JPH0147855B2 - - Google Patents
Info
- Publication number
- JPH0147855B2 JPH0147855B2 JP57044003A JP4400382A JPH0147855B2 JP H0147855 B2 JPH0147855 B2 JP H0147855B2 JP 57044003 A JP57044003 A JP 57044003A JP 4400382 A JP4400382 A JP 4400382A JP H0147855 B2 JPH0147855 B2 JP H0147855B2
- Authority
- JP
- Japan
- Prior art keywords
- tape
- adhesive
- strip
- shaped
- sealing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【発明の詳細な説明】
この発明は乾電池の陽極端子の封印に用いられ
る乾電池用封印テープの製造方法に関する。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a method for producing a dry cell sealing tape used for sealing the anode terminal of a dry cell.
従来乾電池の陽極端子を封印テープにて封印し
乾電池が未使用であることを表わすと同時に陽極
端子を保護することが行なわれている。 Conventionally, the anode terminal of a dry cell battery has been sealed with sealing tape to indicate that the dry cell is unused and at the same time to protect the anode terminal.
ところが、このように封印テープにて陽極端子
を封印するとテープの粘着剤が端子に付着し接触
不良の原因になつたり、テープ中に含まれる水分
により端子に錆を生じたり、あるいは使用時封印
テープの切り離しが面倒であるなどの問題点があ
つた。 However, if the anode terminal is sealed with sealing tape in this way, the adhesive of the tape may adhere to the terminal and cause poor contact, or the moisture contained in the tape may cause rust on the terminal, or the sealing tape may not be used properly. There were problems such as the difficulty of separating the
この発明は上記事情に鑑みてなされたもので、
陽極端子の接触不良および錆発生を確実に除去で
きるとともに封印後の切り離しも簡単にできるよ
うな乾電池用封印テープの製造方法を提供するこ
とを目的とする。 This invention was made in view of the above circumstances,
To provide a method for producing a sealing tape for a dry battery, which can reliably eliminate poor contact and rust of an anode terminal, and can also be easily separated after sealing.
以下、この発明の一実施例を説明する。 An embodiment of this invention will be described below.
まず、上質紙、アート紙又はポリフイルムなど
からなる帯状のテープ本体を用意し、このテープ
本体の一面に粘着剤を塗布する。次に粘着剤を塗
布したテープ本体の略中央部に沿つて巾10〜15
mm、厚さ20〜30μ程度のポリプロピレン(PP)、
ポリ塩化ビニル(PVC)、ポリエチレン(PE)
などの帯状フイルムを接着する。そして、このよ
うにフイルムを接着したテープ本体の粘着面を離
型剤のパラフインワツクスを片面にコーテイング
した市販により入手可能な台紙上に接着する。こ
の状態を第1図および第2図に示している。ここ
で、図中1はテープ本体、2は粘着剤、3は帯状
のフイルム、4は台紙である。 First, a belt-shaped tape body made of high-quality paper, art paper, polyfilm, etc. is prepared, and an adhesive is applied to one side of the tape body. Next, apply a width of 10 to 15 mm along the approximate center of the tape body coated with adhesive.
mm, polypropylene (PP) with a thickness of about 20 to 30μ,
Polyvinyl chloride (PVC), polyethylene (PE)
Glue strip-shaped film such as. Then, the adhesive surface of the tape body to which the film has been adhered is adhered onto a commercially available mount coated on one side with paraffin wax as a release agent. This state is shown in FIGS. 1 and 2. Here, in the figure, 1 is a tape body, 2 is an adhesive, 3 is a strip-shaped film, and 4 is a mount.
次に、第1図に示すようにテープ本体1の上面
の巾方向に短冊状の切欠み6を形成し封印テープ
5が離型剤のパラフインワツクスによつて粘着力
が弱められを引きはがし可能に形成する。このよ
うな封印テープ5はテープ本体1に沿つて多数形
成される。 Next, as shown in FIG. 1, a strip-shaped notch 6 is formed in the width direction of the upper surface of the tape body 1, and the adhesive strength of the sealing tape 5 is weakened by the release agent paraffin wax, so that it can be peeled off. form possible. A large number of such sealing tapes 5 are formed along the tape body 1.
この場合切り込み6の深さは第2図に示すよう
に台紙4の肉厚方向の途中まで達するようにする
ことによつて短冊状の封印テープ5のみが台紙4
からはがれる。また、第1図に示すように封印テ
ープ5は周縁にくびれ部51を有するようにして
いる。 In this case, the depth of the notch 6 is set so that it reaches halfway in the thickness direction of the mount 4, as shown in FIG.
It can be peeled off. Furthermore, as shown in FIG. 1, the sealing tape 5 has a constricted portion 51 at its periphery.
このような状態から必要に応じて封印テープ5
が引きはがされる。この場合封印テープ5は切り
込み6の深さが台紙4の途中まで達しているので
第3図に示すようにテープ本体1の中央部にフイ
ルム3が位置するように構成される。 If necessary in this situation, seal tape 5
is torn off. In this case, the depth of the cut 6 in the sealing tape 5 reaches halfway through the mount 4, so that the film 3 is positioned at the center of the tape body 1, as shown in FIG.
そして、このようにして得られた封印テープ5
は粘着面をもつて第4図に示すように乾電池7の
陽極端子側に接着される。この場合封印テープ5
はフイルム3部分が陽極端子上に位置するように
する。 And the sealing tape 5 obtained in this way
has an adhesive surface and is adhered to the anode terminal side of the dry battery 7 as shown in FIG. In this case sealing tape 5
Position the third portion of the film over the anode terminal.
したがつて、このような方法にて得られた封印
テープによれば乾電池の陽極端子側を封印すると
テープのフイルム部分が陽極端子上に位置するの
で粘着剤が端子に付着することがなく端子の接触
不良の原因を除去することができる。またテープ
本体部分に多少水分が含まれていたとしてもフイ
ルム部分にて陽極端子への影響を除去できるので
端子に錆を生じるような不都合も除去できる。更
にテープはくびれ部を有しているので乾電池の使
用の際くびれ部の近くを引つ張るのみで簡単に切
り取ることができる。 Therefore, according to the sealing tape obtained by this method, when the anode terminal side of a dry battery is sealed, the film part of the tape is positioned on the anode terminal, so the adhesive does not adhere to the terminal and the terminal is protected. The cause of poor contact can be eliminated. Furthermore, even if the tape body contains some moisture, the influence on the anode terminal can be removed by the film portion, thereby eliminating inconveniences such as rust on the terminal. Furthermore, since the tape has a constriction, it can be easily cut off by simply pulling near the constriction when using a dry battery.
なお、この発明は上記実施例にのみ限定されず
要旨を変更しない範囲で適宜変形して実施でき
る。 It should be noted that the present invention is not limited to the above-mentioned embodiments, but can be implemented with appropriate modifications without changing the gist.
以上述べたようにこの発明によれば陽極端子の
接触不良および錆発生を確実に除去できるととも
に封印後の切り離しも簡単にできるような乾電池
用封印テープの製造方法を提供できる。 As described above, according to the present invention, it is possible to provide a method for manufacturing a sealing tape for a dry battery, which can reliably eliminate poor contact and rust of the anode terminal, and also allows easy separation after sealing.
第1図はこの発明の一実施例を説明する概略構
成図、第2図は第1図の断面図、第3図は同実施
例により得られるテープを示す正面図、第4図は
テープを乾電池に接着した状態を示す斜視図であ
る。
1……テープ本体、2……粘着剤、3……フイ
ルム、4……台紙、5……テープ片、51……く
びれ部、6……切り込み部、7……乾電池。
FIG. 1 is a schematic configuration diagram illustrating an embodiment of the present invention, FIG. 2 is a sectional view of FIG. 1, FIG. 3 is a front view of a tape obtained by the same embodiment, and FIG. FIG. 3 is a perspective view showing a state in which it is adhered to a dry battery. DESCRIPTION OF SYMBOLS 1... Tape body, 2... Adhesive, 3... Film, 4... Mounting paper, 5... Tape piece, 51... Constriction, 6... Notch, 7... Dry battery.
Claims (1)
布する工程と、 粘着剤2面の中央部に沿つて帯状フイルム3を
接着する工程と、 帯状フイルム3を接着した帯状のテープ本体1
の粘着剤2面を台紙4に接着する工程と、 前記台紙4は、粘着剤2に対して引きはがし可
能な離型剤を塗布したものであり、 帯状のテープ本体1に切込みするとともに台紙
4の厚み方向の途中まで切込み6を入れて帯状の
テープ本体1の幅方向に短冊状の封印テープ5を
形成する工程とを有することを特徴とする乾電池
用封印テープの製造方法。[Claims] 1. A step of applying an adhesive 2 to one side of a strip-shaped tape body 1, a step of adhering a strip-shaped film 3 along the center portion of the adhesive 2 surface, and a step of adhering the strip-shaped film 3. Band-shaped tape body 1
The step of adhering two sides of the adhesive to a backing paper 4; The backing paper 4 is made by coating the adhesive 2 with a release agent that can be peeled off. A method for producing a sealing tape for a dry battery, comprising the step of forming a strip-shaped sealing tape 5 in the width direction of a strip-shaped tape main body 1 by making a cut 6 halfway in the thickness direction.