JPH0537999U - Papermaking dryer canvas - Google Patents
Papermaking dryer canvasInfo
- Publication number
- JPH0537999U JPH0537999U JP8842491U JP8842491U JPH0537999U JP H0537999 U JPH0537999 U JP H0537999U JP 8842491 U JP8842491 U JP 8842491U JP 8842491 U JP8842491 U JP 8842491U JP H0537999 U JPH0537999 U JP H0537999U
- Authority
- JP
- Japan
- Prior art keywords
- canvas
- paper
- warp
- woven
- weft
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】
【目的】 扁平糸を経糸(2)として用いて二重織ある
いは多重織されたカンバスの両端の経糸(2)を折り返
して形成される接合用ループ(1)の接紙面(a)側へ
の膨らみを防止し、紙の表面平滑性が損なわれることを
防止する。
【構成】 扁平糸を経糸(2)として使用する二重織あ
るいは多重織組織の抄紙用ドライヤーカンバスにおい
て、両端の経糸(2)を折り返して接合用ループ(1)
を形成するに当って、接紙面(a)側の最終端緯糸(3
a)を挿入せずにカンバスの両端部を織成する。
(57) [Abstract] [Purpose] The paper-bonding surface of the joining loop (1) formed by folding back the warp yarns (2) at both ends of a double-woven or multi-woven canvas using a flat yarn as the warp yarn (2). It prevents bulging toward the (a) side and prevents the surface smoothness of the paper from being impaired. [Construction] In a dryer canvas for double-woven or multi-woven paper making, which uses flat yarns as warp yarns (2), the warp yarns (2) at both ends are folded back to form a joining loop (1).
In forming the final weft (3)
Weave both ends of the canvas without inserting a).
Description
【0001】[0001]
本考案は抄紙機のドライパートで使用される抄紙用ドライヤーカンバスに関す るものである。 The present invention relates to a paper machine dryer canvas used in the dry part of a paper machine.
【0002】[0002]
抄紙用ドライヤーカンバスを無端状に接合する手段は種々提案され、織り上っ たカンバスの両端部の緯糸を所定の幅に亘って除去し、すだれ状の経糸を作り、 この経糸をカンバス織組織内に織り込んで接合用ループを形成し、カンバスの両 端を突合わせ状態にした後、上記接合用ループ同士を噛み合わせ、その内部に芯 線を挿通する方法が一般に用いられている。扁平糸を経糸として使用したカンバ スにおいても同様な方法で接合用ループを形成することが考えられる。 Various means for joining endlessly the dryer canvas for papermaking have been proposed.The weft yarns at both ends of the woven canvas are removed over a specified width to form a comb-shaped warp, and this warp is incorporated into the canvas weave design. A method is generally used in which a joining loop is formed by weaving the joining loop, and both ends of the canvas are brought into abutment with each other, the joining loops are meshed with each other, and the core wire is inserted therein. It is conceivable to form a joining loop by the same method in a canvas using flat yarn as the warp.
【0003】 しかしながら、扁平糸の場合は、第2図に示すように、接紙面(a)側と機械 面(b)側とが非対称の組織においては、接合用ループ(1)を形成するために は、経糸(2)を180゜捩じる必要がある。However, in the case of the flat yarn, as shown in FIG. 2, in the structure in which the paper-contact surface (a) side and the machine-surface (b) side are asymmetric, the joining loop (1) is formed. It is necessary to twist the warp (2) 180 °.
【0004】[0004]
接合用ループ(1)を形成するために、経糸(2)を捩じると、扁平糸の捩れ が接紙面(a)側の最終端緯糸(3a)を接紙面(a)側に押す形になる。この ため、接合用ループ(1)が膨らみ接紙面(a)側に突出することになり、継手 部分の表面平滑性が得られなくなる。このため、上質紙や薄葉紙などの微妙な紙 肌を要求される紙に対しては、マークを発生する場合があった。 When the warp (2) is twisted to form the joining loop (1), the twist of the flat yarn pushes the final end weft (3a) on the paper-contacting surface (a) side toward the paper-contacting surface (a) side. become. Therefore, the joining loop (1) swells and protrudes toward the paper contact surface (a) side, and the surface smoothness of the joint portion cannot be obtained. For this reason, marks may be generated on paper that requires a delicate surface such as high-quality paper or thin paper.
【0005】[0005]
上記課題の解決手段として本考案は、扁平糸を経糸として二重織あるいは多重 織に織成された抄紙用ドライヤーカンバスであって、カンバスの両端部の経糸を 180゜捩り折り返して接合用ループを形成するに当って、接紙面側の最終端緯糸 を挿入せずに織成したことを特徴とする抄紙用ドライヤーカンバスを提供するも のである。 As a means for solving the above-mentioned problems, the present invention is a papermaking dryer canvas woven with a flat yarn as a warp in a double weave or a multiple weave, in which warp yarns at both ends of the canvas are twisted back by 180 ° to form a joining loop. It is intended to provide a dryer canvas for papermaking, which is formed by weaving without inserting the final end weft on the side of the paper contacting surface.
【0006】[0006]
カンバスの両端部で接紙面側の最終端緯糸を挿入せずにカンバスを織成するこ とにより、扁平な経糸を180゜捩り折り返して接合用ループを形成した場合、接 合用ループが膨らむことがなくなり、継手部が平滑となるため、紙にマークなど の悪影響を及ぼすことがなくなる。 When weaving a canvas at both ends of the canvas without inserting the final weft yarn on the paper contact side, when the flat warp is twisted back 180 ° to form a loop for joining, the loop for joining may swell. Since it disappears and the joint part becomes smooth, there is no adverse effect such as marks on the paper.
【0007】[0007]
図1は本考案の一実施例を示す抄紙用ドライヤーカンバスの端部拡大組織図で あって、経糸(2)には、0.30mm×0.56mmのテトロン(T−商標名−ポリエチレ ンテレフタレート繊維)モノフィラメント(TM030×056)の断面扁平な扁平糸 を使用し、緯糸(3)には、直径0.80mmのテトロンモノフィラメント(TM080 )を表裏2層にして二重綾組織で織成したもので、織密度は、経密度を54.7本/ 2.54cmとし、緯密度を16.0×2本/2.54cmとしている。 上記カンバスの両端部の経糸(2)は、接合用ループ(1)を形成させるもの と、形成させないものとを交互に或いは適宜の設定間隔で分け、接合用ループ( 1)を形成させないものは、そのまま折り返して元の組織へ綴り込み、カンバス 端部の緯糸(3)の脱落を防止させている。 FIG. 1 is an enlarged structural diagram of the edge of a papermaking dryer canvas showing an embodiment of the present invention. The warp (2) has a 0.30 mm × 0.56 mm tetron (T-trade name-polyethylene terephthalate fiber). A monofilament (TM030 × 056) is used, which is a flat yarn with a flat cross section. The weft yarn (3) is a double twill weave composed of two layers of Tetoron monofilament (TM080) with a diameter of 0.80 mm. Has a warp density of 54.7 strands / 2.54 cm and a weft density of 16.0 × 2 strands / 2.54 cm. The warp yarns (2) at both ends of the canvas are divided into those for forming the joining loop (1) and those for not forming the joining loop (1) alternately or at appropriate setting intervals so that the joining loop (1) is not formed. , It is folded back and stitched into the original tissue to prevent the weft thread (3) at the end of the canvas from falling off.
【0008】 しかして、接合用ループ(1)を形成させる経糸(2)は、そのまま折り返し て元の組織へ綴り込むことができないため、180゜捩れを与えて元の組織へ綴り 込まれる。この場合、本考案は、カンバスの接紙面(a)側の最終端緯糸(3a )を挿入することなくカンバスを織成しておくものである。このように、カンバ スの接紙面(a)側の最終端緯糸(3a)を挿入せずにカンバスを織成しておく と、接合用ループ(1)を形成するための緯糸(2)を180゜捩り折り返して元 の組織へ綴り込んでも、この経糸(2)の捩れ部分によって上記接紙面(a)側 の最終端緯糸(3a)が接紙面(a)側に押されることがなく、したがって、接 合用ループ(1)が膨らむことがなくなり、継手部が平滑となる。However, since the warp (2) forming the joining loop (1) cannot be folded back and stitched into the original tissue as it is, it is twisted by 180 ° and is stitched into the original tissue. In this case, according to the present invention, the canvas is woven without inserting the final weft (3a) on the paper contacting surface (a) side of the canvas. In this way, if the canvas is woven without inserting the final end weft (3a) on the paper contacting surface (a) side of the canvas, the weft (2) for forming the joining loop (1) is 180 °. Even when it is twisted back and bound into the original tissue, the twisted portion of the warp (2) does not push the final end weft (3a) on the paper contacting surface (a) side toward the paper contacting surface (a) side. The joining loop (1) will not swell and the joint will be smooth.
【0009】 上記実施例は、二重織の場合を例示したが、これ以外の多重織の場合にも同様 に適用するものである。Although the above-mentioned embodiments exemplify the case of the double weave, they are similarly applied to the case of the multiple weave other than this.
【0010】[0010]
本考案に係る抄紙用カンバスは、接合用ループが膨らむことがないので、継手 部分が平滑となり、紙にマークなどの悪影響を及ぼすことがなくなる効果がある 。 In the papermaking canvas according to the present invention, since the joining loop does not swell, the joint portion becomes smooth and there is an effect that a mark or the like is not adversely affected on the paper.
【提出日】平成4年7月23日[Submission date] July 23, 1992
【手続補正2】[Procedure Amendment 2]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0004[Correction target item name] 0004
【補正方法】変更[Correction method] Change
【0004】[0004]
一般的に接紙面(a)側と機械面(b)側とが非対称の組織においては、接紙 面(a)側の最終端緯糸(3a)部が接紙面(a)側に突出する傾向がある。こ の突出は非対称組織のカンバス接合用ループ部における組織上の持つ欠点である 。特に経糸(2)に偏平糸を用いたカンバスでは、接紙面(a)側への突出が著 しい。接合用ループ(1)を形成するために、経糸(2)を捩じると、扁平糸の 捩れが接紙面(a)側の最終端緯糸(3a)を接紙面(a)側に押す形になる。 このため、接合用ループ(1)が膨らみ接紙面(a)側に突出することになり、 継手部分の表面平滑性が得られなくなる。このため、上質紙や薄葉紙などの微妙 な紙肌を要求される紙に対しては、マークを発生する場合があった。 Generally, in a design in which the paper-contacting surface (a) side and the machine-surface (b) side are asymmetric, the final end weft (3a) portion on the paper-contacting surface (a) side tends to protrude toward the paper-contacting surface (a) side. There is. This protrusion is a tissue defect in the loop for joining the asymmetric tissue canvas. Particularly in a canvas using a flat yarn as the warp yarn (2), the protrusion toward the paper contact surface (a) side is remarkable. When the warp (2) is twisted to form the joining loop (1), the twist of the flat yarn pushes the final end weft (3a) on the paper-contacting surface (a) side toward the paper-contacting surface (a) side. become. For this reason, the joining loop (1) bulges and projects toward the paper contact surface (a) side, and the surface smoothness of the joint portion cannot be obtained. For this reason, marks may be generated on paper that requires a delicate surface such as high-quality paper and thin paper.
【手続補正3】[Procedure 3]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0005[Correction target item name] 0005
【補正方法】変更[Correction method] Change
【0005】[0005]
上記課題の解決手段として本考案は、扁平糸を経糸として二重織あるいは多重 織に織成された抄紙用ドライヤーカンバスであって、カンバスの両端部の経糸を 180°捩り折り返して接合用ループを形成するに当って、接紙面側の最終端糸 となる緯糸を用いずに織成したことを特徴とする抄紙用ドライヤーカンバスを提 供するものである。 As a means for solving the above problems, the present invention is a papermaking dryer canvas woven with a flat yarn as a warp in a double weave or a multiple weave, in which warp yarns at both ends of the canvas are twisted back by 180 ° to form a joining loop. The present invention provides a dryer canvas for papermaking, which is characterized by being woven without using a weft that is the final end yarn on the paper contact side.
【手続補正4】[Procedure amendment 4]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0006[Correction target item name] 0006
【補正方法】変更[Correction method] Change
【0006】[0006]
カンバスの両端部で接紙面側の最終端糸となる緯糸を用いずにカンバスを織成 することにより、扁平な経糸を180°捩り折り返して接合用ループを形成した 場合、接合用ループが膨らむことがなくなり、継手部が平滑となるため、紙にマ ークなどの悪影響を及ぼすことがなくなる。 When weaving the canvas without using the weft that becomes the final end yarn on the paper contact side at both ends of the canvas, when the flat warp is twisted back 180 ° to form the joining loop, the joining loop should swell. Is eliminated and the joint becomes smooth, so there is no adverse effect such as marking on the paper.
【手続補正5】[Procedure Amendment 5]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】0008[Correction target item name] 0008
【補正方法】変更[Correction method] Change
【0008】 しかして、接合用ループ(1)を形成させる経糸(2)は 、そのまま折り返して元の組織へ綴り込むことができないため、180°捩れを 与えて元の組織へ綴り込まれる。この場合、本考案は、カンバスの接紙面(a) 側の最終端糸となる緯糸(3a)を用いることなくカンバスを織成しておくもの である。このように、カンバスの接紙面(a)側の最終端糸となる緯糸(3a) を用いずにカンバスを織成しておくと、接合用ループ(1)を形成するための経 糸(2)を180°捩り折り返して元の組織へ綴り込んでも、この経糸(2)の 捩れ部分によって上記接紙面(a)側の最終端緯糸(3a)が接紙面(a)側に 押されることがなく、したがって、接合用ループ(1)が膨らむことがなくなり 、継手部が平滑となる。However, the warp yarn (2) forming the joining loop (1) cannot be folded back and stitched into the original tissue as it is, and therefore is twisted by 180 ° and stitched into the original tissue. In this case, the present invention is to weave the canvas without using the weft thread (3a) which is the final end thread on the paper contact surface (a) side of the canvas. In this way, when the canvas is woven without using the weft thread (3a) which is the final end thread on the paper contacting surface (a) side of the canvas, the warp thread (2) for forming the joining loop (1) is formed. Even when it is twisted back by 180 ° and stitched into the original tissue, the twisted portion of the warp (2) does not push the final end weft (3a) on the paper contact surface (a) side toward the paper contact surface (a) side. Therefore, the joining loop (1) does not swell and the joint portion becomes smooth.
【図1】本考案の一実施例を示す抄紙用ドライヤーカン
バスの端部拡大組織図FIG. 1 is an enlarged organization chart of the edge of a papermaking dryer canvas showing an embodiment of the present invention.
【図2】抄紙用ドライヤーカンバス従来例を示す組織図[Fig. 2] Organization chart showing a conventional example of a paper dryer dryer canvas.
1 接合用ループ 2 経糸 3 緯糸 3a 接紙面側の最終端緯糸 a 接紙面 1 Loop for joining 2 Warp 3 Weft 3a Final end weft on the side of the paper surface a Paper contact surface
─────────────────────────────────────────────────────
─────────────────────────────────────────────────── ───
【手続補正書】[Procedure amendment]
【提出日】平成4年7月23日[Submission date] July 23, 1992
【手続補正1】[Procedure Amendment 1]
【補正対象書類名】明細書[Document name to be amended] Statement
【補正対象項目名】実用新案登録請求の範囲[Item name to be amended] Scope of utility model registration request
【補正方法】変更[Correction method] Change
【補正内容】[Correction content]
【実用新案登録請求の範囲】[Scope of utility model registration request]
Claims (1)
織に織成された抄紙用ドライヤーカンバスであって、カ
ンバスの両端部の経糸を180゜捩り折り返して接合用ル
ープを形成するに当って、接紙面側の最終端緯糸を挿入
せずに織成したことを特徴とする抄紙用ドライヤーカン
バス。1. A dryer canvas for papermaking, which is woven in a double weave or a multiple weave using flat yarns as warp yarns, wherein the warp yarns at both ends of the canvas are twisted back by 180 ° to form a joining loop. A dryer canvas for papermaking, characterized by being woven without inserting the final end weft on the paper-contacting surface side.