FR838515A - Installation à vide, notamment pour la métallisation d'objets - Google Patents
Installation à vide, notamment pour la métallisation d'objetsInfo
- Publication number
- FR838515A FR838515A FR838515DA FR838515A FR 838515 A FR838515 A FR 838515A FR 838515D A FR838515D A FR 838515DA FR 838515 A FR838515 A FR 838515A
- Authority
- FR
- France
- Prior art keywords
- metallization
- objects
- vacuum installation
- vacuum
- installation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C14/00—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material
- C23C14/22—Coating by vacuum evaporation, by sputtering or by ion implantation of the coating forming material characterised by the process of coating
- C23C14/56—Apparatus specially adapted for continuous coating; Arrangements for maintaining the vacuum, e.g. vacuum locks
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
DE838515X | 1937-05-29 |
Publications (1)
Publication Number | Publication Date |
---|---|
FR838515A true FR838515A (fr) | 1939-03-08 |
Family
ID=6761684
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR838515D Expired FR838515A (fr) | 1937-05-29 | 1938-05-28 | Installation à vide, notamment pour la métallisation d'objets |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR838515A (fr) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2767682A (en) * | 1951-03-22 | 1956-10-23 | Syntron Co | Vaporizing apparatus for producing selenium rectifiers |
US2975753A (en) * | 1958-11-18 | 1961-03-21 | Nat Res Corp | Vacuum coating apparatus |
DE1279857B (de) * | 1961-08-07 | 1968-10-10 | Babcock & Wilcox Dampfkessel | Schleusenkammer fuer kerntechnische Anlagen |
US4068617A (en) * | 1976-05-03 | 1978-01-17 | The Goodyear Tire & Rubber Company | Apparatus for coating wire on a spool |
US4109609A (en) * | 1976-05-03 | 1978-08-29 | The Goodyear Tire & Rubber Company | Vacuum-pressurized immersion coater |
US4188420A (en) * | 1976-05-03 | 1980-02-12 | The Goodyear Tire & Rubber Company | Method for coating wire on a spool |
-
1938
- 1938-05-28 FR FR838515D patent/FR838515A/fr not_active Expired
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2767682A (en) * | 1951-03-22 | 1956-10-23 | Syntron Co | Vaporizing apparatus for producing selenium rectifiers |
US2975753A (en) * | 1958-11-18 | 1961-03-21 | Nat Res Corp | Vacuum coating apparatus |
DE1279857B (de) * | 1961-08-07 | 1968-10-10 | Babcock & Wilcox Dampfkessel | Schleusenkammer fuer kerntechnische Anlagen |
DE1279857C2 (de) * | 1961-08-07 | 1973-02-22 | Babcock & Wilcox Dampfkessel W | Schleusenkammer fuer kerntechnische Anlagen |
US4068617A (en) * | 1976-05-03 | 1978-01-17 | The Goodyear Tire & Rubber Company | Apparatus for coating wire on a spool |
US4109609A (en) * | 1976-05-03 | 1978-08-29 | The Goodyear Tire & Rubber Company | Vacuum-pressurized immersion coater |
US4188420A (en) * | 1976-05-03 | 1980-02-12 | The Goodyear Tire & Rubber Company | Method for coating wire on a spool |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR836633A (fr) | Systèmes d'antennes | |
FR840410A (fr) | Systèmes d'attache pour boutons | |
FR838909A (fr) | Multiplicateur d'électrons | |
FR838515A (fr) | Installation à vide, notamment pour la métallisation d'objets | |
CH253220A (fr) | Machine pour la fabrication d'objets moulés en verre. | |
FR837382A (fr) | Frein d'écrou | |
FR858939A (fr) | Dispositif d'herméticite pour chambres à vide | |
FR837422A (fr) | Coussins d'épaules | |
FR866695A (fr) | Perfectionnements apportés aux procédés de balisage, notamment pour l'atterrissage sans visibilité des avions | |
FR851596A (fr) | Systèmes d'antennes | |
Stewart | The development of the American white ware industry: a geographical interpretation | |
FR860542A (fr) | Composition augmentant l'adhérence | |
CH193849A (fr) | Installation d'électroculture. | |
Hall | Extra Supplement: The Coasts of High Barbary | |
FR873954A (fr) | Perfectionnements apportés aux soupapes d'étranglement notamment pour appareils à vide élevé | |
FR838813A (fr) | Perfectionnement à l'ornementation de l'habillement | |
FR816669A (fr) | Perfectionnement au montage des hauts-parleurs d'appareils de t. s. f. | |
FR857250A (fr) | Cadre profilé pour radiogoniométrie d'avion | |
FR834823A (fr) | Installation pour le dégraissage des vêtements ou analogues | |
FR841173A (fr) | Ponceuse perfectionnée de bords pour l'industrie de la chapellerie | |
FR829253A (fr) | Installation d'arrosage | |
FR834437A (fr) | Articles d'ameublement | |
FR834683A (fr) | Aspirateurs et refouleurs pour la ventilation et pour tous usages | |
FR850523A (fr) | Bêche spéciale pour l'armée | |
CA377295A (fr) | Traitement de composes solides |