JPH0355030B2 - - Google Patents

Info

Publication number
JPH0355030B2
JPH0355030B2 JP60189139A JP18913985A JPH0355030B2 JP H0355030 B2 JPH0355030 B2 JP H0355030B2 JP 60189139 A JP60189139 A JP 60189139A JP 18913985 A JP18913985 A JP 18913985A JP H0355030 B2 JPH0355030 B2 JP H0355030B2
Authority
JP
Japan
Prior art keywords
cadmium
electrode plate
negative electrode
paste
intramolecular
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP60189139A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6247960A (ja
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP60189139A priority Critical patent/JPS6247960A/ja
Publication of JPS6247960A publication Critical patent/JPS6247960A/ja
Publication of JPH0355030B2 publication Critical patent/JPH0355030B2/ja
Granted legal-status Critical Current

Links

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/62Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
    • H01M4/00Electrodes
    • H01M4/02Electrodes composed of, or comprising, active material
    • H01M4/24Electrodes for alkaline accumulators
    • H01M4/26Processes of manufacture
    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries

Landscapes

  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • General Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Manufacturing & Machinery (AREA)
  • Battery Electrode And Active Subsutance (AREA)
JP60189139A 1985-08-27 1985-08-27 アルカリ蓄電池用カドミウム負極板の製造法 Granted JPS6247960A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP60189139A JPS6247960A (ja) 1985-08-27 1985-08-27 アルカリ蓄電池用カドミウム負極板の製造法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP60189139A JPS6247960A (ja) 1985-08-27 1985-08-27 アルカリ蓄電池用カドミウム負極板の製造法

Publications (2)

Publication Number Publication Date
JPS6247960A JPS6247960A (ja) 1987-03-02
JPH0355030B2 true JPH0355030B2 (enrdf_load_stackoverflow) 1991-08-22

Family

ID=16236062

Family Applications (1)

Application Number Title Priority Date Filing Date
JP60189139A Granted JPS6247960A (ja) 1985-08-27 1985-08-27 アルカリ蓄電池用カドミウム負極板の製造法

Country Status (1)

Country Link
JP (1) JPS6247960A (enrdf_load_stackoverflow)

Also Published As

Publication number Publication date
JPS6247960A (ja) 1987-03-02

Similar Documents

Publication Publication Date Title
JPH0350384B2 (enrdf_load_stackoverflow)
JPH0355030B2 (enrdf_load_stackoverflow)
CN110993897A (zh) 一种提高阀控式密封铅酸电池使用寿命的正极添加剂及其应用
JPH0424823B2 (enrdf_load_stackoverflow)
JPS6149374A (ja) アルカリ蓄電池用ニツケル正極
JPH041992B2 (enrdf_load_stackoverflow)
JPS61203566A (ja) アルカリ蓄電池用カドミウム負極板の製造法
JPH0619987B2 (ja) アルカリ蓄電池用カドミウム負極板の製造法
JP3287165B2 (ja) アルカリ蓄電池用ニッケル正極の製造法
JPS61124060A (ja) アルカリ蓄電池用ペ−スト式正極板
JPH0554221B2 (enrdf_load_stackoverflow)
JP2553624B2 (ja) ペースト式カドミウム負極
JPH0824041B2 (ja) ニッケル極板の製造法
JPH0555982B2 (enrdf_load_stackoverflow)
JP2642623B2 (ja) アルカリ蓄電池用非焼結式カドミウム陰極
JPS5848990B2 (ja) アルカリ蓄電池用カドミウム陰極板の製法
JPS63164162A (ja) アルカリ蓄電池用カドミウム負極
JPH0724216B2 (ja) アルカリ蓄電池用非焼結式カドミウム陰極
JPH041466B2 (enrdf_load_stackoverflow)
JPH07105232B2 (ja) 非水電解液二次電池およびそれに用いる正極活物質の製造方法
JPH0569264B2 (enrdf_load_stackoverflow)
JPS6191873A (ja) アルカリ蓄電池用カドミウム負極板の製造法
JPS63148549A (ja) アルカリ蓄電池用カドミウム負極板及びその製造方法
JPS6113564A (ja) カドミウム負極板の製造方法
JPH0685327B2 (ja) アルカリ蓄電池用カドミウム負極板の製造法

Legal Events

Date Code Title Description
LAPS Cancellation because of no payment of annual fees