ES2067120T3 - Procedimiento para la fabricacion de un acumulador de plomo con un electrolito de acido sulfurico inmovilizado en forma de gel. - Google Patents
Procedimiento para la fabricacion de un acumulador de plomo con un electrolito de acido sulfurico inmovilizado en forma de gel.Info
- Publication number
- ES2067120T3 ES2067120T3 ES91118813T ES91118813T ES2067120T3 ES 2067120 T3 ES2067120 T3 ES 2067120T3 ES 91118813 T ES91118813 T ES 91118813T ES 91118813 T ES91118813 T ES 91118813T ES 2067120 T3 ES2067120 T3 ES 2067120T3
- Authority
- ES
- Spain
- Prior art keywords
- electrolyte
- gel
- procedure
- manufacture
- sulfuric acid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
LA CONFIGURACION DEL ELECTROLITO DE GEL SOLIDO SE LLEVA A CABO DE FORMA NORMAL SOBRE EL ENVASADO DEL LIQUIDO DE ACIDO DE AZUFRE Y DENTRO DEL ACUMULADOR CARGADO CON ELECTRODOS POSITIVOS Y NEGATIVOS. ESTA FORMACION PUEDE ESTAR UNIDA AL PROCESO DE FABRICACION EN TANTO EN CUANTO NO INSTALEN LAS PLACAS (PIEZA BRUTA), QUE TIENE CONEXIONES DE CORRIENTE ACABADAS (POLOS , PUENTES DE LOS POLOS), CON EL GEL EN FORMA DE ACIDO DE SILICIO DISPERSADO FINAMENTE. DESPUES DE LLEVAR A CABO ESTE PROCEDIMIENTO DE RELLENO DE LA BATERIA CON ELECTROLITO LIQUIDO, ESTA ESTA PREPARADA PARA SU FUNCIONAMIENTO Y DISPONE DE UN ELECTROLITO INMOVIL.
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| DE4040202A DE4040202A1 (de) | 1990-12-15 | 1990-12-15 | Verfahren zur herstellung eines bleiakkumulators mit einem als gel festgelegten schwefelsaeureelektrolyten |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| ES2067120T3 true ES2067120T3 (es) | 1995-03-16 |
Family
ID=6420477
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| ES91118813T Expired - Lifetime ES2067120T3 (es) | 1990-12-15 | 1991-11-05 | Procedimiento para la fabricacion de un acumulador de plomo con un electrolito de acido sulfurico inmovilizado en forma de gel. |
Country Status (4)
| Country | Link |
|---|---|
| EP (1) | EP0491150B1 (es) |
| AT (1) | ATE117129T1 (es) |
| DE (2) | DE4040202A1 (es) |
| ES (1) | ES2067120T3 (es) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE19513343C1 (de) * | 1995-04-08 | 1996-10-10 | Europ Accumulateurs | Verfahren zur Herstellung eines Bleiakkumulators |
| CN1156931C (zh) * | 2001-06-12 | 2004-07-07 | 王立都 | 铅蓄电池使用的液态硅盐化成液及内化成方法 |
| EP1495502A4 (en) | 2002-02-07 | 2006-12-13 | Kvg Technologies Inc | GELIFIED ELECTROLYTE LEAD BATTERY BATTERY, FORMED BY FILTRATION OF ABSORBENT SEPARATORS, ITS ELECTROLYTES, AND ITS ABSORBENT SEPARATORS |
| DE102004011270A1 (de) * | 2004-03-09 | 2005-09-29 | Deutsche Exide Standby Gmbh | Wartungsfreier Akkumulator und Verfahren zu dessen Herstellung |
| ATE496402T1 (de) | 2004-09-16 | 2011-02-15 | Hoppecke Batterien Gmbh & Co Kg | Verfahren und vorrichtung zur herstellung einer wartungsfreien batterie mit festgelegtem elektrolyten |
Family Cites Families (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| BE432980A (es) * | 1939-03-07 | |||
| DE3041953C2 (de) * | 1980-11-06 | 1983-12-08 | Accumulatorenfabrik Sonnenschein GmbH, 6470 Büdingen | Verfahren zum Herstellen eines Bleiakkumulators sowie nach diesem Verfahren hergestellter Bleiakkumulator |
| DE3521200A1 (de) * | 1985-06-13 | 1986-12-18 | Otto 6470 Büdingen Jache | Bleiakkumulator mit einem thixotropen gel als elektrolyt und verfahren zu seiner herstellung |
| DE3603196A1 (de) * | 1986-02-03 | 1987-08-06 | Varta Batterie | Verfahren zur herstellung eines bleiakkumulators mit gel-elektrolyten |
| US4687718A (en) * | 1986-10-24 | 1987-08-18 | Exide Corporation | Method of making a sealed lead-acid battery with a gel electrolyte and sealed lead-acid storage battery made according to this method |
| DE3644420C2 (de) * | 1986-12-22 | 1998-07-09 | Hagen Batterie Ag | Verfahren zum Herstellen eines Bleiakkumulators mit einem thixotropen Gel als Elektrolyt |
| US4871428A (en) * | 1988-03-24 | 1989-10-03 | C & D Charter Power Systems, Inc. | Method for in situ forming lead-acid batteries having absorbent separators |
-
1990
- 1990-12-15 DE DE4040202A patent/DE4040202A1/de not_active Withdrawn
-
1991
- 1991-11-05 DE DE59104250T patent/DE59104250D1/de not_active Expired - Fee Related
- 1991-11-05 EP EP91118813A patent/EP0491150B1/de not_active Expired - Lifetime
- 1991-11-05 AT AT91118813T patent/ATE117129T1/de not_active IP Right Cessation
- 1991-11-05 ES ES91118813T patent/ES2067120T3/es not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| EP0491150A2 (de) | 1992-06-24 |
| ATE117129T1 (de) | 1995-01-15 |
| EP0491150B1 (de) | 1995-01-11 |
| DE59104250D1 (de) | 1995-02-23 |
| DE4040202A1 (de) | 1992-06-17 |
| EP0491150A3 (en) | 1992-07-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0851522A3 (en) | Method of fabricating a lithium ion secondary battery | |
| ES2067120T3 (es) | Procedimiento para la fabricacion de un acumulador de plomo con un electrolito de acido sulfurico inmovilizado en forma de gel. | |
| JPS609065A (ja) | シ−ル鉛蓄電池 | |
| DE59208459D1 (de) | Verfahren zur Herstellung eines Bleiakkumulators mit einem thixotropen Gelelekrolyten | |
| JPS56123675A (en) | Manufacture of closed type lead-acid battery | |
| JPH10208745A5 (es) | ||
| JP2001185206A (ja) | 鉛蓄電池及びその製造方法 | |
| ES466217A2 (es) | Mejoras introducidas en el objeto de la patente principal num. 438.459, por:un metodo de produccion de placas para ba-terias de plomo acido | |
| JPH10223212A5 (es) | ||
| GB1513019A (en) | Electrical storage batteries and methods of making them | |
| JPS62126565A (ja) | 密閉型鉛電池の製造法 | |
| JPS5790864A (en) | Initial charging method for fabricated lead-acid storage battery assembled with unformed plate | |
| JPH0733377Y2 (ja) | 密閉型鉛蓄電池 | |
| SU1067554A1 (ru) | Способ зар да никель-водородной аккумул торной батареи | |
| Das | Preliminary studies on a rechargeable acidic lead/mercury battery | |
| JPS5696462A (en) | Manufacture of lead acid battery | |
| JPS57165959A (en) | Production of plate for lead storage battery | |
| JPS57113555A (en) | Initial charging method of unformated plate fabricating lead-acid battery | |
| JPS6313262A (ja) | 鉛電池の充電方法 | |
| JPH0278160A (ja) | 密閉形鉛蓄電池の製造方法 | |
| JPS61121661U (es) | ||
| JPS57113554A (en) | Initial charging method of unformated plate fabricating lead-acid battery | |
| JPS61138451A (ja) | 密閉式鉛蓄電池 | |
| JPH05242878A (ja) | 密閉形鉛蓄電池の端子部 | |
| JPS61114658U (es) |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| FG2A | Definitive protection |
Ref document number: 491150 Country of ref document: ES |