CN2731241Y - 环氧、聚乙烯粉末复合涂层防腐管 - Google Patents
环氧、聚乙烯粉末复合涂层防腐管 Download PDFInfo
- Publication number
- CN2731241Y CN2731241Y CN 200420007424 CN200420007424U CN2731241Y CN 2731241 Y CN2731241 Y CN 2731241Y CN 200420007424 CN200420007424 CN 200420007424 CN 200420007424 U CN200420007424 U CN 200420007424U CN 2731241 Y CN2731241 Y CN 2731241Y
- Authority
- CN
- China
- Prior art keywords
- corrosion
- epoxy
- steel pipe
- pipe
- powder coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种环氧、聚乙烯粉末复合涂层防腐管。解决了单层熔结环氧粉末涂层和聚乙烯层防腐管的防腐效果差的问题。其特征在于:钢管(1)外壁依次置有150~250μm的环氧粉末涂料层(2)及450~550μm的聚乙烯粉末涂料层(3)。该防腐管具有防腐效果好的特点,能延长钢管的使用寿命。
Description
技术领域:
本实用新型涉及一种防腐管,属于环氧、聚乙烯粉末复合涂层防腐管。
背景技术:
为了保证钢管在不同环境下的使用效果及延长其使用寿命,经常采用钢管外置有防腐层的方法,目前,单层的熔结环氧粉末和聚乙烯粉末的防腐层在钢管的防腐技术中有比较广泛的应用,但熔结环氧粉末形成的防腐涂层具有渗水性,聚乙烯粉末形成的涂层和钢管的附着力较差;其次,在综合利用熔结环氧粉末和聚乙烯材料时,多使用挤出聚乙烯片材,不能和熔结环氧粉末层很好的结合,致使防腐层的防腐效果差,同时使钢管容易产生腐蚀,而再外加过渡胶层,又会大大增加生产成本。
发明内容:
为了克服现有单层熔结环氧粉末涂层和聚乙烯层防腐管的防腐效果差的不足,本实用新型提供一种环氧、聚乙烯粉末复合涂层防腐管,该防腐管具有防腐效果好的特点,能延长钢管的使用寿命。
本实用新型所采取的技术方案是:该环氧、聚乙烯粉末复合涂层防腐管包括钢管,钢管外壁依次置有150~250μm的环氧粉末涂料层及450~550μm的聚乙烯粉末涂料层。
本实用新型的有益效果是:该钢管是在钢管外壁喷涂环氧粉末涂料层,环氧粉末涂料层与钢管的吸附性能好,对钢管的防腐效果好,在环氧粉末涂料层实现胶化而未完全固化时,把聚乙烯粉末涂料喷吐在胶化的环氧粉末涂料层上,经二次加热后固化为完整的防腐层;这种防腐钢管的防腐性能远远高于单层熔结环氧粉末涂层和聚乙烯层防腐管的防腐效果,延长了钢管的使用寿命。
附图说明:
附图1是本实用新型的结构剖视图。
图1中1-钢管,2-环氧粉末涂料层,3-聚乙烯涂料层。
具体实施方式:
下面结合附图对本实用新型作进一步说明:
在图1中,该环氧、聚乙烯粉末复合涂层防腐管包括钢管1,钢管1经除油、除脂预处理后,采用喷抛射除锈的方式进行表面处理,利用静电喷涂的方式将环氧粉末涂料吸附在钢管1的外壁,形成厚度为150~250μm的环氧粉末涂料层2,环氧粉末涂料层2与钢管1的吸附性能好,对钢管1的防腐效果好;然后采用中频也可以是高频方式把钢管1加热到230~250℃,在粉末涂料实现胶化而未完全固化时,把聚乙烯粉末涂料利用火焰喷吐或静电喷吐的方式涂敷在胶化的粉末涂膜上,形成厚度为450~550μm的聚乙烯粉末涂料层3,经二次中频也可以是高频加热后固化为完整的防腐层,保证两种涂料层(2,3)的良好结合,防腐效果好。
由于使用了该环氧、聚乙烯粉末复合涂层防腐管,具有防腐效果好的特点,其防腐性能远远高于单层熔结环氧粉末涂层和聚乙烯层防腐管的防腐效果,延长了钢管的使用寿命。
Claims (1)
1、一种环氧、聚乙烯粉末复合涂层防腐管,包括钢管(1),其特征在于:钢管(1)外壁依次置有150~250μm的环氧粉末涂料层(2)及450~550μm的聚乙烯粉末涂料层(3)。