DE325274C - Method and glue fritter for making paper glue tight in the paper machine - Google Patents

Method and glue fritter for making paper glue tight in the paper machine

Info

Publication number
DE325274C
DE325274C DE1918325274D DE325274DD DE325274C DE 325274 C DE325274 C DE 325274C DE 1918325274 D DE1918325274 D DE 1918325274D DE 325274D D DE325274D D DE 325274DD DE 325274 C DE325274 C DE 325274C
Authority
DE
Germany
Prior art keywords
glue
paper
fritter
paper machine
tight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
DE1918325274D
Other languages
German (de)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
PAUL KLEMM DR
Original Assignee
PAUL KLEMM DR
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by PAUL KLEMM DR filed Critical PAUL KLEMM DR
Application granted granted Critical
Publication of DE325274C publication Critical patent/DE325274C/en
Expired legal-status Critical Current

Description

Es ist bekannt, daß bei der Stoffleimung von Papier mit !Harz die Art der Trocknung für "eine gute Leimfestigkeit von Einfluß ist. Besonders ist die Erwärmung der Papierbahn von großer Bedeutung, weil der als Niederschlagshaut auf den Fasern bei der richtig geleiteten chemischen Umsetzung von Harzseifen mit schwefelsaurer Tonerde entstandene, aus winzigen Körnern bestehende NiederschlagIt is known that the type of drying when sizing paper with resin For "good glue strength is important. The heating of the paper web is particularly important of great importance because it acts as a precipitate on the fibers when properly guided chemical conversion of resin soaps with sulphate of alumina, Precipitation composed of tiny grains

ίο der Leimbestandteile einer Frittung, d. h. eines Aneinanderschmelzens der Leimbestandteile, bedarf, um Leimfestigkeit zu erreichen. Nur durch Frittung werden lückenlose Schichten der wässerunbenetzbaren Leimsubstanz erhalten, die bei der Stoffleimung das Eindringen von Flüssigkeiten in die Fasern verhindern. ίο the glue components of a frying, d. H. the glue constituents must melt together in order to achieve glue strength. Only through fritting are gapless layers of the water-non-wettable glue substance which prevent liquids from penetrating the fibers during the sizing of the fabric.

Je nach der Gründlichkeit dieser Frittung kann man an ein und derselben Papierbahn die verschiedensten Abstufungen der Leimfestigkeit erhalten. An der Luft ohne Erwärmung getrocknet, können Stücke einer Papierbahn sich wie Saugpapiere verhalten, also Flüssigkeiten rasch eindringen und durch das Papier hindurchdringen lassen, die bei gelungener Frittung hochleimfestes Papier liefern. Depending on the thoroughness of this frying process, one and the same paper web can be used obtain the most varied grades of glue strength. In the air without heating When dried, pieces of a paper web can behave like absorbent paper, i.e. liquids can quickly penetrate and through allow the paper to penetrate, which, if frying is successful, deliver highly glue-resistant paper.

Die Leimfestigkeit bildet sich also bei normaler Leimung mit Harz und entsprechend wie Harz bei der Stoffleimung sich verhaltenden Leimstoffen erst in der Trockenpartie der Papiermaschine heraus. Daß die chemischen Vorgänge fehlerlos verlaufen sind, ist dabei yorauszusetzen. The glue strength is thus formed with normal glueing with resin and accordingly how Resin in fabric sizing, sizing agents only behave in the dryer section of the paper machine out. It must be assumed that the chemical processes proceeded flawlessly.

Wenn man nämlich Schichten der nassen, einen Schlamm darstellenden Fällung an der Luft bei Zimmerwärme auf einer Unterlage eintrocknen läßt, so entstehen auf einer gewissen Stufe des Wasserverlustes Haarrisse, die zu einem Netz zusammenlaufen, so daß die Schicht schließlich in Schollen zerreißt.If you have layers of the wet precipitation, which is a sludge, on the If air is allowed to dry up on a surface when it is warm in the room, then arise on a certain surface Stage of water loss Hairline cracks that converge to form a network, so that the layer finally tears into clods.

Die Frittung zu lückenlosen Häutchen erfolgt nur bei einem höheren Wärmegrad, bei dem das Harz erweicht und klebrig wird. Diese Beschaffenheit ist bei der Erwärmung ein Übergangszustand zum Schmelzen. Wenn das Zerreißen verhindert werden soll, muß der Frittungserwärmegrad erreicht werden, ehe die Wasserverdunstung so weit· vorgeschritten ist, daß Haarrisse entstehen konnten. Daraus folgt, 5" daß eine bestimmte Feuchterwärmung der Papierbahn Bedingung für. das sichere Erreichen von Leimfestigkeit ist. Also muß die feuchte Papierbahn bei einem Feuchtigkeitsgehalt, bei dem noch keine Haarrisse entstehen konnten, zielbewußt auf Wärmegrade gebracht werden, bei denen die Frittung des Niederschlags der Leimbestandteile eintritt. Bei Harz ha.t die Erfahrung gelehrt, daß durch Erwärmen der Papierbahn auf 75 ° bis 900C die Frittung in der erwünschten Weise eintritt. Je nach der Beschaffenheit des Harzes ist die untere Grenze innerhalb eines gewissen Spielraums verschieden. Bei anderen Leimmitteln, Bienenwachs, Montanwachs u. a., verschiebt sich die Frittungswärme je nach dem Verhalten der Leimbestandteile bei der Erwärmung.The frying into complete skins only takes place at a higher degree of heat, at which the resin softens and becomes sticky. This condition is a transition state to melting when heated. If the tearing is to be prevented, the degree of frying temperature must be reached before the evaporation of water has progressed so far that hairline cracks could occur. From this it follows that a certain moisture heating of the paper web is a condition for the reliable achievement of glue strength. Thus, at a moisture content at which no hairline cracks could develop, the moist paper web must be purposefully brought to a temperature at which the fritting of the precipitate is possible the glue components occurs. with resin experience ha.t taught that the fritting occurs by heating of the paper web at 75 ° to 90 0 C in the desired way. Depending on the nature of the resin, the lower limit varies within a certain margin. in other glues, beeswax, montan wax, etc., the frying heat shifts depending on the behavior of the glue components when heated.

Der Feuchtigkeitsgehalt der Papierbahn, bei dem die Haarrißbildung eintritt, ist je nach der Stoffbeschaffenheit verschieden, Was mit dem Schrumpfungsvermögen des PapierstoffsThe moisture content of the paper web at which hairline cracking occurs is dependent on the texture of the fabric, what about the shrinkage capacity of the paper stock

zusammenhängt; sie liegt meist in dem Spielraum eines Wassergehalts der Papiermasse zwischen 50 und 60 Prozent über Aera Luftfeuchtigkeitsgehalt des Papiers.
Diese beiden Bedingungen wurden bisher nur unbewußt und deshalb vielfach mangelhaft und nicht mit Sicherheit erfüllt, sei es, daß die außerordentlich verschiedene, oft ungünstige Bauart der Trockenpartie oder Art und Handhabung der Beheizung die Erfüllung erschwerten oder selbst unmöglich machten, was bei gewissen Arten der Trockenpartie gerade moderner Papiermaschinen der Fall ist. Rätselhafte vorübergehende, ebenso wie ständige Leimschwierigkeiten beruhten viel-
related; it is usually in the range of a water content of the paper pulp between 50 and 60 percent above the Aera air humidity content of the paper.
These two conditions have so far only been met unconsciously and therefore often inadequately and not with certainty, be it that the extraordinarily different, often unfavorable design of the dryer section or the type and handling of the heating made it difficult or even impossible, which with certain types of dryer section is the case with modern paper machines. Mysterious temporary as well as constant gluing difficulties were based on many

- fach allein oder doch zum Teil darauf, daß diese beiden Bedingungen nicht oder schwer zu erfüllen .waren, wie Erfinder in vielen Fällen feststellen konnte. Meist suchte man durch hohen Aufwand an Leimungsmengen zum Ziele zu kommen, ohne es doch voll und sicher zu erreichen.- subject alone or at least partly to the fact that these two conditions are not or difficult had to be fulfilled, as inventors found in many cases. Mostly one searched through To achieve the goal with a high expenditure of glue quantities without fully and safely reach.

Zielbewußte Feuchterwärmung ist das Mittel, um mit geringstem Aufwand an Leimmenge größtmögliche Wirkung zu erreichen. Eigens dem Zweck der zielbewußten Feuchterwärmung dienende Verfahren und Vorrichtungen waren bisher nicht bekannt. Der Gedanke, durch eine besondere Vorrichtung — Leimfritter — die zielbewußte Feuchterwärmung zu gewähr-Targeted humidity heating is the means of applying glue with the least amount of glue to achieve the greatest possible effect. Specifically for the purpose of targeted humidity warming serving methods and devices were not previously known. The thought through a special device - glue fritter - to ensure targeted moisture heating

- leisten, ist also neu.- afford is new.

Ebenso waren Vorrichtungen nicht bekannt, durch die die Bedingungen zur Frittung der ausgefällten Leimungsbestandteile sichergestellt werden, nämlich die Papierbahn in noch genügend feuchtem Zustande auf die Frittungswärme zu bringen und während des Frittungsvorgangs ohne wesentliche schädliche Schwankungen des Feuchtigkeitsgehalts und des Wärmegrades (nach oben oder unten) auf dieser zu erhalten.Likewise, devices were not known through which the conditions for frying the Precipitated glue components are ensured, namely the paper web in still sufficient to bring to the frying heat in a moist state and during the frying process without substantial deleterious fluctuations in moisture content and To get degree of warmth (up or down) on this.

Formen für Leimungsfritter sind in verschiederer Ausführung denkbar. Eine zweckmäßige Form des Leimfritters besteht in der Anordnung von zwei durch heizbare Zylinderpaare Z1, Z2, Z3, Z4 erwärmbare und durch diese in Umlauf zu' setzende endlose Tücher T1, T2 aus Filz oder ähnlichem weichen Stoff, zwischen denen die Papierbahn P auf eine gewisse Strecke, in der sie das Papier berühren, hindurchgeführt wird. Durch Verstellbarkeit eines oder zweier Heizzylinder kann die Strecke geregelt werden. Die freien Züge können durch Schirme ScA1, Sch„ vor schädlicher Abkühlung geschützt werden. Die Spannung der umlaufenden Tücher" erfolgt in bekannter Weise durch Spannwalzen Sp1, Sf2. Die Stellung der Vorrichtung kann aufrecht, wagerecht oder geneigt sein.Different designs are conceivable for molds for glue fritters. An expedient form of the glue fritter consists in the arrangement of two by heatable cylinder pairs Z 1 , Z 2 , Z 3 , Z 4 heatable and circulating through these endless towels T 1 , T 2 made of felt or similar soft material, between which the paper web P is passed through a certain distance in which it touches the paper. The distance can be regulated by adjusting one or two heating cylinders. The free trains can be protected from harmful cooling by ScA 1 , Sch “screens. The tensioning of the rotating cloths "takes place in a known manner by tension rollers Sp 1 , Sf 2. The position of the device can be upright, horizontal or inclined.

Claims (2)

Patent-Ansprüche:Patent Claims: 1. Verfahren zum Leimfestmachen von Papier in der Papiermaschine, dadurch gekennzeichnet, daß ein eine bestimmte Feuchterwärmung der Harzleimung für eine bestimmte Zeitdauer gewährleistender Leimfritter in die Troekenzylinderpartie der Papiermaschine eingeschaltet ist.1. Method of making paper sizing in the paper machine, thereby characterized in that a glue fritter which ensures a certain moisture heating of the resin sizing for a certain period of time is switched on in the dry cylinder section of the paper machine. 2. Leimfritter nach Patentanspruch 1, bestehend aus zwei durch heizbare Zylinder (Z1, ,Z2, Z3, Z4) erwärmbaren und durch diese in Umlauf zu setzenden endlosen Tüchern (T1, T2) aus Filz oder ähnlichem2. Glue fritter according to claim 1, consisting of two heatable cylinders (Z 1 , Z 2 , Z 3 , Z 4 ) which can be heated and which are to be put into circulation by endless cloths (T 1 , T 2 ) made of felt or the like . weichen Stoff, zwischen denen .die Papierbahn (P) auf eine gewisse regelbare Strecke hindurchgeführt wird.'. soft fabric, between which .the paper web (P) on a certain controllable distance is passed through. ' Hierzu ι Blatt Zeichnungen,For this purpose ι sheet of drawings,
DE1918325274D 1918-12-13 1918-12-13 Method and glue fritter for making paper glue tight in the paper machine Expired DE325274C (en)