JPH08227741A - Connecting part structure of aluminum conductor and copper conductor - Google Patents
Connecting part structure of aluminum conductor and copper conductorInfo
- Publication number
- JPH08227741A JPH08227741A JP5374595A JP5374595A JPH08227741A JP H08227741 A JPH08227741 A JP H08227741A JP 5374595 A JP5374595 A JP 5374595A JP 5374595 A JP5374595 A JP 5374595A JP H08227741 A JPH08227741 A JP H08227741A
- Authority
- JP
- Japan
- Prior art keywords
- aluminum
- copper
- conductor
- exposed surface
- corrosion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【0001】[0001]
【産業上の利用分野】本発明は銅導体と接続して用いる
アルミニウム導体において銅導体と接触する部分に銅貼
りをしたアルミニウム導体と銅導体の接続部に関する。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a connecting portion between an aluminum conductor and a copper conductor, in which a portion of the aluminum conductor used for connecting to the copper conductor is in contact with the copper conductor.
【0002】[0002]
【従来の技術】図4乃至図6に示すよう銅導体1と接続
して用いるアルミニウム導体2において、銅導体1と接
触する部分に銅貼りをしたアルミニウム導体(以下アル
ミニウム導体と記す)2は、銅導体1と接続する場合、
アルミニウム部分5と銅貼りの銅4の境界は露出したま
まである。2. Description of the Related Art In an aluminum conductor 2 used by connecting to a copper conductor 1 as shown in FIGS. 4 to 6, an aluminum conductor (hereinafter referred to as an aluminum conductor) 2 having copper adhered to a portion in contact with the copper conductor 1 is When connecting with the copper conductor 1,
The boundary between the aluminum part 5 and the copper-clad copper 4 remains exposed.
【0003】[0003]
【発明が解決しようとする課題】アルミニウム導体2
は、銅導体1と接続する場合、銅貼りの銅4とアルミニ
ウム部分5の境界の露出する面(以下露出面と記す)3
に、雨水など電解質水溶液が滞留すると、電解質水溶液
と銅とアルミニウムの三者で電池を形成し、陽極となる
アルミニウムと陰極となる銅は電気的に短絡状態であ
り、異種金属の接触腐食により陽極のアルミニウムは腐
食し、その結果くぼみを生じる。Aluminum conductor 2
When connecting to the copper conductor 1, the exposed surface of the boundary between the copper-bonded copper 4 and the aluminum portion 5 (hereinafter referred to as the exposed surface) 3
In addition, when an aqueous electrolyte solution such as rainwater stays, the electrolyte solution and copper and aluminum form a battery, and the aluminum that serves as the anode and the copper that serves as the cathode are in an electrically short-circuited state. Aluminum corrodes, resulting in depressions.
【0004】この場合、陽極のアルミニウムと陽極の銅
の間に流れる電流量は同じであるからアルミニウムの面
積に対する銅の面積比が大きい程、アルミニウム面の電
流密度は大きく、その腐食量は多くなる。したがってア
ルミニウム導体2は銅導体1と接続すると、露出面3で
のアルミニウムに対する銅の面積は大きくなり、アルミ
ニウムの腐食量は大きくなり、くぼみを生じ易く、その
中に雨水などの電解質水溶液が滞留し易すく、漸次くぼ
みは深くなり、銅貼りの銅4とアルミニウム部分5の電
気抵抗が増大したり、銅貼りの銅4が剥離するという欠
点がある。In this case, since the amount of current flowing between the aluminum of the anode and the copper of the anode is the same, the greater the area ratio of copper to the area of aluminum, the greater the current density on the aluminum surface and the greater the amount of corrosion thereof. . Therefore, when the aluminum conductor 2 is connected to the copper conductor 1, the area of copper with respect to aluminum on the exposed surface 3 becomes large, the amount of corrosion of aluminum becomes large, and cavities are easily generated, and electrolyte solution such as rainwater stays therein. There are drawbacks that the recesses are easily and gradually deepened, the electric resistance of the copper-clad copper 4 and the aluminum portion 5 is increased, and the copper-clad copper 4 is peeled off.
【0005】そこで本発明は上記のような従来技術の欠
点を解消するために創案されたものであり、アルミニウ
ム導体1の露出面3のアルミニウム部分5の腐食を低減
する。Therefore, the present invention was devised to solve the above-mentioned drawbacks of the prior art, and reduces corrosion of the aluminum portion 5 of the exposed surface 3 of the aluminum conductor 1.
【0006】[0006]
【課題を解決するための手段】本発明では銅貼りをした
アルミニウム導体2の露出面3を、アルミニウムより自
然電極電位が低い金属より成る犠牲陽極板6で覆う状態
で固定する。In the present invention, the exposed surface 3 of the copper-bonded aluminum conductor 2 is fixed in a state of being covered with a sacrificial anode plate 6 made of a metal whose natural electrode potential is lower than that of aluminum.
【0007】[0007]
【作用】図面を使って本発明の作用を説明する。本発明
の接続部で犠牲陽極板6は露出面3を覆っており、水溶
液の露出面3への付着を防いでいる。また水溶液が露出
面3に付着滞留した場合は、水溶液と銅貼りの銅4とア
ルミニウム部分5と犠牲陽極板6で電池を形成し、水溶
液における自然電極電位が低い犠牲陽極板6が陽極とな
って腐食し、アルミニウム部分5の腐食を防ぐ。The operation of the present invention will be described with reference to the drawings. The sacrificial anode plate 6 covers the exposed surface 3 with the connection portion of the present invention, and prevents the aqueous solution from adhering to the exposed surface 3. When the aqueous solution adheres to and remains on the exposed surface 3, a battery is formed by the aqueous solution, the copper-clad copper 4, the aluminum portion 5 and the sacrificial anode plate 6, and the sacrificial anode plate 6 having a low natural electrode potential in the aqueous solution serves as an anode. To prevent corrosion of the aluminum part 5.
【0008】[0008]
【実施例】図1乃至図3に示すように犠牲陽極板6はア
ルミニウム導体2の露出面3を覆う状態で固定する。犠
牲陽極板5は銅およびアルミニウムより自然電極電位の
低い金属、例えば亜鉛より成り、露出面3を覆っている
から、露出面3に水溶液の付着を防いでいる。 露出面
3に水溶液が付着滞留した場合、銅貼りの銅4、アルミ
ニウム部分5、犠牲陽極板6の内、自然電極電位の低い
犠牲陽極板6が陽極となり、アルミニウム部分5の腐食
を低減する。EXAMPLE As shown in FIGS. 1 to 3, the sacrificial anode plate 6 is fixed in a state of covering the exposed surface 3 of the aluminum conductor 2. The sacrificial anode plate 5 is made of a metal having a lower natural electrode potential than copper and aluminum, such as zinc, and covers the exposed surface 3, so that adhesion of the aqueous solution to the exposed surface 3 is prevented. When the aqueous solution adheres to and remains on the exposed surface 3, the sacrificial anode plate 6 having a low natural electrode potential among the copper 4 adhered to copper, the aluminum portion 5, and the sacrificial anode plate 6 serves as an anode to reduce corrosion of the aluminum portion 5.
【0009】[0009]
【発明の効果】本発明によってアルミニウム導体2の露
出面3に設けた犠牲陽極板6が、露出面3への水溶液の
付着滞留を防ぎ、アルミニウム導体2の露出面3のアル
ミニウム部分5の腐食を低減する。露出面3に水溶液が
付着滞留した場合は、犠牲陽極板6が陽極となり腐食し
アルミニウム部分5の腐食を低減する。これらの効果に
より接続部の劣化を防止できる。The sacrificial anode plate 6 provided on the exposed surface 3 of the aluminum conductor 2 according to the present invention prevents the aqueous solution from adhering to the exposed surface 3 and prevents corrosion of the aluminum portion 5 of the exposed surface 3 of the aluminum conductor 2. Reduce. When the aqueous solution adheres to and remains on the exposed surface 3, the sacrificial anode plate 6 serves as an anode and corrodes to reduce the corrosion of the aluminum portion 5. These effects can prevent the deterioration of the connection part.
【図1】本発明の実施例の導体接続部を示す平面図であ
る。FIG. 1 is a plan view showing a conductor connecting portion according to an embodiment of the present invention.
【図2】図1の側面図である。FIG. 2 is a side view of FIG.
【図3】図1のA−A断面図である。FIG. 3 is a sectional view taken along line AA of FIG. 1;
【図4】従来の導体接続部を示す平面図である。FIG. 4 is a plan view showing a conventional conductor connecting portion.
【図5】図4の側面図である。FIG. 5 is a side view of FIG.
【図6】図4のB−B断面図である。6 is a sectional view taken along line BB of FIG.
1 銅導体 2 アルミニウム導体 3 露出面 4 銅貼りの銅 5 アルミニウム部分 6 犠牲陽極板 1 Copper Conductor 2 Aluminum Conductor 3 Exposed Surface 4 Copper with Copper 5 Aluminum Part 6 Sacrificial Anode Plate
Claims (1)
て銅導体と接触する部分に銅貼りをしたアルミニウム導
体の銅とアルミニウムの境界露出部を、アルミニウムよ
り自然電極電位が低い金属よりなる犠牲陽極でもって覆
う状態で固定したアルミニウム導体−銅導体の接続部構
造。1. A sacrificial anode made of a metal having a natural electrode potential lower than that of aluminum is used as an exposed portion of a copper-aluminum boundary of an aluminum conductor having copper bonded to a portion in contact with the copper conductor in an aluminum conductor connected to the copper conductor. Connection structure of aluminum conductor-copper conductor fixed while covering.