JPH0258221B2 - - Google Patents
Info
- Publication number
- JPH0258221B2 JPH0258221B2 JP57066108A JP6610882A JPH0258221B2 JP H0258221 B2 JPH0258221 B2 JP H0258221B2 JP 57066108 A JP57066108 A JP 57066108A JP 6610882 A JP6610882 A JP 6610882A JP H0258221 B2 JPH0258221 B2 JP H0258221B2
- Authority
- JP
- Japan
- Prior art keywords
- quicklime
- water
- nitrate
- added
- mixture
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Compounds Of Alkaline-Earth Elements, Aluminum Or Rare-Earth Metals (AREA)
- Soil Conditioners And Soil-Stabilizing Materials (AREA)
- Curing Cements, Concrete, And Artificial Stone (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6610882A JPS58185458A (ja) | 1982-04-20 | 1982-04-20 | 生石灰の消化促進方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP6610882A JPS58185458A (ja) | 1982-04-20 | 1982-04-20 | 生石灰の消化促進方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58185458A JPS58185458A (ja) | 1983-10-29 |
| JPH0258221B2 true JPH0258221B2 (cg-RX-API-DMAC7.html) | 1990-12-07 |
Family
ID=13306358
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP6610882A Granted JPS58185458A (ja) | 1982-04-20 | 1982-04-20 | 生石灰の消化促進方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58185458A (cg-RX-API-DMAC7.html) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE4034417C2 (de) * | 1990-10-29 | 2002-02-07 | Walhalla Kalk Entwicklungs Und | Hochreaktive Reagentien und Zusammensetzungen für die Abgas- und Abwasserreinigung, ihre Herstellung und ihre Verwendung |
| US5348583A (en) * | 1992-01-28 | 1994-09-20 | W. R. Grace & Co.-Conn. | Hydraulic cement set-accelerating admixtures incorporating glycols |
| CA2086648C (en) * | 1992-01-28 | 1999-03-23 | Ahmad Arfaei | Hydraulic cement set-accelerating admixtures incorporating glycols |
| JP4862812B2 (ja) * | 2007-12-11 | 2012-01-25 | 株式会社イトーキ | 歯付ベルトの連結装置 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS58135161A (ja) * | 1982-02-04 | 1983-08-11 | 大阪セメント株式会社 | 高温焼成石灰の消化促進方法 |
-
1982
- 1982-04-20 JP JP6610882A patent/JPS58185458A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58185458A (ja) | 1983-10-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Gillott et al. | Mechanism of the alkali-carbonate rock reaction | |
| Chen et al. | The carbon uptake and mechanical property of cemented paste backfill carbonation curing for low concentration of CO2 | |
| Jin et al. | Effects of different reactive MgOs on the hydration of MgO-activated GGBS paste | |
| Jun et al. | Chloride-bearing characteristics of alkali-activated slag mixed with seawater: Effect of different salinity levels | |
| JP4913303B2 (ja) | 反応性酸化マグネシウムセメント | |
| Liu et al. | Hydration and material properties of blended cement with ground desert sand | |
| Jin et al. | Effect of different MgO on the hydration of MgO-activated granulated ground blastfurnace slag paste | |
| Fu et al. | Durability and mechanism of high-salt resistance concrete exposed to sewage-contaminated seawater | |
| JPH0379394B2 (cg-RX-API-DMAC7.html) | ||
| Dai et al. | Preparation and properties of hydrotalcite-foamed magnesium phosphate cement for fire protection of steel structures | |
| GB2067176A (en) | Demolition-facilitating substance | |
| JP4107825B2 (ja) | スラグ系注入材スラリー | |
| JPH0258221B2 (cg-RX-API-DMAC7.html) | ||
| JP4498560B2 (ja) | セメント急結剤 | |
| CN113173725A (zh) | 一种高效混凝土膨胀抗裂防水剂及其制备方法 | |
| Fu et al. | Synthesis of low-carbon ternary slag-based binder for cemented tailings backfill: Effect of slag and activator characteristics | |
| Cheng et al. | Performance analysis and mechanistic insights of penetrating crystalline self-healing cement (PCSHC) in dynamically sealing borehole cracks | |
| Bilginer et al. | Enhancing magnesium oxalate cements with copper slag and silica fume | |
| Liu et al. | Sulfate attack on portland-dolomite cement exposed to sodium sulfate solution at 5℃ and 20℃ | |
| Zhang et al. | Effect of calcined dolomite addition on sodium carbonate-activated slag cements with different curing methods | |
| JP4657417B2 (ja) | セメント急結剤 | |
| Kızıltepe et al. | Development of one-part geopolymer binder produced from alkali fused boron mine tailings | |
| Rovnanik | Influence of C 12 A 7 admixture on setting properties of fly ash geopolymer | |
| Rizk et al. | Preparation and Characterization of Low Cost Geopolymer Cement | |
| Balinee et al. | Use of discarded aluminium foil in cementitious material as fire retardant-An experimental study |