JPH0366384B2 - - Google Patents
Info
- Publication number
- JPH0366384B2 JPH0366384B2 JP6514485A JP6514485A JPH0366384B2 JP H0366384 B2 JPH0366384 B2 JP H0366384B2 JP 6514485 A JP6514485 A JP 6514485A JP 6514485 A JP6514485 A JP 6514485A JP H0366384 B2 JPH0366384 B2 JP H0366384B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- content
- sscc
- less
- resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6514485A JPS61223166A (ja) | 1985-03-29 | 1985-03-29 | 耐硫化物応力腐食割れ性に優れた高強度鋼 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6514485A JPS61223166A (ja) | 1985-03-29 | 1985-03-29 | 耐硫化物応力腐食割れ性に優れた高強度鋼 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61223166A JPS61223166A (ja) | 1986-10-03 |
| JPH0366384B2 true JPH0366384B2 (enExample) | 1991-10-17 |
Family
ID=13278392
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6514485A Granted JPS61223166A (ja) | 1985-03-29 | 1985-03-29 | 耐硫化物応力腐食割れ性に優れた高強度鋼 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61223166A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2006037147A (ja) | 2004-07-26 | 2006-02-09 | Sumitomo Metal Ind Ltd | 油井管用鋼材 |
| JP5839465B2 (ja) | 2011-12-22 | 2016-01-06 | 曙ブレーキ工業株式会社 | 球状黒鉛鋳鉄の製造方法および球状黒鉛鋳鉄部材の製造方法 |
-
1985
- 1985-03-29 JP JP6514485A patent/JPS61223166A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS61223166A (ja) | 1986-10-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| AU2006282411B2 (en) | Seamless steel pipe for line pipe and method for its manufacture | |
| CN101542002B (zh) | 低合金钢、油井用无缝钢管和无缝钢管的制造方法 | |
| KR101011072B1 (ko) | 고강도 후강판 및 그 제조 방법 | |
| JP2003193204A (ja) | マルテンサイト系ステンレス鋼 | |
| JP2001271134A (ja) | 耐硫化物応力割れ性と靱性に優れた低合金鋼材 | |
| JPS6354765B2 (enExample) | ||
| CN113584407A (zh) | 一种高强度耐高温腐蚀马氏体不锈钢及其制造方法 | |
| JPH0967624A (ja) | 耐sscc性に優れた高強度油井用鋼管の製造方法 | |
| JPS61270355A (ja) | 耐遅れ破壊性の優れた高強度鋼 | |
| CN1138880A (zh) | 具有良好焊接性和耐蚀性的马氏体不锈钢及其制造方法 | |
| WO2022181164A1 (ja) | 油井用高強度ステンレス継目無鋼管およびその製造方法 | |
| EP3330398B1 (en) | Steel pipe for line pipe and method for manufacturing same | |
| JPH05287381A (ja) | 高強度耐食性鋼管の製造方法 | |
| JPS634046A (ja) | 耐硫化物割れ性に優れた高張力油井用鋼 | |
| JP2861024B2 (ja) | 油井用マルテンサイト系ステンレス鋼材とその製造方法 | |
| CN114086083B (zh) | 一种1100MPa级抗硫高压气瓶钢、高压气瓶及其制造方法 | |
| JPH06271975A (ja) | 耐水素脆化特性に優れた高強度鋼およびその製法 | |
| JPS6164815A (ja) | 耐遅れ破壊性の優れた高強度鋼の製造法 | |
| JPS648686B2 (enExample) | ||
| JPH0366384B2 (enExample) | ||
| JP3666388B2 (ja) | マルテンサイト系ステンレス継目無鋼管 | |
| JPH0741855A (ja) | 細粒フェライト主体の金属組織を呈した低降伏比高靭性継目無鋼管の製造法 | |
| JPS61227129A (ja) | 耐硫化物応力腐食割れ性に優れた高強度鋼の製造方法 | |
| JPH0375336A (ja) | 耐食性の優れたマルテンサイト系ステンレス鋼およびその製造方法 | |
| JPS644566B2 (enExample) |