FR2289623A2 - Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusion - Google Patents
Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusionInfo
- Publication number
- FR2289623A2 FR2289623A2 FR7440332A FR7440332A FR2289623A2 FR 2289623 A2 FR2289623 A2 FR 2289623A2 FR 7440332 A FR7440332 A FR 7440332A FR 7440332 A FR7440332 A FR 7440332A FR 2289623 A2 FR2289623 A2 FR 2289623A2
- Authority
- FR
- France
- Prior art keywords
- metal
- zinc
- hot dip
- coolant
- dip coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C2/00—Hot-dipping or immersion processes for applying the coating material in the molten state without affecting the shape; Apparatus therefor
- C23C2/34—Hot-dipping or immersion processes for applying the coating material in the molten state without affecting the shape; Apparatus therefor characterised by the shape of the material to be treated
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7440332A FR2289623A2 (fr) | 1974-10-28 | 1974-10-28 | Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusion |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR7440332A FR2289623A2 (fr) | 1974-10-28 | 1974-10-28 | Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusion |
Publications (2)
Publication Number | Publication Date |
---|---|
FR2289623A2 true FR2289623A2 (fr) | 1976-05-28 |
FR2289623B2 FR2289623B2 (sv) | 1978-06-30 |
Family
ID=9145779
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
FR7440332A Granted FR2289623A2 (fr) | 1974-10-28 | 1974-10-28 | Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusion |
Country Status (1)
Country | Link |
---|---|
FR (1) | FR2289623A2 (sv) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4589367A (en) * | 1984-10-01 | 1986-05-20 | Empire Enterprises, Inc. | System for automatically painting pencils |
-
1974
- 1974-10-28 FR FR7440332A patent/FR2289623A2/fr active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4589367A (en) * | 1984-10-01 | 1986-05-20 | Empire Enterprises, Inc. | System for automatically painting pencils |
Also Published As
Publication number | Publication date |
---|---|
FR2289623B2 (sv) | 1978-06-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
YU131275A (en) | Process for the pretreatment of metallic surfaces of articles of low alloyed steel for the deposition of molten metal | |
ES369658A1 (es) | Metodo para fabricar vidrio plano. | |
ES480543A1 (es) | Un aparato para controlar recubrimientos metalicos sobre a- lambre, fleje o similar. | |
ZA812368B (en) | Protective atmosphere and gas wiping apparatus and method of using | |
DE3477586D1 (en) | Apparatus for coating steel objects with an alloy of zinc and aluminium | |
FR2289623A2 (fr) | Perfectionnement aux traitements de protection des metaux par depot d'une couche d'un metal en fusion | |
GB1292921A (en) | Process and apparatus for finishing coated wire | |
GB911066A (en) | Improvements in or relating to methods of desulphurizing a bath of metal | |
GB1272604A (en) | Improvements in hot-dip metal coating processes and apparatus | |
ES8200927A1 (es) | Un metodo mejorado para esferoidizar un articulo de metal ferreo | |
JPS5266813A (en) | Method and apparatus for steel recovering from metal articles containing carbon | |
GB808556A (en) | A process for the heat treatment of an unalloyed or low-alloy structural steel containing from 0.03% to 0.12% of aluminium nitride | |
GB676198A (en) | Process for coating metallic objects with other metals | |
ES362056A1 (es) | Procedimiento y aparato para el revestimiento de alambres. | |
JPS56146869A (en) | Continuously hot dipping method for steel strip | |
SE8101552L (sv) | Gasseparation | |
GB1336194A (en) | Method of and apparatus for cleaning molten metal contaiminated with dross | |
JPS57200546A (en) | Preparation of molten zinc plating and alloying treated steel plate | |
GB739322A (en) | Process for removing organic polymers from processing equipment | |
GB1072932A (en) | Method of and apparatus for surface hardening bodies by gaseous treatment | |
FR2289624A1 (fr) | Procede et dispositif pour le traitement d'objets metalliques tubulaires par depot d'un metal | |
GB1341255A (en) | Oil hardening process and equipment for the hardening of metals | |
ES461204A1 (es) | Sistema para el tratamiento en continuo de piezas a esmal- tar. | |
GB1438376A (en) | Themral treatment of metal parts | |
GB961878A (en) | Improvements relating to the continuous processing of ferrous metal |