JP3259909B2 - Deflection yoke tightening band, deflection yoke, and method of manufacturing deflection yoke tightening band - Google Patents

Deflection yoke tightening band, deflection yoke, and method of manufacturing deflection yoke tightening band

Info

Publication number
JP3259909B2
JP3259909B2 JP16300998A JP16300998A JP3259909B2 JP 3259909 B2 JP3259909 B2 JP 3259909B2 JP 16300998 A JP16300998 A JP 16300998A JP 16300998 A JP16300998 A JP 16300998A JP 3259909 B2 JP3259909 B2 JP 3259909B2
Authority
JP
Japan
Prior art keywords
deflection yoke
bolt
lubricant
pair
tightening band
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP16300998A
Other languages
Japanese (ja)
Other versions
JP2000030634A (en
Inventor
崇▲祐▼ 古賀
雄輔 大川
洋二 本宮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Victor Company of Japan Ltd
Original Assignee
Victor Company of Japan Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Victor Company of Japan Ltd filed Critical Victor Company of Japan Ltd
Priority to JP16300998A priority Critical patent/JP3259909B2/en
Priority to TW87116096A priority patent/TW379352B/en
Priority to KR1019980043103A priority patent/KR100306100B1/en
Publication of JP2000030634A publication Critical patent/JP2000030634A/en
Application granted granted Critical
Publication of JP3259909B2 publication Critical patent/JP3259909B2/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は、偏向ヨークを陰極
線管(CRT)のネック部に固定するための偏向ヨーク
締付バンド及び偏向ヨーク、並びに、偏向ヨーク締付バ
ンドの製造方法に関する。
The present invention relates to the deflection yoke clamping band and a deflection yoke for securing to the neck of a cathode ray tube (CRT) deflection yoke, and relates to the production how dated deflection yoke clamping band.

【0002】[0002]

【従来の技術】漏斗状に形成されたセパレータを備えた
偏向ヨークをCRTのネック部に固定する際には、セパ
レータの小径側の先端の円筒部を偏向ヨーク締付バンド
によって締め付けることは周知のことである。
2. Description of the Related Art It is well known that when a deflection yoke having a funnel-shaped separator is fixed to a neck portion of a CRT, a cylindrical portion at a small diameter side of the separator is fastened by a deflection yoke tightening band. That is.

【0003】ここで、偏向ヨーク締付バンド(以下、締
付バンドと略記する)の一般的構成について、図7を用
いて説明する。図7は一般的な締付バンド8を示す斜視
図である。図7に示すように、締付バンド8は、円周部
8aと、この円周部8aの両端部より突出した突出片8
b,8bと、この突出片8bに形成された穴を貫通する
ように取り付けられたボルト8cとよりなる。なお、円
周部8aと突出片8bとは一体的に形成されている。締
付バンド8は、偏向ヨークが発生する磁界特性に影響を
与えないよう、例えばオーステナイト系ステンレス鋼等
の非磁性材を用いるのが一般的である。
Here, a general configuration of a deflection yoke tightening band (hereinafter, abbreviated as a tightening band) will be described with reference to FIG. FIG. 7 is a perspective view showing a general fastening band 8. As shown in FIG. 7, the tightening band 8 includes a circumferential portion 8a and protruding pieces 8 protruding from both ends of the circumferential portion 8a.
b, 8b and a bolt 8c attached so as to pass through a hole formed in the protruding piece 8b. The circumferential portion 8a and the protruding piece 8b are formed integrally. The tightening band 8 is generally made of a non-magnetic material such as austenitic stainless steel so as not to affect the magnetic field characteristics generated by the deflection yoke.

【0004】この締付バンド8の円周部8aには、ここ
では図示していない偏向ヨークにおけるセパレータの小
径側の先端の円筒部に設けられた一対の突起に係合する
ための2つの係合穴8a1,8a1が設けられている。円周
部8aの径は、セパレータの円筒部の径より若干大きく
形成されており、締付バンド8は、円周部8aがセパレ
ータの円筒部の外周を覆うように装着される。そして、
係合穴8a1,8a1を前述の突起に係合させて円筒部に係
止させる。
The circumferential portion 8a of the tightening band 8 is provided with two engaging members for engaging a pair of projections provided on a cylindrical portion at the distal end of the deflection yoke (not shown) on the small diameter side of the separator. The mating holes 8a1 and 8a1 are provided. The diameter of the circumferential portion 8a is slightly larger than the diameter of the cylindrical portion of the separator, and the tightening band 8 is mounted so that the circumferential portion 8a covers the outer periphery of the cylindrical portion of the separator. And
The engaging holes 8a1 and 8a1 are engaged with the above-mentioned projections and are locked on the cylindrical portion.

【0005】突出片8bに形成された穴の内、ボルト8
cの頭8c1とは反対側の穴にはねじが切られていて、ボ
ルト8cはこのねじ穴に螺合している。従って、ボルト
8cを回転させることにより、締付バンド8の円周内寸
法が変化する。締付バンド8を円筒部に嵌め込んだ状態
で、円周内寸法を小さくする方向にボルト8cを回転さ
せると、円筒部は可撓性を有しているので、円周部8a
が円筒部を介してCRTのネック部を締め付ける。この
ようにして、偏向ヨークは締付バンド8によってCRT
のネック部に固定される。
[0005] Of the holes formed in the protruding piece 8b, the bolt 8
The hole on the side opposite to the head 8c1 of c is threaded, and the bolt 8c is screwed into this screw hole. Therefore, by rotating the bolt 8c, the inner circumferential size of the tightening band 8 changes. When the bolt 8c is rotated in a direction to reduce the inner circumferential size in a state where the tightening band 8 is fitted in the cylindrical portion, the cylindrical portion has flexibility, so that the circumferential portion 8a is formed.
Tightens the neck of the CRT through the cylindrical part. In this way, the deflection yoke is connected to the CRT by the tightening band 8.
It is fixed to the neck part.

【0006】[0006]

【発明が解決しようとする課題】ところで、締付バンド
8を偏向ヨークにおけるセパレータの円筒部に装着して
偏向ヨークをCRTのネック部に固定するに際しては、
偏向ヨークが外部からの衝撃や振動でCRTから外れた
りすることがないよう、ボルト8cを高トルクで回転さ
せてCRTのネック部を締め付けるようにしている。こ
のとき、偏向ヨークのCRTへの固定作業時間を短縮し
て生産性を向上させるべく、電動ドライバ等の工具を用
いることが一般的である。従って、ボルト8cにはかな
りの力がかかることとなる。
When the fastening band 8 is mounted on the cylindrical portion of the separator of the deflection yoke and the deflection yoke is fixed to the neck portion of the CRT,
The bolt 8c is rotated with a high torque to tighten the neck of the CRT so that the deflection yoke does not come off the CRT due to an external shock or vibration. At this time, it is common to use a tool such as an electric screwdriver in order to shorten the time for fixing the deflection yoke to the CRT and improve productivity. Therefore, a considerable force is applied to the bolt 8c.

【0007】また、締付バンド8が偏向ヨークにおける
セパレータの円筒部に正しく装着されていない状態でボ
ルト8cを回転させてしまった場合にも、ボルト8cに
は無理な力がかかってしまうことがある。さらには、一
旦CRTに装着した偏向ヨークを、再調整等のためにC
RTより外して再装着することもある。この場合には複
数回の締め付け作業が行われ、ボルト8cには無理な力
がかかってしまうこととなる。
Also, if the bolt 8c is rotated in a state where the tightening band 8 is not properly mounted on the cylindrical portion of the separator in the deflection yoke, an excessive force may be applied to the bolt 8c. is there. Further, the deflection yoke once mounted on the CRT is moved to C
It may be removed from the RT and remounted. In this case, a plurality of tightening operations are performed, and an excessive force is applied to the bolt 8c.

【0008】以上のようにして、突出片8bのねじ穴に
螺合したボルト8cを回転させる際、ねじ穴のねじ部と
ボルト8cとの間に強い力が加わったり、必要以上に摺
動が繰り返されたりすると、ボルト8cが突出片8bの
ねじ部にかじってしまったり、焼き付いてしまうことが
ある。
As described above, when the bolt 8c screwed into the screw hole of the protruding piece 8b is rotated, a strong force is applied between the screw portion of the screw hole and the bolt 8c, or the sliding is performed more than necessary. If repeated, the bolt 8c may bite or seize the thread of the protruding piece 8b.

【0009】ボルト8cと突出片8bのねじ部との間に
かじりや焼き付きが一旦発生してしまうと、ボルト8c
は回転しなくなってしまい、円周部8aの円周内寸法を
変化させることができなくなってしまう。この場合に
は、その締付バンド8を装着した偏向ヨークは不良品と
なってしまい、その締付バンド8を破壊して取り外し、
新たな締付バンド8を装着しなければならない。従っ
て、余分なコストがかかり、余分な作業が発生してしま
うこととなる。
Once galling or seizure occurs between the bolt 8c and the thread of the protruding piece 8b, the bolt 8c
Will not rotate, and it will not be possible to change the in-circle dimension of the circumferential portion 8a. In this case, the deflection yoke to which the tightening band 8 is attached becomes defective, and the tightening band 8 is destroyed and removed.
A new tightening band 8 must be fitted. Therefore, extra cost is required and extra work is required.

【0010】さらには、締付バンド8が変形してしま
い、この変形した締付バンド8を取り外すために、偏向
ヨークやCRTを破壊させてしまうということもあっ
た。
Furthermore, the fastening band 8 may be deformed, and in order to remove the deformed fastening band 8, the deflection yoke or the CRT may be broken.

【0011】本発明はこのような問題点に鑑みなされた
ものであり、ねじ部に対するボルトのかじりや焼き付き
を極めて効果的に防止することができる偏向ヨーク締付
バンド及び偏向ヨーク、並びに、偏向ヨーク締付バンド
の製造方法を提供することを目的とする。
SUMMARY OF THE INVENTION The present invention has been made in view of the above problems, and a deflection yoke tightening band and a deflection yoke capable of extremely effectively preventing galling and seizure of a bolt on a thread portion, and a deflection yoke. an object of the present invention is to provide a manufacturing how the tightening band.

【0012】[0012]

【課題を解決するための手段】本発明は、上述した従来
の技術の課題を解決するため、以下の偏向ヨーク締付バ
ンド及び偏向ヨーク、並びに、偏向ヨーク締付バンドの
製造方法を提供する。 (1)漏斗状のセパレータを備えた偏向ヨークを陰極線
管のネック部に固定するための偏向ヨーク締付バンドで
あり、前記セパレータの小径側先端の円筒部に当接する
円周部と、この円周部の両端部より外方向に突出した1
対の突出片と、この1対の突出片に形成された少なくと
も一方がねじ穴とされた1対の穴を貫通するように取り
付けられたボルトとを備えた偏向ヨーク締付バンドにお
いて、前記ボルトの表面に、以下の分子構造を有する液
状のフッ素系潤滑剤を3×10-3〜13×10-3mg/
mm2なる付着量で付着させたことを特徴とする偏向ヨ
ーク締め付けバンド。
SUMMARY OF THE INVENTION In order to solve the above-mentioned problems of the prior art, the present invention provides the following deflection yoke tightening bar.
And deflection yoke, and deflection yoke tightening band
A manufacturing method is provided. (1) A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, and a circumferential portion abutting on a cylindrical portion at a small diameter end of the separator; 1 protruding outward from both ends of the periphery
A deflection yoke tightening band, comprising: a pair of projecting pieces; and a bolt attached to the pair of projecting pieces so that at least one of the projecting pieces passes through a pair of screw holes. Liquid having the following molecular structure on the surface of
Jo fluorine Cajun lubricant to 3 × 10 -3 ~13 × 10 -3 mg /
A deflection yoke tightening band, wherein the band is attached with an attachment amount of mm 2 .

【化1】 (2)陰極線管のネック部に装着される漏斗状のセパレ
ータを備えた偏向ヨークであり、前記セパレータの小径
側先端の円筒部に当接する円周部と、この円周部の両端
部より外方向に突出した1対の突出片と、この1対の突
出片に形成された少なくとも一方がねじ穴とされた1対
の穴を貫通するように取り付けられたボルトとを備えた
偏向ヨーク締付バンドによって前記ネック部に固定され
る偏向ヨークにおいて、前記偏向ヨーク締付バンドの前
記ボルトの表面に、以下の分子構造を有する液状のフッ
系潤滑剤を3×10-3〜13×10-3mg/mm2
る付着量で付着させたことを特徴とする偏向ヨーク。
Embedded image (2) A deflection yoke provided with a funnel-shaped separator attached to the neck of a cathode ray tube, wherein the deflection yoke is in contact with a cylindrical portion at the tip on the small diameter side of the separator, and is located outside both ends of the circumference. Deflection yoke tightening comprising: a pair of projecting pieces projecting in the direction; and a bolt formed so as to pass through a pair of holes formed at least one of the threaded holes in the pair of projecting pieces. in the deflection yoke fixed to the neck portion by the band, said the surface of the bolt of the deflection yoke clamping band, hydrofluoric <br/> containing Cajun lubricant to 3 × 10 -3 ~ liquid having the following molecular structure A deflection yoke having an adhesion amount of 13 × 10 −3 mg / mm 2 .

【化1】 (3)漏斗状のセパレータを備えた偏向ヨークを陰極線
管のネック部に固定するための偏向ヨーク締付バンドで
あり、両端部より外方向に突出した1対の突出片を有
し、前記セパレータの小径側先端の円筒部に当接する円
周部と、前記1対の突出片に形成された少なくとも一方
がねじ穴とされた1対の穴を貫通するように取り付けら
れたボルトとよりなる偏向ヨーク締付バンドを製造する
ための偏向ヨーク締付バンドの製造方法において、前記
ボルトの表面に、以下の分子構造を有する液状のフッ素
系潤滑剤を3×10-3〜13×10-3mg/mm2なる
付着量で付着させる第1の工程と、前記突出片の前記1
対の穴に前記ボルトを取り付けて、前記円周部と前記ボ
ルトとを一体化する第2の工程とをいずれかの順で含む
ことを特徴とする偏向ヨーク締付バンドの製造方法。
Embedded image (3) A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, the separator having a pair of projecting pieces projecting outward from both ends. A deflection portion comprising: a circumferential portion abutting on a cylindrical portion at the tip of the small diameter side; and a bolt attached to at least one of the pair of projecting pieces so as to pass through a pair of screw holes. In a method of manufacturing a deflection yoke tightening band for manufacturing a yoke tightening band , a liquid fluorine having the following molecular structure is provided on the surface of the bolt.
A first step of adhering the Cajun lubricant at 3 × 10 -3 ~13 × 10 -3 mg / mm 2 comprising attachment amount, the said projecting piece 1
A second step of attaching the bolts to the pair of holes and integrating the circumferential portion and the bolts in any order.

【化1】 (4)漏斗状のセパレータを備えた偏向ヨークを陰極線
管のネック部に固定するための偏向ヨーク締付バンドで
あり、両端部より外方向に突出した1対の突出片を有
し、前記セパレータの小径側先端の円筒部に当接する円
周部と、前記1対の突出片に形成された少なくとも一方
がねじ穴とされた1対の穴を貫通するように取り付けら
れたボルトとよりなる偏向ヨーク締付バンドを製造する
ための偏向ヨーク締付バンドの製造方法において、前記
ボルトを、以下の分子構造を有する液状のフッ素系潤
剤を含んだ液体に、その液体を循環もしくは撹拌させつ
つ所定時間浸漬させて、3×10 -3 〜13×10 -3 mg
/mm 2 なる付着量で付着させる第1の工程と、前記第
1の工程によって前記潤滑剤が付着した前記ボルトを、
前記突出片の前記1対の穴に取り付けて、前記円周部と
前記ボルトとを一体化する第2の工程とを含むことを特
徴とする偏向ヨーク締付バンドの製造方法。
Embedded image (4) A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, the separator having a pair of projecting pieces projecting outward from both ends. A deflection portion comprising: a circumferential portion abutting on a cylindrical portion at the tip of the small diameter side; and a bolt attached to at least one of the pair of projecting pieces so as to pass through a pair of screw holes. the method of manufacturing a deflection yoke clamping band for producing yoke clamping band, the bolt, the liquid containing the fluorine Cajun lubricant liquid having the following molecular structure, with recycled or stirring the liquid given 3 × 10 -3 to 13 × 10 -3 mg
A first step of adhering with an adhesion amount of / mm 2 and the bolt to which the lubricant has adhered in the first step.
A second step of attaching to the pair of holes of the protruding piece to integrate the circumferential portion and the bolt.

【化1】 Embedded image

【0013】[0013]

【発明の実施の形態】以下、本発明の偏向ヨーク締付バ
ンド及び偏向ヨーク、並びに、偏向ヨーク締付バンドの
製造方法について、添付図面を参照して説明する。図1
は本発明の偏向ヨーク締付バンドの一実施例を示す斜視
図、図2は本発明の偏向ヨークの一実施例を示す斜視図
で、図3は本発明の偏向ヨーク締付バンドによって偏向
ヨークを陰極線管に装着した状態を示す側面図、図4は
本発明の偏向ヨーク締付バンドの製造方法を説明するた
めの一部破断の断面図、図5及び図6は本発明の偏向ヨ
ーク締付バンドの製造方法を説明するための平面図
る。なお、図1及び図2において、図7と同一部分には
同一符号が付してある。
DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, the deflection yoke clamping band and deflection yoke of the present invention, as well, with the production how dated deflection yoke clamping band will be described with reference to the accompanying drawings. FIG.
FIG. 2 is a perspective view showing one embodiment of the deflection yoke tightening band of the present invention, FIG. 2 is a perspective view showing one embodiment of the deflection yoke of the present invention, and FIG. 3 is a deflection yoke using the deflection yoke tightening band of the present invention. FIG. 4 is a side view showing a state in which is mounted on a cathode ray tube, FIG. 4 is a partially cutaway sectional view for explaining a method of manufacturing a deflection yoke tightening band of the present invention, and FIGS. Oh <br/> Ru in plan view for explaining the manufacturing method of biasing bands. 1 and 2, the same parts as those in FIG. 7 are denoted by the same reference numerals.

【0014】まず、図2を用いて本発明の偏向ヨーク締
付バンド(以下、締付バンドと略記する)を装着する本
発明の偏向ヨークの構成について説明する。図2に示す
偏向ヨーク1は、例えば1対の半環状セパレータ2を組
み合わせることにより、一方が大径部1aとされ、他方
が小径部1bとされた漏斗状に形成されている。なお、
セパレータ2は絶縁樹脂よりなるものであり、一例とし
て変性ポリフェニレンエーテル(変性PPE)によって
形成される。
First, the configuration of the deflection yoke of the present invention to which the deflection yoke tightening band of the present invention (hereinafter, abbreviated as a tightening band) is attached will be described with reference to FIG. The deflection yoke 1 shown in FIG. 2 is formed in a funnel shape having one large diameter portion 1a and the other small diameter portion 1b by combining, for example, a pair of semi-annular separators 2. In addition,
The separator 2 is made of an insulating resin, and is formed of, for example, modified polyphenylene ether (modified PPE).

【0015】セパレータ2の内部には水平偏向コイル
(図示せず)が装着され、セパレータ2の外部には垂直
偏向コイル3が装着されている。垂直偏向コイル3の外
側には、フェライトで形成されたコア4が取り付けられ
ている。セパレータ2の小径部1b側には、フランジ5
a,5bが設けられており、このフランジ5a,5bに
は種々の部品が取り付けられる。
A horizontal deflection coil (not shown) is mounted inside the separator 2, and a vertical deflection coil 3 is mounted outside the separator 2. A core 4 made of ferrite is attached to the outside of the vertical deflection coil 3. A flange 5 is provided on the small diameter portion 1b side of the separator 2.
a, 5b are provided, and various components are attached to the flanges 5a, 5b.

【0016】セパレータ2の小径部1b側の端部は、フ
ランジ5a,5bに立設した複数の舌片によって形成さ
れた円筒部6となっている。円筒部6には、一対の突起
7,7(ここでは、一方の突起7は見えず)が形成され
ている。この円筒部6の外周には、本発明の締付バンド
80が装着されている。なお、図2に示す偏向ヨーク1
は、いわゆるサドル・サドル型と呼ばれているものであ
るが、本発明の偏向ヨークはこれに限定されるものでは
なく、サドル・トロイダル型等の他の構成であってもよ
い。
The end of the separator 2 on the small diameter portion 1b side is a cylindrical portion 6 formed by a plurality of tongues erected on the flanges 5a and 5b. A pair of protrusions 7, 7 (here, one protrusion 7 is not visible) is formed on the cylindrical portion 6. A tightening band 80 of the present invention is mounted on the outer periphery of the cylindrical portion 6. The deflection yoke 1 shown in FIG.
Is a so-called saddle-saddle type, but the deflection yoke of the present invention is not limited to this, and may have another configuration such as a saddle-toroidal type.

【0017】ここで、本発明の締付バンド80につい
て、図1を用いて詳細に説明する。図1に示すように、
本発明となる締付バンド80は、従来と同様、円周部8
aと、この円周部8aの両端部より突出した突出片8
b,8bと、この突出片8bに形成された穴を貫通する
ように取り付けられたボルト8cとよりなる。なお、円
周部8aと突出片8bとは一体的に形成されている。締
付バンド80は、偏向ヨークが発生する磁界特性に影響
を与えないよう、例えばオーステナイト系ステンレス鋼
等の非磁性材を用いる。
Here, the tightening band 80 of the present invention will be described in detail with reference to FIG. As shown in FIG.
The tightening band 80 according to the present invention has a circumferential
a and projecting pieces 8 projecting from both ends of the circumferential portion 8a.
b, 8b and a bolt 8c attached so as to pass through a hole formed in the protruding piece 8b. The circumferential portion 8a and the protruding piece 8b are formed integrally. The tightening band 80 is made of a non-magnetic material such as austenitic stainless steel so as not to affect the magnetic field characteristics generated by the deflection yoke.

【0018】この締付バンド80の円周部8aには、図
2に示す偏向ヨーク1におけるセパレータ2の一対の突
起7,7に係合するための2つの係合穴8a1,8a1が設
けられている。円周部8aの径は、セパレータ2の円筒
部6の径より若干大きく形成されており、締付バンド8
0は、図2に示すように、円周部8aがセパレータ2の
円筒部6の外周を覆うように装着される。そして、係合
穴8a1,8a1を前述の突起7,7に係合させて円筒部6
に係止させる。
The circumferential portion 8a of the tightening band 80 is provided with two engaging holes 8a1, 8a1 for engaging with a pair of projections 7, 7 of the separator 2 in the deflection yoke 1 shown in FIG. ing. The diameter of the circumferential portion 8 a is formed slightly larger than the diameter of the cylindrical portion 6 of the separator 2, and
2 is mounted so that the circumferential portion 8a covers the outer periphery of the cylindrical portion 6 of the separator 2 as shown in FIG. Then, the engaging holes 8a1, 8a1 are engaged with the projections 7, 7, so that the cylindrical portion 6
To lock.

【0019】突出片8bに形成された穴の内、ボルト8
cの頭8c1とは反対側の穴にはねじが切られていて、ボ
ルト8cはこのねじ穴に螺合している。従って、ボルト
8cを回転させることにより、締付バンド80の円周内
寸法が変化する。本発明の締付バンド80のボルト8c
には潤滑剤9が塗布されている。突出片8bに形成され
たねじ穴に潤滑剤9を塗布してもよい。また、ボルト8
cとねじ穴との双方に潤滑剤9を塗布してもよい。この
ように、本発明の締付バンド80においては、ねじ穴と
ボルト8cとの間に、潤滑剤9が介在している。
Of the holes formed in the protruding piece 8b, the bolt 8
The hole on the side opposite to the head 8c1 of c is threaded, and the bolt 8c is screwed into this screw hole. Therefore, by rotating the bolt 8c, the inner circumferential dimension of the tightening band 80 changes. Bolt 8c of tightening band 80 of the present invention
Is coated with a lubricant 9. The lubricant 9 may be applied to a screw hole formed in the protruding piece 8b. Also, bolt 8
The lubricant 9 may be applied to both c and the screw hole. Thus, in the tightening band 80 of the present invention, the lubricant 9 is interposed between the screw hole and the bolt 8c.

【0020】ボルト8cに潤滑剤9を塗布する場合に
は、ボルト8cの全体に塗布してもよく、また、突出片
8bのねじ穴に接触する部分のみに塗布してもよい。ま
た、ボルト8cをねじ穴に螺合させる前に予めボルト8
cもしくはねじ穴に潤滑剤9を塗布してもよいし、締付
バンド80を偏向ヨーク1の円筒部6に装着し、ボルト
8cを回転させてCRT100(図3に図示)のネック
部100N(図3に図示)を締め付ける直前に潤滑剤9
を塗布してもよい。これは、ボルト8cが突出片8bの
ねじ部にかじってしまったり、焼き付いてしまうのは、
ボルト8cを回転させてCRT100のネック部100
Nを締め付けるときにボルト8cとねじ部との間に強い
力が加わるからである。
When applying the lubricant 9 to the bolt 8c, the lubricant 9 may be applied to the entire bolt 8c, or may be applied only to the portion of the protruding piece 8b that contacts the screw hole. Before screwing the bolt 8c into the screw hole,
c or the screw hole may be coated with the lubricant 9, or the fastening band 80 may be attached to the cylindrical portion 6 of the deflection yoke 1 and the bolt 8c may be rotated to rotate the neck portion 100N of the CRT 100 (shown in FIG. 3). Immediately before tightening the lubricant 9 (shown in FIG. 3)
May be applied. This is because the bolt 8c may bite or seize the thread of the protruding piece 8b.
By rotating the bolt 8c, the neck 100 of the CRT 100 is rotated.
This is because a strong force is applied between the bolt 8c and the screw portion when N is tightened.

【0021】この潤滑剤9としては、ボルト8cと突出
片8bのねじ部との間のかじりや焼き付きの発生を良好
に防止するということから、フッ素系の潤滑剤であるこ
とが最も好ましいことが、本発明者による実験によって
確かめられた。
It is most preferable that the lubricant 9 is a fluorine-based lubricant because it can prevent galling and seizure between the bolt 8c and the thread portion of the protruding piece 8b. Was confirmed by experiments by the present inventors.

【0022】フッ素系の潤滑剤9としては、一例とし
て、NOKクリューバー(株)製の“J100”に代表
される“BARRIERTA J FLUID”を用い
ることができる。この潤滑剤の分子構造は、以下に示す
化1となっている。
As the fluorine-based lubricant 9, for example, "BARRIERTA J FLUID" represented by "J100" manufactured by NOK Kluber Co., Ltd. can be used. The molecular structure of this lubricant is as shown below.

【0023】[0023]

【化1】 Embedded image

【0024】ボルト8cと突出片8bのねじ部との間に
かじりや焼き付きが発生する際の局部温度は140℃に
も達することが確認されている。従って、潤滑剤9とし
ては、140℃以上に耐えるような温度特性を有するこ
とが望ましい。上記の“J100”は、200℃以上に
も耐えるような温度特性を有しており、かじりや焼き付
き発生の防止に抜群の効果を発揮する。
It has been confirmed that the local temperature at which galling or seizure occurs between the bolt 8c and the thread portion of the protruding piece 8b reaches as high as 140 ° C. Therefore, it is desirable that the lubricant 9 has a temperature characteristic that can withstand 140 ° C. or more. The above-mentioned “J100” has a temperature characteristic that can withstand even 200 ° C. or more, and exhibits an excellent effect in preventing galling and image sticking.

【0025】そして、締付バンド80を円筒部6に嵌め
込んだ状態で、円周内寸法を小さくする方向にボルト8
cを回転させると、円筒部6は可撓性を有しているの
で、図3に示すように、円周部8aが円筒部6を介して
CRT100のネック部100Nを締め付ける。このと
き、ボルト8cには潤滑剤9が予め塗布されているの
で、ボルト8cと突出片8bのねじ部との間にかじりや
焼き付きが発生することはなく、極めて良好にボルト8
cを回転させることができる。このようにして、偏向ヨ
ーク1は締付バンド80によってCRT100のネック
部100Nに固定される。なお、図3において、101
は電子銃である。
Then, with the tightening band 80 fitted in the cylindrical portion 6, the bolt 8
When c is rotated, the cylindrical portion 6 has flexibility, so that the circumferential portion 8a tightens the neck portion 100N of the CRT 100 via the cylindrical portion 6, as shown in FIG. At this time, since the lubricant 9 is applied to the bolt 8c in advance, there is no galling or seizure between the bolt 8c and the threaded portion of the protruding piece 8b, and the bolt 8c is extremely excellent.
c can be rotated. Thus, the deflection yoke 1 is fixed to the neck 100N of the CRT 100 by the tightening band 80. Note that in FIG.
Is an electron gun.

【0026】ここで、突出片8bのねじ穴とボルト8c
との間に潤滑剤9が介在させる際の好適な実施例につい
て説明する。突出片8bのねじ穴やボルト8cに予め潤
滑剤9を塗布する場合には、円周部8aとボルト8cと
を組み合わせて締付バンド80を製造する製造工程の一
部として潤滑剤9を塗布することができる。また、CR
T100のネック部100Nを締め付ける直前に潤滑剤
9を塗布する場合には、偏向ヨーク1をCRT100に
装着する装着工程の一部として潤滑剤9を塗布すること
もできる。
Here, the screw hole of the projecting piece 8b and the bolt 8c
A preferred embodiment in which the lubricant 9 is interposed between the first embodiment and the second embodiment will be described. When the lubricant 9 is applied in advance to the screw hole of the protruding piece 8b or the bolt 8c, the lubricant 9 is applied as a part of a manufacturing process of manufacturing the tightening band 80 by combining the circumferential portion 8a and the bolt 8c. can do. Also, CR
When the lubricant 9 is applied immediately before the neck portion 100N of the T100 is tightened, the lubricant 9 may be applied as a part of a mounting process of mounting the deflection yoke 1 on the CRT 100.

【0027】潤滑剤9の塗布量(付着量)は、コスト面
及び環境面等から、かじりや焼き付き発生の防止効果が
得られる範囲内で必要最小限とすることが好ましい。こ
のため、潤滑剤9をボルト8cに塗布する場合、以下の
各実施例を用いることができる。なお、ここでは、潤滑
剤9をボルト8cに塗布する場合について示すが、ねじ
穴に塗布する場合でも同様である。
The amount of the lubricant 9 to be applied (adhered amount) is preferably set to a necessary minimum within a range where the effect of preventing galling and seizure can be obtained from the viewpoint of cost and environment. Therefore, when the lubricant 9 is applied to the bolt 8c, the following embodiments can be used. Although the case where the lubricant 9 is applied to the bolt 8c is shown here, the same applies to the case where the lubricant 9 is applied to the screw hole.

【0028】<第1実施例>潤滑剤9を希釈剤によって
希釈し、ボルト8cをそれに浸して取り出し、希釈剤を
揮発させる。この場合には、希釈剤としては揮発性希釈
剤あるいは水等を用いる。なお、潤滑剤9を溶解させる
ことが困難な場合には、潤滑剤9と希釈剤とをよく撹拌
し、均一に混合させる。これによって、潤滑剤9を薄く
塗布することが可能となる。
<First Embodiment> The lubricant 9 is diluted with a diluent, and the bolt 8c is immersed in the diluent and taken out to volatilize the diluent. In this case, a volatile diluent or water is used as the diluent. When it is difficult to dissolve the lubricant 9, the lubricant 9 and the diluent are thoroughly stirred and uniformly mixed. This makes it possible to apply the lubricant 9 thinly.

【0029】<第2実施例>潤滑剤9の粘度を加熱等に
より一旦下げ、ボルト8cをそれに浸して取り出す。潤
滑剤9の粘度を下げることによって、ボルト8cに必要
以上の量の潤滑剤9が付着しない。これによって、潤滑
剤9を薄く塗布することが可能となる。
<Second Embodiment> The viscosity of the lubricant 9 is temporarily reduced by heating or the like, and the bolt 8c is immersed therein and taken out. By lowering the viscosity of the lubricant 9, an unnecessary amount of the lubricant 9 does not adhere to the bolt 8c. This makes it possible to apply the lubricant 9 thinly.

【0030】<第3実施例>潤滑剤9をボルト8cに塗
布した後、脱水槽や遠心分離機等を用いて余分な量の潤
滑剤9を機械的に取り除く。これによって、潤滑剤9を
薄く塗布することが可能となる。
<Third Embodiment> After the lubricant 9 is applied to the bolt 8c, an extra amount of the lubricant 9 is mechanically removed by using a dehydration tank, a centrifuge, or the like. This makes it possible to apply the lubricant 9 thinly.

【0031】<第4実施例>潤滑剤9を希釈剤によって
希釈し、ボルト8cをそれに浸して取り出す。その後、
その希釈剤を溶解する薬品等によって溶解させ、さらに
洗浄して希釈剤を化学的に除去する。これによって、潤
滑剤9を薄く塗布することが可能となる。
<Fourth Embodiment> The lubricant 9 is diluted with a diluent, and the bolt 8c is immersed in the lubricant 9 and taken out. afterwards,
The diluent is dissolved by a dissolving chemical or the like, and further washed to chemically remove the diluent. This makes it possible to apply the lubricant 9 thinly.

【0032】これらの潤滑剤9の塗布方法は、ボルト8
cを潤滑剤9に浸す方法について示したが、刷毛等によ
って必要な部分に塗布する方法であってもよい。但し、
ボルト8cを潤滑剤9に一括して浸す方法が最も簡単で
ある。また、上記の第1〜第4実施例は適宜に組み合わ
せてもよい。
The method of applying these lubricants 9 is as follows.
Although the method of immersing c in the lubricant 9 has been described, a method of applying it to a necessary portion with a brush or the like may be used. However,
The simplest method is to immerse the bolts 8c in the lubricant 9 all at once. Further, the above-described first to fourth embodiments may be appropriately combined.

【0033】以上をまとめると、締付バンド80の製造
方法は以下の工程により行えばよい。ボルト8cもしく
は円周部8aにおける突出片8bのねじ穴の少なくとも
一方にフッ素系の潤滑剤9を塗布し、その後、ボルト8
cを突出片8bの1対の穴に取り付けて円周部8aとボ
ルト8cとを一体化する。あるいは、ボルト8cを突出
片8bの1対の穴に取り付けて円周部8aとボルト8c
とを一体化し、その後、ボルト8cもしくは円周部8a
における突出片8bのねじ穴の少なくとも一方にフッ素
系の潤滑剤9を塗布する。
In summary, the method of manufacturing the fastening band 80 may be performed by the following steps. A fluorine-based lubricant 9 is applied to at least one of the bolt hole 8c or the screw hole of the protruding piece 8b in the circumferential portion 8a.
c is attached to a pair of holes of the protruding piece 8b to integrate the circumferential portion 8a and the bolt 8c. Alternatively, the bolt 8c is attached to a pair of holes of the protruding piece 8b, and the circumferential portion 8a and the bolt 8c are attached.
And then the bolt 8c or the circumferential portion 8a
A fluorine-based lubricant 9 is applied to at least one of the screw holes of the protruding piece 8b.

【0034】このとき、潤滑剤9を塗布する際には、潤
滑剤9を希釈する工程、潤滑剤9を加熱する工程、余分
な潤滑剤9を取り除く工程の少なくとも1つを含むこと
が望ましい。
At this time, when applying the lubricant 9, it is desirable to include at least one of a step of diluting the lubricant 9, a step of heating the lubricant 9, and a step of removing excess lubricant 9.

【0035】さらに、潤滑剤9を塗布していない従来の
締付バンド8を用いる場合には、偏向ヨークをCRTに
装着する装着方法を、以下の工程により行えばよい。こ
こでは、便宜上、図2に示す番号を用いて説明する。ま
ず、締付バンド8のボルト8cもしくは円周部8aにお
ける突出片8bのねじ穴の少なくとも一方にフッ素系の
潤滑剤9を塗布して、本発明の締付バンド80とする。
その後、偏向ヨーク1のセパレータ2の小径部1b側の
端部である円筒部6に締付バンド80を装着する。
Further, when the conventional tightening band 8 to which the lubricant 9 is not applied is used, a method for mounting the deflection yoke on the CRT may be performed by the following steps. Here, the description will be made using the numbers shown in FIG. 2 for convenience. First, a fluorine-based lubricant 9 is applied to at least one of the bolt 8c of the tightening band 8 or the screw hole of the protruding piece 8b in the circumferential portion 8a to obtain the tightening band 80 of the present invention.
Thereafter, the tightening band 80 is attached to the cylindrical portion 6 which is the end of the deflection yoke 1 on the side of the small diameter portion 1b of the separator 2.

【0036】あるいは、偏向ヨーク1のセパレータ2の
小径部1b側の端部である円筒部6に予め装着された締
付バンド8に対し、ボルト8cもしくは円周部8aにお
ける突出片8bのねじ穴の少なくとも一方にフッ素系の
潤滑剤9を塗布する。
Alternatively, the bolt 8c or the screw hole of the protruding piece 8b in the circumferential portion 8a is inserted into the tightening band 8 previously mounted on the cylindrical portion 6 which is the end of the separator 2 of the deflection yoke 1 on the small diameter portion 1b side. Is coated with a fluorine-based lubricant 9.

【0037】その後、偏向ヨーク1をCRT100に装
着し、ボルト8cを回転させて円周部8aを締め付け、
円筒部6を介してCRT100のネック部100Nを締
め付ける。
Thereafter, the deflection yoke 1 is mounted on the CRT 100, and the bolt 8c is rotated to tighten the circumferential portion 8a.
The neck portion 100N of the CRT 100 is tightened via the cylindrical portion 6.

【0038】他の方法として、セパレータ2の円筒部6
に締付バンド8が予め装着された偏向ヨーク1をCRT
100に装着し、締付バンド8のボルト8cもしくは円
周部8aにおける突出片8bのねじ穴の少なくとも一方
にフッ素系の潤滑剤9を塗布して、本発明の締付バンド
80とする。その後、ボルト8cを回転させて円周部8
aを締め付け、円筒部6を介してCRT100のネック
部100Nを締め付ける。
As another method, the cylindrical portion 6 of the separator 2
The deflection yoke 1 on which the tightening band 8 is mounted in advance
100, a fluorine-based lubricant 9 is applied to at least one of the bolt 8c of the tightening band 8 or the threaded hole of the protruding piece 8b in the circumferential portion 8a to obtain the tightening band 80 of the present invention. Then, the bolt 8c is rotated to rotate the circumferential portion 8
a, and the neck portion 100N of the CRT 100 is tightened via the cylindrical portion 6.

【0039】これらの場合においても、潤滑剤9を塗布
する際には、潤滑剤9を希釈する工程、潤滑剤9を加熱
する工程、余分な潤滑剤9を取り除く工程の少なくとも
1つを含むことが望ましい。
Also in these cases, when applying the lubricant 9, at least one of a step of diluting the lubricant 9, a step of heating the lubricant 9, and a step of removing the excess lubricant 9 is required. Is desirable.

【0040】上記のように、潤滑剤9の塗布量(付着
量)は、コスト面及び環境面等から、かじりや焼き付き
発生の防止効果が得られる範囲内で必要最小限とするこ
とが好ましい。本発明者は、詳細な実験の結果、突出片
8bのねじ穴とボルト8cとの間に介在させる潤滑剤9
は、その塗布量が少なすぎれば、かじりや焼き付き発生
の防止効果が得られないことは勿論のこと、逆にその塗
布量が多すぎても、かじりや焼き付き発生の防止効果が
得られないことを見いだした。換言すれば、本発明者
は、潤滑剤9の望ましい塗布量を見いだした。以下、こ
れについて詳細に説明する。
As described above, it is preferable that the applied amount (adhered amount) of the lubricant 9 be minimized within a range where the effect of preventing galling and seizure can be obtained from the viewpoint of cost and environment. As a result of detailed experiments, the inventor has found that the lubricant 9 interposed between the screw hole of the projecting piece 8b and the bolt 8c
Means that if the coating amount is too small, the effect of preventing galling and image sticking cannot be obtained, and conversely, if the coating amount is too large, the effect of preventing galling and image sticking cannot be obtained. Was found. In other words, the inventor has found a desirable application amount of the lubricant 9. Hereinafter, this will be described in detail.

【0041】ここでは、潤滑剤9として上記の“J10
0”を用い、ボルト8cに単位面積当たりの潤滑剤9の
付着量を種々異ならせて塗布した試験用の締付バンド8
0を用いた。そして、それぞれの締付バンド80のサン
プルに対し、1.96[N・m]の締め付けトルクでボ
ルト8cを締め付け、これを緩め、この「締め付け−緩
め」を連続的に繰り返した。以下の表1に示す実験結果
は、以上のような実験によるかじり発生率を評価したも
のである。
Here, the above-mentioned “J10” is used as the lubricant 9.
0 ", and the test tightening band 8 is applied to the bolt 8c with various amounts of the lubricant 9 per unit area applied thereto.
0 was used. Then, the bolt 8c was tightened with a tightening torque of 1.96 [N · m] to each of the samples of the tightening band 80, loosened, and this “tightening-loosening” was continuously repeated. The experimental results shown in Table 1 below are evaluations of the rate of galling by the above experiments.

【0042】[0042]

【表1】 [Table 1]

【0043】表1に示すように、試験用の締付バンド8
0は、サンプル番号1〜11の11種類とし、この11
種類の締付バンド80のサンプルをそれぞれ多数用意し
て実験を行った。それぞれの潤滑剤9の付着量は表1に
示す通りである。
As shown in Table 1, the test tightening band 8
0 is 11 types of sample numbers 1 to 11, and
An experiment was conducted by preparing a large number of samples of each type of tightening band 80. The amount of each lubricant 9 attached is as shown in Table 1.

【0044】かじり防止効果は、◎が効果極大、○が効
果大、△が効果小、×が効果極小を示している。なお、
◎の効果極大とは、上記の「締め付け−緩め」の回数が
20回まででかじりが全く発生せず、かつ、その回数が
100回まででかじり(焼き付きを含む)が発生した個
数が10%以下のものとし、○の効果大とは、その回数
が20回まででかじりが全く発生せず、かつ、その回数
が100回まででかじりが発生した個数が10%を越
え、25%以下のものとした。また、△の効果小とは、
その回数が20回まででかじりが発生した個数が25%
以下で、かつ、その回数が100回まででかじりが発生
した個数が50%以下のものとし、×の効果極小とは、
その回数が20回まででかじりが発生した個数が25%
を越え、50%以下で、かつ、その回数が100回まで
でかじりが発生した個数が75%以下のものとした。
Regarding the galling prevention effect, ◎ indicates the maximum effect, ○ indicates the maximum effect, Δ indicates the small effect, and x indicates the minimum effect. In addition,
The maximal effect of ◎ means that no galling occurs when the above-mentioned “tightening-loosening” is performed up to 20 times, and the number of galling (including seizure) occurs up to 100 times is 10%. In the following, the large effect of ○ means that no galling occurs up to 20 times, and the number of galling occurs up to 100 times is more than 10% and 25% or less. It was taken. In addition, the small effect of △
Up to 20 times, 25% of galling occurred
And the number of occurrences of galling is 50% or less and the number of times is up to 100 times.
Up to 20 times, 25% of galling occurred
And 50% or less, and the number of times of galling has occurred is 75% or less with the number of times being up to 100 times.

【0045】この表1より分かるように、潤滑剤9は、
3×10-3〜13×10-3mg/mm2 なる付着量でボ
ルト8cに付着させることが望ましい。さらに望ましく
は、5×10-3〜9×10-3mg/mm2 なる付着量で
ある。潤滑剤9の付着量が3×10-3〜13×10-3
g/mm2 であれば、偏向ヨーク1(締付バンド80)
の通常の使用状態によって、締付バンド80におけるか
じりや焼き付きが発生して問題となることはほとんどな
い。さらに、潤滑剤9の付着量が5×10-3〜9×10
-3mg/mm2 であれば、偏向ヨーク1の過酷な使用状
態、即ち、締付バンド80を頻繁に円筒部6に着脱して
も、締付バンド80におけるかじりや焼き付きが発生し
て問題となることはほとんどない。
As can be seen from Table 1, the lubricant 9 is
It is desirable to attach to the bolt 8c with an attachment amount of 3 × 10 −3 to 13 × 10 −3 mg / mm 2 . More preferably, the adhesion amount is 5 × 10 −3 to 9 × 10 −3 mg / mm 2 . The amount of the lubricant 9 applied is 3 × 10 −3 to 13 × 10 −3 m
g / mm 2 , deflection yoke 1 (tightening band 80)
According to the normal use condition, there is almost no problem that galling or seizure occurs in the fastening band 80. Further, the adhesion amount of the lubricant 9 is 5 × 10 −3 to 9 × 10
-3 mg / mm 2 , even if the deflection yoke 1 is used in a severe condition, that is, even if the fastening band 80 is frequently attached to and detached from the cylindrical portion 6, galling and seizure of the fastening band 80 may occur. Hardly ever.

【0046】ここで、潤滑剤9を、3×10-3〜13×
10-3mg/mm2 なる付着量でボルト8cに付着させ
る際の詳細な付着方法を、上記の<第1実施例>の場合
について説明する。希釈剤の一例として、住友スリーエ
ム株式会社製の「HFE−7100」(ハイドロフルオ
ロエーテル)(以下“7100”と称する)を使用す
る。希釈比率(“J100”:“7100”)を体積比
で1:8〜1:15とし、適度に撹拌する。“J10
0”は“7100”によく溶解する。その希釈液にボル
ト8cを所定の時間浸して取り出し、“7100”を揮
発させる。希釈液にボルト8cを浸す時間は、10分間
程度で充分である。“7100”は揮発性が高く、速や
かに揮発する。
Here, the lubricant 9 is used in an amount of 3 × 10 −3 to 13 ×
A detailed method of attaching to the bolt 8c with an attachment amount of 10 −3 mg / mm 2 will be described for the case of the above-described <First Embodiment>. As an example of the diluent, "HFE-7100" (hydrofluoroether) (hereinafter referred to as "7100") manufactured by Sumitomo 3M Limited is used. The dilution ratio ("J100": "7100") is adjusted to 1: 8 to 1:15 by volume, and the mixture is appropriately stirred. “J10
“0” dissolves well in “7100.” The bolt 8c is immersed in the diluent for a predetermined time and taken out to volatilize “7100.” The immersion time of the volt 8c in the diluent is about 10 minutes. “7100” is highly volatile and evaporates quickly.

【0047】ところで、本発明者の実験によると、潤滑
剤9を含んだ希釈液に浸すボルト8cの本数によって、
ボルト8cに付着する潤滑剤9の付着量が異なる場合が
あることが確かめられた。具体的には、“J100”:
“7100”=1:9なる体積比とし、0.5リットル
の希釈液に本数の異なるボルト8cを浸漬処理した結
果、ボルト8cを20本としたときには、9.03×1
-3mg/mm2 であり、ボルト8cを140本とした
ときには、5.98×10-3mg/mm2 であった。こ
の例では、3.05×10-3mg/mm2 の付着量の差
が生じており、ボルト8cの本数を増やすと、ボルト8
cに対する潤滑剤9の付着量が減少する傾向があること
が確かめられた。
According to an experiment conducted by the present inventor, the number of bolts 8c immersed in a diluent containing a lubricant 9 is
It has been confirmed that the amount of the lubricant 9 attached to the bolt 8c may be different. Specifically, “J100”:
A volume ratio of “7100” = 1: 9, and as a result of immersion treatment of different numbers of bolts 8c in 0.5 liter of diluent, when the number of bolts 8c is 20, 9.03 × 1
0 -3 mg / mm 2 , and 5.98 × 10 -3 mg / mm 2 when 140 bolts 8c were used. In this example, there is a difference in the amount of adhesion of 3.05 × 10 −3 mg / mm 2 , and when the number of bolts 8c is increased,
It was confirmed that the amount of the lubricant 9 adhered to c tended to decrease.

【0048】このように、潤滑剤9を含んだ液体にボル
ト8cを浸漬処理する際に、ボルト8cの本数によって
ボルト8cに対する潤滑剤9の付着量が変化してしまう
ということは、潤滑剤9を上記のような望ましい付着量
でボルト8cに付着させるためには、ボルト8cを浸漬
処理する際のボルト8cの本数を厳密に管理しなければ
ならないことを意味する。これは、締付バンド80の製
造工程にとっては好ましいことではない。
As described above, when the bolt 8c is immersed in the liquid containing the lubricant 9, the amount of the lubricant 9 attached to the bolt 8c changes depending on the number of the bolts 8c. Means that the number of bolts 8c must be strictly controlled when the bolts 8c are immersed in order to cause the bolts 8c to adhere to the bolts 8c with the desired amount of adhesion as described above. This is not preferable for the manufacturing process of the tightening band 80.

【0049】本発明者は、種々の実験の結果、潤滑剤9
を含んだ液体にボルト8cを浸漬処理する際に、その液
体を循環もしくは撹拌させることによって、ボルト8c
の本数によらず、ボルト8cに対する潤滑剤9の付着量
をほぼ一定とすることができることを見いだした。図4
〜図6は、ボルト8cに対する潤滑剤9の付着量を安定
化させるための締付バンド80の製造方法を説明するた
めの図である。
As a result of various experiments, the inventor found that the lubricant 9
When the bolt 8c is immersed in the liquid containing
It has been found that the amount of the lubricant 9 attached to the bolt 8c can be made substantially constant regardless of the number of the bolts 8c. FIG.
6A to 6C are diagrams for explaining a method of manufacturing the tightening band 80 for stabilizing the amount of the lubricant 9 attached to the bolt 8c.

【0050】図4において、槽10には、潤滑剤9と希
釈剤とを所定の体積割合で混合した希釈液20が入って
いる。槽10には、希釈液20を循環させるためのポン
プ11が取り付けてある。希釈液20は排出口12より
ポンプ11へと送り出され、パイプ管14を通って、吐
出口13より槽10へと戻される。排出口12と吐出口
13は、希釈液20の液面より下側に位置し、槽10の
対角方向に高さ違いとなるように設けられている。これ
は、希釈液20循環時の空気の巻き込みを防止し、ま
た、より大きな対流を発生させるためである。
In FIG. 4, a tank 10 contains a diluent 20 obtained by mixing a lubricant 9 and a diluent at a predetermined volume ratio. The tank 10 is provided with a pump 11 for circulating the diluent 20. The diluent 20 is sent from the outlet 12 to the pump 11, passes through the pipe 14, and returns to the tank 10 from the outlet 13. The discharge port 12 and the discharge port 13 are located below the level of the diluent 20 and are provided so as to be different in height in the diagonal direction of the tank 10. This is to prevent the entrainment of air during the circulation of the diluent 20, and to generate a larger convection.

【0051】ポンプ11を駆動することによって、希釈
液20は、排出口12からパイプ管14を通り、吐出口
13から槽10に戻るという循環を繰り返すことにな
る。ポンプ11の駆動力は、槽10内で希釈液20が充
分に対流する程度の力とする。これによって、希釈液2
0は槽10内で均一に混合され、撹拌状態とされる。希
釈液20のより均一な混合・撹拌状態を保つために、吐
出口13の近傍にファン15を設けてもよい。
By driving the pump 11, the diluent 20 repeats the circulation of returning from the outlet 12 through the pipe 14 and returning from the outlet 13 to the tank 10. The driving force of the pump 11 is such that the diluent 20 sufficiently convects in the tank 10. Thereby, the diluent 2
0 is uniformly mixed in the tank 10 and brought into a stirring state. A fan 15 may be provided near the discharge port 13 in order to maintain a more uniform mixing and stirring state of the diluent 20.

【0052】このように構成される槽10の上部からは
任意の本数のボルト8cを入れた網籠16が吊り下げら
れており、ボルト8cは希釈液20に浸漬されている。
希釈液20が循環もしくは撹拌することによって、ボル
ト8cの本数が何本であろうとも、潤滑剤9はボルト8
cにほぼ一定の付着量で付着する。さらに、網籠16は
モータ17に連結されており、網籠16をモータ17に
よって適当な速度で回転させることによって、希釈液2
0のより均一な混合・撹拌状態を保つことができ、潤滑
剤9の付着量をさらに安定化させることができる。な
お、網籠16を上下もしくは左右方向に揺動させてもよ
い。
A mesh basket 16 containing an arbitrary number of bolts 8c is suspended from the upper portion of the tank 10 thus configured, and the bolts 8c are immersed in the diluent 20.
By circulating or agitating the diluting liquid 20, the lubricant 9 is supplied to the bolt 8c regardless of the number of bolts 8c.
It adheres to c with a substantially constant amount. Further, the mesh basket 16 is connected to a motor 17, and by rotating the mesh basket 16 at an appropriate speed by the motor 17, the diluent 2
0 can be maintained in a more uniform mixing / stirring state, and the amount of the lubricant 9 attached can be further stabilized. The basket 16 may be swung up and down or left and right.

【0053】さらに、より均一な混合・撹拌状態を保つ
ために、図5,図6に示すように、網籠16の外周部や
上部に羽根18を装着してもよい。なお、図5は網籠1
6を側面より見た図であり、図6は網籠16を下面より
見た図である。羽根18を装着した網籠16を回転させ
ると、羽根18によって希釈液20により強い対流が発
生し、希釈液20が網籠16の内部へと誘導される。以
上のようにして、潤滑剤9を含んだ液体にボルト8cを
浸漬処理する際に、その液体を循環もしくは撹拌させる
ことによって、ボルト8cの本数によらず、ボルト8c
に対する潤滑剤9の付着量をほぼ一定とすることができ
る。
Further, in order to maintain a more uniform mixing / stirring state, as shown in FIGS. 5 and 6, a blade 18 may be attached to the outer peripheral portion or upper portion of the net basket 16. In addition, FIG.
FIG. 6 is a diagram of the net basket 16 viewed from the side, and FIG. When the mesh basket 16 on which the blades 18 are mounted is rotated, strong convection is generated in the diluent 20 by the blades 18, and the diluent 20 is guided into the inside of the net basket 16. As described above, when the bolt 8c is immersed in the liquid containing the lubricant 9, the liquid is circulated or agitated so that the bolt 8c can be irrespective of the number of bolts 8c.
Can be made substantially constant.

【0054】このようにして潤滑剤9を付着させたボル
ト8cは、前述のように、希釈剤を揮発させた後、突出
片8bに形成された1対の穴に取り付けられて円周部8
aとボルト8cとが一体化され、締付バンド80とされ
る。
As described above, the bolt 8c having the lubricant 9 adhered thereto is attached to the pair of holes formed in the protruding piece 8b after the diluent is volatilized as described above.
a and the bolt 8 c are integrated into a tightening band 80.

【0055】なお、図4〜図6に示す実施例は、潤滑剤
9を含んだ液体を循環もしくは撹拌させるための好適な
実施例であるが、本発明の締付バンド80の製造方法
は、これに限定されることはない。ポンプ11による希
釈液20の循環、ファン15による希釈液20の撹拌、
網籠16の回転もしくは揺動、網籠16に対する羽根1
8の付加は必ずしも全て実施する必要はなく、適宜組み
合わせて使用すればよい。また、同様の効果を得る他の
方法を用いてもよいし、それらを組み合わせて使用して
もよい。
Although the embodiment shown in FIGS. 4 to 6 is a preferred embodiment for circulating or stirring the liquid containing the lubricant 9, the method for manufacturing the tightening band 80 of the present invention is as follows. It is not limited to this. Circulation of the diluent 20 by the pump 11, stirring of the diluent 20 by the fan 15,
Rotation or swing of the mesh basket 16, the blade 1 for the mesh basket 16
It is not always necessary to carry out all the additions of 8, and they may be used in an appropriate combination. Further, another method for obtaining the same effect may be used, or a combination thereof may be used.

【0056】さらに、本実施例では、潤滑剤9を含んだ
液体にボルト8cのみを浸漬処理したが、円周部8aと
ボルト8cとを一体化し、その全体を潤滑剤9を含んだ
液体に浸漬処理してもよい。即ち、ボルト8cを、潤滑
剤9を含んだ液体に、その液体を循環もしくは撹拌させ
つつ所定時間浸漬させる第1の工程と、この第1の工程
によって潤滑剤9が付着したボルト8cを、突出片8b
の1対の穴に取り付けて、円周部8aとボルト8cとを
一体化する第2の工程とによって、締付バンド80を製
造するか、突出片8bの1対の穴にボルト8cを取り付
けて、円周部8aとボルト8cとを一体化する第1の工
程と、この第1の工程によって一体化した円周部8a及
びボルト8cを、潤滑剤9を含んだ液体に、その液体を
循環もしくは撹拌させつつ所定時間浸漬させる第2の工
程とによって、締付バンド80を製造すればよい。な
お、潤滑剤9が必要なのは、上記のように、ボルト8c
がねじ穴に接触する部分であるので、ボルト8cのみを
潤滑剤9を含んだ液体に浸漬処理する方がより好まし
い。
Further, in this embodiment, only the bolt 8c is immersed in the liquid containing the lubricant 9, but the circumferential portion 8a and the bolt 8c are integrated, and the whole is converted into the liquid containing the lubricant 9. An immersion treatment may be performed. That is, a first step of immersing the bolt 8c in a liquid containing the lubricant 9 for a predetermined time while circulating or stirring the liquid, and projecting the bolt 8c to which the lubricant 9 has adhered in the first step. Piece 8b
A second step of integrating the circumferential portion 8a and the bolt 8c by attaching the bolt 8c to the pair of holes, or attaching the bolt 8c to the pair of holes of the protruding piece 8b. Then, the first step of integrating the circumferential portion 8a and the bolt 8c, and the circumferential portion 8a and the bolt 8c integrated by the first step are combined with the liquid containing the lubricant 9 to obtain the liquid. The fastening band 80 may be manufactured by the second step of immersing for a predetermined time while circulating or stirring. The reason why the lubricant 9 is required is that the bolt 8c
Is a portion that comes into contact with the screw hole, and it is more preferable to immerse only the bolt 8c in a liquid containing the lubricant 9.

【0057】[0057]

【発明の効果】以上詳細に説明したように、本発明の偏
向ヨーク締付バンド及び偏向ヨーク、並びに、偏向ヨー
ク締付バンドの製造方法は、ボルトの表面に、上述した
分子構造を有する液状のフッ素系潤滑剤を3×10-3
13×10-3mg/mm2なる付着量で付着させたの
で、ねじ部に対するボルトのかじりや焼き付きを極めて
効果的に防止することができる。即ち、潤滑剤が少なす
ぎたり多すぎたりすることによるかじりや焼き付きが発
生せず、また、必要以上の無駄な潤滑剤を使用すること
もない。従って、偏向ヨーク締付バンドを交換するため
のコストや交換作業の発生を防止することが可能とな
る。
As described in more detail, according to the present invention, the deflection yoke clamping band and deflection yoke of the present invention, as well as producing how dated band deflection yoke tightening, on the surface of the bolt, the above-described
A liquid fluorine Cajun lubricants having a molecular structure 3 × 10 -3 ~
Since the adhesion was performed at an adhesion amount of 13 × 10 −3 mg / mm 2 , galling and seizure of the bolt to the screw portion can be extremely effectively prevented. That is, galling or seizure does not occur due to too little or too much lubricant, and no unnecessary lubricant is used. Therefore, it is possible to prevent the cost for replacing the deflection yoke tightening band and the occurrence of replacement work.

【0058】また、本発明の偏向ヨーク締付バンドの製
造方法は、ボルトを、フッ素系の潤滑剤を含んだ液体
に、その液体を循環もしくは撹拌させつつ所定時間浸漬
させるようにしたので、ボルトの本数によらず、ボルト
に対する潤滑剤の付着量をほぼ一定とすることができ
る。従って、ボルトに潤滑剤を望ましい付着量で付着さ
せることできるので、潤滑剤が少なすぎたり多すぎたり
することによるかじりや焼き付きが発生せず、また、必
要以上の無駄な潤滑剤を使用することもない。
In the method of manufacturing the deflection yoke tightening band according to the present invention, the bolt is immersed in a liquid containing a fluorine-based lubricant for a predetermined time while circulating or stirring the liquid. Irrespective of the number of the bolts, the amount of the lubricant attached to the bolt can be made substantially constant. Therefore, since the lubricant can be applied to the bolts in a desired amount, the galling and seizure due to too little or too much lubricant do not occur, and use of unnecessary lubricant more than necessary Nor.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明の偏向ヨーク締付バンドの一実施例を示
す斜視図である。
FIG. 1 is a perspective view showing one embodiment of a deflection yoke tightening band of the present invention.

【図2】本発明の偏向ヨークの一実施例を示す斜視図で
ある。
FIG. 2 is a perspective view showing one embodiment of a deflection yoke of the present invention.

【図3】本発明の偏向ヨーク締付バンドによって偏向ヨ
ークを陰極線管に装着した状態を示す側面図である。
FIG. 3 is a side view showing a state in which the deflection yoke is mounted on the cathode ray tube by the deflection yoke tightening band of the present invention.

【図4】本発明の偏向ヨーク締付バンドの製造方法を説
明するための一部破断の断面図である。
FIG. 4 is a partially cutaway sectional view for explaining the method of manufacturing the deflection yoke tightening band of the present invention.

【図5】本発明の偏向ヨーク締付バンドの製造方法を説
明するための平面図ある。
FIG. 5 is a plan view for explaining a method of manufacturing the deflection yoke tightening band of the present invention.

【図6】本発明の偏向ヨーク締付バンドの製造方法を説
明するための平面図ある。
FIG. 6 is a plan view for explaining a method of manufacturing the deflection yoke tightening band of the present invention.

【図7】従来の偏向ヨーク締付バンドの一例を示す斜視
図である。
FIG. 7 is a perspective view showing an example of a conventional deflection yoke tightening band.

【符号の説明】[Explanation of symbols]

1 偏向ヨーク 1a 大径部 1b 小径部 2 セパレータ 3 垂直偏向コイル 4 コア 5a,5b フランジ 6 円筒部 7 突起 8a 円周部 8a1 係合穴 8b 突出片 8c ボルト 8c1 頭 9 潤滑剤 10 槽 11 ポンプ 12 排出口 13 吐出口 14 パイプ管 15 ファン 16 網籠 17 モータ 18 羽根 20 希釈液 80 偏向ヨーク締付バンド 100 陰極線管(CRT) 100N ネック部 101 電子銃 DESCRIPTION OF SYMBOLS 1 Deflection yoke 1a Large diameter part 1b Small diameter part 2 Separator 3 Vertical deflection coil 4 Core 5a, 5b Flange 6 Cylindrical part 7 Projection 8a Circular part 8a1 Engagement hole 8b Projection piece 8c Bolt 8c1 Head 9 Lubricant 10 Tank 11 Pump 12 Discharge port 13 Discharge port 14 Pipe tube 15 Fan 16 Mesh basket 17 Motor 18 Blade 20 Diluent 80 Deflection yoke tightening band 100 Cathode ray tube (CRT) 100N Neck part 101 Electron gun

───────────────────────────────────────────────────── フロントページの続き (56)参考文献 特開 昭50−126734(JP,A) 特公 昭55−9566(JP,B1) 実公 平2−32686(JP,Y2) (58)調査した分野(Int.Cl.7,DB名) H01J 29/76 H01J 29/82 H01J 9/236 H01J 9/44 F16B 33/06 F16B 25/00 F16B 2/08 B05D 7/00 ──────────────────────────────────────────────────続 き Continuation of front page (56) References JP-A-50-126734 (JP, A) JP-B-55-9566 (JP, B1) Jikyo Hei 2-32686 (JP, Y2) (58) Field (Int.Cl. 7 , DB name) H01J 29/76 H01J 29/82 H01J 9/236 H01J 9/44 F16B 33/06 F16B 25/00 F16B 2/08 B05D 7/00

Claims (5)

(57)【特許請求の範囲】(57) [Claims] 【請求項1】漏斗状のセパレータを備えた偏向ヨークを
陰極線管のネック部に固定するための偏向ヨーク締付バ
ンドであり、前記セパレータの小径側先端の円筒部に当
接する円周部と、この円周部の両端部より外方向に突出
した1対の突出片と、この1対の突出片に形成された少
なくとも一方がねじ穴とされた1対の穴を貫通するよう
に取り付けられたボルトとを備えた偏向ヨーク締付バン
ドにおいて、 前記ボルトの表面に、以下の分子構造を有する液状の
ッ素系潤滑剤を3×10-3〜13×10-3mg/mm2
なる付着量で付着させたことを特徴とする偏向ヨーク締
め付けバンド。【化1】
1. A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, a circumferential portion abutting on a cylindrical portion at a small-diameter end of the separator; A pair of projecting pieces projecting outward from both ends of the circumferential portion, and at least one of the pair of projecting pieces is attached so as to pass through a pair of screw holes. in the deflection yoke clamping band that includes a bolt, a surface of the bolt, the following liquid having a molecular structure of full <br/> Tsu containing Cajun lubricant to 3 × 10 -3 ~13 × 10 -3 mg / mm 2
A deflection yoke tightening band, wherein the band is attached with a variable amount of attachment. Embedded image
【請求項2】陰極線管のネック部に装着される漏斗状の
セパレータを備えた偏向ヨークであり、前記セパレータ
の小径側先端の円筒部に当接する円周部と、この円周部
の両端部より外方向に突出した1対の突出片と、この1
対の突出片に形成された少なくとも一方がねじ穴とされ
た1対の穴を貫通するように取り付けられたボルトとを
備えた偏向ヨーク締付バンドによって前記ネック部に固
定される偏向ヨークにおいて、 前記偏向ヨーク締付バンドの前記ボルトの表面に、以下
の分子構造を有する液状のフッ素系潤滑剤を3×10-3
〜13×10-3mg/mm2なる付着量で付着させたこ
とを特徴とする偏向ヨーク。【化1】
2. A deflection yoke provided with a funnel-shaped separator mounted on a neck portion of a cathode ray tube, wherein a circumferential portion abuts a cylindrical portion at a small-diameter end of the separator, and both ends of the circumferential portion. A pair of projecting pieces projecting more outward,
A deflection yoke fixed to the neck by a deflection yoke tightening band including a bolt attached so that at least one formed in the pair of projecting pieces penetrates a pair of screw holes. on the surface of the bolt of the deflection yoke clamping band, below
3 fluorine Cajun lubricant liquid having a molecular structure × 10 -3
A deflection yoke having a deposition amount of about 13 × 10 −3 mg / mm 2 . Embedded image
【請求項3】漏斗状のセパレータを備えた偏向ヨークを
陰極線管のネック部に固定するための偏向ヨーク締付バ
ンドであり、両端部より外方向に突出した1対の突出片
を有し、前記セパレータの小径側先端の円筒部に当接す
る円周部と、前記1対の突出片に形成された少なくとも
一方がねじ穴とされた1対の穴を貫通するように取り付
けられたボルトとよりなる偏向ヨーク締付バンドを製造
するための偏向ヨーク締付バンドの製造方法において、 前記ボルトの表面に、以下の分子構造を有する液状の
ッ素系潤滑剤を3×10-3〜13×10-3mg/mm2
なる付着量で付着させる第1の工程と、 前記突出片の前記1対の穴に前記ボルトを取り付けて、
前記円周部と前記ボルトとを一体化する第2の工程とを
いずれかの順で含むことを特徴とする偏向ヨーク締付バ
ンドの製造方法。【化1】
3. A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, comprising a pair of projecting pieces projecting outward from both ends. A circumferential portion that abuts a cylindrical portion at a small-diameter end of the separator, and a bolt that is attached to at least one of the pair of projecting pieces so as to penetrate a pair of screw holes. the method of manufacturing a deflection yoke clamping band for producing deflection yoke clamping band of the on the surface of the bolt, liquid full <br/> Tsu containing Cajun lubricant to 3 × 10 having the following molecular structure - 3 to 13 × 10 -3 mg / mm 2
A first step of attaching with a given amount of attachment; attaching the bolt to the pair of holes of the projecting piece;
A method for manufacturing a deflection yoke tightening band, comprising: in any order, a second step of integrating the circumferential portion and the bolt. Embedded image
【請求項4】前記第1の工程は、前記潤滑剤を希釈する
工程、前記潤滑剤を加熱する工程、余分な前記潤滑剤を
取り除く工程の少なくとも1つを含むことを特徴とする
請求項3記載の偏向ヨーク締付バンドの製造方法。
4. The method according to claim 3, wherein the first step includes at least one of a step of diluting the lubricant, a step of heating the lubricant, and a step of removing excess lubricant. A manufacturing method of the deflection yoke tightening band described in the above.
【請求項5】漏斗状のセパレータを備えた偏向ヨークを
陰極線管のネック部に固定するための偏向ヨーク締付バ
ンドであり、両端部より外方向に突出した1対の突出片
を有し、前記セパレータの小径側先端の円筒部に当接す
る円周部と、前記1対の突出片に形成された少なくとも
一方がねじ穴とされた1対の穴を貫通するように取り付
けられたボルトとよりなる偏向ヨーク締付バンドを製造
するための偏向ヨーク締付バンドの製造方法において、 前記ボルトを、以下の分子構造を有する液状のフッ素
滑剤を含んだ液体に、その液体を循環もしくは撹拌さ
せつつ所定時間浸漬させて、3×10 -3 〜13×10 -3
mg/mm 2 なる付着量で付着させる第1の工程と、 前記第1の工程によって前記潤滑剤が付着した前記ボル
トを、前記突出片の前記1対の穴に取り付けて、前記円
周部と前記ボルトとを一体化する第2の工程とを含むこ
とを特徴とする偏向ヨーク締付バンドの製造方法。【化1】
5. A deflection yoke tightening band for fixing a deflection yoke provided with a funnel-shaped separator to a neck portion of a cathode ray tube, comprising a pair of projecting pieces projecting outward from both ends. A circumferential portion that abuts a cylindrical portion at a small-diameter end of the separator, and a bolt that is attached to at least one of the pair of projecting pieces so as to penetrate a pair of screw holes. A method of manufacturing a deflection yoke tightening band for manufacturing a deflection yoke tightening band, comprising : forming a bolt as a liquid fluorine- based material having the following molecular structure:
A liquid containing or lubricants, is immersed a predetermined time while circulating or stirring the liquid, 3 × 10 -3 ~13 × 10 -3
a first step of depositing in mg / mm 2 comprising attachment amount, the first of said bolts the lubricant is attached by a process, attached to the pair hole of said projecting pieces, said circumferential portion And a second step of integrating said bolt with said bolt. Embedded image
JP16300998A 1997-10-17 1998-05-27 Deflection yoke tightening band, deflection yoke, and method of manufacturing deflection yoke tightening band Expired - Fee Related JP3259909B2 (en)