JP2966549B2 - 非焼結式カドミウム負極の製造方法 - Google Patents
非焼結式カドミウム負極の製造方法Info
- Publication number
- JP2966549B2 JP2966549B2 JP3035910A JP3591091A JP2966549B2 JP 2966549 B2 JP2966549 B2 JP 2966549B2 JP 3035910 A JP3035910 A JP 3035910A JP 3591091 A JP3591091 A JP 3591091A JP 2966549 B2 JP2966549 B2 JP 2966549B2
- Authority
- JP
- Japan
- Prior art keywords
- negative electrode
- cadmium
- battery
- electrode plate
- hydroxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3035910A JP2966549B2 (ja) | 1991-03-01 | 1991-03-01 | 非焼結式カドミウム負極の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3035910A JP2966549B2 (ja) | 1991-03-01 | 1991-03-01 | 非焼結式カドミウム負極の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH04274162A JPH04274162A (ja) | 1992-09-30 |
| JPH04274162A5 JPH04274162A5 (enExample) | 1998-09-11 |
| JP2966549B2 true JP2966549B2 (ja) | 1999-10-25 |
Family
ID=12455188
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3035910A Expired - Fee Related JP2966549B2 (ja) | 1991-03-01 | 1991-03-01 | 非焼結式カドミウム負極の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2966549B2 (enExample) |
-
1991
- 1991-03-01 JP JP3035910A patent/JP2966549B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH04274162A (ja) | 1992-09-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US5935732A (en) | Hydrogen absorbing electrode and its manufacturing method | |
| JP3019094B2 (ja) | アルカリ蓄電池用電極の製造方法 | |
| CN1307739C (zh) | 镍氢电池的制造方法 | |
| CA2321293C (en) | Nickel electrode for alkali storage battery, method of producing nickel electrode for alkali storage battery, and alkali storage battery | |
| EP1168471B1 (en) | Nickel electrode for alkaline storage battery and alkaline storage battery | |
| JPH04274162A (ja) | 非焼結式カドミウム負極の製造方法 | |
| JP2584280B2 (ja) | アルカリ蓄電池及びその製造方法 | |
| JP3086525B2 (ja) | 密閉型アルカリ蓄電池及びその製造方法 | |
| JP2925764B2 (ja) | アルカリ蓄電池の製造方法 | |
| JP2786889B2 (ja) | アルカリ蓄電池用カドミウム負極板の製造方法 | |
| JPH05174869A (ja) | 密閉型ニッケル水素電池の処理法 | |
| JP3182225B2 (ja) | アルカリ蓄電池用カドミウム負極の製造方法 | |
| JP2755690B2 (ja) | アルカリ蓄電池用カドミウム負極板の製造方法 | |
| JP3225608B2 (ja) | アルカリ電池用水酸化ニッケル正極板およびその製造方法 | |
| JPS63126163A (ja) | アルカリ蓄電池 | |
| JP3454612B2 (ja) | 水素吸蔵合金電極の製造方法 | |
| JP2968813B2 (ja) | アルカリ蓄電池用カドミウム負極の製造方法 | |
| JP3827023B2 (ja) | 水素吸蔵電極およびその製造方法 | |
| JP3995288B2 (ja) | アルカリ蓄電池用カドミウム負極およびその製造方法 | |
| JP3118357B2 (ja) | アルカリ蓄電池用非焼結正極板 | |
| JP2966497B2 (ja) | アルカリ蓄電池用カドミウム負極板の製造方法 | |
| JP3241441B2 (ja) | アルカリ蓄電池用カドミウム負極 | |
| JPH0963573A (ja) | 水素吸蔵合金電極の製造方法 | |
| CN1153404A (zh) | 镍氢电池负极合金材料及用其制做镍氢电池的方法 | |
| JPH10275619A (ja) | ペースト式カドミウム電極 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20070813 Year of fee payment: 8 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20080813 Year of fee payment: 9 |
|
| LAPS | Cancellation because of no payment of annual fees |