JPH02149904A - Production of composite type magnetic head - Google Patents
Production of composite type magnetic headInfo
- Publication number
- JPH02149904A JPH02149904A JP30446188A JP30446188A JPH02149904A JP H02149904 A JPH02149904 A JP H02149904A JP 30446188 A JP30446188 A JP 30446188A JP 30446188 A JP30446188 A JP 30446188A JP H02149904 A JPH02149904 A JP H02149904A
- Authority
- JP
- Japan
- Prior art keywords
- core
- core block
- joint surface
- depositing
- thin metallic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【発明の詳細な説明】
〔産業上の利用分野〕
本発明は、一対のコアブロックを接合したときに、均一
な磁気ギャップを形成するようにした複合型磁気ヘッド
の製造方法に関する。DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a method of manufacturing a composite magnetic head in which a uniform magnetic gap is formed when a pair of core blocks are joined.
磁気ヘッドは、従来、フェライトからなるコアチップで
形成していた。フェライトは、強磁性体であり、固有抵
抗が大きく渦電流損が少ないこと等の利点がある。Conventionally, magnetic heads have been formed with a core chip made of ferrite. Ferrite is a ferromagnetic material and has advantages such as high resistivity and low eddy current loss.
しかし、フェライトは、飽和磁束密度が小さく、抗磁力
の大きな記録媒体に対しては、磁気飽和により、高密度
記録ができないという欠点があった。However, ferrite has a drawback in that it has a low saturation magnetic flux density and cannot perform high-density recording due to magnetic saturation in a recording medium with a large coercive force.
高密度記録が可能な飽和磁束密度の大きい鉄合金に、セ
ンダストやパーマロイがあるが、これらは、固有抵抗が
小さく渦電流損が大きいという欠点がある。固有抵抗を
大きくするためには、ラミネート状の多数層にしなけれ
ばならない。Sendust and permalloy are iron alloys with a high saturation magnetic flux density that enable high-density recording, but these have the disadvantage of low resistivity and high eddy current loss. In order to increase the resistivity, it is necessary to use multiple laminated layers.
そこで、コアチップ自体は、フェライトで形成し、磁気
飽和しないように、磁気ギャップ間にセンダストやパー
マt」イ等庖−・面にのみ被着したヘッド(以下片M
I G−ソドと呼ぶ)が開発されている。この片MIG
−\ン1′を第3図Gこ示して説明する。Therefore, the core chip itself is made of ferrite, and in order to prevent magnetic saturation, the head (hereinafter referred to as part M) is coated only on the surface of the core chip, such as sendust or permanent
(called IG-Sodo) has been developed. This piece MIG
-\n1' will be explained with reference to FIG. 3G.
同図において、(1)は、金属酸化物強磁性体であるフ
ェライトからなる6ニスアチソフ′で、−・対の第1、
第2コアC2)(3)を低融点のガラス(4)(4)で
接合一体化したものである。この3コアチツプ(1)の
頂端面く5)には、磁気ギヤノブ(g)が形成され、磁
気ギャップ(g)の両側は、ガラス(4)(4)で保護
される。(6)は、センダスト又はパーマt’lイ等の
高飽和磁束密度強磁性体からなる金属薄膜で、前記磁気
ギヤツブ(g)に位置する第1′:1ア(2)のエツジ
部に被着形成される。(7)(7)は、絶1!被覆処理
された線材で、第1、第2コア(2)(3)の各脚部(
2a) (3a)に所定ターン数巻回される。(8)
は、フy、ライト製のバックコアで、第1、第2コア(
2)(3)の各脚部(2a) (3a)の末端部に貼
着固定され、閉磁路を形成すイ1゜更乙、−1’J ’
y ”f−ツブ(1)の両側に、非磁性体であるセラミ
ックや結晶ガラスがスライダ〔図示せず〕として貼着固
定される3゜
この上・うな磁気−、フドのコアチップ(1)の製造り
法を第4図乃至第6図に示して説明する。In the same figure, (1) is a 6-varnish atisof' made of ferrite, which is a metal oxide ferromagnetic material, and the first of the pair,
The second core C2) (3) is integrally bonded with low melting point glass (4) (4). A magnetic gear knob (g) is formed on the top end face (5) of this three-core chip (1), and both sides of the magnetic gap (g) are protected by glasses (4) (4). (6) is a thin metal film made of a high saturation magnetic flux density ferromagnetic material such as sendust or perma-t'l, which covers the edge portion of the 1':1a (2) located in the magnetic gear (g). A deposit is formed. (7) (7) is absolutely the best! Each leg (2) and (3) of the first and second cores (2) and (3) is made of coated wire
2a) (3a) is wound a predetermined number of turns. (8)
is a light back core made of fiber, and the first and second cores (
2) The legs (2a) and (3a) of (3) are attached and fixed to the ends of each other to form a closed magnetic circuit.
A non-magnetic material such as ceramic or crystal glass is stuck and fixed as a slider (not shown) on both sides of the f-tub (1). The manufacturing method will be explained with reference to FIGS. 4 to 6.
先ず、第4図に示すようにフェライトからなる直ツノ体
形状の第1、第2コアブロック(12)(13)を用意
する。First, as shown in FIG. 4, first and second core blocks (12) and (13) made of ferrite and having a straight horn shape are prepared.
次に、第5図に示すよ・うに、両コ了ブロック(12)
(13)の接合面に、トラック溝(14)(15)
と@線係止溝(16) (17)を切削加工する。ト
ラック溝(14) (15)は、両コアブロック(1
2) (13)の接合面上側短手方向に、トランク@
(T)を残しC1複数箇所切削除去し、形成する。巻線
係止i (16) (17)は、両−1アブロツク(
12) (13)の接合面中央部長手方向に1本ずつ
切削加工し、前記トラック溝(14)(15)を形成し
た側をフロントギセソブ部(12a)(13a)とし、
反対側をリアギヤツブ部(12b)(13b)とする。Next, as shown in Figure 5, both blocks (12)
Track grooves (14) and (15) are placed on the joint surface of (13).
and @line locking grooves (16) and (17) are cut. The track grooves (14) (15) are connected to both core blocks (1
2) In the upper short side direction of the joint surface of (13), trunk @
(T) is left and C1 is cut and removed in multiple places to form. Winding lock i (16) (17) is both -1 a block (
12) Cut one piece at a time in the longitudinal direction of the center of the joint surface of (13), and use the sides on which the track grooves (14) and (15) are formed as the front gear parts (12a) and (13a),
The opposite side is the rear gear part (12b) (13b).
第1のコアブロック(12)に形成したフl:jントギ
ャップ部(12a)、リアギャップ部(12b) 、!
−ラック溝(13)及び巻線係止溝(16)の全面に、
金属薄膜(18)をスパッタリングにより、加熱し7な
がら被着形成する。Front gap portion (12a), rear gap portion (12b), ! formed on the first core block (12).
- On the entire surface of the rack groove (13) and the winding locking groove (16),
A metal thin film (18) is deposited by sputtering while heating 7.
次に、第1コアブ1.Jツク(12)に、ギ4ソゲスペ
ーサとなるSi02等の非磁性体薄膜〔図示上ず〕を被
着形成した後、第6図に示すよ・つ(、:、第1、第2
コアブlニオツク(12) (13)を衝合して天地
逆転させ、両巻縁係止溝(16) (17)で形成さ
れる空間内に、ガラス棒(20)を収納配置する。ガラ
ス棒(20)を加熱して、熔融すると、トラック溝(1
4) (15)内にガラス(4)が充填され、第1、
第2コアブロック(12)(13)が接合一体化される
。そして、頂端面が研磨された後、点線に示すように、
第1、第2コアブロックの列側及び内偵jを切1折除去
し、点鎖線に示す箇所で、所定の厚さにスライスして、
コアチップ (1)を得る。Next, the first core 1. After forming a non-magnetic thin film such as Si02 (not shown in the figure), which will serve as a spacer on the J-tsuku (12), as shown in FIG.
The core blanks (12) and (13) are abutted and turned upside down, and the glass rod (20) is housed in the space formed by both the winding edge locking grooves (16) and (17). When the glass rod (20) is heated and melted, the track groove (1
4) Glass (4) is filled in (15), and the first
The second core blocks (12) and (13) are joined and integrated. Then, after the top surface is polished, as shown by the dotted line,
Cut and remove the row side and inner side j of the first and second core blocks, and slice them to a predetermined thickness at the locations indicated by the dotted chain line.
Obtain Core Chip (1).
金屈薄方史(18)を第にllアフロック(12)に被
着形成する際には、第1コアブロック(12)が加g4
されCいる。When forming the first core block (18) on the first core block (12), the first core block (12) is
There is C.
しかし、第1コアブロック(12)を構成するフェライ
トと金属薄1)j!! (18)を構成する一ヒンダス
ト又はパー・マロイとは熱膨張係数が異なるため、スパ
ッタリングが終了し、コアブロック(12) (13
)を冷却すると、金属薄膜(18)側を内1則にL7て
、コアブロック(12) (13)が、高さ方向にば
0゜5−0.6 〔μ謡〕程反って、全体として湾曲し
、てしまう。すると、第1S第2コアブロック(12)
(13)を衝合させたときに、両者間(12)
(13)に隙間が生15で、第7図に示すように、トラ
ンク溝(14) (15)内にガラスが充填される。However, the ferrite and thin metal 1) that constitute the first core block (12)! ! Since the coefficient of thermal expansion is different from that of the one-hin dust or per-malloy that constitutes the core block (18), the sputtering is completed and the core block (12) (13
), the core blocks (12) and (13) warp in the height direction by about 0°5-0.6 [μut], with the metal thin film (18) side L7 inside, and the whole core block It becomes curved and ends up. Then, the 1S second core block (12)
When (13) is collided, between the two (12)
A gap 15 is left at (13), and the trunk grooves (14) and (15) are filled with glass, as shown in FIG.
この活用、均一な磁気ギトソブ(g)を形成することが
できなくなる。特に、第1コアブしドック(12)は、
高さ方向にも湾曲しているため、両コアブロフク(12
) t(il’F磨したときに、磁気ギトノブ(g)の
間隔が増々大きくなる。This utilization makes it impossible to form a uniform magnetic field (g). In particular, the first core dock (12) is
Since it is also curved in the height direction, both core blocks (12
) t(il'F) When polishing, the distance between the magnetic knobs (g) becomes larger and larger.
このため、従来、湾曲した第1)第2コアブロックの膨
出した両側から締付けていたが、0.15 Ckgf
)以下の締付は力であると、均一な磁気ギャップ(g)
の形成ができず、品質の低下をもたらし、逆に、押圧力
を強くすると、コアチップ(1)に歪が残り、出力特性
の劣下をもたらせていた。For this reason, conventionally, the curved first and second core blocks were tightened from both sides of their bulges, but the
) less than the tightening force and uniform magnetic gap (g)
could not be formed, leading to deterioration in quality, and conversely, if the pressing force was increased, distortion remained in the core chip (1), resulting in deterioration of output characteristics.
また、最悪の場合は、コアチップ(1)に割れが生じ、
生産性の低下をもたらせていた。In the worst case, the core chip (1) may crack,
This was causing a decline in productivity.
そこで、本発明は、均一な磁気ギャップを形成すること
ができる複合型磁気ヘッドの製造方法を提供することを
目的とする。SUMMARY OF THE INVENTION Therefore, an object of the present invention is to provide a method for manufacturing a composite magnetic head that can form a uniform magnetic gap.
本発明は、上記目的を達成するため、金属酸化物強磁性
体からなる直方体形状の第1、第2コアブロックに、接
合面上側短手方向のトラック溝と接合面中央部長手方向
の巻線係止溝とを切削加工する工程と、第1コアブロッ
クの接合面と、第2コアブロックの接合面とは反対側の
面に、高飽和磁束密度強磁性体からなる金属薄膜を被着
形成する工程と、第1、第2コアブロックを衝合し、ト
ラック溝内にガラスを充填して、両者を接合一体化する
工程と、接合一体化された第1、第2コアブロックをス
ライスしてコアチップを得る工程とを含むものである。In order to achieve the above object, the present invention provides a rectangular parallelepiped-shaped first and second core blocks made of metal oxide ferromagnetic material, a track groove in the upper transverse direction of the joint surface, and a winding wire in the longitudinal direction in the center of the joint surface. A step of cutting the locking groove, and forming a metal thin film made of a high saturation magnetic flux density ferromagnetic material on the joint surface of the first core block and the surface opposite to the joint surface of the second core block. a step of abutting the first and second core blocks, filling the track grooves with glass and joining them together, and slicing the joined and integrated first and second core blocks. and obtaining a core chip.
第1、第2コアブロックは、金属薄膜を形成した面を内
側にして、同一の曲率半径で湾曲する。第1コアブロッ
クは接合面が凹部となり、第2コアブロックは接合面が
凸部となるから、両者は、密着して磁気ギャップが均一
に形成される。The first and second core blocks are curved with the same radius of curvature, with the surface on which the metal thin film is formed facing inside. Since the first core block has a concave joint surface and the second core block has a convex joint surface, the two are in close contact with each other and a uniform magnetic gap is formed.
本発明に係る一実施例を第1図及び第2図を参照して説
明する。但し、従来と同一部品は、同一符号を付して、
その説明は省略する。An embodiment of the present invention will be described with reference to FIGS. 1 and 2. However, parts that are the same as before are given the same symbols,
The explanation will be omitted.
本実施例においても、先ず、従来と同様、直方体形状の
第1)第2コアブロック(12) (13)の接合面
に、トラック溝(14) (15)と巻線係止溝(1
6) (17)を切削加工し、第1コアブロック(1
2)の接合面側全面にセンダスト等の高飽和磁束密度強
磁性体からなる金属薄膜(1日)をスパッタリングによ
り、加熱しながら被着形成する。In this embodiment as well, first, as in the conventional case, the track grooves (14) (15) and the winding locking grooves (1
6) Cutting (17) to form the first core block (1
2) A thin metal film (1 day) made of a high saturation magnetic flux density ferromagnetic material such as Sendust is deposited on the entire surface of the joint surface by sputtering while heating.
そして、本実施例においては、第2コアブロック(13
)の接合面とは反対側の面に、金R薄l*(19)をス
パッタリングにより、加熱しながら被着形成する。第2
コアブロック(13)に被着形成する金属I!膜(19
)の量は、第1コアブロック(12)に被着形成する金
属薄膜(18)の量とほぼ同一にする。第1コアブロッ
ク(12)の被着面には、トラック1) (14)や巻
線係止溝(16)等が形成されているための表面積が、
第2コアブロック(13)の被着よりも大きい。従って
、第2コアブロック(13)に被着形成する金属薄li
t (19)は、第1コアブロックに被着形成される金
属薄I1) (1B)より厚くする。In this embodiment, the second core block (13
) on the surface opposite to the bonding surface, gold R thin l* (19) is deposited by sputtering while heating. Second
Metal I to be deposited on the core block (13)! Membrane (19
) is approximately the same as the amount of the metal thin film (18) deposited on the first core block (12). The surface area of the first core block (12) has tracks 1) (14), winding locking grooves (16), etc.
It is larger than the adhesion of the second core block (13). Therefore, the thin metal li formed on the second core block (13)
t (19) is made thicker than the metal thin film I1) (1B) which is deposited on the first core block.
このようにして金属薄II! (1B) (19)が
被着形成された第1)第2コアブロック(12) (
13)は、スパッタリング後、第1図に示すように、第
1コアブロック(12)は接合面が凹部となって湾曲し
、第2コアブロック(13)は接合面が凸部となって湾
曲する。但し、湾曲の原因となる金属薄膜(18)
(19)の量が、第1コアブロック(12)と第2コア
ブロック(13)とでほぼ同一であるから、湾曲した両
者(12) (13)の曲率半径は同程度となる。即
ち、第1)第2のコアブロック(12) (13)は
密着し、所望の磁気ギャップ(g)が形成される。In this way, Metal Thin II! (1B) (19) is adhered to the first and second core blocks (12) (
13), after sputtering, as shown in FIG. 1, the first core block (12) is curved with a concave joint surface, and the second core block (13) is curved with a convex joint surface. do. However, metal thin film (18) that causes curvature
Since the amount of (19) is almost the same between the first core block (12) and the second core block (13), the radius of curvature of both curved core blocks (12) and (13) is approximately the same. That is, the first and second core blocks (12) and (13) are in close contact with each other, and a desired magnetic gap (g) is formed.
磁気ギャップ(g)は、従来と同様、第1、第2コアブ
ロック(12) (13)を衝合密着し、ガラス(4
)によって接合一体化することにより、形成することが
できる。さらに、第2図に示すように、第1、第2コア
ブロックの外側及び内側を切断除去し、同図−点鎖線に
示す箇所で、所定の厚さにスライスすると、コアチップ
(1)を得る。第1、第2コアブロック(12)(13
)は湾曲したものであるが、その曲率半径は僅かである
から、得られたコアチップ(1)は、湾曲していた状態
を無視することができる。The magnetic gap (g) is created by bringing the first and second core blocks (12) (13) into close contact with each other and by using glass (4) as in the conventional case.
) can be formed by joining and integrating. Furthermore, as shown in Fig. 2, the outer and inner parts of the first and second core blocks are cut and removed, and the core chips (1) are obtained by slicing them to a predetermined thickness at the locations indicated by the dashed lines in the same figure. . First and second core blocks (12) (13
) is curved, but since its radius of curvature is small, the curved state of the obtained core chip (1) can be ignored.
本発明によれば、第1.第2コアブロックが同一の曲率
半径で、接合面を凹状、凸状に汎曲するため、接合面が
完全に密着する。この結果両者を密着させるための押■
:力を加える必要がなく、所望の磁気ギヤツブを形成す
ることができる。従って、二1アチップ内に歪が残るこ
とがなく、出力特性の劣化を招くことがなくなる。According to the present invention, first. Since the second core block has the same radius of curvature and the joint surfaces are generally curved in a concave and convex shape, the joint surfaces are in perfect contact with each other. As a result, a push is made to bring the two into close contact.
: A desired magnetic gear can be formed without the need to apply force. Therefore, no distortion remains in the 21-chip, and no deterioration of output characteristics occurs.
また、割れ等に起因する生産性の低下も解消することが
できる。Further, it is possible to eliminate the decrease in productivity caused by cracks and the like.
第1図及び第2図は本発明に係る複合型磁気ヘッドの製
造方法を示す工程図である。
第3図は複合型磁気・1ノドの斜視図2.第4図乃至第
6図は同じく(ガニ来の製造方法を示す工程図、第7図
は課題を説明Jるための斜視図である。
(4)・・−ガラス、
(12)−・第1コアブロック、
(13)−・第2コアブロック、1 and 2 are process diagrams showing a method for manufacturing a composite magnetic head according to the present invention. Figure 3 is a perspective view of a composite magnetic one-nod. Figures 4 to 6 are process diagrams showing the manufacturing method of the crab, and Figure 7 is a perspective view for explaining the problem. (4) - Glass, (12) - 1 core block, (13)--2nd core block,
Claims (1)
第2コアブロックに、接合面上側短手方向のトラック溝
と接合面中央部長手方向の巻線係止溝とを切削加工する
工程と、 第1コアブロックの接合面と、第2コアブロックの接合
面とは反対側の面に、等分量の高飽和磁束密度強磁性体
からなる金属薄膜を被着形成する工程と、 第1、第2コアブロックを衝合し、トラック溝内にガラ
スを充填して、両者を接合一体化する工程と、 接合一体化された第1、第2コアブロックをスライスし
てコアチップを得る工程とを含むことを特徴とする複合
型磁気ヘッドの製造方法。(1) A first rectangular parallelepiped made of metal oxide ferromagnetic material,
cutting a track groove in the upper transverse direction of the joint surface and a winding locking groove in the longitudinal direction at the center of the joint surface in the second core block; A process of depositing and forming an equal amount of a metal thin film made of a high saturation magnetic flux density ferromagnetic material on the surface opposite to the bonding surface, and abutting the first and second core blocks and inserting glass into the track grooves. 1. A method for manufacturing a composite magnetic head, comprising the steps of: filling the first and second core blocks to form a single unit; and slicing the first and second core blocks that have been combined into one core block to obtain a core chip.