CN2738075Y - 耐磨损喷煤金属软管 - Google Patents
耐磨损喷煤金属软管 Download PDFInfo
- Publication number
- CN2738075Y CN2738075Y CN 200420029875 CN200420029875U CN2738075Y CN 2738075 Y CN2738075 Y CN 2738075Y CN 200420029875 CN200420029875 CN 200420029875 CN 200420029875 U CN200420029875 U CN 200420029875U CN 2738075 Y CN2738075 Y CN 2738075Y
- Authority
- CN
- China
- Prior art keywords
- wear
- resisting
- metal
- bellow
- metal hose
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种耐磨损喷煤金属软管,属管件技术领域。用于解决输送煤粉的金属波纹管内壁易磨损的技术问题。它由金属波纹管和置于波纹管外部的金属丝网构成,在软管的端部设有法兰盘,其特别之处是:波纹管内设有防磨内套,防磨内套由数个金属管件组成,两相邻金属管件在端部凹凸嵌套形成活动连接,防磨内套的两端与法兰盘固接。本实用新型针对用于输送煤粉的金属波纹管耐磨性差的问题,在其内壁设置了具有一定自由度的防磨内套,该防磨内套既可以保证金属软管具有一定的自由度,确保计量准确和便于安装,又可以大大提高其耐磨性,有效解决了金属波纹管使用寿命短、生产成本高的问题。本实用新型可提高金属波纹管的使用寿命10~20倍。
Description
技术领域
本实用新型涉及一种金属软管,特别是用于高炉喷煤生产中的金属波纹管,属管件技术领域。
背景技术
煤粉喷吹是采用具有一定压力的空气作为喷吹载体,向加热设备中喷入煤粉帮助燃烧,这项技术在冶金行业中被广泛应用。如高炉冶炼时,为节约能源,减少高价值焦炭用量,多采用煤粉喷吹技术。金属软管是高炉喷煤和喷煤系统中大量使用的耐压管件,它有很好的耐压性和自由弯曲度,可以在喷煤罐与输煤系统之间实现软连接,以确保喷吹计量的准确性。现场使用的金属软管一般是由金属波纹管外包金属丝网构成,它通常工作在十分恶劣的条件下,既要承受一定压力,又要受到高速流动煤粉的强烈摩擦,而金属波纹管的壁厚一般为0.5~0.8毫米,所以普通金属波纹管的使用寿命仅为1~2个月,最短的不足一周。金属波纹管价格较高,大量的消耗增加了企业的生产成本,且由于经常更换波纹管,造成设备的维护工作量加大、维护时间增加,给生产造成一定的不利影响。若在其内壁增设刚性耐磨层,又无法保证金属软管的自由弯曲度从而影响正常使用。有鉴于此,应当研制新的耐磨损喷煤金属软管。
发明内容
本实用新型的目的在于克服现有技术的不足,提供一种使金属软管在具备必要的自由度、便于安装并能确保计量准确的基础上,能够大大延长其使用寿命的耐磨损喷煤金属软管。
本实用新型所称问题是由以下技术方案解决的:
一种耐磨损喷煤金属软管,由金属波纹管和置于波纹管外部的金属丝网构成,在软管的端部设有法兰盘,其特别之处是:所述波纹管1内设有防磨内套3,防磨内套由数个金属管件4组成,两相邻金属管件在端部凹凸嵌套形成活动连接,防磨内套的两端与法兰盘7固接。
上述耐磨损喷煤金属软管,所述金属管件4的外径略小于波纹管内径,两端嵌套部位轴向长度为8-20毫米,两管件嵌套处的径向间隙0.5~2毫米。
上述耐磨损喷煤金属软管,所述金属管件壁厚4~8毫米,长100-400毫米。
本实用新型金属管件的具体参数和个数可根据所采用波纹管的长度、内径及现场的安装条件确定。
本实用新型针对用于输送煤粉的金属波纹管耐磨性差的问题,在其内壁设置了防磨内套,该防磨内套由数个活动连接的金属管件构成,它们既可以保证金属软管具有必要的自由度,能够确保计量准确、便于安装,又可以大大提高其耐磨性,有效解决了金属波纹管使用寿命短、生产成本高的问题。本实用新型可提高金属波纹管的使用寿命10~20倍。此外,本实用新型具有结构简单、造价低廉、易于实现等特点,在冶金行业或其它相关行业中很有推广价值。
附图说明
图1是本实用新型结构示意图;
图2是防磨内套结构示意图;
图3是金属管件结构示意图。
图中标号表示如下:1.波纹管;2.金属丝网;3.防磨内套;4.金属管件;5.凹孔,6.凸台;7.法兰盘。
具体实施方式
参看图1,本实用新型由金属波纹管1和置于波纹管外部的金属丝网2构成,在软管的端部设有法兰盘7,为防止波纹管很快磨损,在波纹管内设置了防磨内套3。为保证波纹管原有的自由度,防磨内套采用由数个金属管件4形成活动连接的结构,防磨内套的长度与波纹管相匹配,其两端可以采用焊接的方式与法兰盘固接。
参看图2,金属管件一端设有凹孔5,另一端设有凸台6,两相邻金属管件在端部由凹孔和凸台形成凹凸嵌套,形成活动连接。为保证防磨内套具有一定的自由度,两金属管件在嵌套处需留有0.5~2毫米的径向间隙。考虑到金属管件嵌套部位不至于因外力作用而滑脱,其端嵌套部位轴向长度14毫米。
金属管件壁厚为5~6毫米,长度为300毫米。视所使用的波纹管长度和现场安装条件,一般以3~5节构成一个防磨内套为宜。金属管件位于防磨内套两端处可不设置凹孔或凸台。
Claims (3)
1.一种耐磨损喷煤金属软管,由金属波纹管和置于波纹管外部的金属丝网构成,在软管的端部设有法兰盘,其特征在于:所述波纹管(1)内设有防磨内套(3),防磨内套由数个金属管件(4)组成,两相邻金属管件在端部凹凸嵌套形成活动连接,防磨内套的两端与法兰盘(7)固接。
2.根据权利要求1所述的耐磨损喷煤金属软管,其特征在于:所述金属管件(4)的外径略小于波纹管内径,两端嵌套部位轴向长度8~20毫米,两管件嵌套处的径向间隙0.5~2毫米。
3.根据权利要求2所述的耐磨损喷煤金属软管,其特征在于:所述金属管件壁厚4~8毫米,长100~400毫米。