CN212239515U - Constant-temperature tin soldering system between metal pieces - Google Patents

Constant-temperature tin soldering system between metal pieces Download PDF

Info

Publication number
CN212239515U
CN212239515U CN202020465826.6U CN202020465826U CN212239515U CN 212239515 U CN212239515 U CN 212239515U CN 202020465826 U CN202020465826 U CN 202020465826U CN 212239515 U CN212239515 U CN 212239515U
Authority
CN
China
Prior art keywords
soldering
welding
constant temperature
workbench
heating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202020465826.6U
Other languages
Chinese (zh)
Inventor
郑振礼
毛文棪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujian Gens Metal Technology Development Co ltd
Original Assignee
Fujian Gens Metal Technology Development Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fujian Gens Metal Technology Development Co ltd filed Critical Fujian Gens Metal Technology Development Co ltd
Priority to CN202020465826.6U priority Critical patent/CN212239515U/en
Application granted granted Critical
Publication of CN212239515U publication Critical patent/CN212239515U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a constant temperature tin soldering system between metal parts, which comprises a workbench and a constant temperature heater, wherein the workbench is used for placing the metal parts, and a welding area, a welding area and a cooling area are sequentially arranged on the workbench; the constant temperature heater is arranged below the welding area and used for heating the welding area; the workbench is also matched with a soldering iron, the soldering iron is connected with a flame spray gun, the flame spray gun is used for heating the soldering iron, and the soldering iron is used for heating tin solder; the constant temperature heater is an electric furnace. The utility model discloses can realize constant temperature soldering, bidirectional heating during the welding has the advantage that is heated evenly, stable in temperature, welding efficiency are high, and the product that the soldering obtained has characteristics such as the welding seam is firm, welding edge levels.

Description

Constant-temperature tin soldering system between metal pieces
[ technical field ] A method for producing a semiconductor device
The utility model relates to a constant temperature soldering system between metalwork.
[ background of the invention ]
Soldering is a welding method in which a low-melting-point metal solder is melted by heating and then penetrates into and fills a gap at a joint of metal parts. The soldering tin wire is generally heated and welded by using a soldering iron, and the main defects are that the temperature is invariable by using the soldering iron, the molten depth of a soldering welding line is not uniform, the operation is slow, the efficiency is low and the like.
[ Utility model ] content
The to-be-solved technical problem of the utility model lies in providing a constant temperature soldering system between metalwork, can realize constant temperature soldering, and bidirectional heating has the advantage that is heated evenly, temperature stability, welding efficiency are high during the welding, and the product that the soldering obtained has characteristics such as the welding seam is firm, welding edge levels.
The utility model discloses a realize like this:
a constant-temperature tin soldering system between metal pieces comprises a workbench and a constant-temperature heater, wherein the workbench is used for placing the metal pieces, and a region to be welded, a welding region and a cooling region are sequentially arranged on the workbench; the constant temperature heater is arranged below the welding area and used for heating the welding area; the workbench is further matched with a soldering iron, the soldering iron is connected with a flame spray gun, the flame spray gun is used for heating the soldering iron, and the soldering iron is used for heating tin solder.
Further, the constant temperature heater is an electric furnace.
The utility model has the advantages that:
the welding area of the workbench of the utility model is provided with the constant temperature heater, the constant temperature heater heats the metal piece to be welded through the welding area, meanwhile, the soldering iron heats the tin soldering bar, the temperature of the welding area and the temperature of the high temperature soldering iron can be adjusted according to different working requirements, the bidirectional heating enables the tin soldering temperature to be more uniform, and the melting of the tin soldering bar is more controllable and stable; therefore, the utility model discloses can realize the constant temperature soldering, bidirectional heating during the welding has the advantage that is heated evenly, stable in temperature, welding efficiency are high, and the product that the soldering obtained has characteristics such as the welding seam is firm, welding edge levels.
[ description of the drawings ]
The invention will be further described with reference to the following examples with reference to the accompanying drawings.
Fig. 1 is a schematic view of a constant temperature soldering system between metal members according to the present invention.
[ detailed description ] embodiments
The embodiment of the utility model provides a through providing a constant temperature soldering system between metalwork, solved among the prior art and used the flatiron to probably meet the temperature invariable, the soldering welding seam depth of fusion differs, the operation is slow, the technical problem of inferior potential such as inefficiency, but realized constant temperature soldering, bidirectional heating during the welding has the advantage of being heated evenly, the temperature is stable, welding efficiency is high, and the product that the soldering obtained has the technical effect of characteristics such as the welding seam is firm, welding edge levels.
Referring to fig. 1, in order to solve the above problems, the embodiment of the present invention provides the following general ideas:
a constant-temperature soldering system between metal pieces comprises a workbench 1 and a constant-temperature heater 2, wherein the workbench 1 is used for placing metal pieces 3, and a region to be welded 11, a welding region 12 and a cooling region 13 are sequentially arranged on the workbench 1; the constant temperature heater 2 is arranged below the welding zone 12 and used for heating the welding zone 12; the workbench 1 is further matched with a soldering iron 4, the soldering iron 4 is connected with a flame spray gun 5, the flame spray gun 5 is used for heating the soldering iron 4, and the soldering iron 4 is used for heating tin soldering bars.
The constant temperature heater 2 is an electric furnace.
For better understanding of the above technical solutions, the following detailed descriptions will be provided in conjunction with the drawings and the detailed description of the embodiments.
Referring to fig. 1, the working process of the present invention is as follows:
placing a metal piece 3 (such as a copper plate) to be soldered in a region 11 to be soldered, opening an electric furnace below a soldering region 12 of a workbench 1 before soldering, and preheating the soldering region 12 to keep the temperature of the soldering region 12 at about 260 ℃; open flame spray gun 5 and preheat flatiron 4, the temperature of flatiron 4 can adjust the temperature as required, and the temperature adjustable range of high temperature flatiron 4 is: 300-500 ℃;
then transferring the two metal pieces 3 to be welded onto the welding area 12 from the area 11 to be welded, coating soldering flux on the welding seam 31 between the metal pieces 3, and heating the soldering tin by using a soldering iron 4 to enable the soldering tin 6 to uniformly fill the welding seam 31;
and finally, transferring the welding finished product of the metal piece 4 from the welding area 12 to the cooling area 13 for natural cooling.
The utility model discloses a workstation 1 welded area 12 is provided with constant temperature heater 22, and constant temperature heater heats the metalwork 3 that treats the welding through welded area 12, and flatiron 4 heats the soldering tin strip simultaneously, and can adjust the temperature of welded area 12 and the temperature of high temperature flatiron 4 according to different work demands, and bidirectional heating makes the soldering tin temperature more even, and the melting of soldering tin strip is more controllable, stable; therefore, the utility model discloses can realize the constant temperature soldering, bidirectional heating during the welding has the advantage that is heated evenly, stable in temperature, welding efficiency are high, and the product that the soldering obtained has characteristics such as the welding seam is firm, welding edge levels.
Although specific embodiments of the present invention have been described, it will be understood by those skilled in the art that the specific embodiments described are illustrative only and are not limiting upon the scope of the invention, and that equivalent modifications and variations can be made by those skilled in the art without departing from the spirit of the invention, which is to be limited only by the claims appended hereto.

Claims (2)

1. The utility model provides a constant temperature soldering system between metalwork which characterized in that: the welding device comprises a workbench and a constant temperature heater, wherein the workbench is used for placing metal parts, and a region to be welded, a welding region and a cooling region are sequentially arranged on the workbench; the constant temperature heater is arranged below the welding area and used for heating the welding area; the workbench is further matched with a soldering iron, the soldering iron is connected with a flame spray gun, the flame spray gun is used for heating the soldering iron, and the soldering iron is used for heating tin solder.
2. The system of claim 1, wherein: the constant temperature heater is an electric furnace.
CN202020465826.6U 2020-04-02 2020-04-02 Constant-temperature tin soldering system between metal pieces Active CN212239515U (en)