JPH0140103B2 - - Google Patents
Info
- Publication number
- JPH0140103B2 JPH0140103B2 JP56028429A JP2842981A JPH0140103B2 JP H0140103 B2 JPH0140103 B2 JP H0140103B2 JP 56028429 A JP56028429 A JP 56028429A JP 2842981 A JP2842981 A JP 2842981A JP H0140103 B2 JPH0140103 B2 JP H0140103B2
- Authority
- JP
- Japan
- Prior art keywords
- cod
- less
- value
- steel
- inclusions
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2842981A JPS57143470A (en) | 1981-03-02 | 1981-03-02 | High tensile steel with high cod value |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2842981A JPS57143470A (en) | 1981-03-02 | 1981-03-02 | High tensile steel with high cod value |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS57143470A JPS57143470A (en) | 1982-09-04 |
| JPH0140103B2 true JPH0140103B2 (enExample) | 1989-08-25 |
Family
ID=12248411
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2842981A Granted JPS57143470A (en) | 1981-03-02 | 1981-03-02 | High tensile steel with high cod value |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS57143470A (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH076034B2 (ja) * | 1987-01-26 | 1995-01-25 | 川崎製鉄株式会社 | 溶接部の脆性破壊発生特性の優れた高強度鋼 |
| JPS6421036A (en) * | 1987-07-14 | 1989-01-24 | Kawasaki Steel Co | High strength thick steel having superior cod characteristic in weld zone |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5139522A (ja) * | 1974-10-01 | 1976-04-02 | Sumitomo Metal Ind | Yosetsuyokojinseichoshitsukohan |
| JPS5343663A (en) * | 1976-10-04 | 1978-04-19 | Nippon Kokan Kk | Manufacturing process of good accurate form steel sections for low temperature |
-
1981
- 1981-03-02 JP JP2842981A patent/JPS57143470A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS57143470A (en) | 1982-09-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0649915B1 (en) | High-strength martensitic stainless steel and method for making the same | |
| EP0080809A1 (en) | A method of making wrought high tension steel having superior low temperature toughness | |
| EP0703301B1 (en) | High chromium ferritic heat-resistant steel | |
| JP3255296B2 (ja) | 高強度ばね用鋼およびその製造方法 | |
| JP4317499B2 (ja) | 音響異方性が小さく溶接性に優れる引張強さ570MPa級以上の高張力鋼板およびその製造方法 | |
| JPH0748621A (ja) | 耐ssc,耐hic性に優れた圧力容器用鋼の製造方法 | |
| JP3747585B2 (ja) | 加工性および耐食性に優れた高硬度マルテンサイト系ステンレス鋼 | |
| JP4998708B2 (ja) | 材質異方性が小さく、耐疲労亀裂伝播特性に優れた鋼材およびその製造方法 | |
| JPH08269632A (ja) | 高強度・高耐食含窒素オーステナイ ト系ステンレス鋼 | |
| JP2834654B2 (ja) | 高靱性熱間工具鋼 | |
| JP4924047B2 (ja) | 表面残留応力の絶対値が150N/mm2以下の耐疲労亀裂伝播特性に優れた鋼材の製造方法 | |
| JPH02247357A (ja) | 転造ダイス用鋼 | |
| US4851054A (en) | Method of producing rolled steel having excellent resistance to sulfide stress corrosion cracking | |
| JP3757027B2 (ja) | 溶接性に優れた高強度熱延鋼材及びこれを用いた高強度鋼線並びに高強度棒鋼 | |
| JPH07290275A (ja) | 高強度Cr−Mo鋼用溶接ワイヤ | |
| JP2688312B2 (ja) | 高強度高靭性鋼板 | |
| JPH0140103B2 (enExample) | ||
| JP7534595B2 (ja) | 耐摩耗鋼の製造方法 | |
| JPS59211553A (ja) | 靭性及び高温強度の優れた高Cr鋼 | |
| JPS5940203B2 (ja) | 高清浄度、低降伏比熱延鋼板の製造方法 | |
| JP2834500B2 (ja) | 抵温靭性の優れた高張力鋼板の製造法 | |
| JPH09291344A (ja) | 低硬度マルテンサイト系ステンレス鋼 | |
| JPH07278729A (ja) | 降伏比の低い高張力鋼板 | |
| JP3903996B2 (ja) | 被削性、冷間鍛造性および焼き入れ・焼き戻し後の疲労強度特性に優れた冷間鍛造用棒鋼および機械構造用部材 | |
| JP3338241B2 (ja) | 焼入れ性に優れたCr−Mo鋼 |