DE612634C - Process for welding used rails worn at the joint ends by means of the electrical resistance melting process - Google Patents

Process for welding used rails worn at the joint ends by means of the electrical resistance melting process

Info

Publication number
DE612634C
DE612634C DEW86323D DEW0086323D DE612634C DE 612634 C DE612634 C DE 612634C DE W86323 D DEW86323 D DE W86323D DE W0086323 D DEW0086323 D DE W0086323D DE 612634 C DE612634 C DE 612634C
Authority
DE
Germany
Prior art keywords
rail
electrical resistance
joint ends
resistance melting
worn
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DEW86323D
Other languages
German (de)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Theodor Wuppermann GmbH
Original Assignee
Theodor Wuppermann GmbH
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Theodor Wuppermann GmbH filed Critical Theodor Wuppermann GmbH
Priority to DEW86323D priority Critical patent/DE612634C/en
Application granted granted Critical
Publication of DE612634C publication Critical patent/DE612634C/en
Expired legal-status Critical Current

Description

13JUIi 193513JUIi 1935

Die Erfindung bezieht sich auf ein Verfahren zum Verschweißen gebrauchter, an den Stoßenden abgefahrener Schienen mittels des elektrischen Widerstandsabschmelzverfahr ens.The invention relates to a method for welding used, to the butt ends of worn rails by means of the electrical resistance melting process ens.

Bei den bisher üblichen Verfahren werden die Schienenenden derart in die Stumpfsclnveißmaschine eingespannt, daß die Schienen genau in gleicher Flucht zueinanderliegen. Es zeigte sich jedoch, daß auf diese Weise keine einwandfreie Schweißung zu erzielen ist, daß vielmehr immer noch an der Stoßstelle eine Abnutzung erkennbar bleibt.
Das Verfahren gemäß der Erfindung beseitigt den Mangel dadurch, daß die Schieneiienden so in die Schweißmaschine eingespannt werden, daß die beiden Längsachsen der Schienen an der Einspannstelle einen Winkel miteinander bilden, der nach der Seite der Schienenfüße hin kleiner als i8oJ ist.
In the previously customary methods, the rail ends are clamped into the stump cutting machine in such a way that the rails are exactly in the same alignment with one another. It turned out, however, that a perfect weld cannot be achieved in this way, rather that wear still remains recognizable at the joint.
The method of the invention overcomes the defect in that the Schieneiienden are so clamped in the welding machine, that the two longitudinal axes of the rails form at the mounting point an angle to each other, which according to the side of the rail bases is toward smaller than i8o J.

Während des Abschmelzvorganges ist der Werkstoff an den zu verschweißenden Schienctienden, von der Schweißfuge ausgehend, etwa 40. bis 50 mm weit so stark erwärmt, daß er gut verformbar ist. Durch die erii.11-During the melting process, the material is on the rail ends to be welded, starting from the weld joint, about 40 to 50 mm heated so much that it can be easily deformed. Through the erii.11-

-, dungsgemäße Einspannung weicht beim Zusammenstauchen der frei vorstehenden Schienenenden der weich gewordene Werkstoff nach oben aus. Der auf die nach der Stoifstelle hin ansteigend eingespannten Scliienenenden ausgeübte seitliche Schub oder Stauchdruck erzeugt am Stoß selbst eine nach oben gerichtete Komponente. Diese Komponente drängt die weichgewordenen, frei vorstehenden Schienenenden nach oben. Es bildet sich so nach dem Kopf der Schiene zu eine verstärkte Stauchwulst. Außerdem erhält die Schiene auf diese Weise in der Schweißung ' eine schwache Überhöhung. Nach der Entfernung des Stauchgrates wird die Fahrrläclie mittels des Schienenhobels geschlichtet, und es entsteht dann eine einwandfreie ebene Fahrfläche.-, proper clamping gives way when collapsing the freely protruding rail ends follow the softened material from above. The ends of the lines that are clamped in ascending order towards the stump lateral thrust or compression pressure exerted creates an upwardly directed one at the joint itself Component. This component pushes the softened, freely protruding rail ends upwards. It educates a reinforced compression bulge develops towards the head of the splint. In addition, the In this way, create a slight camber in the weld. After removal of the edging burr, the Fahrrläclie is finished by means of the rail plane, and a perfectly level driving surface is then created.

Es ist zwar schon bekannt, abgefahrene Schienenenden durch. Hochtreiben der Köpfe wieder brauchbar zu machen. Hierbei hat man sich jedoch sehr verwickelter und teuerer Hilfsmittel bedient, besonderer Heizvorrichtungen und Schmiedegeräte, oder man schnitt den Schienensteg ein wenig ein, der dann nach dem Hochtreiben des Kopfes wieder verschweißt werden mußte. Im Gegensatz zu diesen umständlichen Verfahren genügt gemäß der vorliegenden Erfindung das bloße winklig^ Einspannen der Schienenenden in die Schweißmaschine bekannter Bauart, um zu dem Ziele zu gelangen. Jede Schmiedearbeit von Hand erübrigt sich.It is already known to wear worn rail ends. Driving up their heads to make usable again. However, this has become very complicated and expensive Aids operated, special heating devices and forging equipment, or one cut the rail web a little, which then again after driving up the head had to be welded. In contrast to these cumbersome procedures, according to is sufficient of the present invention, the mere angular ^ clamping of the rail ends in the Welding machine of known type to get to the target. Any blacksmith work by hand is not necessary.

Die Erfindung ist in der Zeichnung schematisch veranschaulicht, wobei die winklige Einspannung der Scliienenenden stark übertrieben dargestellt ist.The invention is illustrated schematically in the drawing, the angled The clamping of the ends of the slides is shown greatly exaggerated.

Die Längsachsen der Schienen ι, 2, 3 bilden erfindungsgemäß an der Einspannstelle einen Winkel miteinander, der nach der' Seite der Schienenfüße hin kleiner als iSo° ist. Zu diesem Zwecke können die Spannbacken keilartige Form haben. Einfacher ist es jedoch, keilartige Beilagen zu verwenden. Zwischen den Schienenfüßen 1 und den unteren Spannbacken 11 liegen die keilartigen Beilagen 13, ebenso zwischen den Schienenköpfen 3 und den oberen -Spannbacken 10 die Beilagen 12. Die Schienenenden werden so zwangsläufig in die gewünschte Winkelstellung gebracht.. Die beiderseitigen Schienenlängen liegen auf nicht gezeichneten Rollgängen auf.According to the invention, the longitudinal axes of the rails 1, 2, 3 form one at the clamping point Angle with each other that is smaller than iSo ° on the side of the rail feet. to For this purpose, the jaws can have a wedge-like shape. It is easier, however, to use wedge-like side dishes. Between the rail feet 1 and the lower clamping jaws 11 are the wedge-like supplements 13, likewise between the rail heads 3 and the upper clamping jaws 10 are the shims 12. The rail ends are inevitably brought into the desired angular position. The Rail lengths on both sides rest on roller tables, which are not shown.

Werden nun die Spannbacken im Sinne der waagerechten Pfeile * mit starkem Druck aufeinanderzubewegt, so entsteht am Stoß die lotrechte Kraftkomponente y, welche die gewünschte Hochtreibung der Schienenköpfc hervorruft. Schließlich werden die Schienen mit Luftdruckmeißel vom Schweißgrat befreit und mit dem Schienenhobel geschlichtet, worauf eine vollkommen ebene Fahrfläche an der Schweißstelle fertig ist. Die Schweißstelle kann auch noch, einer geeigneten nachträglichen Warmbehandlung unterzogen werden. If the clamping jaws are now moved towards one another in the direction of the horizontal arrows * with strong pressure, the vertical force component y arises at the joint, which causes the desired upward movement of the rail heads. Finally, the rails are freed from the weld burr with an air chisel and smoothed with the rail planer, after which a completely flat running surface is finished at the weld point. The welding point can also be subjected to a suitable subsequent heat treatment.

Claims (3)

Patentansprüche:Patent claims: ι. Verfahren zum Verschweißen gebrauchter, an den Stoßenden abgefahrener Schienen mittels des elektrischen Widcrstandsabschmelzverfahrens, dadurch gekennzeichnet, daß die Schienenenden so in die Schweißmaschine eingespannt werden, daß die beiden Längsachsen der Schienen · an der Einspannstelle einen Winkel miteinander bilden, der nach der Seite der Schienenfüße hin kleiner als ι So0 ist.ι. Method for welding used rails worn at the joint ends by means of the electrical resistance melting process, characterized in that the rail ends are clamped into the welding machine in such a way that the two longitudinal axes of the rails form an angle with one another at the clamping point which towards the side of the rail feet is less than ι So 0 . 2. Vorrichtung zur Durchführung des Verfahrens nach Anspruch I, dadurch gekennzeichnet, daß die den Schienenenden zugekehrten Flächen der Einspannbacken der Stumpfschweißmaschine so geneigt sind, daß die beiden Längsachsen der Schienen einen Winkel miteinander bilden, der nach der Seite der Schienenfüße hin kleiner als i8o° ist. ■2. Device for performing the method according to claim I, characterized in that that the surfaces of the clamping jaws of the butt welding machine facing the rail ends are so inclined are that the two longitudinal axes of the rails form an angle with each other, which towards the side of the rail feet is smaller than i8o °. ■ 3. Vorrichtung nach Anspruch 2, gekennzeichnet durch keilartige Beilagen, die an Stelle der Backen mit geneigten Einspannfiächen zwischen normale Einspannbacken und die Schienenenden gelegt werden. 3. Apparatus according to claim 2, characterized by wedge-like inserts which instead of the jaws with inclined clamping surfaces between normal clamping jaws and the rail ends are laid. Hierzu 1 Blatt Zeichnungen1 sheet of drawings
DEW86323D 1931-06-23 1931-06-23 Process for welding used rails worn at the joint ends by means of the electrical resistance melting process Expired DE612634C (en)