JPH06336651A5 - - Google Patents
Info
- Publication number
- JPH06336651A5 JPH06336651A5 JP5-154380A JP15438093A JPH06336651A5 JP H06336651 A5 JPH06336651 A5 JP H06336651A5 JP 15438093 A JP15438093 A JP 15438093A JP H06336651 A5 JPH06336651 A5 JP H06336651A5
- Authority
- JP
- Japan
- Prior art keywords
- document
- procedural amendment
- less
- corrected
- wall thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15438093A JP2646061B2 (ja) | 1993-05-31 | 1993-05-31 | 高マンガン非磁性鋳造体 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15438093A JP2646061B2 (ja) | 1993-05-31 | 1993-05-31 | 高マンガン非磁性鋳造体 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH06336651A JPH06336651A (ja) | 1994-12-06 |
| JPH06336651A5 true JPH06336651A5 (enExample) | 1996-05-28 |
| JP2646061B2 JP2646061B2 (ja) | 1997-08-25 |
Family
ID=15582885
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15438093A Expired - Fee Related JP2646061B2 (ja) | 1993-05-31 | 1993-05-31 | 高マンガン非磁性鋳造体 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2646061B2 (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5480325B2 (ja) * | 2012-03-29 | 2014-04-23 | 株式会社日本製鋼所 | モータ回転子支持体およびその製造方法 |
| JP5480326B2 (ja) * | 2012-03-29 | 2014-04-23 | 株式会社日本製鋼所 | モータ回転子支持体およびその製造方法 |
| EP3452248B1 (en) * | 2016-05-02 | 2021-07-14 | ExxonMobil Research and Engineering Company | Field dissimilar metal welding technology for enhanced wear resistant high manganese steel |
-
1993
- 1993-05-31 JP JP15438093A patent/JP2646061B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0273279B1 (en) | Process for the production of a strip of a chromium stainless steel of a duplex structure having high strength and elongation as well as reduced plane anisotropy | |
| KR101054773B1 (ko) | Twip형 초고강도 강판의 제조방법 | |
| EP2034036B1 (en) | Wire rod having excellent wire drawability and its production method | |
| EP3561122A1 (en) | Austenite steel material having superb surface characteristic, and method for producing same | |
| KR101518571B1 (ko) | 고강도 및 고인성 비조질 선재 및 그 제조방법 | |
| JPH0625745A (ja) | 耐遅れ破壊特性の優れた機械構造用鋼の製造方法 | |
| JPS63162818A (ja) | プレス成形性のきわめて優れたフエライト系ステンレス鋼板の製造方法 | |
| JPH0314898B2 (enExample) | ||
| JPH0217608B2 (enExample) | ||
| JPH0254403B2 (enExample) | ||
| JP3137754B2 (ja) | 深絞り性の極めて優れた冷延鋼板の効率的な製造方法 | |
| JP3285055B2 (ja) | 成形機用シリンダ及びその製造方法 | |
| JPH0660345B2 (ja) | 冷間加工性にすぐれ,且つ,浸炭加熱時の結晶粒粗大化を防止した鋼の製造方法 | |
| JP4319879B2 (ja) | 面内異方性の小さな高炭素鋼板 | |
| JPS6244524A (ja) | 焼付硬化性および加工性の優れた冷延鋼板の製造方法 | |
| KR101543850B1 (ko) | 냉간압조성 및 피삭성이 우수한 흑연화 선재 및 이의 제조방법 | |
| JPH11335803A5 (enExample) | ||
| KR100711474B1 (ko) | 소부경화성이 우수한 열연강판의 제조방법 | |
| JPS61166922A (ja) | 浸炭用線材の製造方法 | |
| JPH05105961A5 (enExample) | ||
| KR100617931B1 (ko) | 고가공성 강관 및 그 제조방법 | |
| KR100554748B1 (ko) | 신선용 고강도 선재의 제조방법 | |
| JPH09155406A (ja) | 建築・橋梁用テーパプレートの製造方法 | |
| JPH1161274A (ja) | 焼付硬化性に優れる超深絞り用鋼板の製造方法 | |
| JPH07103420B2 (ja) | ボロン鋼板を素材とする部材の製造方法 |