CN216614801U - Copper smelting furnace and copper smelting equipment - Google Patents

Copper smelting furnace and copper smelting equipment Download PDF

Info

Publication number
CN216614801U
CN216614801U CN202120695068.1U CN202120695068U CN216614801U CN 216614801 U CN216614801 U CN 216614801U CN 202120695068 U CN202120695068 U CN 202120695068U CN 216614801 U CN216614801 U CN 216614801U
Authority
CN
China
Prior art keywords
furnace
furnace body
copper
smelting
zone
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202120695068.1U
Other languages
Chinese (zh)
Inventor
李东波
孙晓峰
李晓霞
黎敏
刘恺
陆金忠
吴玲
李海春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China ENFI Engineering Corp
Original Assignee
China ENFI Engineering Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China ENFI Engineering Corp filed Critical China ENFI Engineering Corp
Priority to CN202120695068.1U priority Critical patent/CN216614801U/en
Application granted granted Critical
Publication of CN216614801U publication Critical patent/CN216614801U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model discloses a copper smelting furnace and copper smelting equipment. The copper smelting furnace includes: the first furnace body is provided with a first furnace chamber and a furnace bottom, the first furnace chamber comprises a smelting region, a converting region and a first settling region, a first charging opening is arranged on the part of the first furnace body opposite to the smelting region, a copper discharging opening is arranged on the part of the first furnace body opposite to the converting region, a slag discharging opening is arranged on the part of the first furnace body opposite to the first settling region, the furnace bottom comprises a first part opposite to the smelting region, a second part opposite to the converting region and a third part opposite to the first settling region, and the first part is positioned above the second part and below the third part; and the first spray gun is arranged on the part of the first furnace body opposite to the smelting area, and the second spray gun is arranged on the part of the first furnace body opposite to the converting area. The copper smelting furnace has the advantages of low construction cost, small environmental pollution, high metal and sulfur recovery rate and the like.

Description

Copper smelting furnace and copper smelting equipment
Technical Field
The utility model relates to the field of metallurgy, in particular to a copper smelting furnace and copper smelting equipment.
Background
In the related art, copper concentrate pyrometallurgy is performed by separate smelting and converting furnaces. Wherein the smelting furnace smelts the copper concentrate into copper matte, and the converting furnace blows the copper matte into blister copper. Because smelting and converting are completed in different furnaces, the furnaces are connected through a launder or the melt is lifted by a crane, so that the problems of a large amount of materials among the furnaces are solved, and the problems of high investment, long flow and low air pollution are caused.
SUMMERY OF THE UTILITY MODEL
The present invention is directed to solving, at least to some extent, one of the technical problems in the related art. Therefore, the utility model provides a copper smelting furnace and copper smelting equipment.
The copper smelting furnace according to the present invention includes: the furnace comprises a first furnace body, a second furnace body and a furnace bottom, wherein the first furnace body is provided with a first furnace chamber and a furnace bottom, the first furnace chamber comprises a smelting area, a converting area and a first settling area, a first charging opening is arranged on the part of the first furnace body opposite to the smelting area, a copper discharge opening is arranged on the part of the first furnace body opposite to the converting area, a slag discharge opening is arranged on the part of the first furnace body opposite to the first settling area, the furnace bottom comprises a first part opposite to the smelting area, a second part opposite to the converting area and a third part opposite to the first settling area, the first part is positioned above the second part, and the third part is positioned above the first part; the first spray gun is arranged on the part, opposite to the smelting area, of the first furnace body, and the second spray gun is arranged on the part, opposite to the converting area, of the first furnace body, wherein the number of the first spray guns is multiple, and the number of the second spray guns is multiple.
The copper smelting furnace has the advantages of low construction cost, small environmental pollution and high metal recovery rate.
Optionally, the smelting zone is located in the direction of predetermineeing the converting zone with between the first settling zone, first furnace body is in it has relative first end and second end to predetermine the direction, the converting zone is close to the first end, first settling zone is close to the second end, wherein it establishes to arrange the copper mouth first end, arrange the cinder notch and establish the second end, optionally, first charge door is established on the roof of first furnace body, arrange the copper mouth with it establishes to arrange the cinder notch on the lateral wall of first furnace body.
Optionally, the copper smelting furnace further comprises a first electrode provided on a portion of the first furnace body opposite to the first subsidence area, optionally, the first electrode is provided on a top wall of the first furnace body.
Optionally, the copper smelting furnace further includes a first partition wall provided within the first furnace chamber so as to separate the smelting zone and the first settling zone.
Optionally, the furnace bottom further comprises a first inclined surface and a second inclined surface, an upper end of the first inclined surface is connected with the first portion, a lower end of the first inclined surface is connected with the second portion, an upper end of the second inclined surface is connected with the third portion, and a lower end of the second inclined surface is connected with the first portion.
Optionally, the first spray gun is arranged on the side wall of the first furnace body, and the second spray gun is arranged on the top wall of the first furnace body.
The copper smelting equipment according to the utility model comprises: a copper smelting furnace according to the present invention; and a depletion furnace, the depletion furnace comprising: the second furnace body is provided with a second furnace chamber, the second furnace chamber comprises a depletion region and a second settling region, a second charging hole and a copper matte outlet are arranged on the part, opposite to the depletion region, of the second furnace body, the second charging hole is communicated with the slag discharge hole, and a depletion slag outlet is arranged on the part, opposite to the second settling region, of the second furnace body; and a third lance provided on a portion of the second furnace body opposite the depletion zone; optionally, the depletion furnace further comprises a second electrode provided on a portion of the second furnace body opposite to the second settling zone, the second electrode being provided on a top wall of the second furnace body, optionally, the third lance being provided on the top wall of the second furnace body, optionally, the depletion furnace further comprises a second partition wall provided in the second furnace chamber so as to partition the depletion zone and the second settling zone.
Drawings
FIG. 1 is a schematic view of a copper smelting furnace according to an embodiment of the present invention;
FIG. 2 is a schematic structural view of a copper smelting plant according to an embodiment of the present invention.
Detailed Description
Reference will now be made in detail to embodiments of the present invention, examples of which are illustrated in the accompanying drawings. The embodiments described below with reference to the drawings are illustrative and intended to be illustrative of the utility model and are not to be construed as limiting the utility model.
A copper smelting furnace 10 according to an embodiment of the present invention will be described below with reference to the accompanying drawings. As shown in fig. 1 and 2, a copper smelting furnace 10 according to an embodiment of the present invention includes a first furnace body 110, a first lance 121, and a second lance 122.
The first vessel 110 has a first furnace chamber 111 and a furnace bottom 112, the first furnace chamber 111 comprising a smelting zone 1111, a blowing zone 1112 and a first settling zone 1113. A first feeding port 1131 is arranged on the part of the first furnace body 110 opposite to the smelting zone 1111, a copper discharging port 1132 is arranged on the part of the first furnace body 110 opposite to the blowing zone 1112, and a slag discharging port 1133 is arranged on the part of the first furnace body 110 opposite to the first settling zone 1113.
The furnace floor 112 includes a first portion 1121, a second portion 1122, and a third portion 1123, the first portion 1121 being opposite the melting zone 1111, the second portion 1122 being opposite the converting zone 1112, and the third portion 1123 being opposite the first settling zone 1113. The first portion 1121 is located above the second portion 1122, and the third portion 1123 is located above the first portion 1121. The up-down direction is shown by arrow a in fig. 1. The first lance 121 is provided on a portion of the first vessel body 110 opposite the melting zone 1111 and the second lance 122 is provided on a portion of the first vessel body 110 opposite the blowing zone 1112. The number of the first spray guns 121 is plural, and the number of the second spray guns 122 is plural.
A process for smelting a copper-containing material using a copper smelting furnace 10 according to an embodiment of the present invention will be described below with reference to fig. 1 and 2.
Copper-containing material, flux and reductant are fed into the smelting zone 1111 via a first feed inlet 1131, and oxygen-enriched gas is fed into the smelting zone 1111 via a first lance 121 to smelt the copper-containing material to obtain copper matte and slag. Since the third portion 1123 is located above the first portion 1121 and the first portion 1121 is located above the second portion 1122, the copper matte of relatively high density flows to the converting area 1112, the slag of relatively low density flows to the first settling zone 1113, and the slag is separated from the copper slag in the first settling zone 1113. Oxygen-enriched gas is fed to the converting zone 1112 through the second lance 122 to obtain slag and blister copper.
According to the copper smelting furnace 10 provided by the embodiment of the utility model, the copper-containing material is smelted by using the molten pool, so that the copper-containing material can be directly fed into the furnace without drying and finely grinding the copper-containing material. Thus, the material homogenizing warehouse and a separate batching station are not required to be built, and the building cost can be reduced.
The copper smelting furnace 10 according to the embodiment of the present invention can perform the smelting process and the converting process by providing the smelting zone 1111 and the converting zone 1112. It is thus not only unnecessary to construct a converting furnace in order to reduce the construction cost, but also it is possible to avoid the transfer of a large amount of material from a furnace for melting copper-containing material to a furnace for converting copper-containing material, so that metal dust and sulfur diffused into the environment can be greatly reduced to avoid environmental pollution and to improve the recovery rate of metal and sulfur. Wherein the recovery rate of sulfur is more than or equal to 98 percent.
The copper smelting furnace 10 according to the embodiment of the present invention is provided with the first settling zone 1113, so that the slag can be subjected to copper-slag separation in the first settling zone 1113, copper matte carried by the slag is settled down from the slag, and the settled copper matte flows to the converting zone 1112, so that the copper content of the slag is reduced, and the copper recovery rate is improved.
Therefore, the copper smelting furnace 10 according to the embodiment of the present invention has the advantages of low construction cost, less environmental pollution, high recovery rate of metals and sulfur, etc.
As shown in fig. 1 and 2, in some embodiments of the present invention, the copper smelting furnace 10 includes a first furnace body 110, a first lance 121, a second lance 122, a first electrode 130, and a first partition wall 140. The first furnace body 110 has a first furnace chamber 111 and a furnace bottom 112, the first furnace chamber 111 comprising a smelting zone 1111, a blowing zone 1112 and a first settling zone 1113.
Alternatively, as shown in fig. 1, the smelting zone 1111 is located between the blowing zone 1112 and the first settling zone 1113 in the preset orientation. The copper smelting furnace 10 may be a horizontal furnace and the predetermined direction may be a length direction of the copper smelting furnace 10. For example, the predetermined direction may be a left-right direction, the blowing zone 1112 may be located to the left of the smelting zone 1111, and the first settling zone 1113 may be located to the right of the smelting zone 1111. The left-right direction is shown by arrow B in fig. 1.
A first feeding port 1131 is arranged on the part of the first furnace body 110 opposite to the smelting zone 1111, a copper discharging port 1132 is arranged on the part of the first furnace body 110 opposite to the blowing zone 1112, and a slag discharging port 1133 is arranged on the part of the first furnace body 110 opposite to the first settling zone 1113. As shown in fig. 1, the first furnace body 110 has a first end 1141 (e.g., left end) and a second end 1142 (e.g., right end) opposite in the predetermined direction, the converting zone 1112 adjacent to the first end 1141 and the first settling zone 1113 adjacent to the second end 1142. The copper discharge opening 1132 is disposed at the first end portion 1141, and the slag discharge opening 1133 is disposed at the second end portion 1142.
As shown in FIG. 1, optionally, a first charging port 1131 is provided on a top wall 1151 of the first furnace body 110, and a copper exhaust port 1132 and a slag exhaust port 1133 are provided on a side wall 1152 of the first furnace body 110.
The furnace floor 112 includes a first portion 1121, a second portion 1122, and a third portion 1123, the first portion 1121 being opposite (in an up-down direction) the melting zone 1111, the second portion 1122 being opposite (in an up-down direction) the converting zone 1112, and the third portion 1123 being opposite (in an up-down direction) the first settling zone 1113. The first portion 1121 is located above the second portion 1122, and the third portion 1123 is located above the first portion 1121. In other words, the height of the third portion 1123 is greater than the height of the first portion 1121, and the height of the first portion 1121 is greater than the height of the second portion 1122.
As shown in fig. 1, the furnace bottom 112 further includes a first inclined surface 1124 and a second inclined surface 1125, an upper end of the first inclined surface 1124 is connected to the first portion 1121, a lower end of the first inclined surface 1124 is connected to the second portion 1122, an upper end of the second inclined surface 1125 is connected to the third portion 1123, and a lower end of the second inclined surface 1125 is connected to the first portion 1121.
Alternatively, an upper end of the first inclined surface 1124 is connected to a left end of the first portion 1121, a lower end of the first inclined surface 1124 is connected to a right end of the second portion 1122, an upper end of the second inclined surface 1125 is connected to a left end of the third portion 1123, and a lower end of the second inclined surface 1125 is connected to a right end of the first portion 1121. By providing the first inclined surface 1124 and the second inclined surface 1125, the (copper matte) melt flow can be guided by the first inclined surface 1124 and the second inclined surface 1125. Wherein the relatively denser matte and blister copper flow along the furnace floor 112 to the converting area 1112 and the slag flows in the opposite direction.
As shown in FIG. 1, a first lance 121 is provided on a portion of the first vessel body 110 opposite the melting zone 1111, and a second lance 122 is provided on a portion of the first vessel body 110 opposite the blowing zone 1112. Alternatively, the first lance 121 is provided on a side wall 1152 of the first furnace body 110, and the second lance 122 is provided on a top wall 1151 of the first furnace body 110. That is, the first lance 121 is a side-blowing lance, and the second lance 122 is a top-blowing lance. The number of the first spray guns 121 is plural, and the number of the second spray guns 122 is plural.
The first electrode 130 is provided on a portion of the first furnace body 110 opposite to the first settling zone 1113. Optionally, the first electrode 130 is disposed on the top wall 1151 of the first furnace body 110. A first partition wall 140 is provided within the first furnace chamber 111 so as to separate the smelting zone 1111 and the first settling zone 1113.
Copper-bearing material (e.g. copper concentrate), flux and reductant are dosed prior to being fed into the smelting zone 1111 via a first feed inlet 1131. Oxygen-enriched gas is introduced into the smelting zone 1111 via the first lance 121 to smelt the copper-bearing material (e.g. side blown smelting). By smelting the copper-containing material, copper matte and slag can be obtained. Alternatively, first lance 121 may be a submerged lance, and first lance 121 injects oxygen-enriched gas into the slag layer of smelting zone 1111.
The smelting can be carried out at 1100-1500 ℃, that is, the operation temperature of the smelting zone 1111 is 1100-1500 ℃. Alternatively, the melting may be performed at 1150-1350 degrees celsius.
The oxygen concentration of the oxygen-enriched gas may be 60% to 85%. The oxygen concentration of the oxygen-enriched gas refers to the percentage of the volume of oxygen in the oxygen-enriched gas to the volume of the oxygen-enriched gas, i.e. the oxygen concentration of the oxygen-enriched gas is equal to the volume of oxygen in the oxygen-enriched gas/the volume of the oxygen-enriched gas.
The copper matte of the smelting zone 1111 flows from the smelting zone 1111 to the blowing zone 1112 and the slag of the smelting zone 1111 flows from the smelting zone 1111 to the first settling zone 1113. Oxygen-enriched gas is introduced into the converting zone 1112 through the second lance 122 in order to convert the matte that is convected to the converting zone 1112 (e.g. for top blowing). The second lance 122 may blow oxygen-rich gas into the surface of the slag layer in the converting area 1112, and the oxygen-rich gas can increase the oxygen potential of the melt in the converting area 1112, thereby realizing further desulfurization and impurity removal of the high-grade copper matte. By converting the copper matte, blister copper (with a copper content of 98.0 wt% to 99 wt%) and slag can be obtained. Alternatively, the oxygen concentration of the oxygen-enriched gas provided by second lance 122 may be 25% to 65%.
The slag flowing from the converting zone 1112 and the smelting zone 1111 to the first settling zone 1113 is subjected to copper slag separation in the first settling zone 1113 so that the copper matte melt carried in the slag settles down from the slag and the settled copper matte melt flows to the converting zone 1112. The first partition wall 140 can reduce agitation of the melt within the first settling zone 1113. The first electrode 130 facilitates maintaining the temperature of the slag within the first settling zone 1113, thereby facilitating the settling separation of the matte and the slag.
A slag layer and a copper matte layer exist in the smelting zone 1111, a slag layer and a copper matte layer exist in the first settling zone 1113, and a slag layer, a copper matte layer and a rough copper layer exist in the converting zone 1112. The slag form of the furnace slag is Fe-SiO2CaO slag type, Fe, SiO in slag2And CaO in a mass ratio of 1: (0.5-0.8): (0.3-0.6). Optionally, the thickness of the slag layer is 300 mm to 800 mm. Optionally, the slag has a copper content of 3 wt% to 10 wt%. Optionally, the temperature of the slag is 1250-1350 ℃, and optionally, the mass ratio of the copper-containing material to the flux and the reducing agent is 100: (6-10): (1-5).
As shown in fig. 2, the blister copper melt discharged from the copper discharge opening 1132 may enter the finer 30, and compressed air and a reducing agent may be injected into the finer 30 to perform oxidation-reduction of the blister copper and generate anode copper and anode slag. The pressure of the compressed air is 0.4MPa-0.6MPa, and the flow rate of the compressed air is 1000Nm3/h-3000Nm3H is used as the reference value. The reducing agent can be natural gas, liquefied petroleum gas or carbon-based reducing agent and the like. The pressure of the natural gas is 0.4MPa-0.6MPa, and the flow rate of the natural gas is 800Nm3/h-1000Nm3/h。
After the refining is finished, the anode copper can enter a casting machine 40 for casting so as to obtain an anode plate, and the anode plate contains 99-99 wt-99.5 wt% of Cu and 0.005 wt% of sulfur.
As shown in fig. 2, slag discharged from the slag discharge port 1133 may enter the lean furnace 20. For example, the slag is flowed from the sidewall slag notch into the lean zone 2111. The impoverishment furnace 20 includes a second furnace body 210 and a third lance (not shown in the drawings). The second furnace body 210 has a second furnace chamber 211, the second furnace chamber 211 comprising a depletion zone 2111 and a second settling zone 2112.
The part of the second furnace body 210 opposite to the depletion area 2111 is provided with a second charging opening and a copper matte outlet, and the second charging opening is communicated with a slag discharge opening 1133. A slag depletion outlet is arranged on the part of the second furnace body 210 opposite to the second sedimentation zone 2112. A third lance is provided on the portion of the second furnace body 210 opposite the depletion zone 2111. Optionally, a third lance is provided on the top wall 1151 of the second furnace body 210.
When the slag is depleted by the depletion furnace 20, the reducing agent and the vulcanizing agent are added into the depletion area 2111 through the second charging port, the oxygen-enriched gas and the fuel are added into the depletion area 2111 through the third spray gun to preserve the temperature of the furnace body, and the molten body in the furnace is stirred so as to carry out depletion on the slag and obtain copper matte and depleted slag, namely, the slag is reduced. Wherein the depleted slag flows to the second settling zone 2112, and the depleted slag is subjected to copper slag separation in the second settling zone 2112, so that copper matte melt carried in the depleted slag is settled down.
The settled matte is mixed with matte produced in the dilution zone 2111 and discharged from the matte outlet. The depleted slag is discharged from the depleted slag outlet. Valuable metals (including lead, zinc, antimony and the like) enter the smoke dust and can be collected and recovered by a dust collector.
When the slag is depleted in the depletion furnace 20, the copper content of the depleted slag can be further reduced, and the copper recovery rate can be further improved.
The enleaning is performed at a temperature of 1200 degrees celsius to 1400 degrees celsius, and optionally, enleaning is performed at a temperature of 1250 degrees celsius to 1300 degrees celsius. Optionally, the mass ratio of the lean slag to the vulcanizing agent and the reducing agent is 100: (1-5): (1-10). Optionally, the fuel is natural gas, the natural gas having a flow rate of 200Nm3/h-500Nm3/h。
The depletion furnace 20 may further include a second electrode and a second partition wall 220. The second electrode is provided on a portion of the second furnace body 210 opposite to the second subsidence area 2112, and the second electrode is provided on the top wall 1151 of the second furnace body 210. A second partition 220 is disposed within second furnace chamber 211 to separate depletion zone 2111 and second settling zone 2112.
Example 1
The flux is quartz stone and limestone, and the mass ratio of the flux to Fe in the copper concentrate is Fe: SiO 22: CaO ═ 1: 0.8: 0.5, the mass ratio of the reducing agent to the copper concentrate is 0.025: 1. the smelting of the copper concentrate is carried out at 1300-1350 ℃, and the thickness of the slag layer is 300-500 mm. The first lance 121 injects into the copper smelting furnace 10 an oxygen-enriched gas having an oxygen concentration of 70%, which is added in an amount of 300 Nm/ton of copper concentrate3
The smelting zone 1111 reacts to produce copper matte containing Cu68 wt-72 wt%, the copper matte flows to the converting zone 1112, and oxygen-enriched gas with oxygen concentration of 40% is blown into the copper smelting furnace 10 through the second spray gun 122, and the adding amount of the oxygen-enriched gas is 250 Nm/ton of copper concentrate3. The blister copper produced in converting zone 1112 contained 98.1 wt% Cu, 0.4 wt% S, and 0.05 wt% oxygen.
The slag flows to the first settling zone 1113 and undergoes a preliminary copper slag separation in the first settling zone 1113. The produced slag contains 3-10 wt% of Cu, and the temperature of the slag is 1300 ℃. The temperature of the smelting flue gas is 1350 ℃, and the smelting flue gas is sent to a flue gas treatment system for treatment.
Adding the blister copper into the refining furnace 30 through a launder, and injecting compressed air with the pressure of 0.4MPa into the blister copper melt in the refining furnace 30 through a spray gun, wherein the flow rate of the compressed air is 2000Nm3And h, further removing impurities such as S, Pb, Zn and the like in the crude copper melt. When the oxygen content in the crude copper melt is more than 0.5 wt%, rotating the furnace body and stopping spraying compressed air into the refining furnace 30; then, a natural gas reducing agent with the pressure of 0.4MPa is sprayed into the furnace, and the flow rate is 800Nm3/h-1000Nm3H is used as the reference value. When the oxygen content in the melt is less than 0.15%, rotating the furnace body and stopping spraying the reducing agent into the furnace; and then rotating the furnace body to start casting anode copper to obtain an anode plate product.
The slag flows into the dilution furnace 20 through the launder, and is reduced and fuming firstly and then settled, with the reaction temperature of 1200 ℃. The reducing agent is lump coal, and the quality of the reducing agent and the slagThe ratio is 0.08: 1. the vulcanizing agent is pyrite, and the mass ratio of the vulcanizing agent to the slag is 0.05: 1. blowing 200m into the dilution furnace 20 through a third spray gun3H of natural gas and 500m3The oxygen of the/h provides combustion-supporting heat compensation, and the obtained copper matte is clarified and separated in the second settling zone 2112 to obtain copper matte and slag. The copper matte is returned to the copper smelting furnace 10, and the barred slag after barred is subjected to water crushing to generate water granulated slag.
And (3) processing results: the obtained anode copper contained 99.1 wt% of Cu and 0.005 wt% of S; the resulting water granulated slag contained 0.35 wt% Cu.
Example 2
The flux is quartz stone and limestone, and the mass ratio of the flux to Fe in the copper concentrate is Fe: SiO 22: CaO 1: 0.6: 0.6, the mass ratio of the reducing agent to the copper concentrate is 0.02: 1. the smelting of the copper concentrate is carried out at 1300-1350 ℃, and the thickness of the slag layer is 500-800 mm. The first lance 121 injects into the copper smelting furnace 10 an oxygen-enriched gas with an oxygen concentration of 75%, which is added in an amount of 280 Nm/ton of copper concentrate3
The smelting zone 1111 reacts to generate copper matte containing Cu72 wt-75 wt%, the copper matte flows to the converting zone 1112, and oxygen-enriched gas with oxygen concentration of 50% is blown into the copper smelting furnace 10 through a second spray gun 122, and the addition amount of the oxygen-enriched gas is 250 Nm/ton of copper concentrate3. The blister copper produced in converting zone 1112 contained 98.5 wt% Cu, 0.05 wt% S, and 0.15 wt% oxygen.
The slag flows to the first settling zone 1113 and undergoes a preliminary copper slag separation in the first settling zone 1113. The produced slag contains 5-12 wt% of Cu, and the temperature of the slag is 1350 ℃. The temperature of the smelting flue gas is 1380 ℃, and the smelting flue gas is sent to a flue gas treatment system for treatment.
Adding the blister copper into the refining furnace 30 through a launder, and injecting compressed air with the pressure of 0.4MPa into the blister copper melt in the refining furnace 30 through a spray gun, wherein the flow rate of the compressed air is 2000Nm3And h, further removing impurities such as S, Pb, Zn and the like in the crude copper melt. When the oxygen content in the crude copper melt is more than 0.5 wt%, rotating the furnace body and stopping spraying compressed air into the refining furnace 30; then, a natural gas reducing agent with the pressure of 0.4MPa is sprayed into the furnace to flowIn an amount of 800Nm3/h-1000Nm3H is used as the reference value. When the oxygen content in the melt is less than 0.15%, rotating the furnace body and stopping spraying the reducing agent into the furnace; and then rotating the furnace body to start casting anode copper to obtain an anode plate product.
The slag flows into the dilution furnace 20 through the launder, is reduced and fuming firstly, and then is settled, and the reaction temperature is 1250 ℃. The reducing agent is lump coal, and the mass ratio of the reducing agent to the slag is 0.1: 1. the vulcanizing agent is pyrite, and the mass ratio of the vulcanizing agent to the slag is 0.07: 1. blowing 150m into the dilution furnace 20 through a third spray gun3H natural gas and 400m3The oxygen of the/h provides combustion-supporting heat supplement, and the obtained copper matte is clarified and separated in the second settling area 2112 to obtain copper matte and slag. The copper matte is returned to the copper smelting furnace 10, and the barred slag after barred is subjected to water crushing to generate water granulated slag.
And (3) processing results: the obtained anode copper contained 99.3 wt% of Cu and 0.005 wt% of S; the resulting water granulated slag contained 0.35 wt% Cu.
Example 3
The flux is quartz stone and limestone, and the mass ratio of the flux to Fe in the copper concentrate is Fe: SiO 22: CaO 1: 0.5: 0.3, the mass ratio of the reducing agent to the copper concentrate is 0.02: 1. the smelting of the copper concentrate is carried out at 1150-1200 ℃, and the thickness of the slag layer is 500-800 mm. The first lance 121 injects oxygen-enriched gas with oxygen concentration of 85% into the copper smelting furnace 10, and the addition amount of the oxygen-enriched gas is 260 Nm/ton of copper concentrate3
The smelting zone 1111 reacts to generate copper matte containing 75 wt-78 wt% of Cu, the copper matte flows to the converting zone 1112, and oxygen-enriched gas with oxygen concentration of 60% is blown into the copper smelting furnace 10 through a second spray gun 122, and the addition amount of the oxygen-enriched gas is 250 Nm/ton of copper concentrate3. The blister copper produced in converting zone 1112 contains 99.3 wt.% Cu, 0.003 wt.% S, and 0.6 wt.% oxygen.
The slag flows to the first settling zone 1113 and undergoes a preliminary copper slag separation in the first settling zone 1113. The produced slag contains 6-10 wt% of Cu and the temperature of the slag is 1350 ℃. The temperature of the smelting flue gas is 1380 ℃, and the smelting flue gas is sent to a flue gas treatment system for treatment.
Adding the crude copper into the refining furnace 30 through a launder, and injecting a natural gas reducing agent with the pressure of 0.4MPa into the refining furnace 30 through a spray gun, wherein the flow rate is 800Nm3/h-1000Nm3H is used as the reference value. When the oxygen content in the melt is less than 0.15%, rotating the furnace body and stopping spraying the reducing agent into the furnace; and then rotating the furnace body to start casting anode copper to obtain an anode plate product.
The slag flows into the depletion furnace 20 through the launder, and is reduced and fuming firstly and then settled, with the reaction temperature of 1300 ℃. The reducing agent is lump coal, and the mass ratio of the reducing agent to the slag is 0.1: 1. the vulcanizing agent is pyrite, and the mass ratio of the vulcanizing agent to the slag is 0.08: 1. blowing 150m into the dilution furnace 20 through a third spray gun3H natural gas and 400m3The oxygen of the/h provides combustion-supporting heat supplement, and the obtained copper matte is clarified and separated in the second settling area 2112 to obtain copper matte and slag. The copper matte is returned to the copper smelting furnace 10, and the barred slag after barred is subjected to water crushing to generate water granulated slag.
And (3) processing results: the obtained anode copper contained 99.3 wt% of Cu and 0.003 wt% of S; the resulting water granulated slag contained 0.36 wt% Cu.
In the description of the present invention, it is to be understood that the terms "central," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," "circumferential," and the like are used in the orientations and positional relationships indicated in the drawings for convenience in describing the utility model and to simplify the description, and are not intended to indicate or imply that the referenced devices or elements must have a particular orientation, be constructed and operated in a particular orientation, and are therefore not to be considered limiting of the utility model.
Furthermore, the terms "first", "second" and "first" are used for descriptive purposes only and are not to be construed as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of the feature. In the description of the present invention, "a plurality" means at least two, e.g., two, three, etc., unless specifically limited otherwise.
In the present invention, unless otherwise expressly stated or limited, the terms "mounted," "connected," "secured," and the like are to be construed broadly and can, for example, be fixedly connected, detachably connected, or integrally formed; may be mechanically coupled, may be electrically coupled or may be in communication with each other; they may be directly connected or indirectly connected through intervening media, or they may be connected internally or in any other suitable relationship, unless expressly stated otherwise. The specific meanings of the above terms in the present invention can be understood by those skilled in the art according to specific situations.
In the present invention, unless otherwise expressly stated or limited, the first feature "on" or "under" the second feature may be directly contacting the first and second features or indirectly contacting the first and second features through an intermediate. Also, a first feature "on," "over," and "above" a second feature may be directly or diagonally above the second feature, or may simply indicate that the first feature is at a higher level than the second feature. A first feature being "under," "below," and "beneath" a second feature may be directly under or obliquely under the first feature, or may simply mean that the first feature is at a lesser elevation than the second feature.
In the present disclosure, the terms "one embodiment," "some embodiments," "an example," "a specific example," or "some examples" and the like mean that a specific feature, structure, material, or characteristic described in connection with the embodiment or example is included in at least one embodiment or example of the present disclosure. In this specification, the schematic representations of the terms used above are not necessarily intended to refer to the same embodiment or example. Furthermore, the particular features, structures, materials, or characteristics described may be combined in any suitable manner in any one or more embodiments or examples. Furthermore, various embodiments or examples and features of different embodiments or examples described in this specification can be combined and combined by one skilled in the art without contradiction.
Although embodiments of the present invention have been shown and described above, it is understood that the above embodiments are exemplary and should not be construed as limiting the present invention, and that variations, modifications, substitutions and alterations can be made to the above embodiments by those of ordinary skill in the art within the scope of the present invention.

Claims (10)

1. A copper smelting furnace, characterized by comprising:
the furnace comprises a first furnace body, a second furnace body and a furnace bottom, wherein the first furnace body is provided with a first furnace chamber and the furnace bottom, the first furnace chamber comprises a smelting area, a converting area and a first settling area, a first charging hole is formed in the part of the first furnace body opposite to the smelting area, a copper discharge hole is formed in the part of the first furnace body opposite to the converting area, a slag discharge hole is formed in the part of the first furnace body opposite to the first settling area, the furnace bottom comprises a first part opposite to the smelting area, a second part opposite to the converting area and a third part opposite to the first settling area, the first part is positioned above the second part, and the third part is positioned above the first part; and
the smelting furnace comprises a first furnace body, a smelting zone and a second furnace body, wherein the smelting zone is arranged in the first furnace body, the first furnace body is arranged in the smelting zone, the second furnace body is arranged in the second furnace body, the first furnace body is arranged in the second furnace body, the second furnace body is arranged in the second furnace body, and the second furnace body is arranged in the second furnace body.
2. The copper smelting furnace of claim 1, characterized in that, the smelting zone is located in the direction of predetermineeing the converting zone with between the first settling zone, first furnace body is in it has relative first end and second end to predetermine the direction, the converting zone is close to the first end, first settling zone is close to the second end, wherein it establishes to arrange the copper mouth first end, arrange the cinder notch and establish the second end, first charge door is established on the roof of first furnace body, arrange the copper mouth with it establishes to arrange the cinder notch on the lateral wall of first furnace body.
3. The copper smelting furnace according to claim 1, further comprising a first electrode provided on a portion of the first furnace body opposite the first settler zone, the first electrode being provided on a top wall of the first furnace body.
4. The copper smelting furnace according to claim 1, further including a first partition wall provided within the first furnace chamber to separate the smelting zone and the first settling zone.
5. The copper smelting furnace according to claim 1, wherein the hearth further includes a first inclined surface and a second inclined surface, an upper end portion of the first inclined surface being connected to the first portion, a lower end portion of the first inclined surface being connected to the second portion, an upper end portion of the second inclined surface being connected to the third portion, a lower end portion of the second inclined surface being connected to the first portion.
6. The copper smelting furnace according to claim 1, wherein the first lance is provided on a side wall of the first furnace body, and the second lance is provided on a top wall of the first furnace body.
7. A copper smelting apparatus, comprising:
a copper smelting furnace according to any one of claims 1 to 6; and
a depleting furnace, said depleting furnace comprising:
the second furnace body is provided with a second furnace chamber, the second furnace chamber comprises a depletion area and a second sedimentation area, a second charging hole and a copper matte outlet are arranged on the part, opposite to the depletion area, of the second furnace body, the second charging hole is communicated with the slag discharge hole, and a depletion slag outlet is arranged on the part, opposite to the second sedimentation area, of the second furnace body; and
a third lance disposed on a portion of the second furnace body opposite the depletion zone.
8. The copper smelting plant according to claim 7, wherein the depleting furnace further includes a second electrode provided on a portion of the second furnace body opposite the second settling zone, the second electrode being provided on a top wall of the second furnace body.
9. The copper smelting plant according to claim 7, wherein the depletion furnace further includes a second partition wall provided within the second furnace chamber to separate the depletion zone and the second settling zone.
10. The copper smelting plant according to claim 7, wherein the third lance is provided in a top wall of the second furnace body.
CN202120695068.1U 2021-04-06 2021-04-06 Copper smelting furnace and copper smelting equipment Active CN216614801U (en)