JPH06212446A5 - - Google Patents
Info
- Publication number
- JPH06212446A5 JPH06212446A5 JP5-259512A JP25951293A JPH06212446A5 JP H06212446 A5 JPH06212446 A5 JP H06212446A5 JP 25951293 A JP25951293 A JP 25951293A JP H06212446 A5 JPH06212446 A5 JP H06212446A5
- Authority
- JP
- Japan
- Prior art keywords
- acid
- zinc
- pinhole
- containing surface
- pinhole prevention
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US964331 | 1992-10-21 | ||
| US07/964,331 US5300323A (en) | 1992-10-21 | 1992-10-21 | Reducing or avoiding pinhole formation in autodeposition on zinciferous surfaces |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH06212446A JPH06212446A (ja) | 1994-08-02 |
| JPH06212446A5 true JPH06212446A5 (enExample) | 2001-03-21 |
| JP3340209B2 JP3340209B2 (ja) | 2002-11-05 |
Family
ID=25508429
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP25951293A Expired - Fee Related JP3340209B2 (ja) | 1992-10-21 | 1993-10-18 | 亜鉛含有表面にピンホール形成が抑制された自己析出ポリマー被覆層を形成する方法、およびピンホール防止処理用組成物 |
Country Status (8)
| Country | Link |
|---|---|
| US (1) | US5300323A (enExample) |
| EP (1) | EP0665772B1 (enExample) |
| JP (1) | JP3340209B2 (enExample) |
| AU (1) | AU673025B2 (enExample) |
| BR (1) | BR9307283A (enExample) |
| CA (1) | CA2143668A1 (enExample) |
| DE (1) | DE69326558D1 (enExample) |
| WO (1) | WO1994008729A1 (enExample) |
Families Citing this family (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5700525A (en) * | 1995-03-29 | 1997-12-23 | Betzdearborn Inc. | Passivation method and composition for galvanized metal surfaces |
| US5868819A (en) * | 1996-05-20 | 1999-02-09 | Metal Coatings International Inc. | Water-reducible coating composition for providing corrosion protection |
| US6218342B1 (en) | 1996-08-02 | 2001-04-17 | M-I Llc | Oil-based drilling fluid |
| US5905061A (en) * | 1996-08-02 | 1999-05-18 | Patel; Avind D. | Invert emulsion fluids suitable for drilling |
| US5869130A (en) * | 1997-06-12 | 1999-02-09 | Mac Dermid, Incorporated | Process for improving the adhesion of polymeric materials to metal surfaces |
| DE19834226C1 (de) * | 1998-07-29 | 2000-02-10 | Excor Korrosionsforschung Gmbh | Dampfphasen-Korrosionsinhibitoren, Verfahren zu deren Herstellung und deren Verwendung |
| US6270884B1 (en) | 1999-08-02 | 2001-08-07 | Metal Coatings International Inc. | Water-reducible coating composition for providing corrosion protection |
| TW546413B (en) * | 2001-08-31 | 2003-08-11 | Lord Corp | Improved autodeposition metal dip coating process |
| US7935274B2 (en) * | 2005-03-25 | 2011-05-03 | Bulk Chemicals, Inc. | Phosphonic acid and polyvinyl alcohol conversion coating |
| WO2008069989A1 (en) * | 2006-12-01 | 2008-06-12 | Henkel Ag & Co. Kgaa | High peroxide autodeposition bath |
| WO2008069977A1 (en) * | 2006-12-01 | 2008-06-12 | HENKEL AG & CO. KGAaA | Acidic zincating solution |
| US7851655B2 (en) * | 2006-12-19 | 2010-12-14 | Nalco Company | Functionalized amine-based corrosion inhibitors for galvanized metal surfaces and method of using same |
| US8518493B2 (en) | 2009-01-06 | 2013-08-27 | Henkel Ag & Co. Kgaa | Co-cure process for autodeposition coating |
| US8512504B2 (en) | 2009-05-06 | 2013-08-20 | Steven A. Castaldi | Process for improving adhesion of polymeric materials to metal surfaces |
| US10323314B2 (en) | 2011-06-17 | 2019-06-18 | Henkel Ag & Co. Kgaa | Single bath autodeposition coating for combination metal substrates and methods therefor |
| EP3997167A1 (en) | 2019-07-12 | 2022-05-18 | Henkel AG & Co. KGaA | Single layer autodepositable coating formulation |
| CN114164430B (zh) * | 2021-11-30 | 2023-06-20 | 哈尔滨工业大学(深圳) | 一种金属缓蚀剂及其制备方法 |
Family Cites Families (15)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3592699A (en) * | 1966-06-01 | 1971-07-13 | Amchem Prod | Process and composition for coating metals |
| US3617368A (en) * | 1968-11-08 | 1971-11-02 | Dow Chemical Co | Process for preparing inherently colloidally stable interpolymers in aqueous dispersion and products coated therewith |
| US4093780A (en) * | 1972-08-21 | 1978-06-06 | Noranda Mines Limited | Treatment of zinc surfaces to inhibit wet storage staining and products employed therein |
| US3922451A (en) * | 1973-12-06 | 1975-11-25 | Dow Chemical Co | Coated beverage container and process of coating |
| US4108817A (en) * | 1976-12-30 | 1978-08-22 | Amchem Products, Inc. | Autodeposited coatings |
| US4199624A (en) * | 1976-12-30 | 1980-04-22 | Union Carbide Corporation | Treatment of substrate prior to autodeposition |
| US4178400A (en) * | 1976-12-30 | 1979-12-11 | Amchem Products, Inc. | Autodeposited coatings |
| FR2375915A1 (fr) * | 1976-12-30 | 1978-07-28 | Amchem Prod | Perfectionnements aux procedes pour la formation de revetements organiques sur des surfaces metalliques sans aide d'electricite |
| US4243704A (en) * | 1978-02-17 | 1981-01-06 | Amchem Products, Inc. | Autodeposition coating process |
| US4242379A (en) * | 1979-07-10 | 1980-12-30 | Amchem Products, Inc. | Acid inhibitor treatment of substrate prior to autodeposition |
| US4313861A (en) * | 1980-02-28 | 1982-02-02 | Union Carbide Corporation | Latex autodeposition coatings |
| US4647480A (en) * | 1983-07-25 | 1987-03-03 | Amchem Products, Inc. | Use of additive in aqueous cure of autodeposited coatings |
| RO95813B1 (ro) * | 1986-08-02 | 1988-10-31 | Institutul De Chimie | Compozitie pentru curatarea suprafetei sticloase |
| US5080937A (en) * | 1989-10-30 | 1992-01-14 | Henkel Corporation | Reducing or avoiding pinhole formation in autodeposition |
| US5248525A (en) * | 1991-01-24 | 1993-09-28 | Henkel Corporation | Treating an autodeposited coating with an alkaline solution containing anions of multifunctional organic acids |
-
1992
- 1992-10-21 US US07/964,331 patent/US5300323A/en not_active Expired - Fee Related
-
1993
- 1993-10-13 DE DE69326558T patent/DE69326558D1/de not_active Expired - Lifetime
- 1993-10-13 WO PCT/US1993/009549 patent/WO1994008729A1/en not_active Ceased
- 1993-10-13 CA CA002143668A patent/CA2143668A1/en not_active Abandoned
- 1993-10-13 AU AU53530/94A patent/AU673025B2/en not_active Ceased
- 1993-10-13 BR BR9307283A patent/BR9307283A/pt not_active Application Discontinuation
- 1993-10-13 EP EP93923788A patent/EP0665772B1/en not_active Expired - Lifetime
- 1993-10-18 JP JP25951293A patent/JP3340209B2/ja not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2002504697A5 (enExample) | ||
| DE69426419D1 (de) | Silylierte Polyamin-Polymere als Schmiermittel mit und ohne andere Komponenten, mit den Polymeren behandelte Substrate und Verfahren zur Behandlung der Substrate | |
| KR980005773A (ko) | 세정처리제 | |
| NZ503269A (en) | Composition containing hydrolysed aminosilane and a fluorine-containing inorganic compound | |
| JPH05247377A5 (enExample) | ||
| CA2161275A1 (en) | Water Repellent Surface Treatment for Plastic and Coated Plastic Substrates | |
| WO2003002698A3 (en) | High amount of beneficial components in the top of a substrates | |
| MX9606288A (es) | Vidrios recubiertos por deposicion catodica que reflejan los rayos infrarrojos, durables, tratables termicamente, adaptables y un metodo para fabricar los mismos. | |
| DE69612469D1 (de) | Verfahren zur Behandlung von Aluminiumlegierungen | |
| ATE195052T1 (de) | Beschichten von kupfer | |
| KR960009043A (ko) | 질화 규소의 에칭 방법 | |
| CA2061728A1 (en) | Self-lubricating device | |
| RU95106612A (ru) | Способ упрочнения и восстановления прочности хрупкой оксидной подложки, контейнер, способ частичного или полного исключения дефектов на поверхности, состав | |
| JPH0655137A5 (enExample) | ||
| IL141595A0 (en) | Method of removing organic materials from substrates | |
| ATE211780T1 (de) | Metallbehandlung mit saurer, seltene erden ionen enthaltenden reinigungslösungen | |
| ATE387187T1 (de) | Mikrogranulat auf wirkstoffbasis und verfahren zu seiner herstellung | |
| KR880001841A (ko) | 표면처리 방법 및 표면처리제 | |
| DE69601401D1 (de) | Überzugszusammensetzung zum Korrosionsschutz von Metallen | |
| EP0401791A3 (de) | Verfahren zur Speicherung von Informationen | |
| JPS57141496A (en) | Method for preventing putrefaction of metal working oil | |
| GB0027432D0 (en) | Treatment of a surface of a polymer | |
| JPS5622219A (en) | Manufacture of magnetic recording medium | |
| JPH1097084A5 (enExample) | ||
| DE60005910D1 (de) | Substrat mit behandelten Oberflächen und Verfahren zu seiner Herstellung |