CS239394B1 - Pull rod welding tool - Google Patents

Pull rod welding tool Download PDF

Info

Publication number
CS239394B1
CS239394B1 CS844157A CS415784A CS239394B1 CS 239394 B1 CS239394 B1 CS 239394B1 CS 844157 A CS844157 A CS 844157A CS 415784 A CS415784 A CS 415784A CS 239394 B1 CS239394 B1 CS 239394B1
Authority
CS
Czechoslovakia
Prior art keywords
pin
jaws
rod
heat
movable jaw
Prior art date
Application number
CS844157A
Other languages
Czech (cs)
Slovak (sk)
Other versions
CS415784A1 (en
Inventor
Aloiz Gaspar
Vladimir Kubistik
Original Assignee
Aloiz Gaspar
Vladimir Kubistik
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Aloiz Gaspar, Vladimir Kubistik filed Critical Aloiz Gaspar
Priority to CS844157A priority Critical patent/CS239394B1/en
Publication of CS415784A1 publication Critical patent/CS415784A1/en
Publication of CS239394B1 publication Critical patent/CS239394B1/en

Abstract

Vynález sa týká přípravku pre zváranie čapu s tiahlom, u ktorého je riešený odvod tepla z povrchu funkčnej plochy čapu, ktorý je chemicko-tepelne alebo tepelne spracovaný na vysokú tvrdost. Prípravok podl'a vynálezu pozostáva z jednej pevnej a jednej pohyblivej čelusti ovládanej přítlačným mechanizmom, ktorého podstata spočívá v tom, že v deliacej rovině týchto čeíustí je vytvořené válcové zahíbenie pre zváraný čap. Taktiež v týchto čelustiach sú vytvořené chladiace otvory pre přívod a odvod chladiaceho média.The invention relates to a device for welding a pin with a rod, in which heat dissipation is solved from the surface of the functional surface of the pin, which is chemically-thermally or thermally treated to high hardness. The device according to the invention consists of one fixed and one movable jaw controlled by a pressing mechanism, the essence of which lies in the fact that a cylindrical recess for the welded pin is formed in the dividing plane of these jaws. Cooling holes for the supply and discharge of the cooling medium are also formed in these jaws.

Description

Vynález sa týká přípravku pre zváranie čapu s tiahlom, u ktorého je riešený odvod tepla z povrchu funkčnej plochy čapu, ktorý je chemicko-tepelne alebo tepelne spracovaný na vysokú tvrdost:. Prípravok podlá vynálezu pozostáva z jednej pevnej a jednej pohyblivej čelustí ovládanej přítlačným mechanizmom, ktorého podstata spočívá v tom, že v deliacej rovině týchto čelustí je vytvořené válcové zahíbenie pre zváraný čap. Taktiež v týchto čelustiach sú vytvořené chladiace otvory pre přívod a odvod chladiaceho média.

239394 239394

Vynález sa týká přípravku pře zváranie čapu s tiahlom, ktorý ,je chemicko-tepelne alebo tepelne spracovaný na vysokú tvrdost u ktorého je riešený odvod tepla z povrchu funkčnej plochy čapu.

Doteraz sa zváranie čapu s ocelovým tiahlom, ktorý je chemicko-tepelne alebo tepelne spracovainý na vysokú tvrdost prevádzala metodou TIG v ochrannej atmosféře argonu s přidáním potřebného detailu pre vyplnenie tvaru zvarového spoja s převýšením. Takto dochádzalo k prehriatiu funkčnej plochy čapu, čím sa znížila jej tvrdost a čap voči tiahlu sa deformoval. Taktiež je známa metoda zvárania čapu s tiahlom s aplikáciou prievarkového zvárania v CO2 pri použití vysokých zvéracích prúdov za mimoriadne krátku dobu pri intenzívnom odvode tepla z povrchu funkčnej plochy čapu, V obidvoch prípadoch je nutné intenzívně odvádzať teplo z funkčnej plochy čapu tak, aby nedošlo k prehriatiu a popusteniu jeho funkčnej plochy a taktiež zamedzií deformácii čapu voči tiahlu.

Uvedené požiadavky zabezpečuje prípravok pre zváranie čapu s tiahlom, ktorý je chemicko-tepelne alebo tepelne spracovaný na vysokú tvrdost, pozostávajúci z jednej pevnej a z jednej pohyblivej čelusti ovládanej přítlačným mechanizmom podlá vynálezu, ktorého podstata spočívá v tom, že v delíacej rovině pevnej a pohyblivej čelusti je vytvořené válcové zahlbenie pre zváraný čap a ďalej sú v nich vytvořené chladiace otvory pře přívod a odvod chladiaceho média. Výhodou přípravku podía vynálezu je, že zabezpečuje regulovaný odvod tepla z povrchu funkčnej plochy zváraného čapu, pričom súčasne zabezpečuje potrebnú polohu čapu s tiahlom, t. j. kolmost a zabraňuje tak vzájomnej deformácii zváraných súčiastok.

Na pripojenom výkrese je znároznený prí- klad prevedemia přípravku pre zváranie čapu s tiahlom podlá vynálezu.

Prípravok podía vynálezu pozostáva z pevnej oefiBSti 1 <a pohyblivej čelusti 2, ktoré sú vytvořené z tepelne vodivého materiálu například médi. V pevnej čelusti 1 je naskrutkovaná závrtná skrutka 3, ktorá prechádza cez otvor vytvořený v pohyblivej čelusti 2 a na konci tejto závrtnej skrutky 3 je naskrúťkované ovládacta matica 4. Medzi pevnou čelusťou 1 a pohyblivou čelusťou 2 posobí tlačná pružina 5, ktorá je nasunutá na závrtnej skrutke 3 a je uložená vo valcovom osadení vytvorenom v pohyblivej čeíusti 2. V delíacej rovině pevnej čelusti 1 a pohyblivej čelusti 2 je vytvořené válcové zahlbenie 6, v ktorom je uložený zváraný čap 7 s tiahlom <8, ktoré dosadá na vodorovná hornú plochu pevnej a pohyblivej čelusti 1 a 2. V pevnej a pohyblivej čelusti 1 a 2 sú vytvořené chladiace otvory 9 pre přívod a odvod chladiaceho média.

Pri uvolnenej matici 4 je pohyblivá čelusť 2 vplyvom tlačnej pružiny 5 odtiahnutá od pevnej čelusti 1. Za tohoto stavu sa vloží do válcového zahíbenia 6 zváraný čap 7 tak, že tiahlo 8 dosadne na vodorovná plochu oboch čelustí 1 a 2. Potom sa zatiahne ovládacia matica 4, čím sa pohyblivá čelusť přiblíží k pevnej čelusti 1 prostredníctvom válcového zahíbenia 6 pevne zovrie zváraný čap 7. Pri zatiahnutej ovládacej matici 4 musí byť medzi čelusťmi 1 a 2 medzera tak, aby zváraný čap 7 bol pevne obopnutý válcovým vybráním 6 pre zabezpečenie dobrého odvodu tepla. Do chladiacich otvorov 9 vytvořených v hornej časti čelustí 1 a 2 je převedený přívod chladiaceho média a v chladiacich otvorech '9 vytvořených v spodnej časti čelustí 1 a 2 je převedený odvod chladiaceho média. Takto je připravený čap 7 s tiahlom 8 pre vytvořeni© zvaru 10.

BACKGROUND OF THE INVENTION 1. Field of the Invention The invention relates to a rod welding rod fixture in which heat is dissipated from the surface of a functional surface of a pin which is chemically-heat-treated or heat-treated to a high hardness. The device according to the invention consists of one fixed and one movable jaw operated by a thrust mechanism, the principle of which is that a cylindrical recess for the welded pin is formed in the dividing plane of the jaws. Also, in these jaws, cooling openings are provided for supply and discharge of the cooling medium.

239394 239394

BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a pre-welded rod welding rod, which is chemically-heat-treated or heat-treated to a high hardness in which heat is dissipated from the surface of the functional surface of the pin.

Up to now, the welding of a pin with a steel rod, which is chemically-heat-treated or heat-treated to a high hardness, has been carried out by the TIG method in an argon protective atmosphere with the addition of the necessary detail to fill the weld seam with the camber. Thus, the functional surface of the pin was overheated, thereby reducing its hardness and deforming the pin against the rod. It is also known to use a method of welding a pin with a welded-on welding in CO2 using high clamping currents for an extremely short period of time with intensive heat removal from the surface of the functional surface of the bolt, in which case it is necessary to intensively dissipate heat from the functional surface of the bolt to avoid overheating and releasing its functional surface and also avoiding deformation of the pin against the rod.

The aforementioned requirements are provided by means of a pin welding rod which is chemically-heat-treated or heat-treated to a high hardness, consisting of one fixed and one movable jaw controlled by a pressing mechanism according to the invention, the principle being that in the dividing plane of the fixed and movable jaw a cylindrical recess is formed for the welded pin, and furthermore, cooling holes are formed therein for supplying and draining the coolant. An advantage of the preparation according to the invention is that it provides controlled heat dissipation from the surface of the functional surface of the welded pin, while at the same time providing the necessary position of the pin with the rod, ie perpendicularity, thus preventing mutual deformation of the welded parts.

In the accompanying drawing, an example is given of a prevedemia of a pin-welding fixture according to the invention.

The composition according to the invention consists of a solid film and a movable jaw 2 which are made of a thermally conductive material, for example a medium. In the fixed jaw 1, a stud bolt 3 is screwed, which passes through an opening formed in the movable jaw 2 and at the end of the stud 3, a nut 4 is clamped between the fixed jaw 1 and the movable jaw 2. A cylindrical recess 6 is provided in the dividing plane of the rigid jaw 1 and the movable jaw 2, in which a welded pin 7 with a rod <8, which abuts the horizontal upper surface of the rigid and is supported. Cooling openings 9 are provided in the fixed and movable jaws 1 and 2 for supply and removal of the cooling medium.

With the nut 4 released, the movable jaw 2 is pulled away from the rigid jaw 1 by the compression spring 5. In this state, the welded pin 7 is inserted into the cylindrical hollow 6 so that the rod 8 abuts the horizontal surface of the two jaws 1 and 2. Then the control nut is retracted 4, whereby the movable jaw is brought closer to the fixed jaw 1 by means of the cylindrical heater 6, the clamping pin 7 is clamped tightly. heat. In the cooling openings 9 formed in the upper part of the jaws 1 and 2, the supply of cooling medium is transferred and in the cooling openings 9 formed in the lower part of the jaws 1 and 2 the cooling medium is transferred. Thus, a pin 7 is provided with a rod 8 for forming the weld 10.

Claims (1)

PREDMET Prípravok pre zváranie čapu s tiahlom, ktorý ije chemicko-tepelne alebo tepelne spracovaný na vysokú tvrdost pozostávajúci z jednej pevnej a z jednej pohyblivej čelusti ovládanej přítlačným mechanizmom, vyznačujúci sa tým, že v delíacej rovině pevnej YNÁLEZU čeluste (1) a pohyblivej čeluste (2) je vytvořené válcové zahlbenie (6) pre zváraný čap (7) a dalej sú v nich vytvořené chladiace otvory (9) pre přívod a odvod chladiaceho média. 1 list výkresov 239394ARTICLE A device for welding a pin with a rod which is chemically-thermally or thermally treated to a high hardness consisting of one fixed and one movable jaw controlled by a thrust mechanism, characterized in that the jaws (1) and the movable jaws (2 ) a cylindrical recess (6) is formed for the welded pin (7) and furthermore there are formed cooling holes (9) for supplying and discharging the cooling medium. 1 sheet of drawings 239394
CS844157A 1984-06-04 1984-06-04 Pull rod welding tool CS239394B1 (en)