JPH043800B2 - - Google Patents
Info
- Publication number
- JPH043800B2 JPH043800B2 JP6230087A JP6230087A JPH043800B2 JP H043800 B2 JPH043800 B2 JP H043800B2 JP 6230087 A JP6230087 A JP 6230087A JP 6230087 A JP6230087 A JP 6230087A JP H043800 B2 JPH043800 B2 JP H043800B2
- Authority
- JP
- Japan
- Prior art keywords
- film
- weight
- metal
- lubricant
- oxalate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Lubricants (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6230087A JPS63227699A (ja) | 1987-03-17 | 1987-03-17 | 高ニッケル系合金鋼の塑性加工用潤滑処理方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6230087A JPS63227699A (ja) | 1987-03-17 | 1987-03-17 | 高ニッケル系合金鋼の塑性加工用潤滑処理方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63227699A JPS63227699A (ja) | 1988-09-21 |
| JPH043800B2 true JPH043800B2 (enExample) | 1992-01-24 |
Family
ID=13196133
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6230087A Granted JPS63227699A (ja) | 1987-03-17 | 1987-03-17 | 高ニッケル系合金鋼の塑性加工用潤滑処理方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63227699A (enExample) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5974920A (en) | 1996-12-27 | 1999-11-02 | Kabushiki Kaisha Matsuo Kogyo Sho | Method for lathing stock |
| JP4414125B2 (ja) * | 2002-05-22 | 2010-02-10 | 出光興産株式会社 | 冷間圧延油組成物 |
| JP2006143988A (ja) * | 2004-10-20 | 2006-06-08 | Yushiro Chem Ind Co Ltd | 塑性加工用潤滑被膜、塑性加工用潤滑被膜形成用組成物、塑性加工用素材、塑性加工品の製造方法並びに金属管、金属線又は金属棒の製造方法 |
-
1987
- 1987-03-17 JP JP6230087A patent/JPS63227699A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS63227699A (ja) | 1988-09-21 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP3517522B2 (ja) | 金属材料の冷間塑性加工用水系潤滑剤 | |
| JP4271573B2 (ja) | ヘッダー加工用金属線材の製造方法 | |
| TWI457431B (zh) | 將金屬表面施以一種潤滑劑組成物的方法 | |
| KR100621693B1 (ko) | 금속 재료의 소성 가공용 수성 윤활제 및 윤활피막의 처리방법 | |
| CN101983234B (zh) | 用含有蜡的润滑剂组合物涂覆金属表面的方法 | |
| JP5224251B2 (ja) | 金属材料の水性塑性加工用潤滑剤組成物 | |
| KR100621692B1 (ko) | 금속 재료의 소성 가공용 수성 윤활제 및 윤활피막의 형성방법 | |
| US5837658A (en) | Metal forming lubricant with differential solid lubricants | |
| JPWO2002012419A1 (ja) | 金属材料塑性加工用水系潤滑剤および潤滑皮膜の処理方法 | |
| JPS638489A (ja) | 金属の冷間加工用潤滑剤 | |
| US5614482A (en) | Lubricant composition for treatment of non-ferrous metals and process using same | |
| JPH043800B2 (enExample) | ||
| JPS62241994A (ja) | 金属材料の冷間塑性加工用油状潤滑剤 | |
| US4755309A (en) | Cold working lubricant for metallic conduits | |
| JP4939172B2 (ja) | 塑性加工用水溶性潤滑剤、塑性加工用金属材および金属加工品 | |
| JP2002361302A (ja) | 金属材料板の圧延方法 | |
| JPS6281221A (ja) | 冷間塑性加工金属製品の製造方法 | |
| JPS62153396A (ja) | 金属引抜加工用潤滑剤およびそれを使用する引抜加工方法 | |
| JPH0448839B2 (enExample) | ||
| RU2497936C2 (ru) | Смазка технологическая для обработки металлов давлением (варианты) | |
| JPH08253780A (ja) | 成形加工用潤滑処理アルミニウム板材 | |
| JPH0631378B2 (ja) | アルミニウム又はアルミニウム合金の冷間加工用潤滑剤及びそれを用いた該金属の冷間加工方法 | |
| CN121022484A (zh) | 具有润滑效果的组合物以及润滑剂 | |
| RU2219007C1 (ru) | Смазка для холодной деформации металлов | |
| JPS62236896A (ja) | 鉄又はその合金の冷間引抜き潤滑方法 |