ES463706A1 - Un aparato mejorado para fabricar vidrio. - Google Patents
Un aparato mejorado para fabricar vidrio.Info
- Publication number
- ES463706A1 ES463706A1 ES463706A ES463706A ES463706A1 ES 463706 A1 ES463706 A1 ES 463706A1 ES 463706 A ES463706 A ES 463706A ES 463706 A ES463706 A ES 463706A ES 463706 A1 ES463706 A1 ES 463706A1
- Authority
- ES
- Spain
- Prior art keywords
- glass
- refractory
- manufacture
- molten metal
- installation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Abstract
Un aparato mejorado para fabricar vidrio que comprende un horno de fusión, refinado y acondicionamiento de vidrio y una cámara de formación de vidrio que contiene un baño de metal fundido para soportar el vidrio mientras está siendo transformado en una lámina de vidrio dimensionalmente estable, continua, estando el horno y la cámara de formación unidos por una instalación de entrega de vidrio fundido que comprende un canal que tiene un fondo, miembros laterales y un miembro de dosificación.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US05/737,318 US4055407A (en) | 1976-11-01 | 1976-11-01 | Apparatus for the manufacture of flat glass having a glass refractory delivery piece and method of installation |
Publications (1)
Publication Number | Publication Date |
---|---|
ES463706A1 true ES463706A1 (es) | 1978-06-01 |
Family
ID=24963431
Family Applications (2)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES463705A Expired ES463705A1 (es) | 1976-11-01 | 1977-10-29 | Un metodo de modificar una camara de formacion de vidrio. |
ES463706A Expired ES463706A1 (es) | 1976-11-01 | 1977-10-29 | Un aparato mejorado para fabricar vidrio. |
Family Applications Before (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES463705A Expired ES463705A1 (es) | 1976-11-01 | 1977-10-29 | Un metodo de modificar una camara de formacion de vidrio. |
Country Status (13)
Country | Link |
---|---|
US (1) | US4055407A (es) |
JP (1) | JPS5465722A (es) |
AR (1) | AR211814A1 (es) |
AU (1) | AU505788B2 (es) |
BE (1) | BE860264A (es) |
BR (1) | BR7706715A (es) |
CA (1) | CA1092823A (es) |
DE (1) | DE2747549C3 (es) |
ES (2) | ES463705A1 (es) |
FR (1) | FR2369219A1 (es) |
IT (1) | IT1091424B (es) |
MX (1) | MX145433A (es) |
SE (1) | SE434389B (es) |
Families Citing this family (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4115092A (en) * | 1977-09-19 | 1978-09-19 | Ppg Industries, Inc. | Method and apparatus for preventing bubble nucleation and growth in a molten glass delivery facility |
US4233047A (en) * | 1979-05-01 | 1980-11-11 | Ppg Industries, Inc. | In situ repair of delaminated float bath bottom refractory |
US4354866A (en) * | 1980-04-04 | 1982-10-19 | Ppg Industries, Inc. | Method of bidirectionally attenuating glass in a float process with edge cooling |
US4375370A (en) * | 1980-04-04 | 1983-03-01 | Ppg Industries, Inc. | Thermal control in a method of bidirectionally attenuating glass in a float process |
US4305745A (en) * | 1980-04-04 | 1981-12-15 | Ppg Industries, Inc. | Method of attenuating glass in a float process |
JPS6049293A (ja) * | 1983-08-30 | 1985-03-18 | バブコツク日立株式会社 | 高温ガス炉後備冷却装置 |
IT1270628B (it) * | 1994-10-06 | 1997-05-07 | Enichem Spa | Manufatti in ossido di silicio e/o altri ossidi metallici misti e procedimento per la loro preparazione in dimensioni finali o quasi finali |
US6495251B1 (en) | 1997-06-20 | 2002-12-17 | Ppg Industries Ohio, Inc. | Silicon oxynitride protective coatings |
MXPA05010170A (es) * | 2003-03-28 | 2005-11-08 | Ppg Ind Ohio Inc | Sustratos recubiertos con mezclas de materiales de titanio y aluminio, metodos para hacer los sustratos, y blancos catodicos de metal titanio y aluminio. |
US9051211B2 (en) * | 2004-04-27 | 2015-06-09 | Ppg Industries Ohio, Inc. | Effects of methods of manufacturing sputtering targets on characteristics of coatings |
DE112006003321B4 (de) * | 2005-12-05 | 2010-01-14 | Schott Ag | Verfahren zur Herstellung von Flachglas nach dem Floatverfahren sowie Gießlippe (Spout Lip) für das Floatverfahren |
CA2702890A1 (en) * | 2007-10-17 | 2009-04-23 | Compania Vidriera, S.A. De C.V. | Glass melting furnace entirely built with refractory concrete |
WO2013180493A1 (ko) * | 2012-05-30 | 2013-12-05 | 주식회사 엘지화학 | 플로트 배스 및 플로트 유리 제조 방법 |
Family Cites Families (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3594147A (en) * | 1967-12-01 | 1971-07-20 | Ppg Industries Inc | Float bath tank construction and method of making the same |
US3884665A (en) * | 1973-03-06 | 1975-05-20 | Ppg Industries Inc | Flat glass manufacturing apparatus and method |
DE2331081A1 (de) * | 1973-06-19 | 1975-01-23 | Hoechst Ag | Neue cyclopentanderivate und verfahren zu ihrer herstellung |
AR204651A1 (es) * | 1974-03-27 | 1976-02-20 | Ppg Industries Inc | Aparato y metodo para producir vidrio plano |
-
1976
- 1976-11-01 US US05/737,318 patent/US4055407A/en not_active Expired - Lifetime
-
1977
- 1977-08-25 CA CA285,511A patent/CA1092823A/en not_active Expired
- 1977-08-30 AU AU28361/77A patent/AU505788B2/en not_active Expired
- 1977-09-21 IT IT69088/77A patent/IT1091424B/it active
- 1977-09-22 SE SE7710647A patent/SE434389B/sv unknown
- 1977-09-28 AR AR269364A patent/AR211814A1/es active
- 1977-10-03 FR FR7729645A patent/FR2369219A1/fr not_active Withdrawn
- 1977-10-07 BR BR7706715A patent/BR7706715A/pt unknown
- 1977-10-20 JP JP12634777A patent/JPS5465722A/ja active Granted
- 1977-10-22 DE DE2747549A patent/DE2747549C3/de not_active Expired
- 1977-10-26 MX MX171100A patent/MX145433A/es unknown
- 1977-10-28 BE BE182175A patent/BE860264A/xx unknown
- 1977-10-29 ES ES463705A patent/ES463705A1/es not_active Expired
- 1977-10-29 ES ES463706A patent/ES463706A1/es not_active Expired
Also Published As
Publication number | Publication date |
---|---|
IT1091424B (it) | 1985-07-06 |
DE2747549B2 (de) | 1980-04-10 |
AU2836177A (en) | 1979-03-08 |
SE434389B (sv) | 1984-07-23 |
DE2747549C3 (de) | 1980-12-11 |
AU505788B2 (en) | 1979-11-29 |
FR2369219A1 (fr) | 1978-05-26 |
CA1092823A (en) | 1981-01-06 |
AR211814A1 (es) | 1978-03-15 |
BR7706715A (pt) | 1978-07-04 |
DE2747549A1 (de) | 1978-05-03 |
JPS5616095B2 (es) | 1981-04-14 |
BE860264A (fr) | 1978-04-28 |
SE7710647L (sv) | 1978-05-09 |
MX145433A (es) | 1982-02-15 |
JPS5465722A (en) | 1979-05-26 |
ES463705A1 (es) | 1978-06-01 |
US4055407A (en) | 1977-10-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES463706A1 (es) | Un aparato mejorado para fabricar vidrio. | |
JPS5323806A (en) | Apparatus for refining of molten metal | |
NZ183215A (en) | Process for modifying the surface of glass by inducing migration of metal ions from a molten body | |
JPS51115218A (en) | Dephosphorization of molten iron | |
GB1555138A (en) | Method for the manufacture of foamed glass | |
JPS5237510A (en) | Dephosphorization method of molten cast iron | |
JPS5249218A (en) | Apparatus for production of float glass | |
AU540689B2 (en) | Tuyere for blowing gas into molten metal bath container | |
DE3164365D1 (en) | Process and furnace for the production of molten glass | |
YU12675A (en) | Process for refining metals on the base of iron | |
YU39246B (en) | Process for the tempering of glass in a gas-fluidization bath | |
JPS531208A (en) | Method of making vitreous ribbon on surface of melted metal pot and apparatus for said process | |
YU148677A (en) | Process for refining molten metal | |
JPS51135916A (en) | Tank furnace for manufacturing glass | |
ZA772668B (en) | Glass melting furnace and process for improving the quality of glass | |
ES291783A1 (es) | Método de fabricación de vidrio plano | |
JPS51136522A (en) | Method of smelting with electric furnace for reduci ng and volatilizing zinc from slag | |
CS186237B2 (en) | Fining method of glass and glass-melting tank furnace for making the said method | |
AU456667B2 (en) | Process and apparatus for the manufacture of float glass on a bath of molten metal | |
CS179116B1 (en) | Method for improving workplace environment in the region of glass-melting furnaces,espscially tank furnaces and apparatus for making this method | |
JPS5286414A (en) | Process and apparatus for production of thin glass plate by elongation of base plate | |
JPS5332813A (en) | Preferential oxidizing method for molten iron | |
JPS537510A (en) | Removing equipment for slag in melting furnace | |
JPS5230376A (en) | Device to support container of getter | |
JPS5236509A (en) | Proces for producing wire-formed additives used in steel manufacture |