JP7218059B2 - CONTAINER WITH SHRINK FILM AND METHOD FOR MANUFACTURING SAME - Google Patents

CONTAINER WITH SHRINK FILM AND METHOD FOR MANUFACTURING SAME Download PDF

Info

Publication number
JP7218059B2
JP7218059B2 JP2019064629A JP2019064629A JP7218059B2 JP 7218059 B2 JP7218059 B2 JP 7218059B2 JP 2019064629 A JP2019064629 A JP 2019064629A JP 2019064629 A JP2019064629 A JP 2019064629A JP 7218059 B2 JP7218059 B2 JP 7218059B2
Authority
JP
Japan
Prior art keywords
shrink film
container
adhesive layer
corner portions
right corner
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2019064629A
Other languages
Japanese (ja)
Other versions
JP2020164174A (en
Inventor
耕太 新渡戸
金光 笹田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yoshino Kogyosho Co Ltd
Original Assignee
Yoshino Kogyosho Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yoshino Kogyosho Co Ltd filed Critical Yoshino Kogyosho Co Ltd
Priority to JP2019064629A priority Critical patent/JP7218059B2/en
Publication of JP2020164174A publication Critical patent/JP2020164174A/en
Application granted granted Critical
Publication of JP7218059B2 publication Critical patent/JP7218059B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、シュリンクフィルム付き容器及びその製造方法に関する。 TECHNICAL FIELD The present invention relates to a container with a shrink film and a method for manufacturing the same.

容器本体の胴部に筒状のシュリンクフィルムが装着されたシュリンクフィルム付き容器が知られている(例えば、特許文献1参照)。シュリンクフィルム付き容器は、形成された容器本体の胴部に筒状のシュリンクフィルムを配置し、シュリンクフィルム全体を加熱することにより、シュリンクフィルムを熱収縮させて胴部に装着することで製造することができる。 BACKGROUND ART A container with a shrink film is known in which a cylindrical shrink film is attached to the trunk of a container body (see, for example, Patent Document 1). A container with a shrink film is manufactured by placing a cylindrical shrink film on the body of a formed container body, heating the entire shrink film to thermally shrink the shrink film, and attaching it to the body. can be done.

特開2014-177302号公報JP 2014-177302 A

ところで、容器本体の胴部が、上面視で長手方向を規定する偏平形状であり、また、長手方向の少なくとも一端部において下方側から上方側に向けて容器内側へ傾斜する左右傾斜部を有する場合がある。このような左右傾斜部に上述したようにシュリンクフィルムを装着しようとすると、熱収縮時にシュリンクフィルムが左右傾斜部に沿ってずり上がってしまい、きれいに装着できないという問題点があった。 By the way, when the body of the container body has a flat shape defining the longitudinal direction in a top view, and has a left-right inclined portion at least one end portion in the longitudinal direction that inclines from the lower side to the upper side toward the inside of the container. There is When the shrink film is attached to the left and right inclined portions as described above, the shrink film slides up along the left and right inclined portions during heat shrinkage, resulting in a problem that the shrink film cannot be attached neatly.

本発明は、このような問題点を解決することを課題とするものであり、その目的は、偏平形状の胴部に位置する左右傾斜部にシュリンクフィルムがきれいに装着されたシュリンクフィルム付き容器及びその製造方法を提供することにある。 SUMMARY OF THE INVENTION An object of the present invention is to solve such problems. It is to provide a manufacturing method.

本発明のシュリンクフィルム付き容器は、口部、胴部及び底部を有する容器本体と、前記胴部に装着された筒状のシュリンクフィルムとを有し、胴部が、上面視で長手方向を規定する偏平形状であり、また、前記長手方向の少なくとも一端部において上下方向の一方側から他方側に向けて容器内側へ傾斜する左右傾斜部を有し、前記シュリンクフィルムが、前記左右傾斜部に装着され、また、前記シュリンクフィルムの前記一方側の端部のみに位置するとともに前記胴部に接着した感熱接着剤で形成される接着層を有し、前記胴部が、前記長手方向の両端部に位置するとともに前記左右傾斜部の前記一方側の端部と当該端部から前記一方側に向けて容器内側へ湾曲する湾曲部とで形成される左右コーナー部を有し、前記接着層が、前記左右コーナー部における前記湾曲部に接着している第1部分と、前記左右コーナー部における前記左右傾斜部の前記一方側の端部に接着している第2部分とを有することを特徴とする。 A container with a shrink film of the present invention has a container body having a mouth portion, a body portion and a bottom portion, and a tubular shrink film attached to the body portion, and the body portion defines a longitudinal direction in top view. At least one end in the longitudinal direction has a laterally inclined portion that slopes toward the inside of the container from one side to the other in the vertical direction, and the shrink film is attached to the laterally inclined portion. Also, an adhesive layer formed of a heat-sensitive adhesive is positioned only at one end of the shrink film and adhered to the body , and the body is attached to both ends in the longitudinal direction. and a left and right corner portion formed by the one end portion of the left and right inclined portion and a curved portion that curves toward the inside of the container from the end portion toward the one side, and the adhesive layer It has a first portion adhered to the curved portion at the left and right corner portions, and a second portion adhered to the one end portion of the left and right inclined portion at the left and right corner portions .

本発明のシュリンクフィルム付き容器は、上記構成において、前記左右コーナー部が、前記胴部の下端部に位置するのが好ましい。 In the container with a shrink film of the present invention having the above configuration, it is preferable that the left and right corner portions are positioned at the lower end portion of the body portion.

本発明のシュリンクフィルム付き容器の製造方法は、口部、胴部及び底部を備えるとともに、前記胴部が、上面視で長手方向を規定する偏平形状であり、また、前記長手方向の少なくとも一端部において上下方向の一方側から他方側に向けて内側へ傾斜する左右傾斜部を有する容器本体を形成する容器本体形成工程と、一端部のみに位置する感熱接着剤で形成される接着層を備える筒状のシュリンクフィルムを、前記一端部が前記一方側に位置するとともに前記シュリンクフィルムが前記左右傾斜部を包囲するように配置し、前記一端部を加熱することにより、前記接着層を前記胴部に接着する接着工程と、前記接着層が前記胴部に接着した状態で前記シュリンクフィルムの全体を加熱することにより、前記シュリンクフィルムを熱収縮させて前記左右傾斜部に装着する熱収縮工程とを有し、前記容器本体形成工程において形成する前記容器本体の前記胴部が、前記長手方向の両端部に位置するとともに前記左右傾斜部の前記一方側の端部と当該端部から前記一方側に向けて容器内側へ湾曲する湾曲部とで形成される左右コーナー部を有し、前記接着工程において、前記接着層の第1部分を前記左右コーナー部における前記湾曲部に接着し、且つ、前記接着層の第2部分を前記左右コーナー部における前記左右傾斜部の前記一方側の端部に接着することを特徴とする。 The method for manufacturing a container with a shrink film according to the present invention includes a mouth portion, a body portion, and a bottom portion, and the body portion has a flat shape defining a longitudinal direction when viewed from above, and at least one end portion in the longitudinal direction. A container body forming step of forming a container body having a left-right inclined portion that inclines inward from one side in the vertical direction to the other side in the above; A shrink film having a shape is placed so that the one end is located on the one side and the shrink film surrounds the laterally inclined portion, and the adhesive layer is attached to the body by heating the one end. and a heat shrinking step of heating the entire shrink film in a state where the adhesive layer is adhered to the trunk portion to heat shrink the shrink film and attach it to the left and right inclined portions. and the body portion of the container body formed in the container body forming step is located at both ends in the longitudinal direction, and the one side end of the left and right inclined portion and the one side from the left and right inclined portion are arranged. a left and right corner portion formed by a curved portion that curves toward the inside of the container; is adhered to the one-side ends of the left and right inclined portions at the left and right corner portions .

本発明のシュリンクフィルム付き容器の製造方法は、上記構成において、前記左右コーナー部が、前記胴部の下端部に位置するのが好ましい。 In the method for manufacturing a container with a shrink film according to the present invention, in the configuration described above, it is preferable that the left and right corner portions are positioned at the lower end portion of the body portion.

本発明によれば、偏平形状の胴部に位置する左右傾斜部にシュリンクフィルムがきれいに装着されたシュリンクフィルム付き容器及びその製造方法を提供することができる。 ADVANTAGE OF THE INVENTION According to this invention, the container with a shrink film which the left-right inclination part located in the flat-shaped body part was neatly mounted|worn with the shrink film, and its manufacturing method can be provided.

本発明の一実施の形態に係るシュリンクフィルム付き容器を示す正面図である。1 is a front view showing a container with a shrink film according to one embodiment of the present invention; FIG. 図1に示すシュリンクフィルム付き容器の斜視図である。FIG. 2 is a perspective view of the container with the shrink film shown in FIG. 1; 図1に示すシュリンクフィルム付き容器のシュリンクフィルムを装着前の状態で示す上面図である。FIG. 2 is a top view showing a state before the shrink film of the container with the shrink film shown in FIG. 1 is attached. 図3Aに示すシュリンクフィルムの正面図である。3B is a front view of the shrink film shown in FIG. 3A; FIG. 本発明の一実施の形態に係るシュリンクフィルム付き容器の製造方法を示すフローチャートである。1 is a flow chart showing a method of manufacturing a container with a shrink film according to one embodiment of the present invention.

以下、本発明の一実施の形態のシュリンクフィルム付き容器及びその製造方法について、図面を参照しつつ詳細に例示説明する。 Hereinafter, a container with a shrink film and a method for manufacturing the same according to an embodiment of the present invention will be described in detail by way of example with reference to the drawings.

図1~図2に示すように、本実施の形態に係るシュリンクフィルム付き容器1(以下、容器1ともいう)は、口部11、胴部12及び底部13を有する容器本体10と、胴部12に装着された筒状のシュリンクフィルム20とを有している。 As shown in FIGS. 1 and 2, a container 1 with a shrink film according to the present embodiment (hereinafter also referred to as container 1) includes a container body 10 having a mouth portion 11, a body portion 12 and a bottom portion 13, and a body portion 12 and a tubular shrink film 20 attached thereto.

容器本体10は、合成樹脂製であるが、これに限らない。また、容器本体10は、押出しブロー成形(EBM:Extrusion Blow Molding)又はプリフォームからの二軸延伸ブロー成形によって形成されているが、これに限らない。容器本体10の内容物は、特に限定されず、例えば液状であってよい。 The container body 10 is made of synthetic resin, but is not limited to this. Further, the container body 10 is formed by extrusion blow molding (EBM: Extrusion Blow Molding) or biaxially stretched blow molding from a preform, but is not limited to this. The contents of the container body 10 are not particularly limited, and may be liquid, for example.

口部11は、中心軸線Oを中心とする円筒状であるが、これに限らず、中心軸線Oを中心とする筒状であればよい。口部11の外周面には、吐出口を備える注出キャップや、ポンプの装着キャップなど、用途に応じて設定されるキャップを口部11に取り付けるための雄ねじ部11aが設けられている。なお、雄ねじ部11aに代えて、打栓用のスナップ嵌合部を設けてもよい。 The mouth portion 11 has a cylindrical shape centered on the central axis O, but is not limited to this, and may have a cylindrical shape centered on the central axis O. As shown in FIG. The outer peripheral surface of the mouth portion 11 is provided with a male screw portion 11a for attaching a cap set according to the application to the mouth portion 11, such as a pouring cap having a discharge port or a mounting cap for a pump. A snap fitting portion for plugging may be provided instead of the male screw portion 11a.

口部11の下端には、上面視で長手方向及び短手方向を規定する偏平形状の胴部12が連なっている。つまり、胴部12は、上面視で左右方向に細長い偏平形状である。胴部12は、上下方向に亘って横断面形状がトラック形状であるが、これに限らず、例えば楕円形状や多角形状であってもよい。胴部12は、長手方向の両端部において下方側から上方側に向けて容器内側へ傾斜する左右傾斜部14を有している。左右傾斜部14は、左右の傾斜角度が互いに同じ(つまり、左右対称形状)であるが、これに限らず、左右非対称形状であってもよい。また、左右傾斜部14は、長手方向の一端部が下方側から上方側に向けて容器内側へ傾斜するとともに長手方向の他端部が傾斜していない(つまり、上下方向に沿って延在している)構成であってもよい。胴部12は、長手方向の両端部、すなわち左右方向の両端部において左右傾斜部14の下端部14aと当該下端部14aから下方側に向けて容器内側へ湾曲する湾曲部15とで形成される左右コーナー部16を有している。左右コーナー部16は、胴部12の下端部12aに位置している。左右コーナー部16は、左右対称形状であるが、これに限らず、左右非対称形状であってもよい。左右傾斜部14の上端部14bは、胴部12の上端部12bに位置している。胴部12の上端部12bには、胴部12の側から口部11の側に向けて段差状に縮径する段差部が形成されている。 A flat-shaped trunk portion 12 that defines the longitudinal direction and the lateral direction in top view continues to the lower end of the mouth portion 11 . That is, the trunk portion 12 has a flat shape elongated in the left-right direction when viewed from above. The trunk portion 12 has a track-shaped cross-section in the vertical direction, but is not limited to this, and may be, for example, an elliptical shape or a polygonal shape. The trunk portion 12 has left and right inclined portions 14 at both ends in the longitudinal direction that are inclined toward the inside of the container from the lower side to the upper side. The left and right inclined portions 14 have the same left and right inclination angles (that is, a symmetrical shape), but are not limited to this, and may have a left and right asymmetrical shape. In addition, the laterally inclined portion 14 has one end in the longitudinal direction inclined toward the inside of the container from the lower side to the upper side, and the other end in the longitudinal direction is not inclined (that is, extends along the vertical direction). configuration). The trunk portion 12 is formed by a lower end portion 14a of a left-right inclined portion 14 at both ends in the longitudinal direction, that is, both ends in the left-right direction, and a curved portion 15 that curves downward from the lower end portion 14a toward the inside of the container. It has left and right corner portions 16 . The left and right corner portions 16 are located at the lower end portion 12 a of the trunk portion 12 . The left and right corner portions 16 have a symmetrical shape, but are not limited to this, and may have a left-right asymmetrical shape. An upper end portion 14 b of the laterally inclined portion 14 is positioned at an upper end portion 12 b of the trunk portion 12 . An upper end portion 12b of the body portion 12 is formed with a stepped portion whose diameter is reduced stepwise from the body portion 12 side toward the mouth portion 11 side.

上下方向とは、口部11の中心軸線Oに沿う方向を意味し、上方とは、底部13から口部11に向かう方向(図1における上方)を意味し、下方とはその反対方向を意味する。また、横断面とは、中心軸線Oと垂直な断面を意味する。左右方向とは、長手方向を意味する。前後方向とは、短手方向を意味する。 The vertical direction means the direction along the central axis O of the mouth portion 11, the upward direction means the direction from the bottom portion 13 toward the mouth portion 11 (upward in FIG. 1), and the downward direction means the opposite direction. do. Moreover, a cross section means a cross section perpendicular to the central axis O. As shown in FIG. A left-right direction means a longitudinal direction. The front-rear direction means the transverse direction.

左右傾斜部14は、正面視で直線状であるが、これに限らず、正面視で湾曲状であってもよい。例えば、左右傾斜部14が、長手方向の少なくとも一端部において下方側から上方側に向けて容器内側への傾斜角度が増加する湾曲状に傾斜していてもよい。なお、左右傾斜部14がこのような湾曲状をなしている場合には、シュリンクフィルム20のずり上がりが特に強く生じる傾向があるため、本実施の形態である接着層22を有するシュリンクフィルム20の必要性が特に大きい。胴部12の周長は、左右傾斜部14の傾斜により、左右傾斜部14の下端部14aから左右傾斜部14の上端部14bまで徐々に減少している。 The laterally inclined portion 14 is straight when viewed from the front, but is not limited to this, and may be curved when viewed from the front. For example, the laterally inclined portion 14 may be inclined at least at one end in the longitudinal direction in a curved shape in which the angle of inclination toward the inside of the container increases from the lower side toward the upper side. When the laterally inclined portion 14 has such a curved shape, the shrink film 20 tends to ride up particularly strongly. especially great need. The circumferential length of the trunk portion 12 gradually decreases from the lower end portion 14a of the laterally inclined portion 14 to the upper end portion 14b of the laterally inclined portion 14 due to the inclination of the laterally inclined portion 14 .

左右傾斜部14の下端部14aにおいて、胴部12の偏平率L1/L2は、約3とされているが、これに限らず、用途等に応じて様々な大きさに設定可能である。L1は胴部12の長手方向の長さであり、L2は胴部12の短手方向の長さである。左右傾斜部14の下端部14aにおいて、胴部12の長手方向の長さL1は、例えば約100mmであってよいが、これに限らず、用途等に応じて様々な大きさに設定可能である。左右傾斜部14の下端部14aにおける胴部12の長手方向の長さL1と左右傾斜部14の上端部14bにおける胴部12の長手方向の長さL1との比(傾斜率)は、約2とされているが、これに限らず、用途等に応じて様々な大きさに設定可能である。胴部12の短手方向の長さL2は、左右傾斜部14の下端部14aから上端部14bまでほとんど変化していないが、これに限らない。 At the lower end portion 14a of the laterally inclined portion 14, the flatness ratio L1/L2 of the body portion 12 is approximately 3, but the ratio is not limited to this and can be set to various sizes depending on the application. L1 is the length of the trunk 12 in the longitudinal direction, and L2 is the length of the trunk 12 in the short direction. At the lower end portion 14a of the laterally inclined portion 14, the longitudinal length L1 of the body portion 12 may be, for example, about 100 mm, but is not limited to this, and can be set to various sizes depending on the application. . The ratio (inclination ratio) of the longitudinal length L1 of the trunk portion 12 at the lower end portion 14a of the laterally inclined portion 14 to the longitudinal length L1 of the trunk portion 12 at the upper end portion 14b of the laterally inclined portion 14 is approximately 2. However, it is not limited to this, and can be set to various sizes according to the application. Although the length L2 of the trunk portion 12 in the lateral direction hardly changes from the lower end portion 14a to the upper end portion 14b of the laterally inclined portion 14, it is not limited to this.

底部13は、胴部12の下端部12aを閉塞している。底部13の外周縁部は、周方向に連続又は断続する接地部を有している。つまり、容器1は、底部13を接地部として水平面上に載置可能である。底部13は、平面状であってもよいし、例えば上面視中央部が隆起する非平面状であってもよい。 The bottom portion 13 closes the lower end portion 12 a of the body portion 12 . The outer peripheral edge of the bottom portion 13 has a grounding portion that is continuous or intermittent in the circumferential direction. That is, the container 1 can be placed on a horizontal surface using the bottom portion 13 as a ground portion. The bottom portion 13 may be planar, or may be non-planar such that the central portion when viewed from the top is raised.

シュリンクフィルム20は、左右傾斜部14に装着されている。シュリンクフィルム20の下端部20aは、左右コーナー部16に位置している。シュリンクフィルム20の上端部20bは、胴部12の上端部12bに位置している。シュリンクフィルム20は、装着前の状態では、図3A~図3Bに示すような、上下方向に亘って周長が変化しない筒状をなすが、熱収縮によって胴部12に装着された状態では、図1~図2に示すような、胴部12の外周面に沿う筒状をなしている。 The shrink film 20 is attached to the left and right inclined portions 14 . Lower ends 20 a of the shrink film 20 are positioned at the left and right corners 16 . The upper end portion 20b of the shrink film 20 is positioned at the upper end portion 12b of the body portion 12. As shown in FIG. The shrink film 20 has a cylindrical shape in which the circumferential length does not change in the vertical direction as shown in FIGS. 3A and 3B before being attached. As shown in FIGS. 1 and 2, it has a tubular shape along the outer peripheral surface of the body portion 12 .

シュリンクフィルム20は、筒状のフィルム本体21と、フィルム本体21の内周面に設けられた接着層22とで構成されている。接着層22は、シュリンクフィルム20の下端部20aのみに設けられている。接着層22は、感熱接着剤で形成されており、加熱により胴部12に接着している。つまり、シュリンクフィルム20は、接着層22により、その下端部20aのみにおいて胴部12に接着している。接着層22は、胴部12の左右コーナー部16のみに接着している。接着層22は、左右コーナー部16における湾曲部15に接着している第1部分22aと、左右コーナー部16における左右傾斜部14の下端部14aに接着している第2部分22bとを有している。なお、図2においては、左右コーナー部16における左右一方側のみに接着層22を示している。 The shrink film 20 is composed of a tubular film body 21 and an adhesive layer 22 provided on the inner peripheral surface of the film body 21 . The adhesive layer 22 is provided only on the lower end portion 20 a of the shrink film 20 . The adhesive layer 22 is made of a heat-sensitive adhesive and is adhered to the trunk portion 12 by heating. That is, the shrink film 20 is adhered to the trunk portion 12 by the adhesive layer 22 only at the lower end portion 20a. The adhesive layer 22 adheres only to the left and right corner portions 16 of the trunk portion 12 . The adhesive layer 22 has a first portion 22a that adheres to the curved portion 15 at the left and right corner portions 16, and a second portion 22b that adheres to the lower ends 14a of the left and right inclined portions 14 at the left and right corner portions 16. ing. 2, the adhesive layer 22 is shown only on one side of the left and right corner portions 16. As shown in FIG.

図3A~図3Bに示すように、フィルム本体21は、容器本体10への装着の際に、折り畳まれた筒状の状態から、上面視で略ひし形形状をなすように広げられた筒状の状態にされ、その中心軸線Xを口部11の中心軸線Oに合わせるとともにその長手方向を胴部12の長手方向に合わせた状態で、胴部12の左右傾斜部14を包囲するように配置される。フィルム本体21は、矩形状の前側シート部21aと、前側シート部21aと同一形状の後側シート部21bとから構成されている。前側シート部21aの左右両端縁は、後側シート部21bの左右両端縁に連なっている。したがって、前側シート部21aと後側シート部21bとを互いに離れる方向に湾曲させることにより、その内側に胴部12を配置することができる。フィルム本体21の内周面を形成する前側シート部21a及び後側シート部21bの内面に、接着層22の第1部分22a及び第2部分22bが設けられている。接着層22の第1部分22aは、前側シート部21a及び後側シート部21bに左右方向に互い違いとなるように断続して設けられている。接着層22の第2部分22bは、上下方向に互い違いとなるように設けられている。このような互い違いの配置により、フィルム本体21が折り畳まれた状態のときに接着層22同士の接触を防止できるので、接着層22同士が意図せずに接着するのを防止することができる。 As shown in FIGS. 3A and 3B, when the film body 21 is attached to the container body 10, the film body 21 changes from a folded cylindrical state to a cylindrical shape expanded to form a substantially rhombic shape when viewed from above. With its central axis X aligned with the central axis O of the mouth portion 11 and its longitudinal direction aligned with the longitudinal direction of the body portion 12, it is disposed so as to surround the laterally inclined portion 14 of the body portion 12. be. The film body 21 is composed of a rectangular front sheet portion 21a and a rear sheet portion 21b having the same shape as the front sheet portion 21a. The left and right edges of the front seat portion 21a are connected to the left and right edges of the rear seat portion 21b. Therefore, by bending the front seat portion 21a and the rear seat portion 21b in directions away from each other, the body portion 12 can be arranged inside them. A first portion 22 a and a second portion 22 b of the adhesive layer 22 are provided on the inner surfaces of the front sheet portion 21 a and the rear sheet portion 21 b that form the inner peripheral surface of the film body 21 . The first portions 22a of the adhesive layer 22 are intermittently provided on the front sheet portion 21a and the rear sheet portion 21b alternately in the left-right direction. The second portions 22b of the adhesive layer 22 are provided alternately in the vertical direction. Such a staggered arrangement can prevent contact between the adhesive layers 22 when the film body 21 is folded, thereby preventing the adhesive layers 22 from unintentionally adhering to each other.

フィルム本体21は、熱収縮性を有するフィルムを基材とし、印刷層等を適宜設けることができる。基材は単層又は複数層で構成することができる。基材の材料は、特に限定されないが、例えば、ポリスチレン(PS)樹脂、ポリエステル樹脂、ポリオレフィン樹脂等が好ましい。フィルム本体21の製法は、特に限定されないが、例えば、溶融製膜、溶液製膜等を利用できる。フィルム本体21を複数層で構成する場合には、例えば、共押出法、ドライラミネート法等を利用できる。フィルム本体21は、熱収縮による装着性を発揮させる観点から、周方向の1軸に配向しているのが好ましいが、2軸又は3軸に配向していてもよい。フィルム本体21に配向を施す方法は、特に限定されないが、ロール方式、テンター方式、チューブ方式等による延伸を利用できる。 The film main body 21 is made of a heat-shrinkable film as a base material, and can be appropriately provided with a printed layer or the like. The substrate can be composed of a single layer or multiple layers. Although the material of the base material is not particularly limited, for example, polystyrene (PS) resin, polyester resin, polyolefin resin and the like are preferable. The method of manufacturing the film body 21 is not particularly limited, but for example, melt film forming, solution film forming, or the like can be used. When the film body 21 is composed of a plurality of layers, for example, a coextrusion method, a dry lamination method, or the like can be used. The film body 21 is preferably uniaxially oriented in the circumferential direction from the viewpoint of exhibiting wearability due to heat shrinkage, but may be oriented biaxially or triaxially. A method for orienting the film body 21 is not particularly limited, but stretching by a roll method, a tenter method, a tube method, or the like can be used.

接着層22は、フィルム本体21に例えば塗布(パートコート処理)によって設けることができる。接着層22を形成する感熱接着剤は、特に限定されないが、例えば、熱可塑性樹脂(ベースポリマー)、粘着付与剤及びワックス等で構成されるエマルジョン型、或いはベースポリマー、粘着付与剤、架橋剤、改質剤、有機溶媒等で構成される溶剤型等であってよい。ベースポリマーは、特に限定されないが、例えば、エチレン-酢酸ビニル共重合体(EVA)樹脂等の酢酸ビニル系重合体、アクリル系重合体、スチレン系重合体等が好ましい。接着層22が接着性を生じる温度(活性化温度)は適宜設定できるが、例えば、60℃以上である。接着層22の接着力は、左右傾斜部14にシュリンクフィルム20を装着する際に生じる熱収縮によるシュリンクフィルム20のずり上がりを十分に抑制できるように、左右傾斜部14の形状やシュリンクフィルム20の熱収縮力等に応じて適宜設定することができる。 The adhesive layer 22 can be provided on the film body 21 by, for example, coating (part coating). The heat-sensitive adhesive that forms the adhesive layer 22 is not particularly limited. It may be a solvent type or the like composed of a modifier, an organic solvent, or the like. Although the base polymer is not particularly limited, vinyl acetate polymers such as ethylene-vinyl acetate copolymer (EVA) resins, acrylic polymers, and styrene polymers are preferred. The temperature (activation temperature) at which the adhesive layer 22 exhibits adhesiveness can be set as appropriate, and is, for example, 60° C. or higher. The adhesive strength of the adhesive layer 22 is determined by the shape of the laterally inclined portion 14 and the thickness of the shrink film 20 so as to sufficiently suppress the shrink film 20 from rising due to heat shrinkage that occurs when the shrink film 20 is attached to the laterally inclined portion 14 . It can be appropriately set according to the heat shrinkage force and the like.

容器1は、例えば、以下に説明する方法(本実施の形態に係るシュリンクフィルム付き容器の製造方法)によって製造することができる。 The container 1 can be manufactured, for example, by the method described below (method for manufacturing a container with a shrink film according to the present embodiment).

図4に示すように、本実施の形態に係るシュリンクフィルム付き容器の製造方法は、容器本体形成工程P1、接着工程P2及び熱収縮工程P3を有している。 As shown in FIG. 4, the method for manufacturing a container with a shrink film according to the present embodiment includes a container body forming step P1, an adhering step P2, and a heat shrinking step P3.

容器本体形成工程P1は、口部11、胴部12及び底部13を備える容器本体10を形成する工程である。この容器本体形成工程P1において形成される容器本体10は、上述したように、胴部12が、左右傾斜部14及び左右コーナー部16を有している。 The container body forming step P<b>1 is a step of forming the container body 10 having the mouth portion 11 , the body portion 12 and the bottom portion 13 . In the container body 10 formed in the container body forming step P1, the trunk portion 12 has the left and right inclined portions 14 and the left and right corner portions 16 as described above.

容器本体形成工程P1に次ぐ接着工程P2は、図3A~図3Bに示したような、一端部(下端部20a)のみに位置する感熱接着剤で形成される接着層22を備える筒状のシュリンクフィルム20を、接着層22が位置する端部(下端部20a)が下方側に位置するとともにシュリンクフィルム20が左右傾斜部14を包囲するように配置し、当該端部を加熱することにより、接着層22を胴部12に接着する工程である。 In the bonding step P2 following the container body forming step P1, a cylindrical shrink having an adhesive layer 22 formed of a heat-sensitive adhesive located only at one end (lower end 20a) as shown in FIGS. 3A and 3B. The film 20 is arranged so that the end portion (lower end portion 20a) where the adhesive layer 22 is located (lower end portion 20a) is located on the lower side and the shrink film 20 surrounds the laterally inclined portion 14, and the end portion is heated to bond the film 20. This is the step of adhering the layer 22 to the body 12 .

この接着工程P2においては、例えば、折り畳まれた長尺な筒状をなすとともに所定の位置に予め接着層22が塗布されたフィルムから所定長さの部分をカットし、このカットした部分を広げて筒状のシュリンクフィルム20とし、このシュリンクフィルム20を左右傾斜部14を包囲するように配置することができる。そして、この配置状態で、接着層22が位置する端部を例えば熱風等により局部的に加熱することにより、接着層22に接着力を発現させるとともに当該端部のみにおいてフィルム本体21を熱収縮させて、フィルム本体21を左右コーナー部16に密着させるとともに接着層22を左右コーナー部16に接着することができる。なお、接着性を向上するために、シュリンクフィルム20の配置前に容器本体10を予備加熱してもよい。 In this bonding step P2, for example, a portion of a predetermined length is cut from a film that is folded into a long cylindrical shape and that has been coated with an adhesive layer 22 in advance at a predetermined position, and the cut portion is expanded. A tubular shrink film 20 may be used and arranged so as to surround the laterally inclined portion 14 . Then, in this arranged state, by locally heating the end portion where the adhesive layer 22 is located, for example, with hot air, the adhesive layer 22 develops adhesive strength and the film body 21 is thermally shrunk only at the end portion. By doing so, the film body 21 can be brought into close contact with the left and right corner portions 16 and the adhesive layer 22 can be adhered to the left and right corner portions 16 . In order to improve adhesiveness, the container body 10 may be preheated before the shrink film 20 is arranged.

接着工程P2に次ぐ熱収縮工程P3は、接着層22が胴部12に接着した状態でシュリンクフィルム20の全体を加熱することにより、シュリンクフィルム20を熱収縮させて左右傾斜部14に装着する工程であり、例えば、スチーム式又は熱風式等の炉を通過させることによって行うことができる。 In the heat shrinking step P3 that follows the bonding step P2, the entire shrink film 20 is heated while the adhesive layer 22 is adhered to the body portion 12, thereby heat shrinking the shrink film 20 and attaching it to the laterally inclined portion 14. and, for example, it can be carried out by passing through a steam type or hot air type furnace.

この熱収縮工程P3においては、熱収縮する筒状のシュリンクフィルム20が、傾斜する左右傾斜部14を容器内側に締め付ける。そのため、シュリンクフィルム20には、シュリンクフィルム20を左右傾斜部14に沿ってずり上げる力が作用する。しかし、本実施の形態では、接着工程P2によりシュリンクフィルム20の下端部20aが左右コーナー部16に接着しているので、シュリンクフィルム20のずり上がりを十分に抑制することができる。特に、本実施の形態ではシュリンクフィルム20をずり上げる力が生じる左右傾斜部14の下部に位置する左右コーナー部16で接着しているので、ずり上がりの効果的な抑制が可能である。また、このような左右コーナー部16での接着によってシュリンクフィルム20のずり上がりを抑制することにより、シュリンクフィルム20全体に張りを与えて胴部12へのきれいな装着を実現することができる。 In this heat-shrinking step P3, the heat-shrinkable cylindrical shrink film 20 tightens the left-right inclined portion 14 inside the container. Therefore, a force acts on the shrink film 20 to lift the shrink film 20 along the left and right inclined portions 14 . However, in this embodiment, since the lower end portion 20a of the shrink film 20 is adhered to the left and right corner portions 16 by the adhesion step P2, the shrink film 20 can be sufficiently prevented from riding up. In particular, in the present embodiment, since the shrink film 20 is adhered at the left and right corner portions 16 positioned below the left and right inclined portions 14 which generate a force that pulls up the shrink film 20, it is possible to effectively prevent the shrink film 20 from being pulled up. In addition, by suppressing the shrink film 20 from riding up due to such adhesion at the left and right corner portions 16, the shrink film 20 as a whole can be stretched and can be neatly attached to the trunk portion 12.例文帳に追加

本発明は前記実施の形態に限定されるものではなく、その要旨を逸脱しない範囲で種々変更可能であることはいうまでもない。 It goes without saying that the present invention is not limited to the above-described embodiments, and various modifications can be made without departing from the gist of the present invention.

例えば、左右コーナー部16は、前記実施の形態では胴部12の下端部12aに位置しているが、これに限らず、胴部12の下端部12aより上方に位置してもよい。また、左右傾斜部14が長手方向の両端部又は一端部のみにおいて上方側から下方側に向けて容器内側へ傾斜する場合には、左右コーナー部16は、胴部12の上端部12bに位置してもよいし、胴部12の上端部12bより下方に位置してもよい。 For example, the left and right corner portions 16 are positioned at the lower end portion 12a of the trunk portion 12 in the above embodiment, but are not limited to this and may be positioned above the lower end portion 12a of the trunk portion 12 . In addition, when the left and right inclined portions 14 are inclined toward the inside of the container from the upper side toward the lower side at both ends or only one end in the longitudinal direction, the left and right corner portions 16 are positioned at the upper end portion 12b of the body portion 12. Alternatively, it may be located below the upper end portion 12b of the trunk portion 12. As shown in FIG.

1 シュリンクフィルム付き容器
10 容器本体
11 口部
11a 雄ねじ部
12 胴部
12a 下端部
12b 上端部
13 底部
14 左右傾斜部
14a 下端部
14b 上端部
15 湾曲部
16 左右コーナー部
20 シュリンクフィルム
20a 下端部
20b 上端部
21 フィルム本体
21a 前側シート部
21b 後側シート部
22 接着層
22a 第1部分
22b 第2部分
O、X 中心軸線
L1/L2 偏平率
L1 胴部の長手方向の長さ
L2 胴部の短手方向の長さ
P1 容器本体形成工程
P2 接着工程
P3 熱収縮工程
1 Container with Shrink Film 10 Container Body 11 Mouth 11a Male Thread 12 Body 12a Lower End 12b Upper End 13 Bottom 14 Left/Right Inclined Part 14a Lower End 14b Upper End 15 Curved Part 16 Left/Right Corner 20 Shrink Film 20a Lower End 20b Upper End Portion 21 Film body 21a Front sheet portion 21b Rear sheet portion 22 Adhesive layer 22a First portion 22b Second portion O, X Center axis L1/L2 Flatness L1 Length in longitudinal direction of trunk L2 Short direction of trunk length P1 container body forming process P2 bonding process P3 heat shrinking process

Claims (4)

口部、胴部及び底部を有する容器本体と、前記胴部に装着された筒状のシュリンクフィルムとを有し、
胴部が、上面視で長手方向を規定する偏平形状であり、また、前記長手方向の少なくとも一端部において上下方向の一方側から他方側に向けて容器内側へ傾斜する左右傾斜部を有し、
前記シュリンクフィルムが、前記左右傾斜部に装着され、また、前記シュリンクフィルムの前記一方側の端部のみに位置するとともに前記胴部に接着した感熱接着剤で形成される接着層を有し、
前記胴部が、前記長手方向の両端部に位置するとともに前記左右傾斜部の前記一方側の端部と当該端部から前記一方側に向けて容器内側へ湾曲する湾曲部とで形成される左右コーナー部を有し、
前記接着層が、前記左右コーナー部における前記湾曲部に接着している第1部分と、前記左右コーナー部における前記左右傾斜部の前記一方側の端部に接着している第2部分とを有することを特徴とするシュリンクフィルム付き容器。
A container body having a mouth, a body and a bottom, and a cylindrical shrink film attached to the body,
The body has a flat shape defining a longitudinal direction when viewed from above, and has a laterally inclined portion that slopes toward the inside of the container from one side in the vertical direction to the other side at at least one end in the longitudinal direction,
The shrink film is attached to the left and right inclined portions, and has an adhesive layer formed of a heat-sensitive adhesive that is positioned only at the one end of the shrink film and adhered to the body,
The body portion is located at both ends in the longitudinal direction and is formed by the one-side end portion of the left-right inclined portion and a curved portion that curves from the end portion toward the one side toward the inside of the container. having corners,
The adhesive layer has a first portion adhered to the curved portion at the left and right corner portions, and a second portion adhered to one end portion of the left and right inclined portion at the left and right corner portions. A container with a shrink film, characterized by:
前記左右コーナー部が、前記胴部の下端部に位置する、請求項に記載のシュリンクフィルム付き容器。 2. The container with a shrink film according to claim 1 , wherein said left and right corner portions are positioned at the lower end portion of said body portion. 口部、胴部及び底部を備えるとともに、前記胴部が、上面視で長手方向を規定する偏平形状であり、また、前記長手方向の少なくとも一端部において上下方向の一方側から他方側に向けて内側へ傾斜する左右傾斜部を有する容器本体を形成する容器本体形成工程と、
一端部のみに位置する感熱接着剤で形成される接着層を備える筒状のシュリンクフィルムを、前記一端部が前記一方側に位置するとともに前記シュリンクフィルムが前記左右傾斜部を包囲するように配置し、前記一端部を加熱することにより、前記接着層を前記胴部に接着する接着工程と、
前記接着層が前記胴部に接着した状態で前記シュリンクフィルムの全体を加熱することにより、前記シュリンクフィルムを熱収縮させて前記左右傾斜部に装着する熱収縮工程とを有し、
前記容器本体形成工程において形成する前記容器本体の前記胴部が、前記長手方向の両端部に位置するとともに前記左右傾斜部の前記一方側の端部と当該端部から前記一方側に向けて容器内側へ湾曲する湾曲部とで形成される左右コーナー部を有し、
前記接着工程において、前記接着層の第1部分を前記左右コーナー部における前記湾曲部に接着し、且つ、前記接着層の第2部分を前記左右コーナー部における前記左右傾斜部の前記一方側の端部に接着することを特徴とするシュリンクフィルム付き容器の製造方法。
In addition to having a mouth portion, a trunk portion and a bottom portion, the trunk portion has a flat shape defining a longitudinal direction in a top view, and at least one end portion in the longitudinal direction extends from one side in the vertical direction to the other side. a container body forming step of forming a container body having left and right inclined portions inclined inward;
A cylindrical shrink film having an adhesive layer formed of a heat-sensitive adhesive positioned only at one end is arranged such that the one end is positioned at the one side and the shrink film surrounds the laterally inclined portion. a bonding step of bonding the adhesive layer to the body by heating the one end;
a heat shrinking step of heating the entire shrink film in a state where the adhesive layer is adhered to the body portion, thereby heat shrinking the shrink film and attaching it to the left and right inclined portions ;
The body portion of the container body formed in the container body forming step is located at both ends in the longitudinal direction, and the one side end of the laterally inclined portion and the container extending from the one side end to the one side. having left and right corner portions formed by a curved portion that curves inward,
In the adhering step, the first portion of the adhesive layer is adhered to the curved portion at the left and right corner portions, and the second portion of the adhesive layer is adhered to the one end of the left and right inclined portion at the left and right corner portions. A method for manufacturing a container with a shrink film, characterized by adhering to a part .
前記左右コーナー部が、前記胴部の下端部に位置する、請求項に記載のシュリンクフィルム付き容器の製造方法。 4. The method for manufacturing a container with a shrink film according to claim 3 , wherein the left and right corner portions are positioned at the lower end portion of the body portion.
JP2019064629A 2019-03-28 2019-03-28 CONTAINER WITH SHRINK FILM AND METHOD FOR MANUFACTURING SAME Active JP7218059B2 (en)