JP4234864B2 - Protruded belt and method of manufacturing the same - Google Patents

Protruded belt and method of manufacturing the same Download PDF

Info

Publication number
JP4234864B2
JP4234864B2 JP28771999A JP28771999A JP4234864B2 JP 4234864 B2 JP4234864 B2 JP 4234864B2 JP 28771999 A JP28771999 A JP 28771999A JP 28771999 A JP28771999 A JP 28771999A JP 4234864 B2 JP4234864 B2 JP 4234864B2
Authority
JP
Japan
Prior art keywords
belt
plate
support portion
protrusion
rod
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP28771999A
Other languages
Japanese (ja)
Other versions
JP2001106318A (en
JP2001106318A5 (en
Inventor
隆史 大田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Bando Chemical Industries Ltd
Original Assignee
Bando Chemical Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Bando Chemical Industries Ltd filed Critical Bando Chemical Industries Ltd
Priority to JP28771999A priority Critical patent/JP4234864B2/en
Publication of JP2001106318A publication Critical patent/JP2001106318A/en
Publication of JP2001106318A5 publication Critical patent/JP2001106318A5/ja
Application granted granted Critical
Publication of JP4234864B2 publication Critical patent/JP4234864B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【0001】
【発明の属する技術分野】
本発明は、ベルト背面に突起が設けられた突起付きベルトに関する。
【0002】
【従来の技術】
ベルト背面に突起が設けられた突起付きベルトが広く用いられている。この突起は、ベルト背面で物品を搬送する場合の物品間の仕切りとなったり、ベルトの走行位置を検知するセンサーを作動させたり、物品を押して移動させたり等する機能を果たすものである。
【0003】
そして、このような突起は、ゴムベルトの場合ではベルト背面の研削加工によって形成され、また、注型タイプの熱硬化性ウレタンベルトの場合ではかかる突起が形成されるようにされた注型用金型にウレタンプレポリマー組成物を注入して硬化させることによって形成される。すなわち、いずれの場合にも突起はベルト本体と一体に設けられているものである。
【0004】
ところで、突起が他の物品と接触する搬送等の用途においては、突起がベルト長さ方向に外力を受けて損傷を受けるという問題がある。これに対し、突起のベルト長さ方向の厚さを厚くして突起の耐荷重性を向上させる、という解決手段が考えられる。
【0005】
【発明が解決しようとする課題】
しかしながら、上記の如く突起はベルト本体と一体に設けられているので、突起の厚さを厚くすると、突起部分のベルト剛性が大きいものとなってしまい、小径のプーリにはベルトを適正に巻き掛けることができない、という問題がある。特に、ベルト本体が歯付ベルトである場合、ベルト歯のプーリ溝への噛み合い不良を起こす可能性がある。
【0006】
また、注型タイプの熱硬化性ウレタンベルトの場合、ベルト背面に大きい突起が形成されると注型用金型からの脱型が困難となって加工性が悪い、という問題もある。
【0007】
本発明は、かかる点に鑑みてなされたものであり、その目的とするところは、ベルト背面の突起の強度を高めるために突起のベルト長さ方向の厚さを厚くした場合でも小径のプーリに適正な巻き掛けが可能となり、且つ注型タイプの熱硬化性ウレタンベルトの場合でも加工性に優れる突起付きベルトを提供することにある。
【0008】
【課題を解決するための手段】
本発明は、突起付きベルトにおいて、ベルト背面に板状支持部を立設し、これを覆うように突起部材を設け、この突起部材を板状支持部にのみ固定することとしたものである。
【0009】
具体的には、本出願の発明は、ベルト背面に突起が設けられた突起付きベルトであって、
ベルト背面に一体に設けられ、板面がベルト長さ方向を向くように立設された板状支持部と、
上記板状支持部を覆うように設けられた突起部材とを備え、
上記板状支持部には、その厚さ方向に貫通して両側に突出した状態に棒状部材が取り付けられ、
上記突起部材は、上記棒状部材が取り付けられた上記板状支持部を埋設するように熱可塑性樹脂で形成されていることにより上記板状支持部にのみ固定されていることを特徴とする。
【0010】
上記の構成によれば、突起をベルト長さ方向に厚くして耐荷重性を向上させても、突起を形成する突起部材は板状支持部にのみ固定されている、すなわち、ベルト背面に固定されていないので、突起によってベルト剛性が高くなるということはなく、小径のプーリにも適正な巻き掛けが可能となる。
【0011】
また、注型タイプの熱硬化性ウレタンベルトを製造する場合でも、ベルト背面に板状支持部が設けられたベルト本体を成型すればよく、加工性にも優れるものとなる。
【0012】
さらに、突起が損傷を受けた場合には、突起部材のみの交換による補修をすることができ、突起部材の形成材料の種類によっては摩耗部位または欠損部位にその形成材料を補充する補修も可能となる。
【0013】
また、棒状部材が板状支持部に、その厚さ方向に貫通して両側に突出した状態に取り付けられているので、突起部材は棒状部材を介して板状支持部に強固に固定されることとなり、突起部材が板状支持部から抜けるのが防止される。加えて、板状支持部を単に突起部材に設けた挿入孔に挿入する場合、またはその挿入孔内で接着剤によって板状支持部に突起部材を接着固定する場合に比べて、固定度のバラツキが少ないものとなる。
【0014】
【発明の効果】
以上説明したように、本発明によれば、突起をベルト長さ方向に厚くして耐荷重性を向上させても、突起を形成する突起部材は板状支持部にのみ固定されている、すなわち、ベルト背面には固定されていないので、突起によってベルト剛性が高くなるということはなく、小径のプーリにも適正な巻き掛けが可能となる。また、注型タイプの熱硬化性ウレタンベルトを製造する場合でも、ベルト背面に板状支持部が設けられたベルト本体を成型すればよく、加工性にも優れるものとなる。さらに、突起が損傷を受けた場合には、突起部材のみの交換による補修をすることができ、突起部材の形成材料の種類によっては摩耗部位または欠損部位にその形成材料を補充する補修も可能となる。
【0015】
また、棒状部材が板状支持部に、その厚さ方向に貫通して両側に突出した状態に取り付けられているので、突起部材は棒状部材を介して板状支持部に強固に固定されることとなり、突起部材が板状支持部から抜けるのが防止される。加えて、板状支持部を単に突起部材に設けた挿入孔に挿入する場合、またはその挿入孔内で接着剤によって板状支持部に突起部材を接着固定する場合に比べて、固定度のバラツキが少ないものとなる。
【0016】
【発明の実施の形態】
本発明の実施形態を図面に基づいて詳細に説明する。
【0017】
図1は本発明の実施形態に係るベルトBを示す。このベルトBは、歯付ベルトの一種であって、内面に所定ピッチの歯部2,2,…を有するポリウレタン組成物からなるベルト本体1を備え、そのベルト本体の各歯部2の底部に沿って抗張体としてのアラミド繊維からなる心線3が埋設されている。
【0018】
そして、本発明の特徴として、ベルト背面には板面がベルト長さ方向を向いた板状支持部4がベルト本体1と一体に立設されており、また、その板状支持部4には棒状部材としてのステンレス(SUS)製ピン5が貫通状態で取り付けられている。さらに、板状支持部4とピン5とを覆うようにアセタール樹脂(POM)製の突起部材6が設けられており、この突起部材6がベルト背面にベルト歯約2つ分の突起を形成している。ここで、突起部材6は、ピン5を介して板状支持部4に固定されることとなるが、突起部材6の底面はベルト背面に固定されていない。
【0019】
以上の構成の突起付きベルトBにおいては、突起部材6によって形成された突起はベルト歯約2つ分の厚さを有し、耐荷重性の向上が図られているが、突起部材6は板状支持部4にピン5を介して固定されているだけであり、突起部材6の底面はベルト背面に固定されていないため、突起部材6によってベルト剛性が高くなるということはなく、突起付きベルトBは小径のプーリにも適正な巻き掛けが可能である。
【0020】
また、熱硬化性ウレタンの注型加工によって、ベルト背面に板状支持部4が立設されたベルト本体1を成型すればよいので、大型の突起を成型する必要がなく、容易に脱型でき、加工性にも優れている。
【0021】
さらに、突起が損傷を受けた場合、突起部材6のみを取り除き、下記に示すベルトの製造方法に準じ、新しい突起部材6を設ける補修も可能である。また、突起部材6表面の摩耗または欠損といった軽微な損傷の場合には、突起部材6を取り除くことなく、突起部材6を再度射出金型にセットし、樹脂を射出して摩耗部位または欠損部位に樹脂を補充する補修も可能である。
【0022】
また、突起部材6は、板状支持部4を貫通した状態で埋設されたピン5によって板状支持部4に固定されているので、突起部材6は強固に板状支持部4に固定されることとなり、突起部材6が板状支持部4から抜けるのが防止される。加えて、板状支持部を単に突起部材に設けた挿入孔に挿入する場合、またはその挿入孔内で接着剤によって板状支持部に突起部材を接着固定する場合に比べて、固定度のバラツキが少ない。
【0023】
そして、上記突起付きベルトBは以下のようにして製造される。
【0024】
<ベルト本体形成工程>
ベルト背面に板状支持部が立設された歯付ベルト本体が形成されるようにされた注型用金型にウレタンプレポリマー組成物を注入し、加熱して硬化させる。これによって、板状支持部がベルト背面に一体に立設されたベルト本体が形成されることとなる。なお、注型用金型には上記組成物の注入前に予め心線を緊張状態でセットしておき、ベルトに心線が埋設されるようにしておく。
【0025】
<ピン装着工程(棒状部材取付工程)
板状支持部の中央部に穴を開け、これに棒状部材としてのステンレス(SUS)製ピンを通し、ピンが板状支持部の厚さ方向に貫通して両側に突出した状態に保持された状態とする。
【0026】
<射出金型セット工程>
突起部材を成型するための射出金型内にピンが貫通した板状支持部のみをインサートし、所定位置にセットする。
【0027】
<樹脂射出工程(突起部材形成工程)
射出金型内に溶融したアセタール樹脂(POM)を射出する。これによって板状支持部にピンが貫通した状態で、それらが樹脂で形成された突起部材に埋設されることとなる。
【0028】
<脱型工程>
射出金型からベルトに取り付けられた突起部材を取り出す。
【0029】
以上の突起付きベルトの製造方法によれば、板状支持部が熱可塑性樹脂によって形成された突起部材に覆われ、しかも棒状部材が板状支持部を貫通した状態で突起部材に埋設された構成が容易に得られることとなる。
【0030】
(その他の実施形態)
上記実施形態では、ベルト本体1を歯付ベルトとしたが、これに限定されるものではなく、平ベルト、Vベルト等であってもよい。
【0031】
また、上記実施形態では、ベルト本体1を熱硬化性ポリウレタンで形成したものとしたが、これに限定されるものではなく、ゴムで形成されたものであってもよい。
【0032】
また、上記実施形態では、棒状部材としてピン5を用いたが、特にこれに限定されるものではなく、ボルト等の棒状のものであればよい。また、棒状部材はステンレス(SUS)、砲金材(BSBM)、アルミニウム等の金属製の他、樹脂製等であってもよい。
【0033】
また、上記実施形態では、板状支持部4に棒状部材としてのピン5を1本だけ取り付けたが、これを複数本取り付けてもよい。このようにすることにより、突起部材の板状支持部への固定がより強固なものとすることができる。
【0034】
また、上記実施形態では、突起部材6をアセタール樹脂(POM)製としたが、特にこれに限定されるものではなく、ポリアミド樹脂(PA)、ポリカーボネート樹脂(PC)、アクリロノトリル−ブタジエン−スチレン樹脂(ABS)等であってもよい。
【0035】
また、上記実施形態では、板状支持部4に貫通したピン5により、突起部材6が板状支持部4に固定された構成としたが、特にこれに限定されるものではなく、例えば板状支持部を挿入できる挿入孔を設けた突起部材を予め形成し、その挿入孔に接着剤を流し込み、それに板状支持部を挿入して接着剤を硬化させる等の構成であってもよい。
【図面の簡単な説明】
【図1】 本発明の実施形態に係るベルトの断面図である。
【符号の説明】
1 ベルト本体
2 歯部
3 心線
4 板状支持部
5 ピン
6 突起部材
[0001]
BACKGROUND OF THE INVENTION
The present invention relates to a belt with protrusions provided with protrusions on the back surface of the belt.
[0002]
[Prior art]
A belt with a protrusion having a protrusion provided on the back surface of the belt is widely used. This protrusion serves as a partition between articles when the article is conveyed on the back of the belt, activates a sensor for detecting the belt running position, or pushes and moves the article.
[0003]
In the case of a rubber belt, such a protrusion is formed by grinding the back surface of the belt, and in the case of a casting type thermosetting urethane belt, such a protrusion is formed. It is formed by injecting and curing a urethane prepolymer composition. That is, in any case, the protrusion is provided integrally with the belt body.
[0004]
By the way, in applications such as conveyance in which the protrusions come into contact with other articles, there is a problem that the protrusions are damaged by receiving an external force in the belt length direction. On the other hand, there can be considered a solution to increase the load resistance of the protrusion by increasing the thickness of the protrusion in the belt length direction.
[0005]
[Problems to be solved by the invention]
However, since the protrusion is provided integrally with the belt body as described above, increasing the thickness of the protrusion increases the belt rigidity of the protrusion, so that the belt is properly wound around a small-diameter pulley. There is a problem that can not be. In particular, when the belt body is a toothed belt, there is a possibility that the meshing failure of the belt teeth with the pulley groove may occur.
[0006]
In addition, in the case of a casting type thermosetting urethane belt, if a large protrusion is formed on the back surface of the belt, it is difficult to remove from the casting mold, resulting in poor workability.
[0007]
The present invention has been made in view of the above points, and the object of the present invention is to make a pulley with a small diameter even when the thickness of the protrusion in the belt length direction is increased in order to increase the strength of the protrusion on the back surface of the belt. An object of the present invention is to provide a protrusion-provided belt that can be properly wound and is excellent in workability even in the case of a cast-type thermosetting urethane belt.
[0008]
[Means for Solving the Problems]
In the belt with protrusions, the present invention is such that a plate-like support portion is erected on the back surface of the belt, a protrusion member is provided so as to cover it, and the protrusion member is fixed only to the plate-like support portion.
[0009]
Specifically, the invention of the present application is a belt with a protrusion provided with a protrusion on the back surface of the belt,
A plate-like support portion that is integrally provided on the back surface of the belt and is erected so that the plate surface faces the belt length direction;
A projection member provided so as to cover the plate-like support portion,
A rod-like member is attached to the plate-like support portion in a state of penetrating in the thickness direction and protruding to both sides,
The protrusion member is fixed only to the plate-like support portion by being formed of a thermoplastic resin so as to embed the plate-like support portion to which the rod-like member is attached .
[0010]
According to the above configuration, even if the protrusion is thickened in the belt length direction to improve the load resistance, the protrusion member forming the protrusion is fixed only to the plate-like support portion, that is, fixed to the back surface of the belt. As a result, the belt rigidity is not increased by the protrusions, and appropriate winding is possible even on a small-diameter pulley.
[0011]
Further, even when a cast type thermosetting urethane belt is manufactured, a belt main body provided with a plate-like support portion on the back surface of the belt may be molded, and the processability is excellent.
[0012]
In addition, if the projection is damaged, it can be repaired by replacing only the projection member, and depending on the type of projection member forming material, it is also possible to repair by replenishing the forming material to the worn part or defective part Become.
[0013]
Further, since the rod-like member is attached to the plate-like support portion so as to penetrate in the thickness direction and protrude on both sides, the protruding member is firmly fixed to the plate-like support portion via the rod-like member. Thus, the protruding member is prevented from coming off from the plate-like support portion. In addition, when the plate-like support portion is simply inserted into the insertion hole provided in the projection member, or when the projection member is bonded and fixed to the plate-like support portion with an adhesive in the insertion hole, the degree of fixation is different. Will be less.
[0014]
【The invention's effect】
As described above, according to the present invention, even if the protrusion is thickened in the belt length direction to improve the load resistance, the protrusion member that forms the protrusion is fixed only to the plate-like support portion. Since the belt is not fixed to the back surface of the belt, the protrusion does not increase the rigidity of the belt, and it is possible to appropriately wind a pulley having a small diameter. Further, even when a cast type thermosetting urethane belt is manufactured, a belt main body provided with a plate-like support portion on the back surface of the belt may be molded, and the processability is excellent. In addition, if the projection is damaged, it can be repaired by replacing only the projection member, and depending on the type of projection member forming material, it is also possible to repair by replenishing the forming material to the worn part or defective part Become.
[0015]
Further, since the rod-like member is attached to the plate-like support portion so as to penetrate in the thickness direction and protrude on both sides, the protruding member is firmly fixed to the plate-like support portion via the rod-like member. Thus, the protruding member is prevented from coming off from the plate-like support portion. In addition, when the plate-like support portion is simply inserted into the insertion hole provided in the projection member, or when the projection member is bonded and fixed to the plate-like support portion with an adhesive in the insertion hole, the degree of fixation is different. Will be less.
[0016]
DETAILED DESCRIPTION OF THE INVENTION
Embodiments of the present invention will be described in detail with reference to the drawings.
[0017]
FIG. 1 shows a belt B according to an embodiment of the present invention. The belt B is a kind of toothed belt, and includes a belt body 1 made of a polyurethane composition having teeth 2, 2,... With a predetermined pitch on the inner surface, and is provided at the bottom of each tooth 2 of the belt body. A cord 3 made of an aramid fiber as a tensile body is embedded along the line.
[0018]
As a feature of the present invention, a plate-like support portion 4 having a plate surface facing the belt length direction is erected integrally with the belt main body 1 on the back surface of the belt. A stainless steel (SUS) pin 5 as a rod-like member is attached in a penetrating state. Further, a projection member 6 made of acetal resin (POM) is provided so as to cover the plate-like support portion 4 and the pin 5, and this projection member 6 forms a projection of about two belt teeth on the back surface of the belt. ing. Here, the protruding member 6 is fixed to the plate-like support portion 4 via the pin 5, but the bottom surface of the protruding member 6 is not fixed to the belt back surface.
[0019]
In the belt B with protrusions having the above-described structure, the protrusion formed by the protrusion member 6 has a thickness equivalent to about two belt teeth, and the load resistance is improved. Since the bottom surface of the protruding member 6 is not fixed to the back surface of the belt, the belt rigidity is not increased by the protruding member 6, and the belt with the protrusion is not fixed. B can be properly wound around a small-diameter pulley.
[0020]
Further, since the belt main body 1 having the plate-like support portion 4 standing on the back surface of the belt may be molded by casting a thermosetting urethane, it is not necessary to mold a large protrusion and can be easily removed from the mold. Excellent workability.
[0021]
Further, when the protrusion is damaged, it is possible to repair only by removing the protrusion member 6 and providing a new protrusion member 6 in accordance with the belt manufacturing method described below. In the case of minor damage such as wear or loss on the surface of the protruding member 6, the protruding member 6 is set again on the injection mold without removing the protruding member 6, and the resin is injected to the worn or defective portion. Repair that replenishes the resin is also possible.
[0022]
Further, since the protruding member 6 is fixed to the plate-like support portion 4 by the pin 5 embedded in a state penetrating the plate-like support portion 4, the protruding member 6 is firmly fixed to the plate-like support portion 4. As a result, the protruding member 6 is prevented from coming off from the plate-like support portion 4. In addition, when the plate-like support portion is simply inserted into the insertion hole provided in the projection member, or when the projection member is bonded and fixed to the plate-like support portion with an adhesive in the insertion hole, the degree of fixation is different. Less is.
[0023]
And the said belt B with a protrusion is manufactured as follows.
[0024]
<Belt body forming process>
A urethane prepolymer composition is poured into a casting mold in which a toothed belt body having a plate-like support portion standing on the back surface of the belt is formed, and is cured by heating. As a result, a belt main body in which the plate-like support portion is integrally provided on the back surface of the belt is formed. Note that the core wire is set in a tensioned state in advance in the casting mold before the composition is injected, and the core wire is embedded in the belt.
[0025]
<Pin mounting process (rod-shaped member mounting process) >
A hole was made in the central part of the plate-like support part, and a stainless steel (SUS) pin as a rod-like member was passed through this, and the pin was held in a state where it penetrated in the thickness direction of the plate-like support part and protruded on both sides . State.
[0026]
<Injection mold setting process>
Insert only the plate-like support part through which the pin penetrates into the injection mold for molding the protruding member, and set it at a predetermined position.
[0027]
<Resin injection process (projection member formation process) >
A molten acetal resin (POM) is injected into the injection mold. As a result, with the pins penetrating the plate-like support portion, they are embedded in the protruding member formed of resin.
[0028]
<Demolding process>
The protruding member attached to the belt is taken out from the injection mold.
[0029]
According to the manufacturing method of the belt with protrusions described above, the plate-like support portion is covered with the protrusion member formed of the thermoplastic resin, and the rod-like member is embedded in the protrusion member in a state of penetrating the plate-like support portion. Is easily obtained.
[0030]
(Other embodiments)
In the above embodiment, the belt main body 1 is a toothed belt, but is not limited thereto, and may be a flat belt, a V belt, or the like.
[0031]
Moreover, in the said embodiment, although the belt main body 1 shall be formed with the thermosetting polyurethane, it is not limited to this, You may be formed with rubber | gum.
[0032]
Moreover, in the said embodiment, although the pin 5 was used as a rod-shaped member, it is not specifically limited to this, What is necessary is just a rod-shaped thing, such as a volt | bolt. The rod-shaped member may be made of metal such as stainless steel (SUS), gun metal (BSBM), aluminum, or resin.
[0033]
Moreover, in the said embodiment, although the single pin 5 as a rod-shaped member was attached to the plate-shaped support part 4, you may attach multiple this. By doing in this way, fixation to the plate-shaped support part of a projection member can be made stronger.
[0034]
Moreover, in the said embodiment, although the projection member 6 was made from acetal resin (POM), it is not specifically limited to this, Polyamide resin (PA), polycarbonate resin (PC), acrylonotriyl-butadiene-styrene resin ( ABS) or the like.
[0035]
Moreover, in the said embodiment, although it was set as the structure by which the projection member 6 was fixed to the plate-shaped support part 4 with the pin 5 penetrated to the plate-shaped support part 4, it is not limited to this in particular, For example, plate shape It may be configured such that a protruding member provided with an insertion hole into which the support portion can be inserted is formed in advance, an adhesive is poured into the insertion hole, and a plate-like support portion is inserted therein to cure the adhesive.
[Brief description of the drawings]
FIG. 1 is a cross-sectional view of a belt according to an embodiment of the present invention.
[Explanation of symbols]
DESCRIPTION OF SYMBOLS 1 Belt main body 2 Tooth part 3 Core wire 4 Plate-shaped support part 5 Pin 6 Projection member

Claims (2)

ベルト背面に突起が設けられた突起付きベルトであって、
ベルト背面に一体に設けられ、板面がベルト長さ方向を向くように立設された板状支持部と、
上記板状支持部を覆うように設けられた突起部材とを備え、
上記板状支持部には、その厚さ方向に貫通して両側に突出した状態に棒状部材が取り付けられ、
上記突起部材は、上記棒状部材が取り付けられた上記板状支持部を埋設するように熱可塑性樹脂で形成されていることにより上記板状支持部にのみ固定されていることを特徴とする突起付きベルト。
A belt with protrusions with protrusions on the back of the belt,
A plate-like support portion that is integrally provided on the back surface of the belt and is erected so that the plate surface faces the belt length direction;
A projection member provided so as to cover the plate-like support portion,
A rod-like member is attached to the plate-like support portion in a state of penetrating in the thickness direction and protruding to both sides,
The projection member is formed of a thermoplastic resin so as to embed the plate-like support portion to which the rod-like member is attached, so that the projection member is fixed only to the plate-like support portion. belt.
請求項1に記載された突起付きベルトの製造方法であって、
板面がベルト長さ方向を向いた板状支持部がベルト背面に一体に立設されたベルト本体を形成するベルト本体形成工程と、
上記ベルト本体形成工程で形成した上記ベルト本体の上記板状支持部に、その厚さ方向に貫通して両側に突出した状態に棒状部材を取り付ける棒状部材取付工程と、
上記棒状部材取付工程で上記棒状部材を取り付けた上記ベルト本体の上記板状支持部を溶融した熱可塑性樹脂で覆い、該熱可塑性樹脂を固化させることによって該棒状部材が取り付けられた該板状支持部を埋設した上記突起部材を形成する突起部材形成工程と、
を備えたことを特徴とする突起付きベルトの製造方法。
It is a manufacturing method of the belt with a projection according to claim 1 ,
A belt body forming step of forming a belt body in which a plate-like support portion whose plate surface faces the belt length direction is integrally provided on the back surface of the belt;
A rod-shaped member attaching step for attaching a rod-shaped member to the plate-like support portion of the belt body formed in the belt body forming step, in a state of penetrating in the thickness direction and projecting on both sides;
Rodlike member attaching step is covered with the plate-like supporting portion thermoplastic resin melt of the belt body fitted with the rod member, said plate supporting said rod-like member is attached by solidifying the thermoplastic resin a protrusion member forming step of forming the protrusion members that are embedded parts,
A method for manufacturing a belt with protrusions.
JP28771999A 1999-10-08 1999-10-08 Protruded belt and method of manufacturing the same Expired - Fee Related JP4234864B2 (en)