JP2008115375A5 - - Google Patents

Download PDF

Info

Publication number
JP2008115375A5
JP2008115375A5 JP2007263869A JP2007263869A JP2008115375A5 JP 2008115375 A5 JP2008115375 A5 JP 2008115375A5 JP 2007263869 A JP2007263869 A JP 2007263869A JP 2007263869 A JP2007263869 A JP 2007263869A JP 2008115375 A5 JP2008115375 A5 JP 2008115375A5
Authority
JP
Japan
Prior art keywords
coating composition
polar amino
adhesion
blended
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2007263869A
Other languages
Japanese (ja)
Other versions
JP2008115375A (en
JP5176252B2 (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2007263869A priority Critical patent/JP5176252B2/en
Priority claimed from JP2007263869A external-priority patent/JP5176252B2/en
Publication of JP2008115375A publication Critical patent/JP2008115375A/en
Publication of JP2008115375A5 publication Critical patent/JP2008115375A5/ja
Application granted granted Critical
Publication of JP5176252B2 publication Critical patent/JP5176252B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (10)

(c)極性アミノ酸、極性アミノ酸重合物およびそれらの塩からなる群から選択される少なくとも1種を配合することを特徴とする、(a)石灰および(b)水を含有するコーティング組成物の流動性向上方法。(C) Flow of a coating composition containing (a) lime and (b) water, characterized in that it contains at least one selected from the group consisting of polar amino acids, polar amino acid polymers and salts thereof Improvement method. さらに(d)キレート化合物を配合することを特徴とする、請求項1に記載する流動性向上方法。Furthermore, (d) a chelate compound is mix | blended, The fluidity improvement method of Claim 1 characterized by the above-mentioned. (c)極性アミノ酸、極性アミノ酸重合物およびそれらの塩からなる群から選択される少なくとも1種を配合することを特徴とする、(a)石灰および(b)水を含有するコーティング組成物の基材に対する付着力向上または付着力の均一安定化方法。(C) Base of coating composition containing (a) lime and (b) water, characterized in that it contains at least one selected from the group consisting of polar amino acids, polar amino acid polymers and salts thereof A method for improving adhesion to materials or uniform stabilizing adhesion. さらに(d)キレート化合物を配合することを特徴とする、請求項3に記載する付着力向上または付着力の均一安定化方法。Furthermore, (d) chelate compound is mix | blended, The adhesive force improvement or the uniform stabilization method of adhesive force of Claim 3 characterized by the above-mentioned. コーティング組成物が、さらに(f)結合材を含むものである、請求項3または4に記載する付着力向上または付着力の均一安定化方法。The method for improving adhesion force or stabilizing adhesion force according to claim 3 or 4, wherein the coating composition further comprises (f) a binder. 請求項3乃至5のいずれかに記載する方法によって基材に対する付着力が向上され、または付着力が均一安定化された水配合コーティング組成物から形成された皮膜を有する被覆物。A coating comprising a film formed from a water-containing coating composition having improved adhesion to the substrate by the method according to any one of claims 3 to 5 or having the adhesion uniformly stabilized. (c)極性アミノ酸、極性アミノ酸重合物およびそれらの塩からなる群から選択される少なくとも1種を配合することを特徴とする、(a)石灰および(b)水を含有するコーティング組成物の耐ひび割れ性向上方法。(C) At least one selected from the group consisting of polar amino acids, polar amino acid polymers and salts thereof is blended, and (a) resistance to a coating composition containing lime and (b) water Cracking improvement method. さらに(d)キレート化合物を配合することを特徴とする、請求項7に記載する耐ひび割れ性向上方法。Furthermore, (d) a chelate compound is mix | blended, The crack-resistant improvement method of Claim 7 characterized by the above-mentioned. コーティング組成物が、さらに(f)結合材を含むものである、請求項7または8に記載する耐ひび割れ性向上方法。The method for improving crack resistance according to claim 7 or 8, wherein the coating composition further comprises (f) a binder. 請求項7乃至9のいずれかに記載する方法によって耐ひび割れ性が向上されたコーティング組成物から形成される、耐ひび割れ性の皮膜を有する被覆物。A coating having a crack resistant film formed from a coating composition having improved crack resistance by the method according to any one of claims 7 to 9 .
JP2007263869A 2006-10-10 2007-10-10 Improvement of water-containing coating composition containing lime Active JP5176252B2 (en)