view showing another embodiment of a striped welding state.

【符号の説明】[Explanation of symbols]

1 樹脂フィルム製袋 1a及び1b 一方の対抗端側 1c及び1d 一対の3角状頂部を形成する他方の対
抗端側 2 一対の3角状頂部の重ね合わせ部 3 溶着帯 4 非溶着帯 5 加熱可能なローラー 6,6,6・・・・ 円周方向に沿って列設した複数の突条 7 軸 8及び9 軸の両端を回動自由に支持するアーム 10 受板
DESCRIPTION OF SYMBOLS 1 Resin film bag 1a and 1b One opposing end side 1c and 1d The other opposing end side forming a pair of triangular peaks 2 Overlapping part of a pair of triangular peaks 3 Welding zone 4 Non-welding zone 5 Heating Possible rollers 6,6,6 ···· A plurality of ridges arranged in a line in the circumferential direction 7 Arms that support both ends of shafts 8 and 9 freely to rotate 10 Receiving plate

Claims (3)

【特許請求の範囲】[Claims] 【請求項1】 複数のロールペーパーを包装した樹脂フ
ィルム製袋の端部折り重ね時に生じる一対の3角状頂部
の重ね合わせ溶着に際して、 円周方向に沿った複数の凹溝又は突条を有する加熱可能
なローラーとそのローラーの受板とを用意し、 前記一対の3角状頂部が互いに重なり合った状態の直下
に前記受板を挿入すると共に、 その受板上で重なり合った状態の前記一対の3角状頂部
の上面における一側から他側へ向けて前記ローラーを転
動させて、 前記重なり合った一対の3角状頂部に対して溶着帯と非
溶着帯とを交互に配した縞状の溶着を生ぜしめる、 ことを特徴とする、複数のロールペーパーを包装した樹
脂フィルム製袋の端部折り重ね時に生じる一対の3角状
頂部の重ね合わせ溶着方法。
1. A plurality of concave grooves or ridges extending in a circumferential direction at the time of overlapping welding of a pair of triangular apexes generated when folding an end portion of a resin film bag wrapped with a plurality of roll papers. Prepare a heatable roller and a receiving plate of the roller, insert the receiving plate immediately below the pair of triangular tops overlapping each other, and, on the receiving plate, the pair of triangular tops The roller is rolled from one side to the other side of the upper surface of the triangular apex to form a striped pattern in which welding zones and non-welding zones are alternately arranged on the pair of overlapping triangular apices. A method for superposing and welding a pair of triangular apexes, which is generated when an end portion of a resin film bag packed with a plurality of roll papers is folded, causing welding.
【請求項2】 前記ローラーを、前記双方の3角状の頂
部間を結ぶ線と平行する方向に転動させる、 ことを特徴とする請求項1に記載の溶着方法。
2. The welding method according to claim 1, wherein the roller is rolled in a direction parallel to a line connecting the two triangular apexes.
【請求項3】 前記ローラーを前記双方の3角状の頂部
間を結ぶ線と交わる方向に転動させる、 ことを特徴とする請求項1に記載の溶着方法。
3. The welding method according to claim 1, wherein the roller is rolled in a direction intersecting a line connecting the two triangular peaks.
JP07322698A 1998-03-06 1998-03-06 A method of superposing and welding a pair of triangular top portions produced when folding end portions of a resin film bag in which a plurality of roll papers are packaged Expired - Fee Related JP4154448B2 (en)