JPH04128407A - Method for heating rubber and asphalt for melt fusion and manufacture of paving construction material - Google Patents

Method for heating rubber and asphalt for melt fusion and manufacture of paving construction material

Info

Publication number
JPH04128407A
JPH04128407A JP25210390A JP25210390A JPH04128407A JP H04128407 A JPH04128407 A JP H04128407A JP 25210390 A JP25210390 A JP 25210390A JP 25210390 A JP25210390 A JP 25210390A JP H04128407 A JPH04128407 A JP H04128407A
Authority
JP
Japan
Prior art keywords
asphalt
construction material
rubber
paving construction
manufacture
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP25210390A
Other languages
Japanese (ja)
Inventor
Moritomo Oosumi
大住 盛智
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP25210390A priority Critical patent/JPH04128407A/en
Publication of JPH04128407A publication Critical patent/JPH04128407A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To obtain the paving construction material comprising both the characteristics of rubber and asphalt by mixing rubber and asphalt at a predetermined ratio for melting, and thereafter, molding it into a desired-shape paving construction material. CONSTITUTION:Rubber and asphalt are mixed and melted, and thereafter, it is molded by mold-cooling to form the paving construction material. A mixture ratio thereof is changed at the time of melting to obtain respective characteristics of rubber and asphalt. The paving construction material to be required for the water-proof material, a shock resistant member and a traffic safety equipment or the like can be thereby manufactured.

Description

【発明の詳細な説明】 本発明はゴムとアスファルトをおのおの加熱溶解して融
合させ、さらに成型冷却して舗装建材を製造する方法で
ある。
DETAILED DESCRIPTION OF THE INVENTION The present invention is a method of producing a paving building material by heating and melting rubber and asphalt to fuse them together, and then molding and cooling them.

従来、ゴムやアスファルトを原料とする舗装建材はあっ
た。しかし各々には粘着性、弾力性柔軟性、摩耗性そし
て耐熱性などに欠点があった。また製造価格や使用後の
廃棄処理の点でも問題はあった。
In the past, there were paving construction materials made from rubber or asphalt. However, each had drawbacks such as adhesion, elasticity, abrasion resistance, and heat resistance. There were also problems in terms of manufacturing cost and disposal after use.

本発明は以」ユの欠点を解決する為のものであって、ゴ
ムの特質とアスファル1〜の特質を引き出し粘着性、弾
力性、柔軟性、摩耗性、耐熱性経済性について解決でき
るものである。
The present invention is intended to solve the following drawbacks, and can solve the problems of adhesiveness, elasticity, flexibility, abrasion resistance, heat resistance, and economy by drawing out the characteristics of rubber and the characteristics of asphalt. be.

更に廃棄物処理に苦慮している古タイヤや廃棄アスファ
ル1〜を再生原料とすれば省資源化につながり、資源の
再生と活用がはかれるものである。
Furthermore, if old tires and waste asphalt 1~, which are difficult to dispose of, are used as recycled raw materials, it will lead to resource conservation and the recycling and utilization of resources.

ゴムとアスファルトの混合の割合を変えることにより、
防水材、緩衝材および交通安全器材等にも利用できる。
By changing the mixing ratio of rubber and asphalt,
It can also be used for waterproofing materials, cushioning materials, traffic safety equipment, etc.

Claims (1)

【特許請求の範囲】[Claims] ゴムとアスファルトを加熱溶解融合し、更に成型冷却し
て舗装建材を製造する方法
A method of manufacturing pavement construction materials by heating, melting, and fusion of rubber and asphalt, then molding and cooling.
JP25210390A 1990-09-18 1990-09-18 Method for heating rubber and asphalt for melt fusion and manufacture of paving construction material Pending JPH04128407A (en)