DE609752C - Method for joining two thin sheets of metal at an angle to one another - Google Patents
Method for joining two thin sheets of metal at an angle to one anotherInfo
- Publication number
- DE609752C DE609752C DES107320D DES0107320D DE609752C DE 609752 C DE609752 C DE 609752C DE S107320 D DES107320 D DE S107320D DE S0107320 D DES0107320 D DE S0107320D DE 609752 C DE609752 C DE 609752C
- Authority
- DE
- Germany
- Prior art keywords
- angle
- joining
- sheet
- another
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Bei der Herstellung von Blechkonstrüktionen traten vielfach dann Schwierigkeiten auf, wenn Kanten senkrecht auf ebene Bleche befestigt werden mußten. Man war gezwungen,- für der-' artige Konstruktionen Lichtbogenschweißun-' gen zu verwenden, da Punkts chweißungen keine genügende Haltbarkeit aufwiesen, selbst wenn die Zapfen der auf die Ebene aufzuschweißenden Blechkante in das Blech versenkt wurden.In the production of sheet metal structures, difficulties often arose when Edges had to be fastened perpendicular to flat metal sheets. One was forced to - for the- ' like constructions to use arc welds, as spot welds did not have sufficient durability, even if the tenons of the to be welded onto the plane The edge of the sheet was sunk into the sheet.
Diese Schwierigkeiten werden erfindungsgemäß dadurch, behoben, daß zum Verbinden zweier Winklig zueinander stehender dünner Bleche ein Zapfen eines Bleches durch das andere Blech hindurchragt und ein den Zapfen kreuzender Draht mit dem Zapfen durch elektrische Pünktschweißung verbunden wird. Es ergibt sich hierbei eine völlig einwand?· freie Verbindung, die allen Anforderungen ao an Festigkeit genügt. Sind Schweißungen an mehreren nebeneinanderliegenden. Stellen vorzunehmen, so können durch besondere Ausbildung der Elektroden zwei oder mehrere Punkte gleichzeitig geschweißt werden, indem entweder über jeden Punkt ein kleiner Querdraht gelegt wird oder ein Querdraht, der über alle Schweißstellen ragt. Um eine gleichmäßige Stromverteilung bei-mehreren gleichzeitigen Punktschweißungen mittels einer Maschine' zu erhalten, kann die Stromzuführung..zu den verschiedenen Elektrodenteilen getrennt erfolgen, um eine gleichmäßige Stromverteilung zu jeder Schweißstelle zu erzielen. These difficulties are solved according to the invention in that for connecting of two thin metal sheets at an angle to each other, a tenon of a sheet metal through the other sheet protrudes through and a wire crossing the pin with the pin electrical spot weld is connected. The result is a completely flawless? · free connection that meets all requirements ao in terms of strength. Are welds at several adjacent. Make places, so can by special Forming the electrodes by welding two or more points at the same time either a small cross wire is placed over each point or a cross wire that protrudes over all welds. In order to ensure an even distribution of electricity when several simultaneous To obtain spot welds by means of a machine, the power supply can be used the different electrode parts are done separately in order to achieve a uniform Achieve power distribution to each welding point.
In der Zeichnung ist ein Ausführungsbeispiel der Erfindung dargestellt. ;Fig. 1 und 2 zeigen eine zur Ausübung des Verfahrens dienende zweckmäßige Anordnung in Vorder- und Seitenansicht. 1 ist das ebene Blech, 2 und 3 sind -zwei senkrecht .dazu stehende anzuschweißende--Bleche, -die- mit den Zapfen 4 und 5 durch das Blech 1 hindurchragen. Zur Ausführung, der Schweißung ist über diese' Zapfen ein "Draht" 6 gelegt. Die Schweißung erfolgt mittels der schwenkbaren Elektrode 7 und der Gegenelektrode 8 durch —Schließung des Schweißstromkreises, der vom Transformator 9 gespeist wird.An exemplary embodiment of the invention is shown in the drawing. ; Fig. 1 and 2 show an expedient arrangement serving to carry out the procedure in front and side view. 1 is the flat sheet, 2 and 3 are two perpendicular to it to be welded - sheets, -the- with the pins 4 and 5 protrude through the sheet metal 1. To execute the weld A "wire" 6 is placed over these 'pegs. the Welding takes place by means of the pivotable electrode 7 and the counter electrode 8 —Closing the welding circuit fed by the transformer 9.
Claims (1)