CN210133383U - Melamine ware with bright-dark gradual-layer type metal color effect on outer surface - Google Patents

Melamine ware with bright-dark gradual-layer type metal color effect on outer surface Download PDF

Info

Publication number
CN210133383U
CN210133383U CN201920610231.2U CN201920610231U CN210133383U CN 210133383 U CN210133383 U CN 210133383U CN 201920610231 U CN201920610231 U CN 201920610231U CN 210133383 U CN210133383 U CN 210133383U
Authority
CN
China
Prior art keywords
color
melamine
melamine vessel
rough
dark
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201920610231.2U
Other languages
Chinese (zh)
Inventor
陈国钦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chi Mei Industrial Co Ltd
Original Assignee
Chi Mei Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chi Mei Industrial Co Ltd filed Critical Chi Mei Industrial Co Ltd
Priority to CN201920610231.2U priority Critical patent/CN210133383U/en
Application granted granted Critical
Publication of CN210133383U publication Critical patent/CN210133383U/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model provides a melamine ware with the outer surface showing the bright-dark gradual-layer type metallic color effect, which comprises a melamine ware body and at least one color stained paper; wherein the melamine vessel body is provided with an inner side surface and an outer side surface, wherein the inner side surface and the outer side surface are respectively provided with a certain degree of rough surfaces to form a non-mirror surface state, and the rough surfaces of the inner side surface and the outer side surface are hot-pressed and formed by utilizing the surface rough surfaces preset on the surfaces for forming of the hot-pressing forming die; wherein, each color stained paper is respectively pressed, pasted and combined to be integrated on the rough surface of the inner side surface and the outer side surface of the melamine vessel body, so that the appearance of the melamine vessel can present the bright and dark gradual-layer metallic color effect by means of the non-mirror surface state formed by the rough surface.

Description

Melamine ware with bright-dark gradual-layer type metal color effect on outer surface
Technical Field
The utility model relates to a melamine vessel, in particular to a melamine vessel with the outer surface showing the bright-dark gradual-layer type metal color effect.
Background
The prior melamine vessel can be made into various vessels, is lighter and less prone to breaking when being used compared with porcelain or glass, and is beneficial to the convenience of users when being used. However, the surface of the melamine vessel is bright after the vessel is formed by die casting from a soft blank, which is not suitable for the industry to have a gradual appearance design like a bright-dark gradual metallic color effect.
From the above, a melamine vessel having a metallic luster effect of a light and shade gradient layer on the outer surface is expected by the related industries.
SUMMERY OF THE UTILITY MODEL
The main object of the present invention is to provide a melamine vessel with at least one color pattern paper, which is laminated and adhered to the inner surface and the outer surface of the melamine vessel integrally, so that the appearance of the melamine vessel can be formed with a non-mirror surface by the rough surface of the inner surface and the outer surface to present a light and shade gradient metallic color effect.
In order to achieve the above object, the present invention provides a melamine vessel with a bright-dark gradual-layer metallic color effect on the outer surface, which is characterized in that the melamine vessel comprises:
a melamine vessel body having an inner surface and an outer surface, wherein the inner surface and the outer surface are respectively provided with a certain degree of rough surface to form a non-mirror surface state; and
at least one color stained paper, each color stained paper is printed with a pattern with light and shade gradient metal color, wherein each color stained paper is respectively pressed and pasted and combined into a whole on the rough surfaces of the inner surface and the outer surface of the melamine vessel body, so that the appearance of the melamine vessel can present the light and shade gradient metal color effect by means of the non-mirror surface state formed by the rough surfaces of the inner surface and the outer surface.
In one embodiment of the present invention, the melamine vessel body is formed by hot pressing melamine powder and/or granular raw material by means of a hot press molding process and a hot press molding die; wherein the hot-pressing forming die comprises an upper die and a lower die, and a rough surface is preset on the forming surface of the upper die and the forming surface of the lower die in a comprehensive manner; wherein the rough surfaces of the inner side surface and the outer side surface are formed by hot pressing directly on the inner side surface and the outer side surface simultaneously when the melamine ware body is formed by hot pressing by utilizing the surface rough surfaces preset on the forming surfaces of the hot pressing forming die.
In an embodiment of the present invention, the melamine vessel comprises a bowl, a cup, a plate, a pot, and a cylinder.
In an embodiment of the present invention, the surface for forming of the upper mold and the surface for forming of the lower mold are formed with a predetermined rough surface by at least one processing procedure selected from a washing procedure, a shaving procedure, and a grinding procedure.
In an embodiment of the present invention, the inner surface of the melamine vessel further includes an inner edge surface and an inner bottom surface.
In an embodiment of the present invention, the outer surface of the melamine vessel further includes an outer edge surface and an outer bottom surface.
In an embodiment of the present invention, the light and dark gradient metallic color patterns printed on the color paper are further light and dark gradient metallic color patterns.
In an embodiment of the present invention, the light and shade gradient copper-like pattern further includes at least one dark copper color block with a darker color, at least one bright copper color block with a brighter color, at least one medium brightness copper color block with a color between the dark copper color block and the bright copper color block, or a combination of any two or more of the dark copper color blocks and the bright copper color block.
The utility model discloses a each color of spangle paper 20 is that the pressfitting subsides respectively are pasted and are combined into an organic whole and establish on the rough surface on the inboard surface of a melamine ware body and outside surface for the outward appearance can rely on the non-mirror surface state that the rough surface of this inboard surface and outside surface formed with the melamine ware household utensils that present the light and shade gradual-progress layer type metal is like color and luster effect, solves the problem that current melamine household utensils can present the bright state of mirror surface for the household utensils rear surface from soft idiosome die-casting shaping effectively.
Drawings
Fig. 1 is a schematic perspective view of an embodiment of the present invention.
Fig. 2 is a side plan view of fig. 1.
Fig. 2A is a partially enlarged sectional view of fig. 2.
Fig. 3 is a schematic view of the manufacturing process of the present invention.
Fig. 4 is a schematic side view of the hot press molding die of the present invention.
Fig. 4A is a partially enlarged sectional view of fig. 4.
Fig. 5 is a perspective view of another embodiment of the present invention.
Description of reference numerals: 1 melamine vessel; 10 Melamine body; 11 an inside surface; 111 an inner edge surface; 112 an inner bottom surface; 12 an outer side surface; 121 outer edge surfaces; 122 outer bottom surface; 13 rough surface; 14 rough surface; 20 color stained paper; 21 pattern; 22 blocks; 23, blocks; 24 blocks; 2 hot-press forming die; 2a, mounting a mold; 2b, lower die; 201 a molding surface; 202 a molding surface; 203 rough surface; 204 rough surface; 3, raw materials; 4, a heater; 5 soft embryo body.
Detailed Description
The structure and the technical features of the present invention are described in detail in the following with reference to the drawings, wherein each drawing is only used to illustrate the structure relationship and related functions of the present invention, and therefore the size of each element is not set according to the actual proportion and is not used to limit the present invention.
Referring to fig. 1 to 5, the present invention relates to a melamine vessel 1 with a bright-dark gradient metallic color effect on the outer surface, wherein the melamine vessel 1 comprises a melamine vessel body 10 and at least one color stained paper 20.
The melamine vessel body 10 is formed by utilizing powdery and/or granular raw materials of melamine and hot pressing by a hot pressing forming process and a hot pressing forming die 2, the melamine vessel body 10 is provided with an inner side surface 11 and an outer side surface 12, wherein the inner side surface 11 and the outer side surface 12 are respectively provided with rough surfaces 13 and 14 to a certain degree to form a non-mirror surface state; wherein the hot press forming mold 2 comprises an upper mold 2a and a lower mold 2b, and a rough surface 203, 204 is pre-arranged on the forming surface 201 of the upper mold 2a and the forming surface 202 of the lower mold 2 b; wherein the rough surfaces 13 and 14 of the inner surface 11 and the outer surface 12 are formed by hot pressing directly on the inner surface 11 and the outer surface 12 at the same time when the melamine body 10 is formed by hot pressing by using the surface rough surfaces 203 and 204 preset on the forming surfaces 201 and 202 of the hot press forming mold 2.
The melamine vessel 1 includes, but is not limited to, a bowl (as shown in fig. 5), a cup, a plate (as shown in fig. 1), a pot, and a cartridge.
Each color paper 20 is printed with a bright and dark gradient metallic pattern 21, wherein each color paper 20 is respectively pressed, pasted and combined to be integrally arranged on the rough surfaces 13 and 14 of the inner surface 11 and the outer surface 12 of the melamine vessel body 10, so that the appearance of the melamine vessel 1 can present bright and dark gradient metallic color effect by virtue of the non-mirror surface state formed by the rough surfaces 13 and 14 of the inner surface 11 and the outer surface 12.
The light and dark gradient type metallic pattern 21 printed on each of the glossy paper 20 is further a light and dark gradient type metallic pattern without limitation.
Referring to fig. 3 to 4A, the rough surfaces 203 and 204 provided on the molding surface 201 of the upper mold 2a and the molding surface 202 of the lower mold 2b are formed by at least one process of a chemical washing process, a shaving process, or a grinding wheel polishing process, but are not limited thereto.
Referring to fig. 1 and 5, the inner surface 11 of the melamine vessel body 10 further includes, but is not limited to, an inner edge surface 111 and an inner bottom surface 112.
Referring to fig. 1 and 5, the outer surface 12 of the melamine vessel 10 further includes, but is not limited to, an outer edge surface 121 and an outer bottom surface 122.
Referring to fig. 1 and 5, the light and dark gradient copper-like pattern 21 further includes at least one dark copper color block 22 with a darker color, at least one bright copper color block 23 with a lighter color, at least one medium brightness copper color block 24 with a color between the dark copper color block 22 and the bright copper color block 23, or a combination of any two or more of the copper color blocks 22, 23, 24, but is not limited thereto.
Referring to fig. 3 again, the manufacturing process of the present invention is schematically illustrated but not limited to the present invention, and the manufacturing process of the present invention includes the following steps:
step 1: providing a raw material 3 (melamine in powder and/or granular form);
step 2: placing the raw material 3 into a heater 4 for preheating and heating the raw material into a soft blank 5;
and step 3: placing the soft blank 5 into the hot-press forming die 2 for hot-press forming;
and 4, step 4: obtaining the formed melamine vessel body 10 from the hot-pressing forming mold 2, and laminating the stained paper 20 of each color on the melamine vessel body 10 to complete the melamine vessel 1 with the bright-dark gradual-layer metallic color effect on the outer surface.
Compared with the prior art, the melamine vessel 1 of the utility model has the following advantages:
the utility model discloses a each color of spangle paper 20 is that the pressfitting pastes respectively and covers and combines to establish on the rough surface 13, 14 of the inboard surface 11 of a melamine ware body 10 and outside surface 12 integratively for the outward appearance can rely on the rough surface 13 of this inboard surface 11 and outside surface 12, the non-mirror surface state that 14 formed is with the melamine ware household utensils 1 that presents the light and shade gradual-type metallic color effect, solve current melamine ware household utensils effectively and can present the bright state's of mirror surface problem for the household utensils rear surface can be presented from soft idiosome die-casting shaping.
The foregoing description is intended to be illustrative rather than limiting, and it will be appreciated by those skilled in the art that many modifications, variations or equivalents may be made without departing from the spirit and scope of the invention as defined in the appended claims.

Claims (8)

1. A melamine ware having a metallic color effect with a gradually changing dark and bright outer surface, comprising:
a melamine vessel body having an inner surface and an outer surface, wherein the inner surface and the outer surface are respectively provided with a certain degree of rough surface to form a non-mirror surface state; and
at least one color stained paper, each color stained paper is printed with a pattern with light and shade gradient metal color, wherein each color stained paper is respectively pressed and pasted and combined into a whole on the rough surfaces of the inner surface and the outer surface of the melamine vessel body, so that the appearance of the melamine vessel can present the light and shade gradient metal color effect by means of the non-mirror surface state formed by the rough surfaces of the inner surface and the outer surface.
2. The melamine vessel according to claim 1, wherein: the melamine vessel body is formed by utilizing powdery and/or granular raw materials of melamine and hot pressing by a hot pressing forming process and a hot pressing forming die; wherein the hot-pressing forming die comprises an upper die and a lower die, and a rough surface is preset on the forming surface of the upper die and the forming surface of the lower die in a comprehensive manner; wherein the rough surfaces of the inner side surface and the outer side surface are formed by hot pressing directly on the inner side surface and the outer side surface simultaneously when the melamine ware body is formed by hot pressing by utilizing the surface rough surfaces preset on the forming surfaces of the hot pressing forming die.
3. The melamine vessel according to claim 1, wherein: the melamine vessel is a bowl, cup, plate, pot or cylinder.
4. The melamine vessel according to claim 1, wherein: the surface for molding of the upper mold and the surface for molding of the lower mold are provided with a predetermined rough surface, which is formed by at least one processing procedure selected from a washing procedure, a shaving procedure or a grinding wheel grinding procedure.
5. The melamine vessel according to claim 1, wherein: the inner surface of the melamine vessel body also comprises an inner edge surface and an inner bottom surface.
6. The melamine vessel according to claim 1, wherein: the outer surface of the melamine vessel body also comprises an outer edge surface and an outer bottom surface.
7. The melamine vessel according to claim 1, wherein: the light and dark gradient type metal-like color patterns printed on the color stained paper are light and dark gradient type copper-like color patterns.
8. The melamine vessel according to claim 6, wherein: the light and shade gradient copper-like pattern also comprises at least one dark copper color block with darker color, at least one bright copper color block with brighter color, at least one medium brightness copper color block with color between the dark copper color block and the bright copper color block, or a combination of any two or more copper color blocks.
CN201920610231.2U 2019-04-29 2019-04-29 Melamine ware with bright-dark gradual-layer type metal color effect on outer surface Expired - Fee Related CN210133383U (en)