JP4791896B2 - 光学用樹脂 - Google Patents
光学用樹脂 Download PDFInfo
- Publication number
- JP4791896B2 JP4791896B2 JP2006171472A JP2006171472A JP4791896B2 JP 4791896 B2 JP4791896 B2 JP 4791896B2 JP 2006171472 A JP2006171472 A JP 2006171472A JP 2006171472 A JP2006171472 A JP 2006171472A JP 4791896 B2 JP4791896 B2 JP 4791896B2
- Authority
- JP
- Japan
- Prior art keywords
- optical
- lens
- resin
- styrene
- molding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Description
(1)スチレン系樹脂が、一般式(1)で表されるフルオレン誘導体を0.1〜20質量%含有してなるスチレン系樹脂組成物。
(2)スチレン系樹脂が、単一のスチレン系単量体を重合して得られたスチレン系樹脂である(1)のスチレン系樹脂組成物。
(3)スチレン系樹脂が、スチレン系単量体及びそのスチレン系単量体と共重合可能な単量体とを重合して得られたスチレン系樹脂であって、該共重合可能な単量体が90質量%以下(但し、0質量%は含まない。)である(1)のスチレン系樹脂組成物。
(4)フルオレン誘導体の、空気気流(200ml/分)中の示差熱分析(昇温速度10℃/分)により測定した10%減量温度が200℃以上である(1)〜(3)のいずれかのスチレン系樹脂組成物。
(5)JIS K7210に基づき測定されたメルトマスフローレイト(MFR)が0.5〜20g/10分である(1)〜(4)のいずれかのスチレン系樹脂組成物。
(6)(1)〜(5)のいずれかのスチレン系樹脂組成物からなる光学用樹脂。
(7)(6)記載の光学用樹脂を成形してなる光学部材。
(8)(6)記載の光学用樹脂を成形してなるレンズ。
(9)レンズが、スクリーンレンズ、フレネルレンズ、レンチキュラーレンズ、眼鏡レンズ、光学機器用レンズ、オプトエレクトロニクス用レンズ、レーザー用レンズ、ピックアップ用レンズ、自動車用ランプレンズ又はOHP用レンズである(8)記載のレンズ。
(10)(6)記載の光学用樹脂を成形してなる光ディスク基板。
(11)(6)記載の光学用樹脂を成形してなる光学シート。
(12)光学シートが、光学用ベースシート、導光板、光拡散板又は集光板である(11)記載の光学シート。
(13)(6)記載の光学用樹脂を成形してなる光学フィルム。
(14)光学フィルムが、光学用ベースフィルム、光反射防止フィルム又は光拡散フィルムである(13)の光フィルム。
(15)(6)記載の光学用樹脂を成形してなる光ファイバー。
である。
容積約20Lの完全混合型攪拌槽である第一反応器と容積約40Lの攪拌機付塔式プラグフロー型反応器である第二反応器を直列に接続し、さらに予熱器を付した脱揮槽を2基直列に接続して構成した。スチレン52質量%、メチルメタクリレート(以下、MMAと略す。)48質量%で構成する単量体溶液85質量部に対し、エチルベンゼン15質量部、t−ブチルパーオキシイソプロピルモノカーボネート0.01質量部、n−ドデシルメルカプタン(以下n−DDMと略す)0.01質量部、オクタデシル−3−(3,5−ジ−t−ブチル−4−ヒドロキシフェニル)プロピオネート0.05質量部を混合し原料溶液とした。
単量体溶液をスチレン100質量%で構成した以外は実験例1と同様に行い高分子樹脂(以下、PSと略す。)を得た。
表1に示す配合で、スチレン系樹脂とフルオレン誘導体を配合し、東芝機械社製2軸押出機TEM−35Bを用いてストランド状に押出し、ペレタイザーにて切断することによりペレット形状のスチレン系樹脂組成物を得た。評価結果を表1に示した。
射出成形機(住友重機械社製サイキャップ165/75)を用いて、シリンダー温度230℃、金型温度50℃で縦90mm、横90mm、厚さ2mmのプレートを成形した。このプレートの中央部を、ASTM D1003に基づきヘーズメーター(日本電色工業社製NDH−1001DP型)を用いてヘーズを測定した(単位:%)。ヘーズが2%以下を合格とした。
透明性と同じプレートの中央部を、色差計(日本電色工業社製Σ−80)を用いて、黄色度の尺度としてb値を測定した。b値が1以下を合格とした。
透明性と同じプレートを用い、プレートの中央部を、位相差測定装置(王子計測社製KOBRA−WR)を用いてリタデーションRe1を測定した(単位:nm)。フルオレン誘導体を配合していない樹脂のリタデーションRe0を用い、下記式でリタデーション保持率(単位:%)を計算した。リタデーション保持率が90%以下を合格とした。
リタデーション保持率(%)=Re1/Re0×100
射出成形機(東芝機械社製IS−50EPN)を用いて、シリンダー温度220℃、金型温度50℃で長さ80mm、幅10mm、厚さ4mmのバーを成形した。この成形品より10mm×10mm×4mmの試験片を切り出し、JIS K7206に基づき、東洋精機製作所社製HDT&VSPT試験装置を用い、50法(荷重50N、昇温速度50℃/時間)でビカット軟化温度(以下、VSTと略す。)を測定した(単位:℃)。VSTが80℃以上を合格とした。
成形中における臭気を1点(無臭)、2点(僅かに臭う)、3点(臭い)、4点(かなり臭い)、5点(耐えられない)の5段階で評価した。2点以下を合格とした。
Claims (15)
- 前記スチレン系樹脂が、単一のスチレン系単量体を重合して得られたスチレン系樹脂であることを特徴とする請求項1記載のスチレン系樹脂組成物。
- 前記スチレン系樹脂が、スチレン系単量体及びそのスチレン系単量体と共重合可能な単量体とを重合して得られたスチレン系樹脂であって、該共重合可能な単量体が90質量%以下(但し、0質量%は含まない。)であることを特徴とする請求項1記載のスチレン系樹脂組成物。
- 前記フルオレン誘導体の、空気気流(200ml/分)中の示差熱分析(昇温速度10℃/分)により測定した10%減量温度が200℃以上であることを特徴とする請求項1〜3のいずれか1項記載のスチレン系樹脂組成物。
- JIS K7210に基づき測定されたメルトマスフローレイト(MFR)が0.5〜20g/10分であることを特徴とする請求項1〜4のいずれか1項記載のスチレン系樹脂組成物。
- 請求項1〜5のいずれか1項に記載のスチレン系樹脂組成物からなることを特徴とする光学用樹脂。
- 請求項6記載の光学用樹脂を成形してなることを特徴とする光学部材。
- 請求項6記載の光学用樹脂を成形してなることを特徴とするレンズ。
- 前記レンズが、スクリーンレンズ、フレネルレンズ、レンチキュラーレンズ、眼鏡レンズ、光学機器用レンズ、オプトエレクトロニクス用レンズ、レーザー用レンズ、ピックアップ用レンズ、自動車用ランプレンズ又はOHP用レンズであることを特徴とする請求項8記載のレンズ。
- 請求項6記載の光学用樹脂を成形してなることを特徴とする光ディスク基板。
- 請求項6記載の光学用樹脂を成形してなることを特徴とする光学シート。
- 前記光学シートが、光学用ベースシート、導光板、光拡散板又は集光板であることを特徴とする請求項11記載の光学シート。
- 請求項6記載の光学用樹脂を成形してなることを特徴とする光学フィルム。
- 前記光学フィルムが、光学用ベースフィルム、光反射防止フィルム又は光拡散フィルムであることを特徴とする請求項13の光フィルム。
- 請求項6記載の光学用樹脂を成形してなることを特徴とする光ファイバー。