JPH0564421B2 - - Google Patents
Info
- Publication number
- JPH0564421B2 JPH0564421B2 JP60190568A JP19056885A JPH0564421B2 JP H0564421 B2 JPH0564421 B2 JP H0564421B2 JP 60190568 A JP60190568 A JP 60190568A JP 19056885 A JP19056885 A JP 19056885A JP H0564421 B2 JPH0564421 B2 JP H0564421B2
- Authority
- JP
- Japan
- Prior art keywords
- nickel
- hydroxide
- cobalt
- nickel oxide
- charging
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/32—Nickel oxide or hydroxide electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/64—Carriers or collectors
- H01M4/70—Carriers or collectors characterised by shape or form
- H01M4/80—Porous plates, e.g. sintered carriers
- H01M4/808—Foamed, spongy materials
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60190568A JPS6251157A (ja) | 1985-08-29 | 1985-08-29 | ニツケル.カドミウムアルカリ蓄電池用陽極板の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60190568A JPS6251157A (ja) | 1985-08-29 | 1985-08-29 | ニツケル.カドミウムアルカリ蓄電池用陽極板の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6251157A JPS6251157A (ja) | 1987-03-05 |
JPH0564421B2 true JPH0564421B2 (enrdf_load_stackoverflow) | 1993-09-14 |
Family
ID=16260226
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60190568A Granted JPS6251157A (ja) | 1985-08-29 | 1985-08-29 | ニツケル.カドミウムアルカリ蓄電池用陽極板の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6251157A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0656762B2 (ja) * | 1986-03-12 | 1994-07-27 | 日本電池株式会社 | アルカリ蓄電池用ニツケル正極板 |
FR2670609B1 (fr) * | 1990-12-13 | 1995-07-07 | Sorapec | Electrode positive de nickel. |
-
1985
- 1985-08-29 JP JP60190568A patent/JPS6251157A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS6251157A (ja) | 1987-03-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4614696A (en) | Negative electrode plate for alkaline storage cells of sealed type | |
JP3387158B2 (ja) | 亜鉛極板 | |
JPH0564421B2 (enrdf_load_stackoverflow) | ||
JP2889669B2 (ja) | アルカリ蓄電池用非焼結式ニッケル正極板 | |
JP2615538B2 (ja) | アルカリ蓄電池用ニツケル正極 | |
JPS6269465A (ja) | ニツケル・カドミウムアルカリ蓄電池用陽極板 | |
JPH0429189B2 (enrdf_load_stackoverflow) | ||
JP4404447B2 (ja) | アルカリ蓄電池の製造方法 | |
JP2680642B2 (ja) | アルカリ蓄電池用亜鉛極の製造方法 | |
JPH06101350B2 (ja) | ニッケルカドミウムアルカリ蓄電池 | |
JP2000077067A (ja) | アルカリ蓄電池用正極 | |
JP2794825B2 (ja) | 水酸化ニッケル電極の化成方法 | |
JP3540558B2 (ja) | アルカリ蓄電池用水酸化ニッケル電極の製造方法とこの製造方法で得られた水酸化ニッケル電極 | |
JP2754800B2 (ja) | ニッケルカドミウム蓄電池 | |
JP2589750B2 (ja) | ニッケルカドミウム蓄電池 | |
JP4458749B2 (ja) | アルカリ蓄電池 | |
JP2926233B2 (ja) | アルカリ二次電池の製造方法 | |
JPS6188453A (ja) | アルカリ蓄電池用ニツケル正極 | |
JP3118357B2 (ja) | アルカリ蓄電池用非焼結正極板 | |
JPS61124060A (ja) | アルカリ蓄電池用ペ−スト式正極板 | |
JP2000106180A (ja) | アルカリ蓄電池用焼結式ニッケル電極の製造方法 | |
JPS612268A (ja) | 密閉型ニツケルカドミウム蓄電池の製造法 | |
JPH09245827A (ja) | アルカリ蓄電池の製造法 | |
JP2005183339A (ja) | アルカリ蓄電池用ニッケル極及びアルカリ蓄電池 | |
JPH04344B2 (enrdf_load_stackoverflow) |