JPH11157592A - Packing method of phase difference film sticker or roll thereof and winding method of sticker and roll - Google Patents

Packing method of phase difference film sticker or roll thereof and winding method of sticker and roll

Info

Publication number
JPH11157592A
JPH11157592A JP9327308A JP32730897A JPH11157592A JP H11157592 A JPH11157592 A JP H11157592A JP 9327308 A JP9327308 A JP 9327308A JP 32730897 A JP32730897 A JP 32730897A JP H11157592 A JPH11157592 A JP H11157592A
Authority
JP
Japan
Prior art keywords
phase difference
film
difference film
core
retardation film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP9327308A
Other languages
Japanese (ja)
Inventor
Masanori Koshioka
雅則 越岡
Keigo Taguchi
慶吾 田口
Kazuto Hosono
和登 細野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kanegafuchi Chemical Industry Co Ltd
Original Assignee
Kanegafuchi Chemical Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kanegafuchi Chemical Industry Co Ltd filed Critical Kanegafuchi Chemical Industry Co Ltd
Priority to JP9327308A priority Critical patent/JPH11157592A/en
Publication of JPH11157592A publication Critical patent/JPH11157592A/en
Withdrawn legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To prevent distortion or scars on a phase difference film during storage or transportation of the film. SOLUTION: Fixing members 22 are attached to both ends of a core 18 and the fixing members 22 are fitted into a packing box 20, whereby a phase difference film sticker 10 wound around the core 18 is packed while floating in the packing box 20. In addition, a stage having a height the same as the thickness of the phase difference film sticker 10 and extending lengthwise along the core 18 is provided on a part of an outer periphery of the core 18, wherein after an end of the phase difference film sticker 10 is butted in the stage, the sticker 10 is wound around the core 18.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は位相差フィルム貼着
体又はその原反の梱包方法及びこれらの巻取り方法に関
し、特に、位相差フィルムを保管又は輸送するとき等に
位相差フィルムを保護するための方法に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method for packing a phase difference film-attached body or a raw material thereof and a method for winding the same, and particularly to protecting the phase difference film when storing or transporting the phase difference film. For how to.

【0002】[0002]

【発明が解決しようとする課題】位相差フィルムを連続
的に製造して出荷するために、その位相差フィルムはコ
アに巻き取られ、梱包されて出荷されている。ここで、
位相差フィルムとは、偏光を高分子の分子鎖に平行に振
動するように入射させた場合と、直角に入射させた場合
とで光の屈折率が異なるフィルムをいい、例えば、黒・
白液晶ディスプレイにおいて光が着色して見えるのを防
止し、液晶を黒・白の表示にするためのフィルムであ
る。この位相差フィルムがポリスルフォン系重合体フィ
ルムなどから製造されたものである場合、フィルム同士
の滑り性が悪いため、コアに巻き取るときに巻き皺が発
生しやすく、また表面に傷が付き易いという問題があっ
た。
In order to continuously manufacture and ship a retardation film, the retardation film is wound around a core, packed and shipped. here,
A retardation film refers to a film in which the refractive index of light differs between when polarized light is incident so as to vibrate parallel to the molecular chain of a polymer and when it is incident at right angles.
This film prevents light from appearing colored in a white liquid crystal display and makes the liquid crystal display black and white. When the retardation film is manufactured from a polysulfone-based polymer film or the like, the film is poor in slipperiness, so that the film is apt to be wrinkled when wound on a core and easily scratched on the surface. There was a problem.

【0003】このため、位相差フィルムをコアに巻き取
って保管あるいは輸送するとき、位相差フィルムに所定
の粘着剤を介して保護フィルムを貼着した位相差フィル
ム貼着体の状態で行われている。例えば、図9に示すよ
うに、コア1を回転させて、位相差フィルム貼着体2を
コア1に巻き取り、巻き取った位相差フィルム貼着体2
を、図8に示すように、梱包箱3に箱詰めし、そして箱
詰めした状態で、保管又は輸送等が行われている。
[0003] Therefore, when winding or storing or transporting the phase difference film around a core, the process is performed in the state of a phase difference film bonded body in which a protective film is bonded to the phase difference film via a predetermined adhesive. I have. For example, as shown in FIG. 9, the core 1 is rotated to wind the retardation film bonded body 2 around the core 1, and the wound retardation film bonded body 2 is wound.
As shown in FIG. 8, is stored in a packing box 3 and stored or transported in the boxed state.

【0004】しかし、このような位相差フィルム貼着体
の梱包方法によれば、図8に示すように、巻き取った位
相差フィルム貼着体2の外周が梱包箱3の内壁に接触し
ているため、梱包箱3の内壁からの圧力や衝撃が位相差
フィルムに負荷される恐れがあった。位相差フィルムに
圧力や衝撃が加わると、位相差フィルムが歪み、又は破
損することにより、位相差フィルムに色むらが生じ、位
相差フィルムの品質を損ねる恐れがあった。また、図9
に示すように位相差フィルム貼着体2を巻き取った場合
には、位相差フィルム貼着体2の端部4との接触部に段
差が数巻きから数十巻きにわたって生じ、位相差フィル
ムの品質を損ねる恐れがあった。
However, according to such a method for packing a phase difference film stuck body, as shown in FIG. 8, the outer periphery of the wound phase difference film stuck body 2 comes into contact with the inner wall of the packing box 3. Therefore, pressure or impact from the inner wall of the packing box 3 may be applied to the retardation film. When pressure or impact is applied to the retardation film, the retardation film may be distorted or broken, causing color unevenness in the retardation film, and possibly deteriorating the quality of the retardation film. FIG.
When the retardation film-attached body 2 is wound up as shown in FIG. 1, a step is generated from several turns to several tens of turns at a contact portion with the end portion 4 of the retardation film-attached body 2, and There was a risk of quality loss.

【0005】そこで、本発明者はこのような課題を解決
するべく、鋭意研究を重ねた結果、本発明に至ったので
ある。
The inventor of the present invention has conducted intensive studies to solve such problems, and as a result, has arrived at the present invention.

【0006】[0006]

【課題を解決するための手段】本発明に係る位相差フィ
ルム貼着体又はその原反の梱包方法の要旨とするところ
は、位相差フィルムの少なくとも片面に保護フィルムが
ラミネートされた位相差フィルム貼着体又はその原反を
略円柱形状のコアに巻き取り、該巻き取られた位相差フ
ィルム貼着体等を梱包箱内に箱詰めする位相差フィルム
貼着体又はその原反の梱包方法において、前記位相差フ
ィルム貼着体等が巻き取られたコアの両端を梱包箱内で
支持して、該位相差フィルム貼着体等の最外表面が該梱
包箱の内面と接触しないようにしたことにある。
The gist of the method for packing a phase difference film-attached body or its raw material according to the present invention is that a phase difference film having a protective film laminated on at least one surface of the phase difference film. A method for packing a phase difference film-adhered body or its raw material, in which the bonded body or its raw material is wound around a substantially cylindrical core, and the wound phase difference film-adhered material or the like is packed in a packing box, Both ends of the core wound with the retardation film-adhered body and the like are supported in a packing box so that the outermost surface of the phase difference film-adhered body and the like does not contact the inner surface of the packing box. It is in.

【0007】この本発明の位相差フィルム貼着体又はそ
の原反の梱包方法は、まず位相差フィルム貼着体等がコ
アに巻き取られる。ここで、少なくともコアの長手方向
両端には固定部材が取り付けられるため、位相差フィル
ム貼着体等はこれら固定部材が取り付けられるコアの両
端部の間に巻き取られることとなる。次いで、位相差フ
ィルム貼着体等が巻き取られたコアの両端には、その直
径よりも大きな固定部材が取り付けられ、梱包箱の中に
収納され蓋が閉じられて、保管又は輸送に供される。そ
の結果、コアの外周に巻き取られた位相差フィルム貼着
体等は梱包箱内に浮かされ、梱包箱の内面と接触するこ
とはなく、フィルム表面に傷が付くことはない。また、
梱包箱の外部から外力が加わっても、箱内のフィルム貼
着体に直接外力が作用することはなく、フィルムに打ち
傷などが付くことはなくなる。
In the method for packing a phase difference film-attached body or its raw material of the present invention, first, a phase difference film-attached body or the like is wound around a core. Here, since fixing members are attached to at least both ends in the longitudinal direction of the core, the phase difference film-adhered body and the like are wound between both end portions of the core to which these fixing members are attached. Next, a fixing member having a diameter larger than the diameter is attached to both ends of the core on which the phase difference film-adhered body or the like is wound up, is housed in a packing box, a lid is closed, and is provided for storage or transportation. You. As a result, the phase difference film stuck body wound around the outer periphery of the core is floated in the packing box, does not contact the inner surface of the packing box, and the film surface is not damaged. Also,
Even when an external force is applied from the outside of the packing box, no external force acts directly on the film-adhered body in the box, and the film is not damaged.

【0008】次に、本発明に係る位相差フィルム貼着体
又はその原反の巻取り方法の要旨とするところは、位相
差フィルムの少なくとも片面に保護フィルムがラミネー
トされた位相差フィルム貼着体又はその原反を略円柱形
状のコアに巻き取る位相差フィルム貼着体又はその原反
の巻取り方法において、前記コアの外周の一部に、位相
差フィルム貼着体等の厚さと同一の高さを有し、該コア
の長手方向に延びる段差を設け、該位相差フィルム貼着
体等の一端を該段差に突き合わせた後、該位相差フィル
ム貼着体等を該コアに巻き取ることにある。
[0008] Next, the gist of the method for winding a retardation film-adhered body or a raw material thereof according to the present invention is that a protective film is laminated on at least one surface of the retardation film. Or, in a method of winding a raw material of a retardation film or a raw material thereof, which is wound around a substantially cylindrical core, a part of the outer periphery of the core has the same thickness as the thickness of the phase difference film bonded body or the like. Providing a step having a height and extending in the longitudinal direction of the core, and abutting one end of the phase difference film-adhered body or the like on the step, and then winding the phase difference film-adhered body or the like around the core. It is in.

【0009】この本発明の位相差フィルム貼着体又はそ
の原反の巻取り方法は、コアの段差に位相差フィルム貼
着体等の一端を合わせて位相差フィルム貼着体等を巻き
取る方法である。ここで、段差の高さが位相差フィルム
貼着体等の厚さと同一又は若干低く形成されているた
め、位相差フィルム貼着体等外周の端部付近と段差形成
部材とが連続した面を形成することとなる。位相差フィ
ルム貼着体等の端部付近と段差形成部材とが連続した平
坦面を形成するため、位相差フィルム貼着体等の端部が
2巻目以降の貼着体の裏面に食い込んで段差ができるこ
とがない。
The method for winding a phase difference film-adhered body or its raw material according to the present invention is a method of winding a phase difference film-adhered body or the like by aligning one end of the phase difference film-adhered body with a step of a core. It is. Here, since the height of the step is formed to be the same as or slightly lower than the thickness of the phase difference film stuck body or the like, the surface where the step forming member and the vicinity of the end portion of the outer periphery such as the phase difference film stuck body are continuous. Will be formed. In order to form a continuous flat surface near the end of the phase difference film stuck body and the step forming member, the end of the phase difference film stuck body cuts into the back surface of the second and subsequent rolls. There is no step.

【0010】また、本発明に係る位相差フィルム貼着体
又はその原反の巻取り方法の他の要旨とするところは、
位相差フィルムの少なくとも片面に保護フィルムがラミ
ネートされた位相差フィルム貼着体又はその原反を略円
柱形状のコアに巻き取る位相差フィルム貼着体又はその
原反の巻取り方法において、前記コアの位相差フィルム
貼着体等が巻き取られる長手方向両端付近外周に当該円
周方向の凸条を設け、該位相差フィルム貼着体等の両端
を該凸条の周りに巻き付け、位相差フィルム貼着体等の
中間部分をコアから浮かせて巻き取ることにある。
Another aspect of the method of winding the retardation film-attached body or the raw material thereof according to the present invention is as follows.
In a method for winding a phase difference film bonded body or a raw material thereof, in which a protective film laminated on at least one surface of a phase difference film or a raw material thereof is wound around a substantially cylindrical core, The circumferential ridges are provided on the outer periphery near both ends in the longitudinal direction where the retardation film-adhered body or the like is wound, and both ends of the retardation film-adhered body or the like are wound around the ridges. An object of the present invention is to lift an intermediate portion such as an adhered body from a core and wind it.

【0011】このような本発明の位相差フィルム貼着体
又はその原反の巻取り方法は、予め、コアの長手方向両
端付近外周に、その円周方向に延びる帯状部材を巻き付
けるなどの手法により凸条を形成しておく。次に、位相
差フィルム貼着体等をその一対の凸条の外周面に巻き取
る。その結果、位相差フィルム貼着体等のうち、一対の
凸条の外周面に接触しない部分すなわち中間部分はコア
から浮かせられることになり、その中間部分においてフ
ィルム同士が強く擦れ合うことはなく、フィルム表面に
傷が付くことはない。
[0011] The method for winding the retardation film-adhered body or the raw material of the present invention is carried out by a method such as winding a belt-like member extending in the circumferential direction around the outer periphery near both ends in the longitudinal direction of the core in advance. A ridge is formed. Next, a phase difference film stuck body or the like is wound around the outer peripheral surfaces of the pair of ridges. As a result, in the retardation film bonded body or the like, the portion that does not come into contact with the outer peripheral surfaces of the pair of ridges, that is, the intermediate portion will be lifted from the core, and the films will not strongly rub at the intermediate portion, No scratches on the surface.

【0012】また、本発明に係る位相差フィルム貼着体
又はその原反の巻取り方法の他の要旨とするところは、
位相差フィルムの少なくとも片面に保護フィルムがラミ
ネートされた位相差フィルム貼着体等を略円柱形状のコ
アに巻き取る位相差フィルム貼着体等の巻取り方法にお
いて、前記保護フィルムを外側にして該位相差フィルム
貼着体等をコアに巻き取ることにある。
Another aspect of the method of winding the retardation film-adhered body or its raw material according to the present invention is as follows.
In a winding method of a phase difference film bonded body or the like in which a phase difference film bonded body or the like in which a protective film is laminated on at least one surface of a phase difference film is wound around a substantially cylindrical core, the protective film is disposed on the outer side. It is to wind a phase difference film stuck body or the like around a core.

【0013】この位相差フィルム貼着体又はその原反の
巻取り方法は、位相差フィルム側をコア側にし、保護フ
ィルム側を外側にして、位相差フィルム貼着体等をコア
に巻き取るものであるため、巻き取られた位相差フィル
ム貼着体等の最外周面が保護フィルムによって覆われる
ことになる。
[0013] The method for winding the retardation film-adhered body or its raw material is such that the retardation film-adhered body or the like is wound around a core with the retardation film side facing the core and the protective film side facing outward. Therefore, the outermost peripheral surface of the wound phase difference film stuck body or the like is covered with the protective film.

【0014】更に、本発明に係る位相差フィルム貼着体
又はその原反の巻取り方法の他の要旨とするところは、
位相差フィルムの少なくとも片面に保護フィルムがラミ
ネートされた位相差フィルム貼着体等を略円柱形状のコ
アに巻き取る位相差フィルム貼着体等の巻取り方法にお
いて、前記保護フィルムの硬度が位相差フィルムの硬度
より低いことにある。
Further, another aspect of the method of winding the retardation film-adhered body or its raw material according to the present invention is as follows.
In a winding method of a phase difference film bonded body or the like in which a phase difference film bonded body or the like in which a protective film is laminated on at least one surface of a phase difference film is wound around a substantially cylindrical core, the hardness of the protective film is determined by the phase difference. Lower than the hardness of the film.

【0015】この位相差フィルム貼着体又はその原反の
巻取り方法によれば、コアに巻き取られた位相差フィル
ム貼着体等における位相差フィルムと保護フィルムとは
接触して強く擦れ合うことになる。その結果、位相差フ
ィルムと保護フィルムとの間に大きな摩擦力などが作用
したとしても、保護フィルムの表面に傷が付いても、位
相差フィルムの表面に傷が付くことはない。
According to the method for winding the retardation film-adhered body or the raw material thereof, the retardation film and the protective film in the retardation film-adhered body wound around the core or the like come into contact with each other and strongly rub against each other. become. As a result, even if a large frictional force or the like acts between the retardation film and the protective film, even if the surface of the protective film is damaged, the surface of the retardation film is not damaged.

【0016】[0016]

【発明の実施の形態】次に、本発明に係る位相差フィル
ム貼着体又はその原反の梱包方法及びこれらの巻取り方
法の実施形態について、図面に基づき詳しく説明する。
BEST MODE FOR CARRYING OUT THE INVENTION Next, an embodiment of a method for packing a phase difference film-attached body or a raw material thereof according to the present invention and a method for winding the same will be described in detail with reference to the drawings.

【0017】図1は、本発明に係る梱包方法によって梱
包された位相差フィルム貼着体10を示す図である。こ
の位相差フィルム貼着体の梱包方法は、位相差フィルム
12に粘着剤14を介して保護フィルム16が貼着され
た位相差フィルム貼着体10を、円柱形状のコア18に
巻き取り、巻き取られた位相差フィルム貼着体10を梱
包箱20内に箱詰めする方法であり、コア18の長手方
向両端に4角形状の固定部材22を取付け、固定部材2
2を梱包箱20内に接触させつつ固定することによっ
て、巻き取られた位相差フィルム貼着体10を梱包箱2
0内に浮かせて収納するように構成している。
FIG. 1 is a view showing a retardation film bonded body 10 packed by the packing method according to the present invention. This packing method of the phase difference film bonded body is performed by winding the phase difference film bonded body 10 in which the protective film 16 is bonded to the phase difference film 12 via the adhesive 14, around a cylindrical core 18, This is a method of packing the obtained retardation film-adhered body 10 in a packing box 20 by attaching rectangular fixing members 22 to both ends of the core 18 in the longitudinal direction.
2 is fixed in the packing box 20 while being in contact with the packing box 20.
It is configured to be housed floating within 0.

【0018】位相差フィルムの材質は、固有複屈折率と
光透過性が比較的高い樹脂であれば用いることができ、
たとえばポリカーボネート系樹脂、セルロース系樹脂、
ポリアリレート系樹脂、塩化ビニル系樹脂、アクリルニ
トリル系樹脂、スチレン系樹脂、ポリフェニレンオキサ
イド系樹脂、ポリスルフォン系樹脂、ポリエステル系樹
脂、ポリオレフィン系樹脂等を挙げることができるが、
特に限定はされない。また、粘着剤14は、EVA等を
用いることができ、その成分や配合は特に限定されな
い。また、保護フィルム16は、アクリル系フィルム、
ポリオレフィン系樹脂フィルム、ポリスチレン系フィル
ム、ポリエステル系樹脂フィルム、セルローストリアセ
テート系フィルム、ポリカーボネート系フィルム、ポリ
エーテルエーテルケトン系フィルム等を用いることがで
きるが、その材質は特に限定されない。
As the material of the retardation film, any resin having a relatively high intrinsic birefringence and light transmittance can be used.
For example, polycarbonate resin, cellulose resin,
Polyarylate resin, vinyl chloride resin, acrylonitrile resin, styrene resin, polyphenylene oxide resin, polysulfone resin, polyester resin, polyolefin resin, etc.
There is no particular limitation. Further, as the pressure-sensitive adhesive 14, EVA or the like can be used, and its components and composition are not particularly limited. The protective film 16 is made of an acrylic film,
Polyolefin-based resin films, polystyrene-based films, polyester-based resin films, cellulose triacetate-based films, polycarbonate-based films, polyetheretherketone-based films, and the like can be used, but the materials are not particularly limited.

【0019】この位相差フィルム貼着体の梱包方法を詳
細に説明すると、まず従来装置により、コア18に位相
差フィルム貼着体10が所定の長さで巻き取られる。次
に、巻き取られた位相差フィルム貼着体10の外径より
も充分大きい外径から成る固定部材22がコア18の両
端に取り付けられる。その後、巻き取られた位相差フィ
ルム貼着体10は、図1に示すように、梱包箱20内へ
入れられる。ここで、コア18の長手方向両端に取り付
けられている固定部材22が4角形状を成しているた
め、固定部材22が梱包箱20の正面板24、側板26
及び底板28の内側に接触し嵌合される。固定部材22
が梱包箱20の正面板24、側板26及び底板28の内
側に嵌合されることにより、位相差フィルム貼着体10
が梱包箱20内に浮かされる。
The packing method of the attached retardation film will be described in detail. First, the attached retardation film 10 is wound around the core 18 to a predetermined length by a conventional apparatus. Next, fixing members 22 each having an outer diameter sufficiently larger than the outer diameter of the wound retardation film bonded body 10 are attached to both ends of the core 18. Thereafter, the wound retardation film-attached body 10 is put into a packing box 20 as shown in FIG. Here, since the fixing members 22 attached to both ends in the longitudinal direction of the core 18 have a quadrangular shape, the fixing members 22 correspond to the front plate 24 and the side plates 26 of the packing box 20.
And is fitted into contact with the inside of the bottom plate 28. Fixing member 22
Is fitted inside the front plate 24, the side plate 26, and the bottom plate 28 of the packing box 20, so that the phase difference film
Is floated in the packing box 20.

【0020】位相差フィルム貼着体10が梱包箱20内
に浮かされた状態で梱包箱20内に入れられた後、蓋3
0が閉じられる。なお、固定部材22を安定して梱包箱
20内に固定するためには、蓋30が閉じられた時、固
定部材22が蓋30にも接触することが望ましい。この
ようにして、位相差フィルム貼着体10が梱包箱20の
正面板24、側板26、底板28及び蓋30に接触し、
梱包箱20内に嵌合された状態で、保管又は輸送され
る。
After the phase difference film stuck body 10 is put in the packing box 20 while being floated in the packing box 20, the lid 3
0 is closed. In order to stably fix the fixing member 22 in the packing box 20, it is desirable that the fixing member 22 also comes into contact with the lid 30 when the lid 30 is closed. In this way, the phase difference film stuck body 10 contacts the front plate 24, the side plate 26, the bottom plate 28, and the lid 30 of the packing box 20,
It is stored or transported in a state fitted in the packing box 20.

【0021】このような位相差フィルム貼着体の梱包方
法によれば、位相差フィルム貼着体10を梱包箱20内
に浮かした状態で、保管又は輸送できるため、保管又は
輸送時に、梱包箱20の内壁からの圧力や衝撃が位相差
フィルム貼着体10に加えられることがない。このた
め、位相差フィルム12の歪み又は破損を防止すること
ができ、位相差フィルムの品質を維持することができ
る。また、コア18に巻き取られた位相差フィルム貼着
体10は、固定部材22によって、梱包箱20内に固定
されるため、保管又は輸送中に位相差フィルム貼着体1
0が梱包箱20内で転動又は摺動することがない。この
ため、巻き取られた位相差フィルム貼着体10の外面に
傷が付くことはなく、位相差フィルム12の品質が損な
われることを防止できる。
According to such a packing method of the phase difference film-attached body, the phase difference film-attached body 10 can be stored or transported in a state of being floated in the packing box 20. No pressure or impact from the inner wall 20 is applied to the retardation film bonded body 10. Therefore, distortion or breakage of the retardation film 12 can be prevented, and the quality of the retardation film can be maintained. In addition, since the retardation film bonded body 10 wound around the core 18 is fixed in the packing box 20 by the fixing member 22, the retardation film bonded body 1 is stored or transported during the storage or transportation.
0 does not roll or slide in the packing box 20. For this reason, the wound outer surface of the phase difference film stuck body 10 is not damaged, and the quality of the phase difference film 12 can be prevented from being impaired.

【0022】以上、本発明の位相差フィルム貼着体の梱
包方法の実施の形態について説明したが、本発明は上述
の実施の形態に限定されるものではない。
Although the embodiment of the method for packing a phase difference film-attached body of the present invention has been described above, the present invention is not limited to the above-described embodiment.

【0023】例えば、本発明の位相差フィルム貼着体の
梱包方法は、図2に示すような梱包方法であっても良
い。この梱包方法は、コア18の両端が固定部材32よ
りも僅かに突き出し、固定部材32を側板26、底板2
8及び蓋30に接触させ、コア18の両端を正面板24
に接触させることにより、位相差フィルム貼着体10を
梱包箱20内に浮かせるようにしてもよい。また、固定
部材32を8角形状に構成し、8角形状の4辺を梱包箱
20内に接触させるようにしてよい。さらに、固定部材
32によって支持された位相差フィルム貼着体10の中
間部分に、位相差フィルム貼着体10と接触しない程度
の孔が開けられた固定部材33を配設することも可能で
ある。
For example, the packing method of the present invention may be a packing method as shown in FIG. In this packing method, both ends of the core 18 slightly protrude from the fixing member 32, and the fixing member 32 is attached to the side plate 26 and the bottom plate 2.
8 and the lid 30, and both ends of the core 18 are connected to the front plate 24.
May be floated in the packaging box 20 by contacting the phase difference film. Further, the fixing member 32 may be formed in an octagonal shape, and four sides of the octagonal shape may be brought into contact with the inside of the packing box 20. Further, it is also possible to dispose a fixing member 33 in which a hole is formed so as not to be in contact with the retardation film bonded body 10 in an intermediate portion of the retardation film bonded body 10 supported by the fixing member 32. .

【0024】このような位相差フィルム貼着体の梱包方
法によっても、固定部材32により、位相差フィルム貼
着体34を梱包箱20内に浮かせた状態で、梱包箱20
内に固定することができる。また、一対の固定部材32
の他に、1又は複数の固定部材33を位相差フィルム貼
着体10の中間部分に配設することによって、梱包箱2
0の強度が増し、保管あるいは輸送するとき、振動や衝
撃、外力により梱包箱20が壊れることがなくなる。
According to such a packing method of the phase difference film-attached body, the fixing member 32 holds the phase difference film-attached body 34 in the
Can be fixed inside. Also, a pair of fixing members 32
In addition, by arranging one or a plurality of fixing members 33 at an intermediate portion of the retardation film stuck body 10, the packing box 2
The strength of the packing box 20 is increased, and when stored or transported, the packing box 20 is not broken by vibration, impact, or external force.

【0025】次に、本発明の位相差フィルム貼着体の巻
取り方法について、実施の形態を説明する。
Next, an embodiment of the method for winding a retardation film-adhered body of the present invention will be described.

【0026】図3は、本発明に係る位相差フィルム貼着
体の巻取り方法を示す。この位相差フィルム貼着体の巻
取り方法は、位相差フィルム12に粘着剤14を介して
保護フィルム16が貼着された位相差フィルム貼着体1
0を円柱形状のコア18へ巻き取る方法であり、コア1
8の外周の一部に、位相差フィルム貼着体10の厚さと
同一の高さを有し、コア18の長手方向に延びる段差3
6を設けておき、位相差フィルム貼着体10の一端を段
差36に突き合わせた後、位相差フィルム貼着体10を
コア18へ巻き取っていく方法である。
FIG. 3 shows a method for winding a retardation film-adhered body according to the present invention. This winding method of the retardation film-attached body is performed by the retardation film-attached body 1 in which the protective film 16 is adhered to the retardation film 12 via the adhesive 14.
0 is wound around a cylindrical core 18.
8, a step 3 having the same height as the thickness of the retardation film bonded body 10 and extending in the longitudinal direction of the core 18
6 is provided, and one end of the phase difference film stuck body 10 is abutted against the step 36, and then the phase difference film stuck body 10 is wound around the core 18.

【0027】この位相差フィルム貼着体の巻き取り方法
を詳細に説明すると、予めコア18の外周には段差形成
部材38が固定されていて、その段差形成部材38の外
周方向一端が段差36を成すとともに、他端はコア18
の外周面に連続する面を成して構成されている。次に、
位相差フィルム貼着体の巻き取り時には、このようなコ
ア18の段差36に位相差フィルム貼着体10の一端が
合わされ、コア18が回転させられることにより、位相
差フィルム貼着体10が巻き取られていく。
A detailed description will be given of a method of winding the phase difference film-adhered body. A step forming member 38 is fixed to the outer periphery of the core 18 in advance, and one end of the step forming member 38 in the outer circumferential direction is formed with the step 36. The other end is the core 18
Is formed so as to form a surface that is continuous with the outer peripheral surface. next,
At the time of winding the retardation film adhered body, one end of the retardation film adhered body 10 is fitted to the step 36 of the core 18 and the core 18 is rotated, so that the retardation film adhered body 10 is wound. Will be taken.

【0028】ここで、段差36の高さが位相差フィルム
貼着体10の厚さと同一であるため、位相差フィルム貼
着体10外周の端部40付近と段差形成部材38とが連
続した面を形成することとなる。位相差フィルム貼着体
10の端部40付近と段差形成部材38とが連続した面
を形成するため、位相差フィルム貼着体10の端部40
が2巻目の裏面に食い込むことがない。
Here, since the height of the step 36 is the same as the thickness of the retardation film bonded body 10, the surface near the end 40 of the outer periphery of the phase difference film bonded body 10 and the step forming member 38 are continuous. Is formed. Since the vicinity of the end portion 40 of the phase difference film stuck body 10 and the step forming member 38 form a continuous surface, the end portion 40 of the phase difference film stuck body 10 is formed.
Does not cut into the back of the second volume.

【0029】このような位相差フィルム貼着体の巻取り
方法によれば、コア18の段差36に位相差フィルム貼
着体10の一端を合わせて、位相差フィルム貼着体10
を巻き取っていくため、位相差フィルム貼着体10の端
部40が2巻目の裏面に食い込むことを防止し、位相差
フィルム貼着体10裏面の端部40との接触面に傷が生
じることを防止できる。このため、位相差フィルム貼着
体10裏面の端部40との接触面に色むらが生じること
はなく、位相差フィルム12の品質を損ねることを防止
できる。
According to such a winding method of the retardation film bonded body, one end of the retardation film bonded body 10 is aligned with the step 36 of the core 18 so that the phase difference film bonded body 10
To prevent the end portion 40 of the phase difference film stuck body 10 from biting into the back surface of the second winding, and the contact surface of the back surface of the phase difference film stuck body 10 with the end portion 40 has a scratch. Can be prevented. For this reason, color unevenness does not occur on the contact surface of the back surface of the retardation film bonded body 10 with the end portion 40, and it is possible to prevent the quality of the retardation film 12 from being impaired.

【0030】また、本発明に係る位相差フィルム貼着体
の巻取り方法は、図4に示すような方法であっても良
い。この位相差フィルム貼着体の巻取り方法は、コア4
2自体に段差44を設けておき、この段差44に位相差
フィルム貼着体10の一端を合わせて、位相差フィルム
貼着体10を巻き取っていく方法である。すなわち、コ
ア42と段差形成部材46とを一体的に形成しておく方
法である。このような位相差フィルム貼着体の巻取り方
法によっても、位相差フィルム貼着体10裏面の端部4
0との接触面に色むらが生じることはなく、位相差フィ
ルム12の品質を損ねることを防止できる。
Further, the winding method of the retardation film bonded body according to the present invention may be a method as shown in FIG. The winding method of this retardation film-adhered body is the same as that of the core 4
This is a method in which a step 44 is provided on 2 itself, and one end of the retardation film bonded body 10 is aligned with the step 44, and the phase difference film bonded body 10 is wound. That is, this is a method in which the core 42 and the step forming member 46 are integrally formed. Even by such a winding method of the retardation film bonded body, the end 4 on the back surface of the retardation film bonded body 10 can be formed.
No color unevenness occurs on the contact surface with 0, and it is possible to prevent the quality of the retardation film 12 from being impaired.

【0031】次に、本発明に係る位相差フィルム貼着体
の巻取り方法は、図5に示すような方法であっても良
い。この位相差フィルム貼着体の巻取り方法は、位相差
フィルム12に粘着剤14を介して保護フィルム16が
貼着された位相差フィルム貼着体10を円柱形状のコア
18へ巻取る方法であり、コア18の長手方向両端付近
外周に円周方向に延びるテープ(帯状部材)48を固定
しておき、位相差フィルム貼着体10をテープ48の外
周面に接触させ、コア18から浮かせつつ、コア18へ
巻き取っていく方法である。
Next, the winding method of the retardation film bonded body according to the present invention may be a method as shown in FIG. This winding method of the phase difference film bonded body is a method of winding the phase difference film bonded body 10 in which the protective film 16 is bonded to the phase difference film 12 via the adhesive 14 onto a cylindrical core 18. A tape (strip-like member) 48 extending in the circumferential direction is fixed to the outer periphery near both ends in the longitudinal direction of the core 18, and the retardation film-adhered body 10 is brought into contact with the outer peripheral surface of the tape 48, while floating from the core 18. , And is wound around the core 18.

【0032】この位相差フィルム貼着体の巻き取り方法
を詳細に説明すると、予め、コア18の長手方向両端付
近外周に、裏面に粘着剤の塗布されたテープ48を巻き
付けて固定して凸条を形成しておく。ここで、テープ4
8を、コア18の長手方向中央部付近にも巻き付けてお
いても良い。
A method of winding the phase difference film-adhered body will be described in detail. A tape 48 coated with an adhesive on the back surface is wound around the core 18 in the vicinity of both ends in the longitudinal direction in advance and fixed. Is formed. Here, tape 4
8 may be wound around the center of the core 18 in the longitudinal direction.

【0033】テープ48が巻き付けられると、位相差フ
ィルム貼着体10がテープ48の外周面に接触させられ
つつコア18へ巻き取られていく。位相差フィルム貼着
体10がテープ48の外周面に接触させられつつ巻き取
られると、位相差フィルム貼着体10の中、テープ48
の外周面に接触しない部分は、コア18から浮かせられ
ることとなる。すなわち、位相差フィルム貼着体10と
コア18との間に隙間50が生じることとなる。なお、
図5において、テープ48及び隙間50の厚さは誇張し
て示している。位相差フィルム貼着体10がコア18か
ら浮かせられることにより、位相差フィルム貼着体10
がある程度の弾性を有する状態でコア18に巻かれるこ
ととなる。
When the tape 48 is wound, the phase difference film bonded body 10 is wound on the core 18 while being in contact with the outer peripheral surface of the tape 48. When the phase difference film stuck body 10 is wound while being brought into contact with the outer peripheral surface of the tape 48, the tape 48 in the phase difference film stuck body 10
The portion that does not contact the outer peripheral surface of the core 18 is floated from the core 18. That is, a gap 50 is generated between the phase difference film stuck body 10 and the core 18. In addition,
In FIG. 5, the thicknesses of the tape 48 and the gap 50 are exaggerated. The retardation film-attached body 10 is lifted from the core 18 so that the retardation film-attached body 10
Is wound around the core 18 with a certain degree of elasticity.

【0034】このような位相差フィルム貼着体の巻取り
方法によれば、位相差フィルム貼着体10をコア18か
ら浮かせつつ巻き取ることができる。このため、位相差
フィルム貼着体10の保管又は輸送中に、コア18と接
触することがなく、位相差フィルム12が破損すること
がない。また、位相差フィルム貼着体10がある程度の
弾性を有する状態でコア18に巻かれるため、多数回巻
かれた位相差フィルム貼着体10同志が強固に接触する
ことはない。このため、位相差フィルム貼着体10同志
の接触による圧力によって位相差フィルム12の品質が
損なわれるのを防止できる。
According to such a method for winding a retardation film-adhered body, the retardation film-adhered body 10 can be wound while being lifted from the core 18. For this reason, there is no contact with the core 18 during storage or transportation of the retardation film bonded body 10, and the retardation film 12 is not damaged. Further, since the phase difference film stuck body 10 is wound around the core 18 in a state having a certain degree of elasticity, the phase difference film stuck bodies 10 wound many times do not come into firm contact with each other. For this reason, it is possible to prevent the quality of the retardation film 12 from being impaired by the pressure due to the contact between the retardation film bonded bodies 10.

【0035】次に、本発明に係る位相差フィルム貼着体
の巻取り方法は、図6に示すような方法であっても良
い。この位相差フィルム貼着体の巻取り方法は、位相差
フィルム12に粘着剤14を介して保護フィルム16が
貼着された位相差フィルム貼着体10を円柱形状のコア
18へ巻き取る方法であり、保護フィルム16側を外側
に向けつつ、位相差フィルム貼着体10をコア18へ巻
き取っていく方法である。すなわち、このような位相差
フィルム貼着体の巻取り方法は、保護フィルム16側を
外側に配置して、位相差フィルム貼着体10がコア18
へ巻き取られる方法である。巻き取られた位相差フィル
ム貼着体10は、保護フィルム16側を外側に向けつ
つ、梱包箱20内に収納される。
Next, the method for winding the adhered retardation film according to the present invention may be a method as shown in FIG. This winding method of the phase difference film bonded body is a method of winding the phase difference film bonded body 10 in which the protective film 16 is bonded to the phase difference film 12 via the adhesive 14 onto a cylindrical core 18. There is a method of winding the retardation film bonded body 10 around the core 18 with the protective film 16 side facing outward. That is, in such a winding method of the phase difference film bonded body, the protective film 16 side is disposed outside, and the phase difference film bonded body 10 is
It is a method that is wound up. The wound phase difference film stuck body 10 is stored in the packing box 20 with the protective film 16 side facing outward.

【0036】このような位相差フィルム貼着体の巻き取
り方法によれば、保護フィルム16側を外側に配置して
巻き取られるため、位相差フィルム貼着体10を梱包箱
20に収納した場合に、内側に向けられた位相差フィル
ム12側が梱包箱20の内壁に接触することがない。こ
のため、位相差フィルム12が梱包箱20の内壁によっ
て損傷することがない。なお、位相差フィルム12側が
内側に向けられているため、コア18によって損傷する
ことも考えられるが、位相差フィルム貼着体10とコア
18との接触面の面積は、梱包箱20との接触面の面積
よりもはるかに少ないため、位相差フィルム12側を外
側に向けて巻き取った場合よりも、その損傷は少なくな
る。
According to such a winding method of the phase difference film-adhered body, the protective film 16 side is wound outside with the protective film 16 side disposed outside. In addition, the side of the retardation film 12 facing inward does not contact the inner wall of the packaging box 20. Therefore, the retardation film 12 is not damaged by the inner wall of the packing box 20. Since the retardation film 12 is directed inward, the core 18 may be damaged. However, the area of the contact surface between the retardation film-attached body 10 and the core 18 is determined by the contact area of the packing box 20. Since it is much smaller than the area of the surface, the damage is less than when the retardation film 12 is wound outward.

【0037】次に、本発明に係る位相差フィルム貼着体
の巻取り方法は、図7に示すような方法であっても良
い。この位相差フィルム貼着体の巻取り方法は、図3で
示したように、位相差フィルム貼着体10の一端を段差
36に合わせるとともに、図6で示したように、保護フ
ィルム16側を外側に配置して巻き取る方法である。こ
のような位相差フィルム貼着体の巻取り方法によれば、
位相差フィルム貼着体10の端部40が2巻目の裏面に
食い込むことを防止できるとともに、位相差フィルム1
2が梱包箱20の内壁によって損傷するのを防止でき
る。
Next, the method for winding the retardation film-adhered body according to the present invention may be a method as shown in FIG. As shown in FIG. 3, this winding method of the retardation film stuck body adjusts one end of the phase difference film stuck body 10 to the step 36 and, as shown in FIG. It is a method of arranging it outside and winding it up. According to such a winding method of the retardation film bonded body,
The end portion 40 of the retardation film bonded body 10 can be prevented from biting into the back surface of the second winding, and the retardation film 1
2 can be prevented from being damaged by the inner wall of the packing box 20.

【0038】また、図示を省略するが、位相差フィルム
12の少なくとも片面に貼着される保護フィルム16の
硬度が位相差フィルム12の硬度より低い材質から成る
ものを選定するのが好ましい。位相差フィルム貼着体1
0をコア18に巻き取ることにより、位相差フィルム1
2と保護フィルム16とが接触し、擦れ合うことになる
ため、接触面に摩擦力などが生じて保護フィルム16の
表面に傷等が付いたとしても、位相差フィルム12の表
面に傷等が付くことはない。
Although not shown, it is preferable that the protective film 16 adhered to at least one side of the retardation film 12 be made of a material whose hardness is lower than the hardness of the retardation film 12. Phase difference film stuck body 1
0 is wound around the core 18 so that the retardation film 1
2 and the protective film 16 come into contact with each other and rub against each other, so that even if a frictional force or the like is generated on the contact surface and the surface of the protective film 16 is scratched, the surface of the phase difference film 12 is scratched. Never.

【0039】以上、本発明に係る位相差フィルム貼着体
の梱包方法及び巻取り方法について、図面に基づいて種
々説明したが、本発明は図示したものに限定されること
はない。例えば、位相差フィルム貼着体の梱包方法及び
巻取り方法について上述したが、本発明に係る梱包方法
及び巻取り方法は、位相差フィルム貼着体だけでなく、
位相差フィルム貼着体が製造される前のその原反に使用
しても良い。また、本発明に係る位相差フィルム貼着体
等の梱包方法及び巻取り方法に使用する位相差フィル
ム、コアの寸法は特に限定されることはない。また、本
発明に係る位相差フィルム貼着体等の梱包方法に使用す
る梱包箱の寸法は、固定部材を嵌合できるものであれ
ば、特に限定されることはない。
As described above, various methods for packing and winding the retardation film-attached body according to the present invention have been described based on the drawings, but the present invention is not limited to the illustrated ones. For example, although the packing method and the winding method of the phase difference film stuck body have been described above, the packing method and the winding method according to the present invention are not limited to the phase difference film stuck body,
You may use it for the raw material before manufacturing a phase difference film bonding body. The dimensions of the retardation film and the core used in the method for packing and winding the retardation film-adhered body and the like according to the present invention are not particularly limited. The dimensions of the packing box used for the method for packing the retardation film-adhered body or the like according to the present invention are not particularly limited as long as the fixing member can be fitted thereto.

【0040】また、本発明に係る位相差フィルム貼着体
等の梱包方法は、図1乃至図7に示す梱包方法乃至巻取
り方法を適宜組み合わせたものであっても良い。さら
に、本発明に係る位相差フィルム貼着体等の巻取り方法
は、図3乃至図7に示す巻取り方法を適宜組み合わせた
ものであっても良い。
The packing method for the retardation film-adhered body and the like according to the present invention may be a combination of the packing method and the winding method shown in FIGS. 1 to 7 as appropriate. Further, the winding method of the retardation film stuck body or the like according to the present invention may be a combination of the winding methods shown in FIGS. 3 to 7 as appropriate.

【0041】その他、本発明の技術的範囲には、その趣
旨を逸脱しない範囲内で、当業者の知識に基づき種々な
る改良、修正、変形を加えた位相差フィルム貼着体等の
梱包方法及び巻取り方法も含むものである。
In addition, the technical scope of the present invention includes, within a range not departing from the gist thereof, a method of packing a phase difference film-attached body or the like with various improvements, corrections and modifications based on the knowledge of those skilled in the art. This also includes a winding method.

【0042】[0042]

【発明の効果】本発明に係る位相差フィルム貼着体又は
その原反の梱包方法によれば、位相差フィルム貼着体等
を梱包箱内に浮かした状態で、保管又は輸送できるた
め、保管又は輸送時に、梱包箱の内壁からの圧力や衝撃
が位相差フィルム貼着体等に加えられることがない。こ
のため、位相差フィルムの歪み又は破損を防止すること
ができ、位相差フィルムの品質を維持することができ
る。また、コアに巻き取られた位相差フィルム貼着体等
は、固定部材によって、梱包箱内に固定されるため、保
管又は輸送中に位相差フィルム貼着体等が梱包箱内で転
動又は摺動することがない。このため、巻き取られた位
相差フィルム貼着体等の外面に傷が付くことはなく、位
相差フィルムの品質が損なわれることを防止できる。
According to the method for packing a phase difference film-attached body or its raw material according to the present invention, the phase difference film-attached body or the like can be stored or transported in a state of being floated in a packing box. Alternatively, during transportation, pressure or impact from the inner wall of the packaging box is not applied to the retardation film-attached body or the like. For this reason, distortion or breakage of the retardation film can be prevented, and the quality of the retardation film can be maintained. Further, since the phase difference film stuck body wound around the core is fixed in the packing box by the fixing member, the phase difference film stuck body etc. rolls or moves in the packing box during storage or transportation. There is no sliding. For this reason, the outer surface of the wound phase difference film stuck body or the like is not damaged, and the quality of the phase difference film can be prevented from being impaired.

【0043】また、コアの長手方向に延びる段差を設け
ておき、位相差フィルム貼着体等の一端を段差に合わせ
た後、位相差フィルム貼着体等をコアへ巻き取っていく
ことを特徴とする本発明に係る位相差フィルム貼着体等
の巻取り方法によれば、コアの段差に位相差フィルム貼
着体等の一端を合わせて、位相差フィルム貼着体等を巻
き取っていくため、位相差フィルム貼着体等の端部が2
巻目の裏面に食い込むことを防止し、位相差フィルム貼
着体等裏面の端部との接触面に傷が生じることを防止で
きる。このため、位相差フィルム貼着体等裏面の端部と
の接触面に色むらが生じることはなく、位相差フィルム
の品質を損ねることを防止できる。
Further, a step extending in the longitudinal direction of the core is provided, and one end of the phase difference film stuck body or the like is adjusted to the step, and then the phase difference film stuck body or the like is wound around the core. According to the winding method of the retardation film pasted body and the like according to the present invention, one end of the phase difference film pasted body and the like to the step of the core, winding the phase difference film pasted body and the like Therefore, the end of the phase difference film stuck body is 2
It is possible to prevent biting into the back surface of the winding and prevent scratches from being generated on the contact surface with the end of the back surface such as the phase difference film-adhered body. For this reason, color unevenness does not occur on the contact surface with the end of the back surface such as the attached retardation film, and it is possible to prevent the quality of the retardation film from being impaired.

【0044】また、少なくともコアの長手方向両端付近
外周に円周方向に延びる帯状部材を固定しておき、位相
差フィルム貼着体等を帯状部材の外周面に接触させ、コ
アから浮かせつつ、コアへ巻き取っていくことを特徴と
する本発明に係る位相差フィルム貼着体等の巻取り方法
によれば、位相差フィルム貼着体等をコアから浮かせつ
つ巻き取ることができる。このため、位相差フィルム貼
着体等の保管又は輸送中に、コアと接触することがな
く、位相差フィルムが破損することがない。また、位相
差フィルム貼着体等がある程度の弾性を有する状態でコ
アに巻かれるため、多数回巻かれた位相差フィルム貼着
体等同志が強固に接触することはない。このため、位相
差フィルム貼着体等同志の接触による圧力によって位相
差フィルムの品質が損なわれるのを防止できる。
Further, a belt-like member extending in the circumferential direction is fixed at least on the outer periphery near both ends in the longitudinal direction of the core, and the phase difference film-adhered body or the like is brought into contact with the outer peripheral surface of the belt-like member, and the core is lifted from the core. According to the method for winding a retardation film-adhered body or the like according to the present invention, which is characterized in that winding is performed, the retardation film-adhered body or the like can be wound while being lifted from the core. Therefore, the core does not come into contact with the core during storage or transportation of the bonded body of the retardation film or the like, and the retardation film is not damaged. Further, since the phase difference film bonded body or the like is wound around the core in a state having a certain degree of elasticity, the phase difference film bonded body or the like wound many times does not come into strong contact with each other. For this reason, it is possible to prevent the quality of the retardation film from being impaired by the pressure due to the contact of the retardation film bonded bodies or the like.

【0045】また、保護フィルム側を外側に向けつつ、
位相差フィルム貼着体等をコアへ巻き取っていくことを
特徴とする本発明に係る位相差フィルム貼着体等の巻取
り方法によれば、保護フィルム側を外側に向けつつ巻き
取られるため、位相差フィルム貼着体等を梱包箱に収納
した場合に、内側に向けられた位相差フィルム側が梱包
箱の内壁に接触することがない。このため、位相差フィ
ルムが梱包箱の内壁によって損傷することがない。
Further, while the protective film side is directed outward,
According to the winding method of the retardation film-adhered body or the like according to the present invention, which is characterized in that the retardation film-adhered body or the like is wound up around the core, since the protective film side is wound outward while being wound up, Also, when the phase difference film-adhered body or the like is stored in the packing box, the side of the phase difference film facing inward does not contact the inner wall of the packing box. Therefore, the retardation film is not damaged by the inner wall of the packing box.

【0046】さらに、位相差フィルムの少なくとも片面
に貼着される保護フィルムの硬度が位相差フィルムの硬
度より低いものとすることにより、位相差フィルムと保
護フィルムとの接触面に摩擦力などが生じて、保護フィ
ルムの表面に傷等が付いたとしても、位相差フィルムの
表面に傷等が付くことはない。
Further, when the hardness of the protective film adhered to at least one side of the retardation film is lower than the hardness of the retardation film, a frictional force or the like is generated on the contact surface between the retardation film and the protective film. Therefore, even if the surface of the protective film is damaged, the surface of the retardation film is not damaged.

【0047】また、本発明に係る位相差フィルム貼着体
等の梱包方法及び巻取り方法によれば、位相差フィルム
に歪みや傷が生じて色むらが生じるのを防止する方法で
あるため、特に、位相差値を均一にすることが重要とな
る位相差フィルムについて利用することにより、その効
果は顕著なものとなる。例えば、位相差フィルムの許容
される位相差値のバラツキは、±1%程度と言われてい
るため、加工、製造時において高度な製造技術が必要と
なるが、保管又は輸送時においても位相差値のバラツキ
を防止するという点で、本発明は優れた効果を奏ずるも
のである。
Further, according to the packing method and the winding method of the retardation film-attached body and the like according to the present invention, the method is to prevent the retardation film from being distorted or damaged, thereby preventing color unevenness. In particular, by using a retardation film for which it is important to make the retardation value uniform, the effect becomes remarkable. For example, it is said that the variation of the allowable retardation value of the retardation film is about ± 1%, which requires advanced manufacturing technology during processing and manufacturing. The present invention has an excellent effect in preventing variation in values.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明に係る位相差フィルム貼着体の梱包方法
を説明するための図であり、同図(a)は側面断面図、
同図(b)はA−A線断面図、同図(c)は位相差フィ
ルム貼着体の要部拡大断面図である。
FIG. 1 is a view for explaining a method of packing a retardation film-attached body according to the present invention, wherein FIG.
FIG. 2B is a cross-sectional view taken along line AA, and FIG. 2C is an enlarged cross-sectional view of a main part of the phase difference film-adhered body.

【図2】本発明に係る位相差フィルム貼着体の梱包方法
の他の実施形態を説明するための図であり、同図(a)
は側面断面図、同図(b)はB−B線断面図である。
FIG. 2 is a view for explaining another embodiment of the method for packing a retardation film-adhered body according to the present invention, and FIG.
Is a side sectional view, and FIG. 4B is a sectional view taken along line BB.

【図3】本発明に係る位相差フィルム貼着体の巻き取り
方法を説明するための正面断面図である。
FIG. 3 is a front cross-sectional view for explaining a method for winding a retardation film-adhered body according to the present invention.

【図4】本発明に係る位相差フィルム貼着体の巻き取り
方法の他の実施形態を説明するための正面断面図であ
る。
FIG. 4 is a front sectional view for explaining another embodiment of the method for winding a retardation film-adhered body according to the present invention.

【図5】本発明に係る位相差フィルム貼着体の巻き取り
方法の更に他の実施形態を説明するための図であり、同
図(a)は正面図、同図(b)は側面断面図である。
5A and 5B are views for explaining still another embodiment of the method for winding a retardation film-adhered body according to the present invention, wherein FIG. 5A is a front view and FIG. FIG.

【図6】本発明に係る位相差フィルム貼着体の巻き取り
方法の更に他の実施形態を説明するための正面断面図で
ある。
FIG. 6 is a front sectional view for explaining still another embodiment of the method for winding a retardation film-adhered body according to the present invention.

【図7】本発明に係る位相差フィルム貼着体の巻き取り
方法の更に他の実施形態を説明するための正面断面図で
ある。
FIG. 7 is a front sectional view for explaining still another embodiment of the method for winding a retardation film stuck body according to the present invention.

【図8】従来の位相差フィルム貼着体の梱包方法を説明
するための図であり、同図(a)は側面断面図、同図
(b)はC−C線断面図である。
8A and 8B are views for explaining a conventional method for packing a phase difference film-attached body, wherein FIG. 8A is a side sectional view, and FIG. 8B is a sectional view taken along line CC.

【図9】従来の位相差フィルム貼着体の巻き取り方法を
説明するための正面断面図である。
FIG. 9 is a front cross-sectional view for explaining a conventional method of winding a retardation film-adhered body.

【符号の説明】[Explanation of symbols]

10,34;位相差フィルム貼着体 12;位相差フィルム 14;粘着剤 16;保護フィルム 18;コア 20;梱包箱 22,32;固定部材 48;テープ(帯状部材) 10, 34; retardation film adhered body 12; retardation film 14, adhesive 16; protective film 18, core 20, packing box 22, 32, fixing member 48, tape (band-shaped member)

───────────────────────────────────────────────────── フロントページの続き (51)Int.Cl.6 識別記号 FI G02F 1/1335 510 G02F 1/1335 510 ──────────────────────────────────────────────────続 き Continued on the front page (51) Int.Cl. 6 Identification code FI G02F 1/1335 510 G02F 1/1335 510

Claims (5)

【特許請求の範囲】[Claims] 【請求項1】 位相差フィルムの少なくとも片面に保護
フィルムがラミネートされた位相差フィルム貼着体又は
その原反を略円柱形状のコアに巻き取り、該巻き取られ
た位相差フィルム貼着体等を梱包箱内に箱詰めする位相
差フィルム貼着体又はその原反の梱包方法において、前
記位相差フィルム貼着体等が巻き取られたコアの両端を
梱包箱内で支持して、該位相差フィルム貼着体等の最外
表面が該梱包箱の内面と接触しないようにしたことを特
徴とする位相差フィルム貼着体又はその原反の梱包方
法。
1. A phase difference film-adhered body in which a protective film is laminated on at least one surface of a phase difference film, or a raw material thereof is wound on a substantially cylindrical core, and the wound phase difference film-adhered body, etc. In a method for packing a phase difference film-attached body or its raw material in a packing box, the both ends of a core around which the phase difference film-bonded body or the like is wound are supported in the packing box, and the phase difference A method for packing a phase difference film-attached body or its raw material, wherein an outermost surface of a film-attached body or the like does not contact an inner surface of the packing box.
【請求項2】 位相差フィルムの少なくとも片面に保護
フィルムがラミネートされた位相差フィルム貼着体又は
その原反を略円柱形状のコアに巻き取る位相差フィルム
貼着体又はその原反の巻取り方法において、前記コアの
外周の一部に、位相差フィルム貼着体等の厚さと同一の
高さを有し、該コアの長手方向に延びる段差を設け、該
位相差フィルム貼着体等の一端を該段差に突き合わせた
後、該位相差フィルム貼着体等を該コアに巻き取ること
を特徴とする位相差フィルム貼着体又はその原反の巻取
り方法。
2. A phase difference film-adhered body in which a protective film is laminated on at least one surface of a phase difference film or an original sheet thereof, and a phase difference film-adhered body or an original sheet thereof wound around a substantially cylindrical core. In the method, a part of the outer periphery of the core has the same height as the thickness of the phase difference film pasted body or the like, and a step extending in the longitudinal direction of the core is provided, and the phase difference film pasted body or the like is provided. A method of winding a retardation film-adhered body or a raw material thereof, wherein one end is abutted on the step, and then the retardation film-adhered body or the like is wound around the core.
【請求項3】 位相差フィルムの少なくとも片面に保護
フィルムがラミネートされた位相差フィルム貼着体又は
その原反を略円柱形状のコアに巻き取る位相差フィルム
貼着体又はその原反の巻取り方法において、前記コアの
位相差フィルム貼着体等が巻き取られる長手方向両端付
近外周に当該円周方向の凸条を設け、該位相差フィルム
貼着体等の両端を該凸条の周りに巻き付け、位相差フィ
ルム貼着体等の中間部分をコアから浮かせて巻き取るこ
とを特徴とする位相差フィルム貼着体又はその原反の巻
取り方法。
3. A phase difference film-adhered body in which a protective film is laminated on at least one surface of a phase difference film or an original sheet thereof, and a phase difference film-adhered body or an original sheet thereof wound around a substantially cylindrical core. In the method, the circumferential ridges are provided on the outer periphery near both ends in the longitudinal direction of the core where the retardation film bonded body or the like is wound, and both ends of the phase difference film bonded body or the like are provided around the ridges. A method for winding a phase difference film-adhered body or a raw material thereof, wherein winding and winding of an intermediate portion such as a phase difference film-adhered body are lifted from a core.
【請求項4】 位相差フィルムの少なくとも片面に保護
フィルムがラミネートされた位相差フィルム貼着体又は
その原反を略円柱形状のコアに巻き取る位相差フィルム
貼着体又はその原反の巻取り方法において、前記保護フ
ィルムを外側にして該位相差フィルム貼着体等をコアに
巻き取ることを特徴とする位相差フィルム貼着体又はそ
の原反の巻取り方法。
4. A phase difference film-adhered body in which a protective film is laminated on at least one surface of a phase difference film or a raw material thereof is wound around a substantially cylindrical core, or a raw material thereof is wound. A method for winding a retardation film-adhered body or its raw material, wherein the protective film is turned outside and the phase-difference film-adhered body or the like is wound around a core.
【請求項5】 位相差フィルムの少なくとも片面に保護
フィルムがラミネートされた位相差フィルム貼着体又は
その原反を略円柱形状のコアに巻き取る位相差フィルム
貼着体又はその原反の巻取り方法において、前記保護フ
ィルムの硬度が位相差フィルムの硬度より低いことを特
徴とする位相差フィルム貼着体又はその原反の巻取り方
法。
5. A phase difference film-adhered body in which a protective film is laminated on at least one surface of a phase difference film, or a raw material thereof is wound on a substantially cylindrical core, or a raw material thereof is wound. In the method, the hardness of the protective film is lower than the hardness of the retardation film.
JP9327308A 1997-11-28 1997-11-28 Packing method of phase difference film sticker or roll thereof and winding method of sticker and roll Withdrawn JPH11157592A (en)