JPH08357Y2 - セラミック内挿金属パイプ - Google Patents
セラミック内挿金属パイプInfo
- Publication number
- JPH08357Y2 JPH08357Y2 JP1989133034U JP13303489U JPH08357Y2 JP H08357 Y2 JPH08357 Y2 JP H08357Y2 JP 1989133034 U JP1989133034 U JP 1989133034U JP 13303489 U JP13303489 U JP 13303489U JP H08357 Y2 JPH08357 Y2 JP H08357Y2
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- ceramic
- layer
- metal
- metal pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Coating By Spraying Or Casting (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1989133034U JPH08357Y2 (ja) | 1989-11-17 | 1989-11-17 | セラミック内挿金属パイプ |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1989133034U JPH08357Y2 (ja) | 1989-11-17 | 1989-11-17 | セラミック内挿金属パイプ |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0374657U JPH0374657U (cs) | 1991-07-26 |
| JPH08357Y2 true JPH08357Y2 (ja) | 1996-01-10 |
Family
ID=31680454
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1989133034U Expired - Lifetime JPH08357Y2 (ja) | 1989-11-17 | 1989-11-17 | セラミック内挿金属パイプ |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH08357Y2 (cs) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP7298403B2 (ja) * | 2019-09-06 | 2023-06-27 | 株式会社デンソー | プラズマ溶射装置 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5767158A (en) * | 1980-10-07 | 1982-04-23 | Maki Seisakusho:Kk | Production of metal heat sprayed clad steel |
| JPS6345357A (ja) * | 1986-08-11 | 1988-02-26 | Nippon Kokan Kk <Nkk> | 低圧プラズマ溶射によるビレツトのコ−テイング方法 |
-
1989
- 1989-11-17 JP JP1989133034U patent/JPH08357Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0374657U (cs) | 1991-07-26 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4120930A (en) | Method of coating a composite mold | |
| EP0909831A3 (en) | Process for depositing a bond coat for a thermal barrier coating system | |
| EP0911422A3 (en) | Method of forming a bond coat for a thermal barrier coating | |
| CA2448361A1 (en) | Method for producing metallic iron | |
| EP1390549B1 (en) | Metal-zirconia composite coating | |
| JP2002506926A (ja) | すべり軸受のライニングの形成 | |
| US4839239A (en) | Metallic coating on an inorganic substrate | |
| JPH07279968A (ja) | 摺動構造物とそれを用いた連続溶融金属メッキ装置 | |
| JPH08357Y2 (ja) | セラミック内挿金属パイプ | |
| US20090223756A1 (en) | Method for producing friction surfaces or friction layers of a carbon-ceramic brake disk as well as a carbon-ceramic brake disk provided with such friction surfaces or friction layers | |
| EP0644016A1 (en) | Process for coating the internal surface of hollow bodies | |
| EP0794931B1 (en) | Process and apparatus for making ceramic articles | |
| JPH0693409A (ja) | ピストンリングの溶射被膜の形成方法 | |
| CN104313528A (zh) | 锅炉、水冷壁管及其防磨喷涂方法 | |
| JP2934911B2 (ja) | 溶射皮膜製造方法 | |
| JPH0144783B2 (cs) | ||
| JPH0543074Y2 (cs) | ||
| CN112176340B (zh) | 一种耐高温耐侵蚀疏渣陶瓷涂层的制备方法 | |
| US20020136917A1 (en) | Metallic tubular components for industrial flowstreams | |
| JPS63157741A (ja) | 連続鋳造用鋳型 | |
| JPH0229391Y2 (cs) | ||
| JP2000120939A (ja) | 耐摩耗性金属管及びその製造方法 | |
| JPH0229740B2 (ja) | Mitsuchakuseinisuguretayoshasonokeiseihoho | |
| JP3025140B2 (ja) | 外面に金属ライニング層を有する金属曲条材の製造方法 | |
| Murthy et al. | Processing and characterization of multi-layered wear-resistant ceramic coatings |