JP2013185228A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2013185228A5 JP2013185228A5 JP2012052765A JP2012052765A JP2013185228A5 JP 2013185228 A5 JP2013185228 A5 JP 2013185228A5 JP 2012052765 A JP2012052765 A JP 2012052765A JP 2012052765 A JP2012052765 A JP 2012052765A JP 2013185228 A5 JP2013185228 A5 JP 2013185228A5
- Authority
- JP
- Japan
- Prior art keywords
- copper foil
- electrolytic copper
- mpa
- tensile strength
- initial tensile
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Links
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 claims description 7
- 239000011889 copper foil Substances 0.000 claims description 7
- 238000002441 X-ray diffraction Methods 0.000 claims description 3
- 238000010438 heat treatment Methods 0.000 claims description 2
- 239000000956 alloy Substances 0.000 description 1
- 229910045601 alloy Inorganic materials 0.000 description 1
- 239000011888 foil Substances 0.000 description 1
Priority Applications (8)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2012052765A JP2013185228A (ja) | 2012-03-09 | 2012-03-09 | 電解銅箔及び二次電池用負極集電体 |
| KR1020157022124A KR20150097821A (ko) | 2011-07-29 | 2012-07-30 | 전해 동합금박, 그 제조 방법, 그것의 제조에 이용하는 전해액, 그것을 이용한 2차 전지용 음극 집전체, 2차 전지 및 그 전극 |
| EP12819841.3A EP2660359A4 (en) | 2011-07-29 | 2012-07-30 | ELECTROLYTIC COPPER ALLOY FOIL, PROCESS FOR THE PRODUCTION THEREOF, ELECTROLYTE SOLUTION USED FOR THE PRODUCTION THEREOF, NEGATIVE ELECTRODE COLLECTOR FOR SECONDARY BATTERIES THEREWITH, SECONDARY BATTERY AND ELECTRODE OF A SECONDARY BATTERY |
| TW101127554A TWI496954B (zh) | 2011-07-29 | 2012-07-30 | An electrolytic copper alloy foil manufacturing method, an electrolytic solution for the production of the alloy foil, a negative electrode current collector for a secondary battery, a secondary battery and an electrode |
| CN201280004436.7A CN103348041B (zh) | 2011-07-29 | 2012-07-30 | 电解铜合金箔、其制备方法、制备中所用的电解液、使用该电解铜合金箔的二次电池用负极集电体、二次电池及其电极 |
| PCT/JP2012/069368 WO2013018773A1 (ja) | 2011-07-29 | 2012-07-30 | 電解銅合金箔、その製造方法、それの製造に用いる電解液、それを用いた二次電池用負極集電体、二次電池及びその電極 |
| KR1020137006252A KR101669087B1 (ko) | 2011-07-29 | 2012-07-30 | 전해 동합금박, 그 제조 방법, 그것의 제조에 이용하는 전해액, 그것을 이용한 2차 전지용 음극 집전체, 2차 전지 및 그 전극 |
| US13/965,291 US9890463B2 (en) | 2011-07-29 | 2013-08-13 | Electrolysis copper-alloy foil, method of the same, electrolytic-solution using the production, negative electrode aggregation used the same, secondary battery, and electrode of the same |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2012052765A JP2013185228A (ja) | 2012-03-09 | 2012-03-09 | 電解銅箔及び二次電池用負極集電体 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2013185228A JP2013185228A (ja) | 2013-09-19 |
| JP2013185228A5 true JP2013185228A5 (enExample) | 2014-02-06 |
Family
ID=49386925
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2012052765A Withdrawn JP2013185228A (ja) | 2011-07-29 | 2012-03-09 | 電解銅箔及び二次電池用負極集電体 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2013185228A (enExample) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN104903495B (zh) * | 2013-01-24 | 2016-12-07 | 古河电气工业株式会社 | 电解铜箔与其制造方法 |
| JP2014101581A (ja) * | 2013-12-25 | 2014-06-05 | Furukawa Electric Co Ltd:The | 電解銅合金箔、その製造方法、その製造に用いる電解液、二次電池用負極集電体、二次電池及びその電極 |
| JP6067910B1 (ja) * | 2015-11-04 | 2017-01-25 | 古河電気工業株式会社 | 電解銅箔、その電解銅箔を用いたリチウムイオン二次電池 |
| CA3220490A1 (en) * | 2022-11-24 | 2024-05-24 | Sk Nexilis Co., Ltd. | Copper foil, electrode comprising the same, secondary battery comprising the same, and method for manufacturing the same |
-
2012
- 2012-03-09 JP JP2012052765A patent/JP2013185228A/ja not_active Withdrawn
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| MY173639A (en) | Electrolytic copper foil and negative electrode current collector for secondary battery | |
| JP2013030472A5 (ja) | 蓄電装置 | |
| WO2012175301A3 (de) | Chemisch behandelte stromableiterfolie aus aluminium oder einer aluminiumlegierung | |
| TWI456827B (zh) | 鋰離子二次電池負極集電體用之銅箔、鋰離子二次電池負極材及鋰離子二次電池負極集電體選定方法 | |
| PL3121885T3 (pl) | Elektrolityczna folia miedziana i kolektor, ujemna elektroda, oraz bateria litowa je zawierająca | |
| PL3121884T3 (pl) | Elektrolityczna folia miedziana i kolektor, elektroda ujemna i bateria litowa je zawierająca | |
| WO2014201275A3 (en) | High capacity hard carbon materials comprising efficiency enhancers | |
| WO2015157324A3 (en) | Energy storage device, anode thereof, and method of fabricating an energy storage device | |
| JP2013028525A5 (enExample) | ||
| EP3032618A3 (en) | Positive active material for rechargeable lithium battery and rechargeable lithium battery | |
| JP2013255365A5 (enExample) | ||
| HUE047961T2 (hu) | Felületkezelt rézfólia és a felületkezelt rézfóliát használó áramkollektor, elektróda és akkumulátor cella | |
| JP2016521442A5 (enExample) | ||
| JP2011222500A5 (ja) | 二次電池 | |
| WO2012161503A3 (ko) | 촉매전극의 제조방법, 이를 통해 제조된 촉매전극 및 이를 포함하는 전지 | |
| HK1244951A1 (zh) | 有机锂电池 | |
| JP2013185228A5 (enExample) | ||
| WO2014110514A3 (en) | Concentrating solar energy collector | |
| ES2397014R1 (es) | Base de bateria de coccion | |
| JP2014067643A5 (enExample) | ||
| WO2014043492A3 (en) | Concentrating solar energy collector | |
| JP2016511925A5 (enExample) | ||
| JP2012009268A5 (enExample) | ||
| TH148360A (th) | ฟอยด์ทองแดงแบบอิเล็กโตรไลติกและตัวเก็บกระแสลบสำหรับแบตเตอรี่ทุติยภูมิ (electrolytic copper foil and negative electrode current collector for secondary battery) | |
| JP2014095122A5 (enExample) |