CN2517814Y - 实竹饰面高密度强化企口地板 - Google Patents

实竹饰面高密度强化企口地板 Download PDF

Info

Publication number
CN2517814Y
CN2517814Y CN 01277046 CN01277046U CN2517814Y CN 2517814 Y CN2517814 Y CN 2517814Y CN 01277046 CN01277046 CN 01277046 CN 01277046 U CN01277046 U CN 01277046U CN 2517814 Y CN2517814 Y CN 2517814Y
Authority
CN
China
Prior art keywords
bamboo
layer
strengthened
high density
real
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 01277046
Other languages
English (en)
Inventor
庄志宏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
MINGZHI BAMBOO PRODUCTS CO Ltd ANJI
Original Assignee
MINGZHI BAMBOO PRODUCTS CO Ltd ANJI
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by MINGZHI BAMBOO PRODUCTS CO Ltd ANJI filed Critical MINGZHI BAMBOO PRODUCTS CO Ltd ANJI
Priority to CN 01277046 priority Critical patent/CN2517814Y/zh
Application granted granted Critical
Publication of CN2517814Y publication Critical patent/CN2517814Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种竹饰面高密度强化企口地板,它包括高密度纤维芯板,所述的板芯表面依次粘贴浸渍纸层、实竹薄木装饰层和浸渍三氧化二铝耐磨纸,所述芯板的底面粘贴有浸渍平衡层。它的实竹薄木装饰层,是选用山地优质毛竹(楠竹、孟宗竹)为原料制成的,因此,它的成本较低,能就地取材,无污染,大大增加了实竹的有效表观面积,且利用竹子表面特有的自然纹理作为装饰面,视觉观感好,使产品更具亲和力。

Description

实竹饰面高密度强化企口地板
                     技术领域
本实用新型涉及一种强化企口地板,特别是采用高密度纤维板为芯板的强化企口地板。
                     背景技术
已有的高密度强化企口地板,在高密度纤维芯板的表面粘贴有木纹装饰层,在木纹装饰层上面再粘贴三氧化二铝耐磨纸,在芯板的底面粘贴防潮阻燃平衡层,从而形成四层构造的层压板。其装饰层之装饰纸均采用白度很高的净化纤维素制作的木浆纸,需耗用大量的优等原木,而且多数依赖进口,并且价格颇高,因此需要大量的外汇采购。并且,装饰纸的表面木纹是采用油墨印刷,纹路不够自然,同时木纹印刷又要消耗大量的油墨,这又会直接或间接地造成一定程度的环境污染。
                     发明内容
本实用新型要解决的是已有的高密度强化企口地板价格较高、视觉观感效果不理想及油墨印刷产生的环境污染以及实竹企口地板需要消耗大量的优质原生实竹及消耗大量胶粘剂的同时造成使用环境污染等问题,提供一种实用性好、成本低和不需要消耗大量原木、原生实竹、大量的胶粘剂和油墨的高密度强化企口地板。解决上述问题采用的技术方案是:竹饰面高密度强化企口地板,包括高密度纤维芯板,所述的板芯表面依次粘帖浸渍纸层、实竹薄木装饰层和浸渍三氧化二铝耐磨纸,所述芯板的底面粘贴有浸渍平衡层。
本实用新型实竹饰面高密度强化企口地板的实竹薄木装饰层,是选用山地优质毛竹(楠竹、孟宗竹)为原料,制成一定规格的竹片,用高耐水性的胶粘剂,胶合成特定尺寸的集成竹方材,经刨切加工制成一定厚度的实竹薄木,因此,它的成本较低,能就地取材,无污染,大大增加了实竹的有效表观面积,且利用竹子表面特有的自然纹理作为装饰面,视觉观感好,使产品更具亲和力。
本实用新型实竹饰面高密度强化企口地板,其表面纹理根据加工方法的不同,分为弦切面(平压型)与径切面(侧压型),最大限度地保持了原实竹企口地板特式。
本实用新型实竹饰面高密度强化企口地板采用五层结构,它的表层采用浸渍三氧化二铝耐磨层,具有良好的耐磨性和透明度,既能有效地保护第二层的实竹薄木,同时,又使实竹薄木装饰层的纹理能清晰显示。它的第三层采用浸渍纸层,可加强竹薄木和高密度纤维芯板之间的粘合力以及竹薄木的强度。它的底层采用浸渍平衡纸,既可防潮、阻燃,又能使整体保持平整,不易变形,可保证产品质量,延长使用寿命。
                        附图说明
下面结合附图和实施例对本实用新型作进一步说明。
附图是本实用新型的结构示意图。
                      具体实施方式
参照附图,实竹饰面高密度强化企口地板包括高密度纤维板芯板4,所述的芯板4表面依次粘贴树脂浸渍层3、实竹薄木装饰层2和浸渍三氧化二铝耐磨层1,所述板芯4的底面粘贴有浸渍平衡层5。
竹薄木饰面高密度强化企口地板,选用优质山地毛竹(楠竹、孟宗竹),经过以下生产加工步骤制得:1、选材
选择通直新鲜的山地优质毛竹为原料,要求生长期为5~6年,眉围300mm以上,干段通直且新鲜。2、备料
2、1、断料:将所选取之新鲜原竹,按所需长度规格锯截定长,常规尺寸为:2000mm、2600mm两种。
2、2、冲片:将所定长之竹筒段料按不同宽度要求加工成竹片坯料,常规尺寸为:21mm、25mm两种。
2、3、干燥:将坯料放于烘干房内低温干燥至要求的含水率,干燥方法采用蒸汽或热风炉间接加热,要求含水率8~10%。
2、4、精刨:将烘干之初坯料加工成定型规格之竹片尺寸,常规尺寸为:宽度18~21mm;厚度5.2~6.0mm。3、胶合:将经精刨之竹片用特种胶粘剂胶合成特定尺寸的竹方材,根据竹方材宽厚和刨切面方向要求,进行涂胶胶合成集成竹方材。4、刨切:用刨切机将集成竹方材刨切成要求厚度的实竹薄木,常规厚度为:0.2~2.2mm。5、干燥:将裁切齐边好之实竹薄木干燥至要求的含水率,采用气浮或热压板加热干燥,要求含水率:≤12%。6、成型
按顺序将经浸渍处理的耐磨纸、竹薄木、底层纸、密度板和平衡纸加温加压成板
组坯:将经浸渍处理的耐磨纸、竹薄木、底层纸、密度板和平衡纸按顺序组坯;
热压:将组坯的坯板在150℃左右的温度下加压使各层紧密结合成整体的板材。7、分切
将高密度纤维板按特定的规格尺寸裁切成小幅面的板材,分切尺寸:长度1217~1225mm,宽度200~210mm,要求大小规格统一。8、加工
将热压成型之板材加工四周互配企口即得实竹饰面强化企口地板,企口尺寸:榫槽高度3.0mm;榫舌厚度3.0mm;榫槽深度5mm;榫舌宽度4mm。成品尺寸:长度1210~1380mm;宽度195~225mm,企口中心高度4mm。9、检验
将经过上述加工之实竹饰面强化企口地板,按标准全数检验,剔除次废品。10、包装
经检验之实竹薄木饰面强化地板,按标准数装箱包装即可。按标准装箱数,同向叠放装箱,加产品说明,标记日期,检字和等级,加热塑封。采用上述方法生产制作的实竹饰面高密度强化企口地板,既保持了现有强化企口地板的耐磨、耐腐、耐湿、涨缩性小、使用寿命长、安装简单、价廉、易于清洁保养的优点,又最大限度地保持和发挥了竹材良好的耐磨性能,使得实竹饰面高密度强化企口地板更具实际使用效果,使普通消费者花较少的钱即可得到既美观又朴素逼真的实竹饰面强化企口地板。

Claims (1)

1、实竹饰面高密度强化企口地板,包括高密度纤维芯板(4),其特征在于所述的板芯(4)表面依次粘帖浸渍纸层(3)、实竹薄木装饰层(2)和浸渍三氧化二铝耐磨纸(1),所述芯板(4)的底面粘贴有浸渍平衡层(5)。
CN 01277046 2001-12-10 2001-12-10 实竹饰面高密度强化企口地板 Expired - Fee Related CN2517814Y (zh)