JPH0468385B2 - - Google Patents
Info
- Publication number
- JPH0468385B2 JPH0468385B2 JP60045899A JP4589985A JPH0468385B2 JP H0468385 B2 JPH0468385 B2 JP H0468385B2 JP 60045899 A JP60045899 A JP 60045899A JP 4589985 A JP4589985 A JP 4589985A JP H0468385 B2 JPH0468385 B2 JP H0468385B2
- Authority
- JP
- Japan
- Prior art keywords
- stainless steel
- treated
- article
- sputtering
- tin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Physical Vapour Deposition (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4589985A JPS61204367A (ja) | 1985-03-08 | 1985-03-08 | TiN被覆ステンレス鋼物品の製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4589985A JPS61204367A (ja) | 1985-03-08 | 1985-03-08 | TiN被覆ステンレス鋼物品の製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61204367A JPS61204367A (ja) | 1986-09-10 |
| JPH0468385B2 true JPH0468385B2 (cs) | 1992-11-02 |
Family
ID=12732088
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4589985A Granted JPS61204367A (ja) | 1985-03-08 | 1985-03-08 | TiN被覆ステンレス鋼物品の製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61204367A (cs) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR2762619B1 (fr) * | 1997-04-24 | 1999-07-02 | Univ Nantes | Procede de formation d'une couche d'un nitrure, en particulier d'un nitrure de bore, a la surface d'un substrat |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5613510A (en) * | 1979-07-16 | 1981-02-09 | Tdk Corp | Magnetic head and its manufacture |
-
1985
- 1985-03-08 JP JP4589985A patent/JPS61204367A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61204367A (ja) | 1986-09-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US3878079A (en) | Method of producing thin tantalum films | |
| JP2892231B2 (ja) | Ti−Si−N系複合硬質膜及びその製造方法 | |
| TW318949B (cs) | ||
| US5217589A (en) | Method of adherent metal coating for aluminum nitride surfaces | |
| US4803094A (en) | Metallized coating | |
| JPH0468385B2 (cs) | ||
| US5024721A (en) | Method of forming metal surface thin film having high corrosion resistance and high adhesion | |
| JP3078853B2 (ja) | 酸化膜形成方法 | |
| JPH0860347A (ja) | 誘電体薄膜堆積方法 | |
| JP3727693B2 (ja) | TiN膜製造方法 | |
| JP3792738B2 (ja) | 表面プラスモン共鳴分析用担体の製造方法 | |
| JPH02156066A (ja) | 基材のクリーニング方法 | |
| JPS63161156A (ja) | 硬質青色薄膜およびその製造方法 | |
| JPS6362862A (ja) | Ti及びTi合金のTiN被覆品の製造方法 | |
| JPS6320444A (ja) | イオンプレ−テイング | |
| JPH03226561A (ja) | カラーコーティング方法 | |
| JP3243319B2 (ja) | 有機質基材表面のメタライズ方法 | |
| JPH089767B2 (ja) | 低抵抗透明導電膜の製造方法 | |
| US5523166A (en) | Process for forming thin film having excellent insulating property and metallic substrate coated with insulating material formed by said process | |
| JPH01172563A (ja) | 高純度膜の形成方法 | |
| JP2957620B2 (ja) | 均一色度のTiN膜とその形成方法 | |
| KR100237166B1 (ko) | 이온빔을 이용한 TiN박막의 코팅방법 | |
| JPH05320872A (ja) | 耐食性被膜付き金属物品及びその製造方法 | |
| JPH05190309A (ja) | 抵抗体膜の製造方法 | |
| JPS6318053A (ja) | 有色薄膜の生成方法 |