GB1329081A - Electrodeposition of composite coatings - Google Patents
Electrodeposition of composite coatingsInfo
- Publication number
- GB1329081A GB1329081A GB1329081DA GB1329081A GB 1329081 A GB1329081 A GB 1329081A GB 1329081D A GB1329081D A GB 1329081DA GB 1329081 A GB1329081 A GB 1329081A
- Authority
- GB
- United Kingdom
- Prior art keywords
- particles
- materials
- metal matrix
- composite
- agitator
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
1329081 Electrodeposition of composite coatings BRISTOL AEROJET Ltd 27 Aug 1970 [4 June 1969] 28191/69 Heading C7B [Also in Division F2] In electrodepositing (e.g. electroforming) a composite coating consisting of an electrolytically deposited metal matrix with particulate additions, a solution containing insoluble particles is agitated by movement generally up and down of a generally horizontal perforated agitator in a part of the solution below the part used for deposition. Fig. 1 shows a perforated agitator plate 3 which is bodily moved up and down within a tank 1 by piston rods 14 at each side of the tank, the rods moving the agitator by means of members 13, 8, 7 and 6. The pistons keep in synchronism since they are linked by means of yokes 13 and endless chains 16 passing around sprockets 19 on a rod 21. The particles used in the deposition may be ceramic, cermet or laminar solids. For example, the metal matrix may be Ni, Co, Cu, Cr or W-Co alloy and the particles may be zirconium diboride or tungsten carbide. Where the composite coating is to act as a bearing it may comprise metal matrix, ceramic particles and graphite particles. The plating may be on to steel, non-ferrous or light alloy components, or on to plastics, glass or composite materials where such materials have been rendered conductive either by incorporation of appropriate materials or by pre-coating with conductive materials.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB2819169 | 1970-08-27 |
Publications (1)
Publication Number | Publication Date |
---|---|
GB1329081A true GB1329081A (en) | 1973-09-05 |
Family
ID=10271735
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB1329081D Expired GB1329081A (en) | 1970-08-27 | 1970-08-27 | Electrodeposition of composite coatings |
Country Status (1)
Country | Link |
---|---|
GB (1) | GB1329081A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE3535548A1 (en) * | 1984-10-05 | 1986-04-17 | Baj Ltd., Weston-Super-Mare, Avon | METAL PROTECTIVE COATING |
WO1991002831A1 (en) * | 1989-08-21 | 1991-03-07 | Christiaan De Boks | Striking implement for a ball game and method for manufacturing such an implement |
US5935407A (en) * | 1997-11-06 | 1999-08-10 | Chromalloy Gas Turbine Corporation | Method for producing abrasive tips for gas turbine blades |
CN111139609A (en) * | 2018-11-06 | 2020-05-12 | 海宁市天一纺织有限公司 | Fabric and processing device thereof |
-
1970
- 1970-08-27 GB GB1329081D patent/GB1329081A/en not_active Expired
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE3535548A1 (en) * | 1984-10-05 | 1986-04-17 | Baj Ltd., Weston-Super-Mare, Avon | METAL PROTECTIVE COATING |
US4789441A (en) * | 1984-10-05 | 1988-12-06 | John Foster | Metallic protective coatings and method of making |
DE3535548C2 (en) * | 1984-10-05 | 1999-03-04 | Baj Coatings Ltd | Coated article and method of making a coating of an article |
WO1991002831A1 (en) * | 1989-08-21 | 1991-03-07 | Christiaan De Boks | Striking implement for a ball game and method for manufacturing such an implement |
US5935407A (en) * | 1997-11-06 | 1999-08-10 | Chromalloy Gas Turbine Corporation | Method for producing abrasive tips for gas turbine blades |
US6194086B1 (en) | 1997-11-06 | 2001-02-27 | Chromalloy Gas Turbine Corporation | Method for producing abrasive tips for gas turbine blades |
CN111139609A (en) * | 2018-11-06 | 2020-05-12 | 海宁市天一纺织有限公司 | Fabric and processing device thereof |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Safranek | The Properties of Electrodeposited Metals and Alloys: a Handbook. | |
DE2543082B2 (en) | Cyanidic silver electrolyte and process for the electrodeposition of silver-graphite dispersion coatings and its application | |
DE69507172T2 (en) | Process for the production of electroplated dispersion coatings of hard chrome and wear-resistant coatings produced in this way | |
GB1329081A (en) | Electrodeposition of composite coatings | |
GB1236954A (en) | Improvements in and relating to electrodeposited composite coatings | |
FR2441669A1 (en) | METHOD AND DEVICE FOR THE CONTINUOUS AND HIGH-CURRENT DENSITY ELECTROLYTE DEPOSITION OF A COATING METAL ON A SHEET METAL | |
US3830711A (en) | Electrodeposition of composite coatings | |
GB1224166A (en) | Improvements in and relating to electrodeposition of composite materials | |
GB1315619A (en) | Abrasion-resistant sliding members | |
GB1347184A (en) | Electrodeposition of composite coatings | |
GB1220331A (en) | Improvements in and relating to the electro-deposition of composite coatings | |
Pavlenko et al. | The copper plating of graphite powders in the manufacture of copper-graphite materials | |
GB1461181A (en) | Electrophoretic enamelling | |
GB1288908A (en) | ||
GB1362558A (en) | Electro-deposited composite coatings of metal and graphite fluoride | |
GB1503885A (en) | Electroplating | |
GB1380055A (en) | Electrodeposition of a composite coating including chromium | |
Birkle et al. | Aluminium Electrocoating for Use by Major Industries | |
Venugopalan et al. | Electroplating of Aluminum and Its Alloys on Mild Steel--A Literature Survey of Efficient Method | |
Benninghoff | Electroplating Components in Difficult Materials | |
Azzerri et al. | Electrodeposition of Complex Coatings and Electrochemical Processes at High Current Density for Continuous Treatment Lines | |
Harding | Aluminum | |
JPS5468727A (en) | Manufacture of carbon fiber-metal composite material | |
Fuvelle | Electrodeposition with a Pulsating Current Depots Electrolytiques Courant Pulse | |
Lemkey et al. | Eutectic superalloys strengthened by aligned delta, Ni3Cb lamellae, gamma-prime, Ni3Al precipitates and reduced interlamellar spacing. |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PS | Patent sealed | ||
PE20 | Patent expired after termination of 20 years |